• Title/Summary/Keyword: 동결/융해실험

Search Result 312, Processing Time 0.04 seconds

Characterization of Freezing-Thawing on the Artificial Weathering of $TiO_2$ Loaded Granite and Their Physical Property ($TiO_2$가 담지된 화강암의 인공풍화에 미치는 수분의 동결-융해의 평가와 물리적 성질)

  • Shon, Byung-Hyun;Jung, Jong-Hyeon;Kim, Hyun-Gyu;Choung, Young-Hean;Cho, Ki-Chul;Oh, Kwang-Joon
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.28 no.2
    • /
    • pp.183-190
    • /
    • 2006
  • An experimental study was conducted to evaluate the effect of freezing-thawing and air pollutants on the weathering of $TiO_2$ loaded granite. And the granite was coated with $TiO_2$ catalyst and tested. After freezing-thawing and air pollutants experiments the mineral compositions of the granite surface were lower then that of the fresh granite. Density of the weathered granite was steadily decreased from $2.60g/cm^3\;to\;2.55{\sim}2.56g/cm^3$, but absorption ratio and porosity were slightly increased. From these results, it was expected that granite could be weathered by freezing-thawing md air pollutants. In the case of $TiO_2$ was coated to the granite, the compressive strength and absorption ratio were slightly enhanced compared to the $TiO_2$ non-coated granite. Therefore, the $TiO_2$ coating method tested in this study considered to be a viable method to assist in the conservation of granite from environmental contaminants.

Weathering Properties of Shale Aggregate in Daegu-Kyeongbuk region and Freezing-Thawing Characteristics of Concrete in response to Usage of Shale Aggregate (대경권 셰일 골재의 풍화특성 및 셰일 골재 사용량에 따른 콘크리트의 동결융해 특성)

  • Lee, Seung-Han;Jung, Yong-Wook;Yeo, In-Dong;Choi, Jong-Oh
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.14 no.8
    • /
    • pp.4033-4038
    • /
    • 2013
  • Sedimentary rocks from construction waste are discarded through open storage and landfilling, which causes an increase in construction cost and inefficient of execution of works. Some sandstone are selected and utilized as aggregates, but shale is buried as industrial waste. Therefore, in this research, we evaluated weathering properties of shale aggregate that is widely distributed throughout Daegu-Kyeongbuk region and freeze-thaw characteristics of concrete according to the replacement ratio of shale aggregate, in an effort to stabilize aggregate supply-demand in Daegu-Kyeongbuk region and develop alternative aggregates. We used red shale and black shale in the experiment, which were exported from a construction site in Deagu. We verified the usage of shale as a concrete aggregate by comparing andesite, which is broadly used as a thick aggregate for concrete, to hornfels, which is a metamorphic sedimentary rock. As a result of the experiment, we observed no degradation phenomenon for andesite and hornfels. However, a part of country rock containing black shale was found to be exfoliated. Red shale started having cracks in the direction of stratification after 1.5 months of direct exposure, and it broke into smaller pieces after approximately 4 months. After 300 cycles of freeze-thaw process on the concrete manufactured according to the replacement ratio of shale aggregate, the modulus of elasticity was 97% for plain and 95% for hornfels. In the case of RS_100, it was 57% after 210 cycles, and for BS_100, it was 54% after 240 cycles. Therefore, we established that, as the number of repetition increases, the freeze-thaw resistance decreases dramatically.

Experimental and Numerical Investigation of the Performance of Vertical Thermosyphon for Frozen Ground Stabilization (실험과 수치해석을 통한 동토지반 안정화용 수직형 열사이펀의 성능평가)

  • Lee, Jangguen;Lee, Chulho;Jang, Changkyu;Choi, Changho
    • Journal of the Korean Geosynthetics Society
    • /
    • v.13 no.4
    • /
    • pp.45-56
    • /
    • 2014
  • Frozen ground in cold region consists of an upper active layer and lower permafrost which is permanently frozen land. During the summer season, the air temperature is high enough to make the frozen ground melt, which causes the reduction of soil strength and thaw settlement. These phenomena result in structural instability, so it is necessary to apply frozen ground stability techniques. Thermosyphon is a closed natural two-phase convection device to maintain the ground temperature below $0^{\circ}C$ by extracting heat from the ground and discharges it into the atmosphere. Experimental and numerical investigation has been performed to estimate the effect of the refrigerant filling ratio in thermosyphon using R-134a refrigerant and the thermal conductance of the thermosyphon.

