• Title/Summary/Keyword: 레이저 점용접

Search Result 36, Processing Time 0.021 seconds

A Study on the In-plane Displacement Measurement of Spot welded Joints by Electronic Speckle Pattern Interferometry Method (레이저 스패클 간섭법에 의한 점 용접부의 면내변위 측정에 관한연구)

  • 성백섭
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 1997.04a
    • /
    • pp.48-53
    • /
    • 1997
  • Electronic Speckle Pattern Interferometry(ESPI) using the Model 95 Ar laserm, a video system and an image processor was applied to the in-plane displacement measurements. Unlike traditional strain gauges or moire method, ESPI method requires no special surface preparation or attachments and can be measured in-plane displacement with no contact and real time. In this experiment wpecimen was loaded in parallel with a loadcell. The specimen was the cold rolled sdteel sheet of 2mm thickness, which was attached strain gauges. The study provides an example of how ESPI have been used to measure strain displacement in this specimen. The results measured by ESPI have been used to measure strain displacement in this specimen. The results measured by ESPI have been used to measure strain displacement in this specimen. The results measured by ESPI compare with the data which was measured by strain gauge method in tensile testing.

  • PDF

Joining of Zinc Coated Steel and Aluminum Alloy for Car Body (자동차용 아연 도금 강판과 알루미늄 합금의 접합)

  • Lee, Woo-Ram;Lee, Jung-Hyun
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.20 no.2
    • /
    • pp.145-150
    • /
    • 2011
  • There is problem to reduce the car body weight for improving fuel consumption and $CO_2$ generation. As one of the solution, the multi material car body concept using aluminum alloys and high strength steels is proposed recently. Therefore, new welding processes by which these dissimilar material can be joined in high reliability and productivity are demanded. Laser spot welding was developed for joining of dissimilar metals. In the present work, Laser spot welding of zinc coated steel and aluminum alloy was investigated, and the process parameters were studied. Otherwise, the influences of process parameters on the weldability, the formation of intermetallic compound layer and the mechanical properties have been investigated. When intermetallic compound layer thickness was more than 1mm, specimen was failure in the interface.

Mechanism of Crack Formation in Pulse Nd:YAG Laser Spot Welding of Al Alloys (Al합금 펄스 Nd:YAG 레이저 점 용접부의 균열 발생기구)

  • 하용수;조창현;강정윤;김종도;박화순
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.86-94
    • /
    • 2000
  • This study was performed to investigate types and formation mechanism of cracks in two Al alloy welds, A5083 and A7N01 spot-welded by pulse Nd : YAG laser, using SEM, EPMA and Micro-XRD. In the weld zone, three types of crack were observed : center line crack({TEX}$C_{C}${/TEX}), diagonal crack({TEX}$C_{D}${/TEX}), and U shape crack({TEX}$C_{U}${/TEX}). Also, HAZ crack({TEX}$C_{H}${/TEX}) was observed in the HAZ region, furthermore, mixing crack({TEX}$C_{M}${/TEX}) consisting of diagonal crack and HAZ crack was observed. White film was formed at th hot crack region in the fractured surface after it was immersed to 10% NaOH water. In the case of A5083 alloy, white films in {TEX}$C_{C}${/TEX} crack and {TEX}$C_{D}${/TEX} crack region were composed of low melting phases, {TEX}$Fe_{2}SiAl_{8}${/TEX} and eutectic phases, $Mg_2$Al$_3$ and $Mg_2$Si. Such films observed $CuAl_2$, {TEX}$Mg_{32}(Al,Zn)_{3}${/TEX}, MgZn$_2$, $Al_2$CuMg and $Mg_2$Si were observed in the whitely etched films near {TEX}$C_{C}${/TEX} crack and {TEX}$C_{D}${/TEX} crack regions. The formation of liquid films was due to the segregation of Mg, Si, Fe in the case of A5083 alloy and Zn, Mg, Cu, Sim in the case of A7N01 alloy, respectively. The {TEX}$C_{C}${/TEX} and {TEX}$C_{D}${/TEX} cracks were regarded as a result of the occurrence of tensile strain during the welding process. The formation of {TEX}$C_{M}${/TEX} crack is likely to be due to the presence of liquid film at the grain boundary near the fusion line in the base metal as well as in the weld fusion zone during solidification. The {TEX}$C_{U}${/TEX} crack is considered a result of the collapsed keyhole through incomplete closure during rapid solidification.

