• Title/Summary/Keyword: 목질 섬유

Search Result 76, Processing Time 0.022 seconds

Production of Lignocellulytic Enzymes from Spent Mushroom Compost of Pleurotus eryngii (큰느타리버섯 수확 후 배지로부터 리그닌섬유소분해효소 생산)

  • Lim, Sun-Hwa;Kim, Jong-Kun;Lee, Yun-Hae;Kang, Hee-Wan
    • The Korean Journal of Mycology
    • /
    • v.40 no.3
    • /
    • pp.152-158
    • /
    • 2012
  • The lignocellulytic enzymes including a-amylase (EC 3.2.1.1), lignin peroxidase (EC 1.11.1.14), laccase (EC 1.10.3.2), xylanase (EC 3.2.1.8), ${\beta}$-xylosidase (EC 3.2.1.37), ${\beta}$-glucosidase (EC 3.2.1.21) and cellulase (EC 3.2.1.4) were extracted from spent mushroom compost (SMC) of Pleurotus eryngii. Different extraction buffers and conditions were tested for optimal recovery of the enzymes. The optimum extraction was shaking incubation (200 rpm) for 2 h at $4^{\circ}C$. ${\alpha}$-Amylase was extracted with the productivity range from 1.20 to 1.6 Unit/SMC g. Cellulase was recovered with the productivity range from 2.10 to 2.80 U/gf. ${\beta}$-glucosidase and ${\beta}$-xylosidase productivities showed lowest recovery producing 0.1 U/g and 0.02 U/g, respectively. The P. eryngii SMCs collected from three different mushroom farms showed different recovery on laccase and xylanse, cellulase. Furthermore, the water extracted SMC was compared to commercial enzymes for its industrial application in decolorization and cellulase activity.

Bonding Quality of Adhesives Formulated with Okara Hydrolyzates and Phenol-formaldehyde Resins for Bonding Fancy Veneer onto High-density Fiberboard (두부비지 가수분해물과 페놀수지로 조제한 마루판 화장용 접착제의 접착성능)

  • Yang, In;Ahn, Sye-Hee;Choi, In-Gyu;Choi, Won-Sil;Kim, Sam-Sung;Oh, Sei-Chang
    • Journal of the Korean Wood Science and Technology
    • /
    • v.37 no.4
    • /
    • pp.388-396
    • /
    • 2009
  • In our study, the potential of okara as an ingredient of new bio-based adhesives was investigated for the production of fancy-veneered flooring boards. Okara was hydrolyzed by 1% sulfuric acid solution (AC) and 1% sodium hydroxide solution (AK). Phenol formaldehyde (PF) prepolymers were prepared as a cross-linker of okara hydrolyzates. Then, okara-based adhesive resins were formulated with 35% AC, 35% AK and 30% PF prepolymer on solid content basis. The adhesive resins were applied on high-density fiberboards (HDF) with the spread rate of $300g/m^2$. After that, oak fancy veneers are covered on the HDF, and then pressed with the pressure of $7kg/m^2$ at $120^{\circ}C$. The experimental variables were three mole ratios of formaldehyde to phenol (1.8, 2.1, 2.4), three assembly time (0, 10, 20 min), and two press time (90 sec, 120 sec), respectively. The fancy-veneered high-density fiberboards were tested by dry tensile strength, glueline failure by wetting and formaldehyde emission. Tensile strength of the boards exceeded the requirement of KS standard. The formaldehyde emissions were approached at the E0 level specified in KS standard. Based on these results, okara can be used as an ingredient of environmentally friendly adhesive resin systems for the production of flooring boards.

