Jung, Youn Seo;Kim, In Sik;Hyeon, Seung Mi;Hwang, Taek Sung
Applied Chemistry for Engineering
/
v.28
no.5
/
pp.539-546
/
2017
In this study, an outstanding anion exchange chemical filter was prepared for acidic gas removal. Commercial anion exchange resin was attached to polyurethane (PU) foam by using different types of pressure sensitive adhesive (PSA). The water and chemical resistance and also adhesive elongation were investigated. Also, the behavior of HCl and HF adsorption was evaluated as functions of the initial concentration and flow rate. ATE-701, AT-4000C and HCA-1000 showed 900, 1,500% and 2,400% of the elongation, respectively. It was confirmed that the desorption ratio of HCA-1000 was less than 6% and had excellent durability in water and chemical resistance tests. The adsorption occurred faster as the concentration and flow rate of HCl and HF increased. But 100% adsorption equilibrium occurred after 110 minutes, regardless of the concentration and flow rate. In addition, SEM morphology showed that the adhesive was uniformly dispersed, while the porous structure of the ion exchange resin was maintained, and the chemical filter exhibited excellent durability for the adsorption/desorption process.
Proceedings of the Korean Institute of Surface Engineering Conference
/
2014.11a
/
pp.27-28
/
2014
투명전극이란 전기 전도도를 갖는 동시에 가시광선 영역에서 빛을 투과하는 성질을 가지는 소재이다. 일반적으로 가시광선 영역(380nm~780nm)에서 80%이상의 광 투과도를 가지며, 비저항이 $10^{-3}{\Omega}{\cdot}cm$ 이하, optical band gap 이 3.3 eV 이상인 물질을 TCO(Transparent Conducting oxide)라고 한다. 현재까지 국내의 TCO 관련 연구는 터치패널, 디스플레이, 태양전지 등 광전자분야에서 가장 널리 사용되고 있는 ITO(Sn:In2O3)에 치중되어 있으며, 관련 연구도 거의 디스플레이 맞춤형 연구개발이 주류를 이루어왔다. ITO가 전기전도성이 우수하고 동시에 가시광선 영역에서의 투과율도 80%이상으로 전기적, 광학적 특성이 우수하다는 장점을 가지고 있으나, In의 희소성으로 인한 고가격, 유독성, 접착력 문제 때문에 이를 대체하기 위해 제조원가가 ITO에 비하여 월등히 저렴하고 내화학성과 내마모성이 우수하면서도, 가시광선 영역에서의 광투과율이 80%이상으로 좋다는 $SnO_2$에 관한 연구가 활발히 진행되어 왔다. 적절한 dopant를 첨가하여 $SnO_2$자체의 높은 광학적 투과도를 유지하면서 전기전도성을 더 높일수 있고, 투명전극이 가져야 할 고온 안정성을 가지고 있으며 비독성이고 수소 플라즈마에 대한 내성이 더 클 뿐만 아니라 저온에서 성장이 가능하다. $SnO_2$의 전기 전도도를 높이기 위한 Al, In, Ga, B와 같은 3족 원소가 $SnO_2$의 n형 dopant로 널리 사용되고 있다. 그 중 Al은 반응성이 커서 박막 증착 중에 산화되기 쉬운 반면, 전기적 특성 및 광학적 특성의 향상을 이룰 수 있다. 본 연구에서는 Rf Sputtering법을 사용하여 quartz기판 위에 다층박막 형태의 투명전도막을 제작한 후, 열처리를 수행, 이에 의한 다층박막 내 계면간 상호확산 현상을 이용하여 투명 전도막의 특성변화를 관찰하였다. 박막의 구조적 특성은 XRD장비를 사용하여 분석하였으며, 전기적, 광학적 특성은 각각 표면저항기, 홀 측정 장비, 그리고 UV-VIS-NI를 사용하여 확인하였다.
Concrete is generally accepted to have good inherent fire resistance. It mainly relies on the assumption that concrete has low heat-transfer characteristic and spatting does not occur during the course of a fire. However, the significant numbers of fire accidents have shown in recent years that incidence of spatting has caused sever damages to many structures. This review has systematically investigated the behaviour of concrete in fire, including phenomenon of spatting, with respect to the theorical consideration and experimental results. Explosive spatting is caused by the build-up of water vapor pressure in concrete subjected to increasing temperatures. When this pressure exceeds the tensile strength of the concrete over a fire-exposed area, explosive spatting can result in a typical temperature range between $200^{\circ}C\;and\;400^{\circ}C$. The major functions are known to be moisture content, pore pressure, load ratio, and heating regime.