  • PDF

Measurement of Out-of-plane Displacement in a Spot Welded Canti-levered Plate using Laser Speckle Interferometry with 4-step Phase Shifting Technique (레이저스펙클 간섭법과 4단계 위상이동법에 의한 외팔보 점용접부의 면외 변위측정)

  • Baek, Tae-Hyun;Kim, Myung-Soo;Na, Eui-Gyun;Koh, Seung-Ki
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.19 no.3
    • /
    • pp.66-72
    • /
    • 2002
  • Electronic Speckle Pattern Interferometry (ESPI) has been recently developed and widely used because it has advantage to be able to measure surface deformations of engineering components and materials in industrial areas with non-contact. The speckle patterns to be formed with interference and scattering phenomena can measure not only out-of-plane but also in-plane deformations, together with the use of digital image equipment to process the informations included in the speckle patterns and to display consequent interferogram on a computer monitor. In this study, the experimental results of a canti-levered plate using ESPI were compared with those obtained from the simple beam theory. The ESPI results of the canti-levered plate analyzed by 4-step phase shifting method are close to the theoretical expectation. Also, out-of-plane displacements of a spot welded cacti-levered plate were measured by ESPI with 4-step phase shifting technique. The phase map of the spot welded cacti-levered plate is quite different from that of the canti-levered plate without spot welding.

Mechanism of Crack Formation in Pulse Nd YAG Laser Spot Welding of Al Alloys (Al합금 펄스 Nd:YAG 레이저 점 용접부의 균열 발생기구)

  • Ha, Yong Su;Jo, Chang Hyeon;Gang, Jeong Yun;Kim, Jong Do;Park, Hwa Sun
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.213-213
    • /
    • 2000
  • This study was performed to investigate types and formation mechanism of cracks in two Al alloy welds, A5083 and A7NO1 spot-welded by pulse Nd: YAG laser, using SEM, EPMA and Micro-XRD. In the weld zone, three types of crack were observed: center line crack($C_{C}$), diagonal crack($C_{D}$), and U shape crack($C_{U}$). Also, HAZ crack($C_{H}$), was observed in the HAZ region, furthermore, mixing crack($C_{M}$), consisting of diagonal crack and HAZ crack was observed.White film was formed at the hot crack region in the fractured surface after it was immersed to 10%NaOH water. In the case of A5083 alloy, white films in C crack and $C_D crack region were composed of low melting phases, Fe₂Si$Al_8$ and eutectic phases, Mg₂Al₃ and Mg₂Si. Such films observed near HAZ crack were also consist of eutectic Mg₂Al₃. In the case of A7N01 alloy, eutectic phases of CuAl₂, $Mg_{32}$ (Al,Zn) ₃, MgZn₂, Al₂CuMg and Mg₂Si were observed in the whitely etched films near $C_{C}$ crack and $C_{D}$ crack regions. The formation of liquid films was due to the segregation of Mg, Si, Fe in the case of A5083 alloy and Zn, Mg, Cu, Si in the case of A7N01 aooly, respectively.The $C_{D}$ and $C_{C}$ cracks were regarded as a result of the occurrence of tensile strain during the welding process. The formation of $C_{M}$ crack is likely to be due to the presence of liquid film at the grain boundary near the fusion line in the base metal as well as in the weld fusion zone during solidification. The $C_{U}$ crack is considered a result of the collapsed keyhole through incomplete closure during rapid solidification. (Received October 7, 1999)

Measurement of Nondestructive Residual Stress by Acoustoelasticity (음탄성에 의한 비파괴적 잔류응력 측정)

