Isolation and Identification of Fungi Associated with Decay of Quercus mongolica (신갈나무의 부후에 관여하는 곰팡이 분리 및 동정)

  • HAM, Youngseok;AN, Ji-Eun;LEE, Soo Min;CHUNG, Sang-Hoon;KIM, Sun Hee;PARK, Mi-Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.49 no.3
    • /
    • pp.234-253
    • /
    • 2021
  • The Quercus mongolica has a high utilization value in industrial economic sector. The species is distributed throughout Korea, however, the damage caused by deterioration such as discoloration and decay is severe. For this reason, the deterioration of Q. mongolica is an obstacle to its use as wood, but research on deterioration factors is insufficient. In this study, we focused on fungi as a factor influencing the deterioration of Q. mongolica, and isolated and identified the fungi from the deteriorated Q. mongolica. In additions, in order to confirm whether the identified fungi actually affects wood deterioration, enzyme activities of the identified fungi were evaluated and related mass loss of wood treated with the fungi was measured by wood decay test. As a result of sequencing analysis using the ITS region of the genomic DNA of the fungi isolated from Q. mongolica, Mucor circinelloides, Cunninghamella elegans, and Umbelopsis isabellina 3 species belonging to Mucoromycota phylum, and Ophiostoma piceae and Aureobasidium melanogenum 2 species belonging to Ascomycota phylum were identified. These five fungi had enzyme (i.e. cellulase, laccase) activities related to wood decay and reduced the mass of heartwood and sapwood of Q. mongolica in practice. In particular, O. piceae and A. melanogenum, which have both cellulase and laccase activities, showed 6.9% and 1.5% mass loss, respectively. These results indicated that five fungi identified in this study influence the deterioration of Q. mongolica and are wood decaying fungi for Q. mongolica potentially.

Model of Drying Stress Distribution in Disks End-wrapped in Korean Paper and Effects of End-wrappings on Prevention of Drying Defects for Vacuum Drying of Disks (한지(韓紙) 엔드래핑처리 원판(圓板)의 감압건조응력(減壓乾燥應力) 분포모형(分布模型) 및 엔드래핑스의 건조결함(乾燥缺陷) 예방효과(豫防效果))

  • Lee, Nam-Ho;Jung, Hee-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.19 no.1
    • /
    • pp.31-63
    • /
    • 1991
  • It was proved that in conventional kiln drying of disks piling position in the kiln exerted a great influence on drying rates, and the larger the variation of disk diameter, the more undulating drying rates of disks. While in vacuum drying disks there was no influence on drying rates. By the end-wrapping treatments and the radial direction of disks tangential surface stresses in the core of disks were slightly compressive in three species. In control disks the drying stresses distributed into one step-style that compressive stresses in the pith side of 6cm from pith were larger than those in the bark side, while in the disks end-wrapped with Korean paper the drying stresses distributed uniformly, because flow rates of free water in disks had no difference between heart-and sap-wood by obstruction of evaporating water from surface of disks by end-wrapping with Korean paper. And end-wrapping with Korean paper considerably restrained those. Tangential differential shrinkage stresses developed the maximum tensile stress near the bark and with approaching the pith the stresses gradually reduced and changed into compressive stresses in near the pith. At the end of vacuum drying the maximum tangential tensile stresses of disks end-wrapped with Korean paper were smaller than those of control disks, and critical moisture contents causing the V-shaped crack of disks end-wrapped with Korean paper were lower than those of control disks because of the set by obstruction of evaporating water of end-wrapping with Korean paper. In the experiment of vacuum drying stress distribution the disks end-wrapped with Korean paper or aluminum foil in three species were free from V-shaped cracks and control disks were defected very slightly by V-shaped cracks. And also disks end-wrapped with Korean paper were free from heart checks in Alnus japonica and Juglans sinensis, and heart checks were occurred very slightly in others. Especially, not to speak of disks end-wrapped with Korean paper, vacuum drying of disks end-wrapped with aluminum foil prevented effectively drying defects, moreover drying times could be shortened, that is. Ginkgo biloba, Alnus japonica, and Juglans sinensis disks could be dried from green to in-use moisture content in 110 hours, 272 hours, and 407 hours, respectively.

