• Title/Summary/Keyword: 레일 표면 결함

Search Result 235, Processing Time 0.035 seconds

The Evaluations of Thermal Stability and Stress Crack Resistance of Geomembranes with Surface Defects in the Landfill (폐기물매립지에서 표면결함이 있는 지오멤브레인의 열적 안정성 및 응력균열저항성 평가)

  • 전한용;이광열;이재영
    • Journal of Soil and Groundwater Environment
    • /
    • v.6 no.1
    • /
    • pp.53-62
    • /
    • 2001
  • Effects of surface defect on thermal stability and stress crack resistance of high density polyethylene geomembranes in environmental conditions were examined by comparing the mechanical properties, chemical resistance and failure times of geomembranes between defective cases under different temperatures. Artificial surface defects were added to the surface of geomembranes by scratch apparatus designed specially. The number of surface defects was increased with the smaller size of scratch induced particles, and the more scratch addition numbers at the shear rate of scratch induced mechanism, 100mm/min. The tensile strength were decreased but the tensile strain was increased with the above conditions. In chemical resistance of defective geomembranes, the tensile strength were decreased but the tensile strain was increased with the longer immersion period and the higher temperature under the same scratch induced conditions. Finally, failure times of defective geomembranes by ESCR test were shifted to the shorter time ranges by increasing temperatures.

  • PDF

Reactive Ceramic Membrane Incorporated with Iron Oxide Nanoparticle for Fouling Control (산화철 나노입자 부착 반응성 세라믹 멤브레인의 막 오염 제어)

  • Park, Hosik;Choi, Heechul
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.35 no.2
    • /
    • pp.144-150
    • /
    • 2013
  • Hybrid ceramic membrane (HCM) processes that combined ozonation with a ceramic membrane (CM) or a reactive ceramic membrane (RM), an iron oxide nanoparticles (IONs) incorporated-CM were investigated for membrane fouling control. Alumina disc type microfiltration and ultrafiltration membranes doped with IONs by sintering method were tested under varying mass fraction of IONs. Scanning electron microscope (SEM) images showed that IONs were well-doped on the CM surface and doped IONs were approximately 50 nm in size. Change in the pure water permeability of RM was negligible compared to that of CM. These results indicate that IONs incorporation onto CM had little effect on CM performance in terms of the flux. Natural organic matter (NOM) fouling and fouling recovery patterns during HCM processes confirmed that the RM-ozonation process enhanced the destruction of NOM and reduced the extent of fouling more than the CM-ozonation process by hydroxyl radical formation in the presence of IONs on RM. In addition, analyses of NOM in the feed water and the permeate showed that the efficiency of membrane fouling control results from the NOM degradation during HCM processes; leading to removal and transformation of relatively high contents of aromatic, high molecular weight and hydrophobic NOM fractions.

Determination of Threshold Value for Extracting Shape Information of the Objects (물체의 형상정보추출에 있어서의 임계값의 선정)

  • 조동욱;이성석;김기영
    • The Journal of Korean Institute of Communications and Information Sciences
    • /
    • v.17 no.2
    • /
    • pp.187-195
    • /
    • 1992
  • This paper propose on the determination of threshold values for extracting shape information of the objects. First, surface curvatures such as mean curvature and gaussian curvature is calculated from given range data. And then local surface regions are classified into the one of 8 primitives by using the sign of mean curvature H and gaussian curvature K. Also from the statistical viewpoint. the range of the zero of H and K in the range is obtained through the analysis of the relation between mean curvature and gaussian curvature. Finally, the effectiveness of the proposed mithod in this paper is demonstrated by comparing with a case, where the zero threshold is arbitrarily obtained.