Freeze-thaw of Durability for Premixed Fly Ash Concrete (프리믹스 플라이애시 콘크리트 동결-융해 특성)

  • Hong, Seung-Ho;Han, Seung-Hwan;Lee, Byung-Duk
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.261-262
    • /
    • 2009
  • The prevent methods of Alkali-Silica Reaction (ASR) are studying after the failure cases by ASR were reported in Korea. In this study, the freeze-thaw test and scaling test for premixed fly ash cement were performed. The ratio of fly ash and cement is 20 percent and 80 percent by weight of total cementious material. The results show that the dynamic modulus after 300 cycles the freeze-thaw test for most of specimen except the specimen have less 3% air was more than 90 % and the loss of weigh the specimen after 50 cycles scaling test was less than 1kg/$m^3$.

  • PDF

A Study on the Properties of Concrete Using Zeolite (제올라이트를 사용한 콘크리트의 기초적 성질에 관한 연구)

  • 최재진
    • Magazine of the Korea Concrete Institute
    • /
    • v.10 no.5
    • /
    • pp.205-216
    • /
    • 1998
  • 천연제올라이트를 사용한 콘크리트의 특성을검토하기 위하여 천연제올라이트의 대체율 및 입자크기에 따라 콘크리트의 압축강도, 동결융해저항성, 건조수축 및 투수성 등을 실험하였다. 이때 천연제올라이트는 입자크기(중간값)가 12.7$\mu\textrm{m}$과 10.39$\mu\textrm{m}$인 것을 사용하였으며 콘크리트실험에서 천연제올라이트의 시멘트 중량에 대한 대체율은 5%, 10%, 15% 및 20%로 하였다. 천연제올라이트의 대체율이 15%이하인 콘크리트는 동일한 물-결합재비에서 천연제올라이트를 사용하지 않은 경우와 비교하여 재령 28일 및 91일의 압축강도가 크게나타났으며 이러한 강도의 증가는 천연제올라이트의 입자크기가 작은 경우 보다 크게 나타났다. 콘크리트의 동결융해에 대한 저항성이나 건조수축에 의한 길이변화는 천연제올라이트의 대체율에 따라 명확한 차이를 보이자 않았으나 다만 천연제올라이트의 대체율이 20%인 경우는 길이변화가 크게 되는 경향을 나타냈다. 수밀성시험에서는 천연제올라트의 입자크기가 12.7$\mu\textrm{m}$인 경우 그의 사용량이 증가함에 따라 수밀성이 저하하였으며 입자크기가 10.39$\mu\textrm{m}$인경우는 천연제올라이트의 대체율이 10% 이하인 경우 수밀성이 다소 개선되는 것으로 나타났으나 그 이상의 대체율에서는 수밀성이 저하되는 경향을 나타냈다.

Freeze and Thaw Durability of Concrete Using Recycled Aggregates (재생골재를 사용한 콘크리트의 동결융해 저항성)

  • 문대중;팽우선;문한영
    • Journal of the Korea Concrete Institute
    • /
    • v.14 no.3
    • /
    • pp.307-314
    • /
    • 2002
  • Utilization of demolished-concrete as recycled aggregate has been researched for the purpose of substituting for insufficient natural aggregate, saving resources and protecting environment. There, however, are some Problems not only the large difference of dualities in recycled aggregates but also a little deterioration of mechanical properties in recycled aggregate concrete in comparison with that of natural aggregate concrete. In this study, the test results of freez and thaw durability of concrete with demolished-concrete recycled aggregate(DRA) arc as follows. Improvement of crushing process is an important assignment because that adhered mortar on source-concrete recycled aggregate(SRA) and DRA highly affects thc qualifies of recycled aggregate. The compressive strength of recycled aggregate concrete was not highly different in comparison with that of control concrete. But the resistance to penetration of Cl in recycled aggregate concrete was shown smaller than that of control concrete because of adhered mortar on recycled aggregate. The resistance to frcezing and thawing of recycled aggregate concrete was highly different due to adhered mortar on recycled aggregate, and durability factor of concrete with NA-SRA and DRA was more decreased than that of control concrete. On the other hand, durability factor of concrete with AA-SRA was larger than that of control concrete. It, therefore, is necessarily required that recycled aggregate including adequate entrained air should be used for satisfying the freez and thaw durability of recycled aggregate concrete.