  • PDF

Effect of fire - retardant treatment and redrying on the mechanical properties of radiata pine (내화처리(耐火處理) 및 재건조(再乾操)가 라디에타소나무의 역학적(力學的) 성질(性質)에 미치는 영향(影響))

  • Chung, Doo-Jin;Jo, Jae-Sung;Yun, Ki-Eon;Kim, Jae-Jin;Kim, Gyu-Hyeok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.1
    • /
    • pp.37-49
    • /
    • 1999
  • The effect of fire-retardant treatment and redrying on the mechanical properties of radiata pine sapwood were evaluated. Small, clear specimens were treated with three different fire-retardant(FR) chemicals, borax-boric acid(BRX), minalith(MIN), and pyresote(PYR), with target retentions of 30 and 60kg/$m^3$, and then redried at maximum dry-bulb temperature of $25^{\circ}C$, $60^{\circ}C$, $80^{\circ}C$ or $110^{\circ}C$. Each specimen, including untreated and water-treated controls, was tested in static bending and in compression parallel to grain. The extent of strength reduction was dependent on the type of FR chemicals, retention, and redrying temperature, and a highly significant interaction existed between FR treatment and redrying temperature. Modulus of rupture(MOR) and work to maximum load(WML) were significantly decreased by FR treatment and redrying. None of three FR chemicals adversely affect modulus of elasticity (MOE) and maximum crushing strength(MCS). MOE of BRX treatment and MCS of both BRX and PYR treatment increased significantly compared to untreated controls. No significant differences existed between retention levels except for MOE and MCS of some combinations of FR chemicals and redrying temperatures. Although MOE and MCS was not significantly affected by any of the redrying temperatures, these properties were generally decreased with the increase in redrying temperature. The significant reduction in MOR and WML was observed in BRX treatment when dried at temperatures of $60^{\circ}C$ and above, and in MIN and PYR treatment when dried at temperatures of $80^{\circ}C$ and above. Consequently, BRX-treated radiata pine should not be redried at temperatures >$60^{\circ}C$, and MIN- and PYR-treated radiata pine should not be redried at temperatures > $80^{\circ}C$ where bending strength and energy-related properties are important design considerations.

  • PDF

Effects of Post Individualities on Treatability of Small Diameter Japanese Larch (Larix Leptolepis) with ACQ and CCA (낙엽송 원주상 소경목의 원목성상과 방부 처리성)

  • Kim, Yeong-Suk;Hong, Soon-Il;Yun, Jeong-Hee
    • Journal of the Korean Wood Science and Technology
    • /
    • v.34 no.1
    • /
    • pp.52-60
    • /
    • 2006
  • This study investigated how wood properties (i.e., annual rings, sapwood, heartwood, and cracks) might affect preservative treatment in Japanese larch (Larix leptolepis) round-wood product. We specially focused on small-diameter (~10 cm diameter) wood that is commercially sold in market. Among 100 wood samples, the groups of sample with 13~16, 17~20 annual rings represented 33 and 27 in each frequency, while 2~3 and 4~5 mm annual ring width accounted for 72 and 68 in frequency. More than a half (54%) of wood samples contained a mix of heartwood and sapwood in its surface. The rest (46%) had only heartwood exposed in the wood surface. A wide range of checks were showed in the wood samples, but the highest frequency was observed in samples with 1~6 surface (1~14 mm in size) checks and 1~4 end-grain (8~14 mm in size) checks in each round-wood sample. Pressure treatment resulted in a wide range of penetration of ACQ (Alkaline Copper Quat) into the wood, showing $4.3{\pm}4.19mm$ penetration in the wood samples contained a mix of heartwood and sapwood in its surface. However preservative treatment was much less effective for the heartwood only wood samples, ranging average 1.3 mm with ACQ and 1.1 mm with CCA (Chromated Copper Arsenate). These penetration results shown in heartwood samples did not meet the penetration standard that is required for H3 by the Korean Forest Service in relation to wood preservation treatment. These low penetration results were not significantly improved even if we incised wood samples to improve treatment effect, showing only small increase of 0.7 mm with ACQ and 0.6 mm with CCA. When preservative treatment was tested with heartwood, penetration of preservatives decrease with increase of annual rings per a cross-section area (r=0.5345). We also found that the length and number of check had no effect on preservative treatment, showing r=0.1301 and r=0.1802, respectively.

The Solubilities Variations of Abies koreana Wilson Wood and their Correlations among the Extraction time, Temperature and pH value of the Solubility (구상나무재(材) 추출성분(抽出成分)의 추출시간(抽出時間) 온도(温度) 및 pH변동(變動)과 그 추출성분(抽出成分) 함량(含量)과의 관계(關係))

