  • Nowaday, High strength concrete(HSC) has been mainly used in high rise building. HSC have superior property as well as improvement in durability compared with ordinary strength concrete. In spite of durability of HSC, explosive spalling in concrete front surface near the source of fire occurs serious problem in structural safety. Thus, this study is concerned with experimentally investigation fire resistance of the inorganic fire protection materials at high temperatures up to $800^{\circ}C$. From the test result, developed inorganic binder becomes general that with rising temperature the compressive strength of the material increases in tendency. Therefore, the results indicate that it is possible to fireproof panels, fire protection of materials, etc.

  • PDF

폭렬방지공법 변화에 따른 RC 기둥부재의 내화특성 (Fire Resistant Properties of the RC Columns Applying Various Splling Prevention Methods)

  • 한천구;배장춘;이종석;이찬영
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제13권3호통권55호
    • /
    • pp.119-126
    • /
    • 2009
  • 본 연구에서는 RC 기둥의 폭렬방지를 위하여 유기섬유의 혼입방식, 내화보드 부착방식, 스프레이 방식의 폭렬방지공법에 따른 내화특성을 검토하였는데, 그 결과를 요약하면 다음과 같다. 굳지않은 콘크리트의 특성으로, 유기섬유의 혼입율이 증가에 따른 유동성은 저하하는 것으로 나타났고, 섬유의 종류에 따라서는 NY섬유를 혼합한 경우 가장 양호하였다. 공기량은 NY섬유가 가장 적게 저하하였고, 그 다음으로 PVA, PP순이었다. 경화 콘크리트의 특성으로, 압축강도는 28일 재령에서 50MPa이상으로 섬유의 혼입율이 증가할 수록 약간 크게 나타났다. 내화시험후 폭렬특성으로, 유기섬유 혼입방식의 경우 PVA섬유를 제외한 PP섬유, NY 섬유는 혼입율 0.05%이상에서 폭렬이 발생하지 않는 것으로 나타났다. 스프레이 방식의 경우는 모든 마감재 부분에서 부분적인 폭렬이 발생하였을 뿐, 모재 콘크리트는 폭렬이 발생하지 않고 본래의 형상을 그대로 유지하는 것으로 나타났다. 또한, 보드방식의 경우는 보편적인 일반 건식공법인 경우를 제외한 건식공법 시공 후 내화페인트로 연결철물을 도포한 경우, 내화모르터로 차폐한 경우, 경량기포 콘크리트로 그라우트 한 경우는 모두 폭렬이 발생하지 않고 본래의 형상을 그대로 유지하고 있었다. 질량감소율은 플레인 콘크리트를 제외한 내화시공공법변화에 따라서 공히 8%미만으로 비교적 양호하게 나타났다.

중인방을 포함한 목골조 경량벽체의 내화성능에 관한 연구 (A Study on the Fire Resistance Performance of Wood Framed Lightweight Wall which Including a Middle Lintel)

  • 여인환;조범연;민병렬;윤명오
    • 한국화재소방학회논문지
    • /
    • 제25권3호
    • /
    • pp.91-98
    • /
    • 2011
  • 이 연구는 전통 벽체 형식으로서 중인방을 포함한 목골조 경량벽체의 내화성능에 대한 것이다. 대상으로 한 경량벽체는 $38{\times}89$ mm($2"{\times}4"$) 목재를 골구로 하고 방회석고보드로 마감하는 형식의 비내력구조 이다. 벽체의 중간부에는 $150{\times}150$ mm 단면의 집성목 중인방을 설치하였다. 실험체는 단열재 유무 등에 따라 3가지 타입으로 제작하였다. 내화실험 결과 실험체-1, 2, 3 모두 90분 이상의 내화성능을 확보하는 것으로 나타났고, 각각 92분, 98분, 99분만에 중인방의 측면과 하부에서 불꽃이 발생하여 실험을 중단하였다. 가열면의 방화석고보드($12.5mm{\times}2$겹)는 약 45분간 내화성능을 유지하는 것으로 나타났고, 중인방의 연소는 일반적인 목재의 탄화속도와 유사한 거동을 보였다 벽체 내부의 목재스터드는 방화석고보드의 기여로 연소가 지연되는 동안 탈수가 일어나 고온에 노출된 이후에는 수분에 의한 온도상승 지연효과가 일어나지 않고 비교적 빠른 연소가 진행되는 것으로 나타났다.