Manufacturing Characteristics of Boards Recycling Waste Wood Particle (폐목재파티클을 이용한 재생보드의 제조특성)

  • Kim, Wae-Jung;Suh, Jin-Suk;Han, Tae-Hyung;Park, Jong-Young
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.2 no.1
    • /
    • pp.120-127
    • /
    • 2006
  • The hammer-milled characteristics of waste wood materials such as lumber, plywood, particleboard(PB), MDF and railroad tic were investigated in this study. The physical and mechanical properties of recycled boards according to types of recycled particle and the mixing ratios were also studied. The hammer-milled, waste wood materials had the dimensional distributions suitable for the core layer panicle. Bending strengths of recycled boards (one layer) were shown in order of plywood, PB(laboratory-fabricated with particles used in the PB factory), lumber, tego film-overlaid plywood, MDF, waste railroad tie, PB(factory-made) and LPL-overlaid PB. Cured resin and creosote containing waste wood contributed to dimensional stability of reconstituted boards. Considering the mixing effects between lumber and plywood with recycled PB particle, lumber particle was contributive to bending strength, MOE and internal bond(IB) strength, whereas plywood particle was contributive to dimensional stability. The bending and IB strength of 3 layer boards composing only recycled waste wood particles in core layer of board were in order of lumber, plywood, PB and MDF. On the other hand, the thickness swelling was in order of PB, lumber, plywood and MDF. Bending strength of the 3 layer boards mixed with recycled PB-particle in the core layer had a decreasing tendency, as the mixing ratios of recycled PB-particles increased. The dimensional stability of 3 layer recycled board was improved as the mixing ratio of recycled PB-particle increased same as in one layer. Formaldehyde emission of boards fabricated with recycled PB-particles in the core layer of the PB was in the range of E2 grade (below 5.0mg/l).

  • PDF

A Study on the Physcial and Mechanical Properties of Hot - Compressed Wood (열압처리(熱壓處理) 목재(木材)의 이학적(理學的) 성질(性質)에 관(關)한 연구(硏究))

  • Park, Young-Kyu;Chung, Dae-Kyo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.15 no.4
    • /
    • pp.45-58
    • /
    • 1987
  • This study was carried out to improve the physical and mechanical properties of Pupulus alba $\times$ glandulosa treated by the heat and compression. The results obtained were as follows. 1. The specific gravity of the wood was conspicuously increased by the lincreasing of pressing level. 2. The shrinkage of the wood was increased. by the increasing of pressing level. The radial shrinkage was 6.41-8.81%, the tangential shrinkage was 8.98-19.81 %, and the longitudinal shrinkage was 1.46-1.91 %. Comparing to the untreated stock, the rate of increase was 48.7-104.4% in radial direction. 1.7-124.4% in tangential direction and 60.4-109.9% in longitudinal direction, respectively. 3. The rate absorption of 30% compressed stock was Similar to that of untreated stock. but the rate of absorption of 40 % or more compressed stock was increased highly. 4. The thickness swelling of the wood was not changed in radial direction at pressing level, but was conspicuously increased in tangential direction under the pressing level of 40% and 50%. 5. The heat and compression treatment affected on the mechanical properties of the wood. The longitudinal compressive strength was increased under the pressing level of up to 40%, but was decreased under the pressing level of 50%. The bending strength was not changed under the compression percentage of up to 30%, but was decreased under the pressing level of 30% or more. And, the absorbed energy in impact bending was increased to 128% under the pressing level of up to 30%, but was decreased under the pressing level of 30% or more. Conclusionly, the mechanical properties of the wood was improved by the heat and compression treatment, but the strength of the wood was decreased under the pressing level of a certain level or more(in this study, pressing level of 30% or more). This was because of the wood deterioration due to the deformation(shrinkage, crack, failure) of wood tissues induced by the heat and compression treatment, the heat analysis of wood components induced by the heating, and the drop of the degree of polymerization.

  • PDF

Enzymatic Hydrolysis of Rice Straw, a Lignocellulosic Biomass, by Extracellular Enzymes from Fomitopsis palustris (Fomitopsis palustris의 균체 외 효소에 의한 볏짚 당화에 관한 연구)