  • Moon, Chang Kuck
    • Journal of Korean Society of Forest Science
    • /
    • v.43 no.1
    • /
    • pp.35-38
    • /
    • 1979
  • The solubility variations of Abies koreana Wilson wood and their correlations ammong the factors which effect the extraction were investigated. In hot water solubility for 10 hours, extracted contents were 2.33% in heart wood, 12.30% in sapwood. In base solubility (here, used NaOH), the solubility content was 8.23% only for 1 hour. In organo-soluble fractions, there was not any variation between the content 4.00% for 1 hour and 4.44% for 10 hours, about the temperature effect, in the neutral solvent, at temperature $25{\pm}3^{\circ}C$, $50{\pm}3^{\circ}C$ and $97{\pm}3^{\circ}C$ and the solubility contents were 2.73%, 3.29%, 7.32% respectably. In the pH variations, initinal pH of solution, 6.5 became as low 5.4 after 10 hours extraction. Generally, the correlation coefficients between solubility and hour, solubility and temperature, solubilities' pH and hours, solubility and part, were r=0.890, r=0.986, r=-0.955, r=0.840 respectably. It is suggested that the most serious factor of the extraction in this material is the temperature.

  • PDF

Studies on the Hardness of Woods (목재(木材)의 경도(硬度)에 관(關)한 연구(硏究))

  • Hong, Soon-Il;Lee, Won Yong
    • Journal of Forest and Environmental Science
    • /
    • v.8 no.1
    • /
    • pp.21-33
    • /
    • 1992
  • This study was performed to investigate the hardness of wood related to the wood surface, sap and heartwood, early and latewood, specific gravity, annual ring width and moisture content on major Korean tree species such as Pinus koraiensis, Abies holophylla, Larix leptolepis and Quercus valiabilis. The results were summarized as follows: 1. The arithmetic mean values of wood hardness on cross section were respectively $8.0kg/mm^2$ on Quercus valiabilis, $7.4kg/mm^2$ on Larix leptolepis, $5.1kg/mm^2$ on Pinus koraiensis and $4.7kg/mm^2$ on Abies hollophylla. 2. Generally hardness of wood on cross section was greater than the others and the proportion of cross section hardness to radial was respectively 2.8 on Quercus valiabilis, 2.6 on Larix leptolepis, 3.8 on Pinus koraiensis, and 4.1 on Abies holophylla and that proportion was tend to be decrease as specific gravity increased. 3. It was recognized that the hardness of sap and heartwood was different from each of the tree species and generally heartwood hardness was somewhat greater than sapwood. 4. Generally latewood hardness with in a ring was greater than earlywood and the proportion of earlywood hardness to latewood decreased as specific gravity increased. 5. The relations between hardness of wood and specific gravity show a high positive correlation on all sample tree species. 6. The values of hardness decreased with increasing annual ring width. 7. Hardness of wood on Abies holophylla was greatest in oven dried wood and it was decreased as moisture content increased, but not changed with moisture content abve F.S.P.. The proportion of oven dried wood hardness to green are respectively 3.0 on cross, 2.4 on radial and 1.9 on tangential section.

  • PDF

Effects of Boliing, Steaming, and Chemical Treatment on Solid Wood Bending of Quercus acutissima Carr. and Pinus densiflora S. et. Z. (자비(煮沸), 증자(蒸煮) 및 약제처리(藥劑處理)가 상수리나무와 소나무의 휨가공성(加工性)에 미치는 영향(影響))