자기 평활성 바닥 마감용 SBR 시멘트 모르타르의 인장부착강도 (Adhesive Strength in Tension of SBR-Modified Cement Mortar with Self-Flowability Material for Floor-Finishing)

  • 도정윤;소양섭
    • 콘크리트학회논문집
    • /
    • 제15권4호
    • /
    • pp.549-556
    • /
    • 2003
  • 시멘트 모르타르의 내마모성, 여러 피착체에 대한 부착성능, 내화학성, 내수성 등의 많은 성능을 개선시키는 데 폴리머 디스퍼젼은 매우 유용한 재료로서 본 실험에 사용한 SBR은 상업적으로 국내에서 생산되고 있는 시멘트 적용성이 우수한 재료이다. 본 실험에서는 시멘트 모르타르에 높은 유동성을 유도하여 자기 평활성을 가지도록 고유동화제와 SBR을 사용하여 시험체를 제작하였으며 SBR에 의한 시험체의 부착강도의 발현 특성을 파악하고자 하였으며 SBR에 의해 개질된 자기 평활성을 가지는 시멘트 모르타르는 재령의 증가에 따라 부착강도는 증가하는 현상을 보여주었으며 파괴형상을 보면 재령이 증가함에 따라 시험체에서 보다는 계면과 피착체에서 외부 인장력에 대하여 파괴가 일어났다. 현재 사무실, 공장, 주차장 등의 바닥 마감재로 널리 사용되고 있는 합성 고분자계 재료인 에폭시 수지나 폴리우레탄 제품은 연도변화가 심하여 가사시간이 상당히 짧다는 것을 확인할 수 있었으며 이에 반하여 본 연구의 시험체는 충분한 가사시간을 확보할 수 있는 이점을 가진 재료로 여겨진다.

Fly Ash 및 Meta-Kaolin을 활용한 내화성 마감재의 고온특성 (High Temperature Properties of Fire Protection Materials Using Fly Ash and Meta-Kaolin)

  • 송훈;추용식;이종규;도정윤
    • 한국세라믹학회지
    • /
    • 제47권3호
    • /
    • pp.223-231
    • /
    • 2010
  • The serious issue of tall building is to ensure the fire-resistance of high strength concrete. The fire resistant finishing method is necessarily essential in order to satisfy the fire resistance time of 3 h required by the law. The fire resistant finishing method is installed by applying a fire resistant material as a method of shotcrete or a fire resistant board to high strength concrete surface. This method can reduce the temperature increase of the reinforcement embedded in high strength concrete at high temperature due to the installation thickness control. This study is interested in identifying the effectiveness of inorganic alumino-silicate compounds including the inorganic admixture such as fly ash and meta-kaolin as the fire resistant finishing materials through the analysis of fire resistance and components properties at high temperature. The study results show that the fire resistant finishing material composed of fly ash and meta-kaolin has the thermal stability of the slight decrease of compressive strength at high temperature. These thermal stability is caused by the ceramic binding capacity induced by alkali activation reaction by the reason of the thermal analysis result not showing the decomposition of calcium hydrate. Inorganic compounds composed of fly ash and meta-kaolin is evaluated to be very effective as the fire resistance material for finishing to protect the concrete substrate by the reason of those simplicity in both application and manufacture. The additional study about the adhesion in the interface with concrete substrate is necessary for the purpose of the practical application.

고도정수처리용 콘크리트 금속용사 피막의 내오존성 및 오존처리 후 부착강도 평가에 관한 실험적 연구 (Experimental Study on Evaluation of Bond Strength after Ozone Treatment and Ozone Resistance of Concrete Metal Spray Coating for Advanced Water Treatment)