Effect of Air Contents, Deicing Salts, and Exposure Conditions on the Freeze-Thaw Durability of the Concrete (콘크리트의 동결융해 내구성에 공기량, 제설제, 노출조건이 미치는 영향에 관한 연구)

  • Lee, Byung-Duk
    • International Journal of Highway Engineering
    • /
    • v.12 no.2
    • /
    • pp.107-113
    • /
    • 2010
  • In this study, the relative effects of low-chloride deicier(LCD) and two other deicing agents on the scaling of concrete were conducted in a series of tests at laboratory accordance with the ASTM C 672. The solutions concentration of deicers tested included 1, 4, 10%. Tap water was used as control. The amount of scaling was evaluated gravimetrically. As test result of deicer solution types, when applied to 4% solutions, surface scaling of concrete after 56 freeze-thaw cycles was produced significantly as about 9 times on LCD solution, as about 18 times on $CaCl_2$ solution, and as about 33 times on NaCl solution comparing with tap water. As test result of deicer solution concentrations, relatively low concentrations (of the 4% by weight) of deicer were produced more surface scaling than higher concentrations (of the 10% by weight) or lower concentrations (of the 1% by weight) of deicer. It show that the damaging concentration is of the order of 3~4% for previous research result. It appears that the mechanism of surface scaling is primarily physical rather than chemical. Also, the effect of chloride deicier types, freeze-thaw cycling, and air contents on the performance of concrete was experimentally investigated. The results show that the concrete specimens subjected to freeze-thaw cycling scaled more severely in exposure to deicing salt than those in non-exposure to deicing salt, weight losses of the specimens tested in exposure to deicing salt were twice as much as those tested in non-exposure to deicing salt. Relative dynamic modulus of elasticity of concrete specimens decreased more quickly in exposure to deicing salt than in non-exposure to deicing salt. Also, relative dynamic modulus of elasticity of concrete specimens in exposure to sodium chloride deicing salt was decreased more quickly comparing with exposure to LCD salt. It is also shown that the chloride contents according to concrete specimen depths was more largely in exposure to LCD salt. When concrete specimen is exposed to chloride deicing salts and freeze-thaw cycling, performance degradation in the entrained air concrete(AE concrete) retarded more considerably comparing with non-entrained air concrete(Non-AE concrete).

Variation of Physical and Microstructural Properties of Limestone caused by Artificial Freezing and Thawing (인공 동결-융해 풍화에 따른 석회암의 물성 및 미세구조 변화 분석)

  • Park, Jihwan;Park, Hyeong-Dong
    • Tunnel and Underground Space
    • /
    • v.25 no.5
    • /
    • pp.435-449
    • /
    • 2015
  • Physical and microstructural properties of Pungchon and Maggol limestone were investigated quantitatively during 50 cycles of artificial freezing and thawing test. There were decrease in dry weight and P,S-wave velocity, and increase in absorption rate in both rock types. Porosity, pore volume, equivalent diameter, throat thickness and pore orientation were analyzed using X-ray computed tomography images. Porosity increased, and initiation and expansion of pores were investigated as weathering progresses. Physical and microstructural variation in Maggol limestone was larger than that of Pungchon limestone because Maggol limestone has more pores and microcracks at initial state. As this study analyzes physical and microstructural properties of rock specimens comprehensively, it can be applied to further rock weathering study and can be used as fundamental data of construction and resource development in cold regions.

Mechanical Properties of Very Rapid Hardening Polymer Mortar for Concrete Repair (보수용 초속경 폴리머 모르타르의 역학적 특성)

  • Hong, Kinam;Shin, Junsu;Han, Sanghoon;Seo, Dongwoo;Ahn, Kwangkuk
    • Journal of the Korean GEO-environmental Society
    • /
    • v.15 no.8
    • /
    • pp.31-37
    • /
    • 2014
  • In this study, mechanical properties of Very-Rapid Hardening Polymer (VRHP) mortar were investigated. To do it, 75 VRHP mortar specimens were tested by the compressive test, bending test, bonding test, freezing and thawing test, length variation test, and water absorption test. From the test results, it was confirmed that the bond strength of VRHP was higher than that of normal concrete by 50 %, and the resistance of freezing and thawing of VRHP was more excellent than normal concrete. In addition, length variation ratio and water absorption ratio of VRHP were smaller than those of normal concrete by 20 %. Therefore, It should be mentioned that VRHP can be successfully used as the material for repairing the crack of concrete structure.