  • PDF

A Tangential Cutting Algorithm using Simulated Annealing (시뮬레이티드 어니얼링을 이용한 경사선분 추출 알고리즘의 개발)

  • 천인국;김승우;방재철;이효진
    • Proceedings of the Korea Multimedia Society Conference
    • /
    • 2002.05d
    • /
    • pp.574-578
    • /
    • 2002
  • 층 단위로 가공하는 RP(Rapid Prototype) 시스템에서 가공되는 물체의 표면에서는 계단형의 윤곽이 나타난다. 이러한 문제점을 보완하기 위해 경사절단 방법으로 3D 모델을 가공하여 기존의 가공방법에 의해 발생하는 계단형 윤곽 모습과 표면 왜곡 둥의 문제를 보완할 수 있다. 최적의 경사선분의 집합을 구하기 위해 경사절단 선분의 길이와 중간층 점의 거리를 정의하여 이를 최소화하는 에너지 함수를 구현한다. 그러나 이 방법은 경사절단 선분이 에너지가 작아지는 방향으로만 움직이기 때문에 레이어의 윤곽이 복잡한 경우 최적의 위치가 아닌 다른 위치에서 더 이상 움직이지 않는 국부적 최적해(Local Minima)가 발생할 수 있다. 본 논문에서는 국부적 최적해를 벗어나기 위해 경사절단 선분 추출 알고리즘에 시뮬레이티드 어니얼링(Simulated Annealing) 방법을 적용하였다. 제안된 방법으로 테스트한 결과 복잡한 레이어 윤곽에서 생길 수 있는 국부적 최적해가 어느 정도 해결되었다.

  • PDF

Quantitative Evaluation of Geotextile Void Structures Using Digital Image Analysis (디지털 이미지 분석을 이용한 지오텍스타일 공극 분포의 정량화)

  • Kim, Duhwan
    • Journal of the Korean Geosynthetics Society
    • /
    • v.12 no.1
    • /
    • pp.51-61
    • /
    • 2013
  • This paper presents results from a study undertaken to quantitatively evaluate the geotextile pore sizes using optical image analysis. The evaluation was conducted by observing surfaces of coupons cut from resin-impregnated specimens of geotextile-geomembrane layered under various load conditions. Stereological concepts were applied to collect representative specimens from a series of laboratory tests. The sizes of voids enclosed by filaments were expressed in terms of the largest inscribing opening size (LIOS) distribution. The opening diameter corresponding to the 50% cumulative frequency decreased by about 45mm as the load increased from 10 to 300kPa and recovered to about 90% of its initial state on unloading back to 10kPa. The average void size was reduced by 32 and 16.5% as the geotextile was sheared against a textured geomembrane under normal stresses of 100 and 300kPa, respectively. The results showed how the LIOS distribution varied as a function of normal stress and interface shear displacement against a smooth and a textured geomembrane surfaces.

Effects of Macrophytes on Budget of Matters in Lake Paldang (대형수생식물이 팔당호의 물질 수지에 미치는 영향)

  • Park, Hae-Kyung;Jung, Dong-Il;Byeon, Myeong-Seop
    • Korean Journal of Ecology and Environment
    • /
    • v.39 no.1 s.115
    • /
    • pp.85-92
    • /
    • 2006
  • To evaluate the primary production and nutrient uptake of macrophytes in Lake Paldang, this study investigate the vegetation areas of six dominant aquatic plants including Typha angustifolia, Zizania latifolia, Phragmites australis, Trapa japonica, Nelumbo nucifera and Savinia natans, and contents of carbon, nitrogen and phosphorus of each macrophyte. Total vegetation area of six dominant aquatic plants was 1.37 $km^2$. Among them, Typha angustifolia was the most wide-distributed species which occupied the 46.7% of total vegetation area. Littoral zone of South Han river had the largest vegetation area with 0.458 $km^2$, and North Han river, Kyungan river and confluence area in the order named. The results of the contents of carbon, nitrogen and phosphorus of macrophytes showed that the carbon contents of emergent macrophytes was higher than that of other life-forms. The nitrogen content of Salvinia natans, free-floating macrophyte was highest and that of Typha angustifolia, emergent macrophyte was lowest. The phosphorus content of Trapa japonica showed the highest content of phosphorus among six macrophytes and emergent macrophytes such as Zizania latifolia and Phragmites australis showed lower contents of phosphorus than other life-forms. The annual net primary production of macrophytes in Lake Paldang, 2004, was calculated as 758.4 ton C $yr^{-1}$ and the annual net nitrogen and phosphorus uptake of macrophyte was 16,921 kg $yr^{-1}$ and 1,841.0 kg P $yr^{-1}$ respectively. Comparing the total budget of organic carbon, nitrogen and phosphorus in Lake Paldang, the amount of primary production and nutrient uptake by macrophytes take a small portion in total budget implying macrophytes do not play an important role in budget of matters in river-type lake, Lake Paldang.

