• Title/Summary/Keyword: 내호

Search Result 5, Processing Time 0.016 seconds

Fatigue Failure Behavior of Pipe Bends with Local Wall-Thinning Under Cyclic Bending Condition (반복굽힘 조건에서 감육 곡관의 피로손상 거동)

  • Yoon, Min-Soo;Kim, Jin-Weon;Kim, Jong-Sung
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.36 no.10
    • /
    • pp.1227-1234
    • /
    • 2012
  • In this study, fatigue tests were carried out using real-scale pipe bend specimens with wall-thinning defects under a cyclic bending load together with a constant internal pressure of 10 MPa. The wall-thinning defect was located at the extrados and the intrados of the pipe bend specimens. A fully reversed cyclic in-plane bending displacement was applied to the specimens. For the pipe bends with wall thinning at the extrados, an axial crack occurred at the crown of the pipe bend rather than at the extrados where the defect was located. In addition, the fatigue life was longer than that of a sound pipe bend predicted from the design fatigue curve in ASME Sec.III, and it was less dependent on the axial length of the wall-thinning defect. For the pipe bends with wall thinning at the intrados, a circumferential crack occurred at the intrados. In this case, the fatigue life was much shorter than that of a sound pipe bend predicted from the design fatigue curve, and it clearly decreased with decreasing axial length of the wall-thinning defect.

Burst Pressure Evaluation for Through-Wall Cracked Tubes in the Steam Generator (관통균열이 존재하는 증기발생기 전열관의 파열압력 평가)

  • Kim, Hyun-Su;Kim, Jong-Sung;Jin, Tae-Eun;Kim, Hong-Deok;Chung, Han-Sup
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.28 no.7
    • /
    • pp.1006-1013
    • /
    • 2004
  • Operating experience of steam generators shows that the tubes are degraded by stress corrosion cracking, fretting wear and so on. These defected tubes could stay in service if it is proved that the tubes have sufficient structural margin to preclude the risk of tube bursting. This paper provides detailed plastic limit pressure solutions for through-wall cracks in the steam generator tubes. These are developed based on three dimensional(3D) finite element analyses assuming elastic-perfectly plastic material behavior. Both axial and circumferential through-wall cracks in free span and in u-bend regions are considered. The resulting limit pressure solutions are given in a polynomial form, and thus can be simply used in practical integrity assessment of the steam generator tubes.

A Study on Failure Mode of Pipe Elbows with Wall Thinning (두께 감소된 배관 엘보우의 파손 모드에 대한 연구)

  • Shin, Kyu-In;Yoon, Kee-Bong
    • Journal of the Korean Institute of Gas
    • /
    • v.12 no.2
    • /
    • pp.57-62
    • /
    • 2008
  • Difference of failure modes was studied by finite element analysis for elbows with local wall thinning area particularly at inner surface of intrados of the elbow. Longitudinal wall thinning length, minimum thickness were kept constant but circumferential wall thinning width was varied to get $90^{\circ}$, $180^{\circ}$ and $360^{\circ}$ thinning width. Elastic-plastic analysis were carried out under the combined loading conditions of internal pressure and in-plane bending moment closing the elbow. Von Mises stress were obtained from the outer surface central surface location in intrados, extrados and crown parts in elbow. The results showed that the plastic deformation and failure started from the crown location when the thinning width small ($90{\sim}180^{\circ}$). However, plastic collapse started from the intrados location when the thinning width is approaching $360^{\circ}C$. This should be reflected to assess structural integrity of elbows after wall thinning measurement is made.

  • PDF

Estimation of Tensile Properties of Pipe Bends Manufactured by Cold-Bending (냉간 굽힘 가공된 곡관의 인장물성치 예측)

  • Kim, Jin-Weon;Lee, Mi-Yeon;Lee, Sa-Yong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.36 no.9
    • /
    • pp.1059-1064
    • /
    • 2012
  • In this study, tensile tests were performed on specimens that simulated the cold-bending and heat-treatment of pipe bends to understand the mechanical properties of pipe bends manufactured by cold-bending followed by heat-treatment for relieving residual stress. The strength and ductility of cold-worked materials were respectively found to be higher and lower than those of the parent material although heat-treatment was carried out to relieve residual stress. In addition, the increase in strength and decrease in ductility were proportional to the applied strain levels for cold-working. It was thus inferred that the intrados and extrados regions of pipe bends that were cold-bended and heat-treated show higher strength and lower ductility compared to the parent straight pipe and that the mechanical properties at the crown region are nearly the same as those of the parent straight pipe.

Material Characteristics of Gold Artifacts of Sarira Reliquary inside Stone Pagoda of Mireuksa Temple Site (미륵사지 석탑 출토 사리장엄 금제유물의 재료학적 특성)

  • Kwon, Hyuk-nam;Yoo, Dong-wan;Lee, Jang-jon;Han, Min-su
    • Korean Journal of Heritage: History & Science
    • /
    • v.47 no.4
    • /
    • pp.210-223
    • /
    • 2014
  • When sarira reliquary was found in stone pagoda of Mireuksa Temple, there were 494 gold artifacts, including inner gold pot, gold plate with inscription for Sarira enshrinement, etc. Most of gold artifacts were crafted, but there were 22 gold plates and 4 gold ingots, which did not have any specific shape. It was considered that they had not been crafted. Since gold exists as a metal rather than a metallic oxide in nature, in general, it can be crafted by melting and shaping. However, gold in nature has impurities so it has to be refined to have malleability. The characteristic features were identified through the analysis of gold artifacts from sarira reliquary found in stone pagoda of Mireuksa Temple. The analysis result showed that there were 3 types of gold; pure gold artifacts, artifacts produced with silver containing gold and natural gold ingots. Inner gold pot, gold earrings and gold small beads were produced with pure gold and they contained less than 1wt.% of copper. It seemed like they were produced as pure gold to be shaped by hammering. Gold plate with inscription, tweezers, gold earrings, ingots, etc. were produced with silver containing gold as they had to be more solid. Gold ingots seemed to be natural gold considering the distribution of silver and copper in them, but it cannot be concluded as there are not enough information on gold ingots in Korea. The comprehensive research on gold ingots from various regions in Korea has to be carried out to confirm the above. Sarira Reliquary showed the very sophisticated gold craftsmanship. Gold ingots with the inscriptions, which say 1 nyang, were approximately 14g. Considering the weight of these ingots as standard, weights of other ingots were half nyang(7g), 2 nyang(28g), etc.