In this study, the experiment conditions for the variation of heat release rate in compartment space were constructed to analyze the effects of fire spread and the operation time of sprinkler in accordance with the heat loss of the sprinkler's heat element. The compartment composed of fire board (width = 0.3 m, height = 0.5 m, length = 3.0 m), are manufactured to measure the temperature distributions in the inner space, the mass loss rate and heat release rate during the experiment of N-heptane pool fire test. Also, the operation time of sprinkler is analyzed with the installation of sprinkler and C-factor using Fire Dynamics Simulator Ver.6 under the experiment conditions. The results show that the operation time of sprinkler, which has RTI $100(m{\cdot}s)^{0.5}$ operating temperature $70^{\circ}C$, is 30 s~60 s for C-factor = 0 and 1, 62 s~92 s for C-factor = 3, and 120 s over for C-factor = 5, respectively.
Polyester/melamine cured coatings had been used for pre-primed coatings and pre-coated metal coatings, because it has good mechanical,chemical properties, and mar resistance. But it has weak points such as stiffness and low formability for making automotive components. Polyester had been synthesized using polycarbonate diol of long alkyl chain which can improve flexibility and formability which is one of the important factors for pre-coated steel sheets (PCM). In this study, strain and tensile strength were examined by the tensile test and formability was examined by the drawing test. Also, Those polyester resins were also measured by DMA to verify flexibility of cured coatings.
Proceedings of the Korean Vacuum Society Conference
/
1999.07a
/
pp.139-139
/
1999
다이아몬드는 지구상에서 가장 단단한 물질로 잘 알려져 있을 뿐만 아니라 공업적 측면에서 볼 때, 여러 가지 특출한 성질들을 동시에 지니고 있다. 인장강도, 압축강도, 탄성계수 등 기계적 특성이 우수하고 넓은 광투과성과 내열, 내화학, 내방사성을 지니고 있으며, 열전도율이 높고 전기적으로 절연체이다. 또한 hole이동도가 높고 도핑에 의해서 반도체적 특성을 나타낸다. 이와 같이 매우 뛰어난 성질을 공업적으로 응용하기 위하여 이전부터 많은 연구가 행해져 왔으며, 1980년대에 들어와 박막이나 코팅 형태로의 합성이 가능한 기상합성법이 큰 발전을 보임으로써 다이아몬드의 우수한 특성을 여러 분야에서 폭넓게 응용할 수 있게 되었다. 특히 마찰 응용분야에 최적의 재료로 추천되고 있다. 지금도 Epitaxial 다이이몬드를 기지 위에 성장시키고 다결정질박막을 여러 가지 비다이아몬드(Si, W, Mo 등) 기지 위에 성장시키는 연구가 계속되고 있으며 공구강 위엥 경질코팅으로써 한층 개선된 다이아몬드박막 제조를 위한 수많은 연구노력들이 집중되고 있다. 그러나 일반탄소강에 다이아몬드박막을 성장시키기 위한 많은 노력들은 크게 바람직하지 않은 non-diamond carbon(black carbon or graphitic soot)의 형성 때문에 방해를 받고 있다. 계면에서 이들의 형성은 증착된 다이아몬드박막과 금속기지의 저조한 밀착력을 나타내게 된다. 이외 같이 다이아몬드박막의 응용을 위하여 다이아몬드피막에 요구되는 중요한 조건은 기지에 대해서 강한 밀착력을 나타내는 것이며, 동시에 상대물에 대하여 낮은 마찰계수를 가져야 한다. 그러나 다이아몬드와 금속기지는 서로 다른 열챙창계수(각각 0.87$\times$10-6K-1, 12$\times$10-6K-1)의 차이로 인하여 밀착력이 현저히 떨어진다는 단점으로 인해 산업화에 많은 제약을 받아왔다. 이러한 문제점을 해결하기 위하여 본 연구에서는 다이아몬드박막과 금속기지 사이에 중간층을 이용하는 방법을 제안하였다. 이러한 시도는 일반적으로 중간층 형성 금속인 Ti 또는 TiN 등이 적용되었으나 원하는 결과를 얻지 못하였다. 즉 carbon과 Fe의 상호확산, non-diamond carbon상의 형성 그리고 열잔류응력을 완화시키고 일반탄소강 위에 다이아몬드박막을 형성시켜 우수한 밀착력을 얻기 위한 목적에 미흡하였던 것이다. 이에 중간층으로 Cr 또는 Cr계 화합물 박막을 이용하였는 바, 이 중간층을 이용한 결과 우수한 밀착력을 나타내는 다이아몬드박막을 얻었으며 열적, 구조저으로 모재와 다이아몬드에 적합한 결과를 얻을 수 있었다. 본 연구에 의해 얻어진 결과들은 재료 가공을 위하여 높은 경도와 내마모성등이 요구되는 절삭공구나 금형의 수명 향항에 크게 기여할 것이며 산업적으로 큰 응용이 기대된다.