  • Kim, Yoon-Hee;Cho, Moon-Jung;Shin, Keum;Kim, Tae-Jong;Kim, Nam-Hun;Kim, Yeong-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.38 no.3
    • /
    • pp.262-273
    • /
    • 2010
  • In the enzymatic hydrolysis of rice straw and wood meals using extra-cellular enzymes from Fomitopsis palustris, key factors which enhanced the sugar conversion yield were investigated in this work, such as enzyme production and enzyme reaction conditions, surfactant effects, and the surface structure of substrates. F. palustris cultured with softwood mixture produced 12.0 U/$m{\ell}$ for endo-${\beta}$-1,4-gulcanase (EG), 116.68 U/$m{\ell}$ for ${\beta}$-glucosidase (BGL), 18.82 U/$m{\ell}$ for cellobiohydrolase (CBH), and 13.33 U/$m{\ell}$ for ${\beta}$-xylosidase (BXL). These levels of BGL, CBH, and BXL activities were two to four folds more than enzyme activities of F. palustris cultured with rice straw. The optimum reaction conditions of cellulase-RS which produced by F. palustris with rice straw and cellulase-SW which produced by F. palustris with softwood mixture were pH 5.0 at $45^{\circ}C$ and pH 5.0 at $50^{\circ}C$, respectively. The sugar conversion yield of cellulase-SW had the highest value of $40.6{\pm}0.6%$ within 72 h when rice straw was used as substrate. By adding 0.1% Tween 20 (w/w-substrate), the sugar conversion yield of rice straw was increased to 44%, which was about four fifths sugar conversion yield of commercial enzyme, Celluclast 1.5L (Novozyme A/S). A low crystallinity and an intensive fibril surface observed by the scanning electron microscope may explain the high sugar conversion yield of rice straw.

Studies on the Organic Tiers Contained Paddy Soils in Honam Area -I. The Characteristcs and Formation of Organic Tiers Contained Paddy Soils (유기질토시(有機質土尸)을 함유(含有)한 호남지역(湖南地域) 답토양(畓土壤)에 관(關)한 연구(硏究) -I. 유기질토시함유(有機質土尸含有) 답토양(畓土壤)의 특성(特性) 및 생성(生成))

  • Yoo, Chul-Hyun;Kim, Eung-Bog;Cho, Guk-Hyun;Kim, Han-Myoung;Yoo, Sug-Jong;Park, Keon-Ho;Bae, Sung-Ho;Um, Ki-Tae
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.18 no.3
    • /
    • pp.265-275
    • /
    • 1985
  • Present studies were carried out to investigate the distribution and formation of organic tiers contained paddy soils in Honam area characteristics to give basic informations on the effective utilization, management and improvement of the soils. The results obtained were summarized as follows; 1. The extent of organic tiers contained paddy soils in Honam area were 6.538㏊ and the amount of peat deposits were presumed about 2.41 million M/T. 2. Out of the total extent of the organic tiers contained paddy soils, about 97.6% was distributed in Honam plains (water-sheds of Mangyeong-Dongjin river), while about 1.5% in the Naju plains (water-sheds of Yeongsan river), and 0.9% in the Wando and Yeocheon areas. 3. The period of peat formation was presumed to be about the early of Seung Moon period (B.C. 4,250), and the Gongdeog series and the Bongnam series were formed in the bog conditions close to the valley mouth of near rolling and hill with small steram channels, and the Gimje series was formed in the out-skirts plains of the Gongdeog and Bongnam soils. 4. In the casue of peat formation, it was presumed to be the Gimje series that accumulated the fibrous peat out of the autochthonous peat such as reeds and grasses etc, to be the Gongdeog and Bongnam series that accumulated the autochtonous peat and the xylem and fibrous peat out of first allochthonous peat. 5. In the Organic horizons of these soils, the range of muck and peat horizons were in 62-68cm and 68-137cm of soil profile in the Gongdeog series, 52-84cm and 84-113cm in the Bongnam series respectively, one of muck horizon was in 46-71cm in the Gimje series. 6. The marks of soil horizons of the soils were expressed that the lower soils than the horizon of muck and peat were formed Cg, Aag for the muck horizon, 0 for the peat horizon, 0 of peat horizon were distingushed with Oag and Oig according to Organic forms. 7. The depthe occurred the muck and peat horizons were positively correlated with the width of local in the Gongdeog series ($r=0.881^{**}$, $r=0.827^{**}$), but not in the Bongnam series and Gimje series.

  • PDF