EVALUATION ON THE ABRASION RESISTANCE OF A SURFACE SEALANT (레진전색제의 마모저항성에 대한 평가)

  • Kim, Soo-Mee;Han, Sae-Hee;Cho, Young-Gon
    • Restorative Dentistry and Endodontics
    • /
    • v.32 no.3
    • /
    • pp.180-190
    • /
    • 2007
  • The purpose of this study was to evaluate the abrasion resistance of surface penetrating sealant which was applied on a composite resin restoration and to provide proper time to reapply sealant on composite resin surface. Two hundred rectangular specimens, sized $8\times3\times2mm$, were made of Micronew (Bisco, Inc., Schaumburg, IL, U.S.A) and divided into two groups; F group (n = 10) was finished with coarse and medium grit of Sof-Lex discs and BisCoverwas applied B group (n = 190) after finishing with discs. B group was again subdivided into nineteen subgroups From B-1 group to B-18 group were subjected to toothbrush abrasion test using a distilled water-dentifrice slurry and toothbrush heads B-IM group was not subjected to toothbrush abrasion test. Average surface roughness (Ra) of each group was calculated using a surface roughness tester (Surfcorder MSE-1700: Kosaka Laboratory Ltd., Tokyo, Japan) . A representative specimen of each group was examined by FE-SEM (S-4700: Hitachi High Technologies Co., Tokyo, Japan). The data were analysed using cluster analysis, paired t-test, and repeated measure ANOVA. The results of this study were as follows; 1. Ra off group was $0.898{\pm}0.145{\mu}m$ and B-IM group was $0.289{\pm}0.142{\mu}m$. Ra became higher from B-1 group $(0.299{\pm}0.48{\mu}m$ to B-18 group $(0.642{\pm}0.313{\mu}m$. 2. Final cluster center of Ra was $0.361{\mu}m$ in cluster 1 $(B-IM\simB-7)$, $0.511{\mu}m$ in cluster 2 $(B-8\simB-14)$ and $0.624{\mu}m$ in cluster 3 ($(B-15\simB-18)$. There were significant difference among Ra of three clusters. 3 Ra of B-IM group was decreased 210.72% than Ra of F group. Ra of B-8 group and B-15 group was increased 35.49% and 51.35% respectively than Ra of B-IM group. 4. On FE-SEM, B-IM group showed the smoothest resin surface. B-8 group and B-15 group showed vertically shallow scratches , and wide and irregular vertical scratches on composite resin surface respectively. Within a limitation of this study, finished resin surface will be again smooth and glazy if BisCover would be reapplied within 8 to 14 months after applying to resin surface.

Study of Surface Properties on Fouling Resistance of Reverse Osmosis Membranes (역삼투 분리막 표면 특성의 내오염성 상관 관계 연구)

  • 김노원
    • Membrane Journal
    • /
    • v.12 no.1
    • /
    • pp.28-40
    • /
    • 2002
  • The primary objective of this study is to elucidate the contribution of the electrostatic and molecula structural properties of an active layer of the thin film compsite (TFC) membranes to fouling tendency. The studies of surface morphology and surface charge were very effective in understanding fouling behaviors of the reverse osmosis (RO) membranes which were the thin film composite type of ployamide. Results of microscopic morphology analyzed by atomic force microscopy (AFM) and surface charge analyzed by electrokinetic analyzer (EKA) showed important factors affecting the fouling of RO membranes. The active layer of the composite membrane possessing realtively neutral streaming charge and less roughness provided a RO membrane with slowly decreasing flux.