The earlier studies on the fire resistance performance of woods used as building materials have focused on confirming combustion characteristics of fire retardant or flame resistant treated wood. In this paper, to confirm internal temperature changes closely related to pyrolysis of woods exposed to the flame, heating experiments were conducted in a heating furnace according to the standard heating temperature curves after Douglas-fir, which is widely used as structural materials, was treated with a flame resistant solution and flame retardant paint. As a result of the experiment, it was confirmed that the thermal diffusion inside the wood has decreased when the wood was treated with the flame resistant solution. However, in high temperature, the flame resistant effect could not be expected due to the peeling of the coating in the case of the flame resistant paint treated wood. Therefore, it can be considered that it is more effective to use the flame resistant solution which penetrates in to the inside of the wood than flame resistant paint which forms the coating on the surface of the wood in order to enhance the flame resistance effect on the thick wood.
Journal of the Korea Academia-Industrial cooperation Society
/
v.20
no.1
/
pp.284-289
/
2019
The Korea Foldable safe pathway system is an evacuation support system to get temporary evacuation route in railway tunnel and large space fires. A prevention smoke screen is unfolded in fires and it is needed to prevent heat and smoke from fire source. Therefore, ventilation system for positive pressure condition is equipped with foldable safe pathway system. Numerical analyses of temperature and pressure distribution with distance from fire source were performed considering fire scenario of new train vehicle. The smoke temperatures did not exceed $200^{\circ}C$ that distance from the fire source was more than 20 m and smoke pressure was reduced with distance from fire source. Maximum smoke pressure was 14 Pa and average pressure was 6 Pa in position of prevention smoke screen. As results, to install foldable safe pathway system, ventilation system is need to maintain 6 Pa positive pressure condition.
Journal of the Korean Recycled Construction Resources Institute
/
v.6
no.4
/
pp.365-372
/
2018
3D printing technology of construction field can be divided into structural materials, interior and exterior finishing materials, and is mainly done by extruding and adapting. Particularly when it is applied as an exterior materials, it is mainly applied to an unstructured exterior materials and high accuracy is required. The exterior materials can be used as a cement composite materials, it is suitable also for a additive type manufacturing, and the role of a redispersible polymer powder is important. But, high temperatures, redispersible polymer cement base material beget dehydration and micro crack of cement matrix. In this research, we developed a EVA, EVCL redispersible polymer cement base material applicable as a 3D printing exterior materials, confirmed density and strength characteristics for application as an exterior materials, a flame retardancy test for improving the fire resistance of buildings and confirmed its possibility. From the test result, developed EVCL redispersible polymer cement mortar showed good stability in high temperatures. These high temperature stability is caused by the ethylene-vinyl chloride binding. Thus, this result indicates that it is possible to fire resistant 3D printing interior and exterior finishing materials.
Currently, fluid transfer steel pipes take a lot of time and expense to maintain all facilities due to new construction and painting or corrosion and aging. Therefore, this study was conducted for designing a CFRP pipe structure with high corrosion resistance and chemical resistance as a substitute for steel pipes. The helical/hoop pattern was cross-laminated to improve durability, and HNT was added to suppress the moisture absorption phenomenon of the epoxy. The HNT/CFRP pipe was manufactured by a filament winding process, and performed a mechanical property test, and a moisture absorption test in distilled water at 70℃. As a result, the highest bending strength was obtained when the hoop pattern was laminated with a thickness equivalent to 0.6% of the pipe. The 0.5 wt% HNT specimen had the highest moisture absorption resistance. Also, the delamination phenomenon at the interlayer interface was delayed, resulting in the lowest strength reduction rate.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.