  • So, Won-Tek
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.1
    • /
    • pp.19-62
    • /
    • 1985
  • This study was performed to investigate: (i) the bending processing properties of silk worm oak (Quercus acutissima Carr.) and Korean red pine (Pinus densiflora S. et Z.) by boiling and steaming treatments; (ii) the effects of interrelated factors - sapwood and heartwood, annual ring placement, softening temperature and time, moisture content. and wood defects on bending processing properties; (iii) the changing rates of bending radii after release from a tension strap, and (iv) the improving methods of bending process by treatment with chemicals. The size of specimens tested was $15{\times}15{\times}350mm$ for boiling and steaming treatments and $5{\times}10{\times}200mm$ for treatments with chemicals. The specimens were green for boiling treatments and dried to 15 percent for steaming treatments. The specimens for treatments with chemicals were soaked in saturated urea solution, 35 percent formaldehyde solution, 25 percent polyethylene glycol -400 solution, and 25 percent ammonium hydroxide solution for 5 days and immediately followed the bending process, respectively. The results obtained were as follows: 1. The internal temperature of silk worm oak and Korean red pine by boiling and steaming time was raised slowly to $30^{\circ}C$ but rapidly from $30^{\circ}C$ to $80-90^{\circ}C$ and then slowly from $80-90^{\circ}C$ to $100^{\circ}C$. 2. The softening time required to the final temperature was directly proportional to the thickness of specimen. The time required from $25^{\circ}C$ to $100^{\circ}C$ for 15mm-squared specimen was 9.6-11.2 minutes in silk worm oak and 7.6-8.1 minutes in Korean red pine. 3. The moisture content (M.C.) of specimen by steaming time was increased rapidly first 4 minutes in the both species, and moderately from 4 to 20 minutes and then slowly and constantly in silk worm oak, and moderately from 4 to 15 minutes and then slowly and constantly in Korean red pine. The M.C. of 15mm-squared specimen in 50 minutes of steaming was increased to 18.0 percent in the oak and 22.4 percent in the pine from the initial conditioned M.C. of 15 percent The rate of moisture adsorption measured was therefore faster in the pine than in the oak. 4. The mechanical properties of the both species were decreased significantly with the increase of boiling rime. The decrement by the boiling treatment for 60 minutes was measured to 36.6-45.0 percent in compressive strength, 12.5-17.5 percent in tensile strength, 31.6-40.9 percent in modulus of rupture, and 23.3-34.6 percent in modulus of elasticity. 5. The minimum bending radius (M.B.R.) of sapwood and heartwood was 60-80 mm and 90 mm in silk worm oak, and 260 - 300 mm and 280 - 300 mm in Korean red pine, respectively. Therefore, the both species showed better bending processing properties in sapwood than in heartwood. 6. The M.B.R. of edge-grained and flat-grained specimen in suk worm oak was 60-80 mm, but the M.B.R. in Korean red pine was 240-280 mm and 260-360 mm, respectively. Comparing the M.B.R. of edge-grained with flat-grained specimen, in the pine the edge-grained showed better bending processing property than the flat-grained. 7. The bending processing properties of the both species were improved by the rising of softening temperature from $40^{\circ}C$ to $100^{\circ}C$. The minimum softening temperature for bending was $90^{\circ}C$ in silk worm oak and $80^{\circ}C$ in Korean red pine, and the dependency of softening temperature for bending was therefore higher in the oak than in the pine. 8. The bending processing properties of the both species were improved by the increase of softening time as well as temperature, but even after the internal temperature of specimen reaching to the final temperature, somewhat prolonged softening was required to obtain the best plastic conditions. The minimum softening time for bending of 15 mm-squared silk worm oak and Korean red pine specimen was 15 and 10 minutes in the boiling treatment, and 30 and 20 minutes in the steaming treatment, respectively. 9. The optimum M.C. for bending of silk worm oak was 20 percent, and the M.C. above fiber saturation point rather degraded the bending processing property, whereas the optimum M.C. of Korean red pine needed to be above 30 percent. 10. The bending works in the optimum conditions obtained as seen in Table 24 showed that the M.B.R. of silk worm oak and Korean red pine was 80 mm and 240 mm in the boiling treatment, and 50 mm and 280 mm in the steaming treatment, respectively. Therefore, the bending processing property of the oak was better in the steaming than in the boiling treatment, but that of the pine better in the boiling than in the steaming treatment. 11. In the bending without a tension strap, the radio r/t of the minimum bending radius t to the thickness t of silk worm oak and Korean red pine specimen amounted to 16.0 and 21.3 in the boiling treatment, and 17.3 and 24.0 in the steaming treatment, respectively. But in the bending with a tension strap, the r/t of the oak and the pine specimen decreased to 5.3 and 16.0 in t he boiling treatment, and 3.3 and 18.7 in the steaming treatment, respectively. Therefore, the bending processing properties of the both species were significantly improved by the strap. 12. The effect of pin knot on the degradation of bending processing property was very severe in silk worm oak by side, e.g. 90 percent of the oak specimens with pin knot on the concave side were ruptured when bent to a 100 mm radius but only 10 percent of the other specimens with pin knot on the convex side were ruptured. 13. The changing rate in the bending radius of specimen bent to a 300 mm radius after 30 days of exposure to room temperature conditions was measured to 4.0-10.3 percent in the boiling treatment and 13,0-15.0 percent in the steaming treatment. Therefore, the degree of spring back after release was higher in the steaming than in the boiling treatment. And the changing rate of moisture-proofing treated specimen by expoxy resin coating was only -1.0.0 percent. 14. Formaldehyde, 35 percent solution, and 25 percent polyethylene glycol-400 solution found no effect on the plasticization of the both species, but saturated urea solution and 25 percent ammonium hydroxide solution found significant effect in comparison to non-treated specimen. But the effect of the treatment with chemicals alone was inferior to that of the steaming treatment, and the steaming treatment after the treatment with chemicals improved 10-24 percent over the bending processing property of steam-bent specimen. 15. Three plasticity coefficients - load-strain coefficient, strain coefficient, and energy coefficient - were evaluated to be appropriate for the index of bending processing property because the coefficients had highly significant correlation with the bending radius. The fitness of the coefficients as the index was good at load-strain coefficient, energy coefficient, and strain coefficient, in order.

  • PDF