MOF-based membrane encapsulated ZnO nanowires for H2 selectivity (MOF 기반 멤브레인 기능화된 ZnO 나노선의 수소 가스 선택성)

  • Kim, Jae-Hun;Lee, Jae-Hyeong;Kim, Jin-Yeong;Kim, Sang-Seop
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.106-106
    • /
    • 2017
  • 가스센서는 사내 및 산업 환경에서의 유독성 또는 폭발성 가스 검출, 환경 모니터링, 질병 진단 등 매우 다양한 응용분야에서 큰 관심을 가지고 있다. 반도체 금속산화물(SMOs) 기반의 센서 분야에서는 이들의 감도 및 선택성을 향상시키기 위해 많은 노력을 기울이고 있다. 이는 센서의 선택성을 부여하게 되면 다양한 가스들이 존재하는 환경에서도 검출자가 원하는 가스만의 응답을 얻을 수 있기 때문이다. 본 연구에서는 MOF(Metal-Organic Framwork) 기반 멤브레인으로 ZIF-8(Zeolitic Imidazolate Frameworks 구조들 중 하나) 멤브레인 쉘 층을 이용하여 ZnO 나노선에 형성하였다. ZnO 나노선은 VLS공정 (Vapor-Liquid-Solid)을 이용하여 패턴된 전극을 갖는 $SiO_2$-grown Si 웨이퍼 상에 성장되었고, 성장된 ZnO 나노선은 2-methyl imidazole과 methanol이 포함된 고용체에 넣고 폐쇄된 압력용기 속에서 가열시켜 얻게 된다. 이렇게 얻어진 ZIF-8@ZnO 나노선의 ZIF-8 멤브레인은 분자 체 구조(molecular sieving structure)를 갖게 되며, 이들의 pore 크기는 약 $3.4{\AA}$을 갖는다. 따라서 이보다 더 큰 동적 직경을(kinetic diameter) 갖는 가스 종은 이 멤브레인을 통과할 수 없음을 나타내므로 제작된 시편은 $H_2$(kinetic diameter : $2.89{\AA}$), $C_7H_8$(kinetic diameter : $5.92{\AA}$), 그리고 $C_6H_6$(kinetic diameter : $5.27{\AA}$) 가스들을 각각 사용함으로써 ZIF-8@ZnO 나노선의 센서 특성을 조사했으며, 보다 정확한 비교를 위해 순수한 ZnO 나노선 역시 동일한 조건에서 측정되었다. 결과를 통해, 수소 가스를 제외한 다른 가스들에 대해서는 반응을 하지 않고, 오직 수소 가스에 대해서만 반응을 나타냈으며, 순수 ZnO 나노선의 수소 감응도보다 낮은 감응도를 나타내었다. 이는 멤브레인 쉘 층을 형성함으로써 ZnO 나노선의 표면적이 감소해 가스 분자와의 접촉점을 감소시키기 때문이라고 판단된다. 이와 같은 MOF 멤브레인의 캡슐화 전략은 가스센서뿐 아니라 바이오 센서 및 광촉매 등과 같은 이온 선택성을 필요로 하는 다양한 응용분야에 적용될 수 있을 것으로 기대된다.

  • PDF

Mechanical properties by resin injection method of orthdontic acrylic resin (교정용 레진장치의 레진주입방법에 따른 기계적 특성)

  • Jo, Jeong-Ki
    • Journal of Digital Convergence
    • /
    • v.18 no.4
    • /
    • pp.341-346
    • /
    • 2020
  • Polymethyl methacrylate (PMMA), a self-curing resin mainly used in removable orthodontic appliances, is an acrylic resin mainly used in the field of modern dentistry. As an advantage, it has been used for a long time as a material for orthodontic devices in dentistry due to its color and volume, tissue affinity, and stability. The production of PMMA can be divided into self-polymerization method and thermal polymerization method according to activation method. Self-curing resins have long been used as orthodontic devices. The resin injection method is largely divided into a sprinkle-on method and a mixing method. In this study, we intend to test the mechanical properties according to the resin injection method of the orthodontic device, such as strength, modulus of elasticity, and surface roughness. There was no significant difference in strength as a result of three-point bending strength test on rectangular specimens (1.4 × 3.0 × 19.0 mm) of orthodontic PMMA. There was also no significant difference in hardness. There was no significant difference in surface roughness. It was confirmed that the orthodontic PMMA had no significant difference in mechanical properties according to the resin injection method of the orthodontic device.