  • 박진호;장현오;이한승
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제22권4호
    • /
    • pp.68-75
    • /
    • 2018
  • 기존의 정수처리 방법으로는 제거되지 않는 물질이 발생함에 고도정수 처리 시설의 도입이 증가하고 있다. 그러나 오존을 이용한 고도정수처리 시설의 내부 방수 방식재는 오존의 산화력에 의해 열화되며 콘크리트까지 영향을 미쳐 내구성 저하의 원인이 된다. 본 연구에서는 내오존성 및 내화학성이 뛰어난 금속 패널을 기존의 시공법 보다 손쉬운 방법으로 시공하기 위한 방법으로 금속용사 공법을 이용하여 수처리 시설 콘크리트 구조물의 열화를 원천적으로 방지하기 위한 마감공법 개발 연구의 일원으로 용사금속 종류 및 피막의 표면처리 방법에 따른 내오존성 평가를 실시하였으며, 오존처리 후의 부착강도를 평가하였다. 실험결과 용사금속 Ti이 용사 후에도 내오존성이 뛰어난 것으로 나타났으며 표면처리 방법으로는 테프론계 봉공처리제를 사용하여 마감하는 것이 내오존성 및 부착성능 확보에 가장 적합한 방법이라 판단된다.

유동성 및 조기강도 확보가 가능한 자기수평 모르타르 배합선정에 관한 연구 (A Study on the Formulation Selection of Self Leveling Floor Mortar with Fluidity and Early Strength Improvements)

  • 류화성;김득모;권성준;박원준;신상헌
    • 한국건축시공학회지
    • /
    • 제18권1호
    • /
    • pp.41-49
    • /
    • 2018
  • 본 연구는 고강도, 고유동의 성질을 갖고, 시공 후 수축현상이 저감되어 균열발생을 저감시킬 수 있는 바닥모르타르 배합선정에 관한 연구로서, 최적배합을 선정하기 위한 배합시험과 선정된 배합의 압축강도, 휨강도, 플로, 길이변화성능 및 염화물침투 저항성, 내화학성 등의 성능시험을 실시하였다. 시험결과, 유동성과 조기강도 발현이 가능하며, 수축저감을 통하여 균열발생 위험성을 개선시킬 수 있을 것이라 판단되는 배합을 선정하였으며, 선정된 배합은 자기수평모르타르 규격에 만족하는 성능을 확보하는 것으로 확인되었다. 본 연구의 결과를 통하여 우수한 재료성능과 경제성, 시공성을 갖는 고성능, 고유동의 바닥모르타르 시공기술을 확보할 예정이다.

노인의료복지시설 화재 시 와상노인의 피난안전성 제고를 위한 피난허용시간 연장과 소방기관으로의 통보시간 연구 (A Study on ASET Elongation & Notification Time to Fire Stations for the Escape Safety of Aged Bedridden Patients in Elderly Long-term Medical Care)

  • 박형주;이영재
    • 한국화재소방학회논문지
    • /
    • 제32권4호
    • /
    • pp.50-59
    • /
    • 2018
  • 고령화 추세에 따라 최근 급속히 증가하고 있는 노인복지시설에서 화재가 빈번하게 발생하고 있으나, 거주하고 있는 와상노인에 대한 피난안전성이 확보되어 있지 않아 대규모 인명피해를 초래하고 있다. 이런 시설에 거주하는 와상노인에 대한 피난안전성의 실효성을 제고하기 위한 방법의 일환으로 비화재구역의 피난허용시간을 최대한 연장시키면서 발코니 등의 일시피난안전구역에 차례로 피난시키고, 소방기관에 통보하는 화재속보설비를 통해 소방대의 출동에 의한 외부 조력피난유도방법이 최선의 대책인 것으로 판명되었다. 따라서 이와 같은 조력피난을 수행하는데 있어 반드시 적용해야할 요소기술을 방화 소방공학적으로 개발하여 4가지로 분류 제시하였다. 방화공학적 요소기술로는 구조 구획의 내화성능확보와 구획의 소규모화 규제 조항과 마감재의 난연 불연성능의 확보 규제 조항인 2가지를 제시하였다. 또한 소방공학적 요소기술로는 스프링클러에 의한 냉각효과 부과 규제 조항과 소방기관으로의 자동화재속보기능의 부여 규제 조항인 2가지를 제시하였다. 제시된 규제 조항에 대하여 일본과 국내의 법조문을 상세히 비교분석하여 국내에서 개정한 법조문상 미흡한 부분을 고찰하고, 국내의 노인복지시설의 피난안전성의 제고를 위해 시급하게 개선되어야 할 안전기준 개정(안)을 제시하였다.