  • 박인근;이철구
    • Journal of Welding and Joining
    • /
    • v.17 no.2
    • /
    • pp.25-28
    • /
    • 1999
  • 국내에 건설되어 거의 20∼30년 가동되고 있는 발전설비, 석유화학 플랜트 등 거대설비 기기의 건전성(integrity) 및 신뢰성 확보와 잔존수명 예측을 위해서는 구조물 내부 또는 표층부에 존재하는 결 함의 특성을 아는 것과 함께 그 재료의 특정 부위에 어느정도의 응력이나 변형이 있는가를 아는 것이 매우 중요하다. 일반적으로 강 용접부의 비파괴적 결함검출에는 주로 SV파(vertically shear wave)와 SH파(horizontally shear wave)라 불리는 횡파를 이용한 초음파사각탐상법이 실용화되어 이용되고 있다. 그러나 비파괴적인 방법에 의한 실험적인 잔류응력 측정, 변형해석법에는 전기 저항 및 자기 스트레인 게이지법, X선회절법, 광탄성법(photoelasticity), 모아레(Mohr's)법, 레이저스펙클(Laser speackle)법, 응 력도료법, Barkhausen Nosise법, Caustics법 등이 제시되어 있으나 그 유용성 면에서는 아직 해결되야할 문제가 많이 남아 있는 실정이다. 응력이나 변형을 해석하는 방법으로 이론적 방법, 계산적 방법 실험적 방법이 잇다. 이론적 방법에는 재료 역학적으로 취급하는 방법, 탄성론 등이 있고, 계산적인 방법에는 유한요소법이 있지만, 이론적 방법이나 계산적 방법만으로는 해석이 불가능한 경우가 많기 때문에 실험 적 방법이 필요하게 된다. 이 글에서는 파괴 시험 또는 다른 비파괴평가기술에 비해 간편한 측정, 높은 측정정도, 시험결과 도출의 신속성, 검사비용의 절감 등 많은 장점을 가지고 있고 실험적으로 유용성이 일부 검증되고 있는 음탄성법(Acoustoelasticity)에 의한 잔류응력 측정법에 관해 소개하고자 한다.TEX> mg/L(평균 49 mg/L)로 비교적 안정적인 처리효율을 보여주었다. 본 연구결과 HVC 공정은 화학약품 사용량의 절감 및 이에 따른 화학슬러지 발생량의 감소를 기대 할 수 있는 친환경기술로 유지관리비를 최소화할 수 있는 장점이 있었다. 않은 사람들 중 미래의 검진실행의지에 건강소식지가 영향을 미친 경우는 48.7%였다. 보건교육을 받은 후 유방암 자가검진 실천율은 사업군에서 53.9%로 받기 전의 27.3%보다 증가하였으나 대조군의 경우는 별 차이가 없었다. 연령별로는 60대가 가장 높았고 사업군에서 검진율의 증가분은 30대가 가장 컸다. 교육수준별로는 사업군은 고졸이, 대조군은 전문대졸이 가장 높았고 사업군에서 검진율의 증가분은 고졸에서 가장 컸다. 보건교육 후 유방암과 관련된 건강지식의 정도는 사업군이 3.7점으로 대조군보다 유의하게 높았으며, 유방암 자가검진법을 실천하는 사람들의 동기는 ‘일반 대중매체의 영향’이 가장 많았으며 건강소식지가 동기인 경우도 20.4%였다. 사업군에서 건강소식지가 유방암 자가검진법 실천에 영향을 미친 경우가 79.6%였으며 유방암 자가검진법에 관한 보건교육을 받고 실천하지 않은 사람들 중 미래의 실천의지에 건강소식지가 영향을 미친 경우는 43.6%였다. 이상의 소견에서 지역주민을 대상으로 인쇄매체를 통한 보건교육은 인쇄물만으로도 쉽게 실천 할 수 있는 유방암 자가검진법이 가장 효과적이었으며, 자궁암검진에 관해서도 검진을 받을 수 있도록 지역사회의 보건의료의 하부구조를 정비하여 제도적 장치를 마련하고 정보를 제공한다면 자궁암검진 실천율도 증가할 것이다.고 12.9% 의 발달율을 보여 유의적인 차이를 보이지 않았다. 이상의 결과로 보아 핵이식 수정란을 효율적으로 생산하기 위하여

  • PDF