• Title/Summary/Keyword: 기계적 합금화

Search Result 373, Processing Time 0.029 seconds

Characteristic of Mechanical Clinching for Al5052 to High-Strength Steels (Al5052 합금소재와 고장력강판의 이종재료 클린칭 접합특성)

  • Lee, Chan-Joo;Lee, Sang-Kon;Lee, Seon-Bong;Kim, Byung-Min
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.34 no.8
    • /
    • pp.997-1006
    • /
    • 2010
  • For manufacturing modern cars, so-called multi-materials, such as aluminum alloy with high-strength steels, are used. For obtaining such materials, a new joining method is required to achieve the multi-material design. Mechanical clinching is one of joining methods used to join the dissimilar materials. The objective of this study is to investigate the characteristics of mechanical clinching of Al5052 alloy to high-strength steels (SPFC440, 590, 780). Using FE-analysis and clinching experiment, the joinability of Al5052 alloy to high-strength steel is evaluated by geometrical shape of mechanical clinched joint, such as neck-thickness and undercut. Further, the joint strength is evaluated by performing a single-lap shear test. The upper high-strength steel SPFC780 was not clinched because of the necking of the upper sheet. The joint strength increased with increasing strength of the upper sheet. For the lower high-strength steel sheet, the joinability and joint strength decreased with increasing strength of the lower sheet.

Effect of V and Nb on Mechanical Properties of Non-Heattreated Hot Forging Steels (열간단조용 비조질강의 기계적 성질에 미치는 V, Nb의 영향)

  • Wee, Kyeom-Bok;Jeong, Woon-Tae;Lee, Kyeong-Seop;Wang, Seong-Do
    • Korean Journal of Materials Research
    • /
    • v.2 no.1
    • /
    • pp.65-75
    • /
    • 1992
  • 0.4wt%C steel added with V and/or Nb were forged and followed by air cooling. The structure-property relationships were examined and multiple regression analysis was conducted to quantify the magnitudes of effects of microalloying elements on the properties of the steels. All material's tensile strength are greater than $70kg/\textrm{mm}^2$, so they are equal to or superior to Q/T material's(S45C). Their impact energies are less than 40J, so they are 50% of Q/T material's. Increasing the content of V from 0.10 to 0.15 wt% had brought improvement in UTS about 20% but with some sacrifice of impact energy. These were the results from the precipitation strengthening by fine dispersion of VC in ferrite, increment of pearlite volume fraction and decrement of pearlite interlamellar spacings. However, increasing the content of Nb from 0.05 to 0.l0wt % slightly improved UTS and impact energy. NbC precipitates were more effective in suppression of austenite grain coarsening than VC precipitates. Combined additions of V+Nb were more effective to bring impact toughness than sole addition. Optimum combination of strength and toughness was accomplished wish 0.4C-1. 19Mn-0.05S-0.12V-0.07Nb steel.

  • PDF

High Temperature Oxidation Behavior of Fe-14Cr Ferritic Oxide Dispersion Strengthened Steels Manufactured by Mechanical Alloying Process (기계적 합금화 공정으로 제조된 Fe-14Cr Ferritic 산화물 분산 강화(ODS) 합금 강의 고온 산화 거동)

  • Kim, Young-Kyun;Park, Jong-Kwan;Kim, Hwi-Jun;Kong, Man-Sik;Lee, Kee-Ahn
    • Journal of Powder Materials
    • /
    • v.24 no.2
    • /
    • pp.133-140
    • /
    • 2017
  • This study investigates the oxidation properties of Fe-14Cr ferritic oxide-dispersion-strengthened (ODS) steel at various high temperatures (900, 1000, and $1100^{\circ}C$ for 24 h). The initial microstructure shows that no clear structural change occurs even under high-temperature heat treatment, and the average measured grain size is 0.4 and $1.1{\mu}m$ for the as-fabricated and heat-treated specimens, respectively. Y-Ti-O nanoclusters 10-50 nm in size are observed. High-temperature oxidation results show that the weight increases by 0.27 and $0.29mg/cm^2$ for the as-fabricated and heat-treated ($900^{\circ}C$) specimens, and by 0.47 and $0.50mg/cm^2$ for the as-fabricated and heat-treated ($1000^{\circ}C$) specimens, respectively. Further, after 24 h oxidation tests, the weight increases by 56.50 and $100.60mg/cm^2$ for the as-fabricated and heat-treated ($1100^{\circ}C$) specimens, respectively; the latter increase is approximately 100 times higher than that at $1000^{\circ}C$. Observation of the surface after the oxidation test shows that $Cr_2O_3$ is the main oxide on a specimen tested at $1000^{\circ}C$, whereas $Fe_2O_3$ and $Fe_3O_4$ phases also form on a specimen tested at $1100^{\circ}C$, where the weight increases rapidly. The high-temperature oxidation behavior of Fe-14Cr ODS steel is confirmed to be dominated by changes in the $Cr_2O_3$ layer and generation of Fe-based oxides through evaporation.

Material Life Cycle Assessment on Mg2NiHx-5 wt% CaO Hydrogen Storage Composites (Mg2NiHx-5 wt% CaO 수소 저장 복합재료의 물질전과정평가)

  • Shin, Hyo-Won;Hwang, June-Hyeon;Kim, Eun-A;Hong, Tae-Whan
    • Clean Technology
    • /
    • v.27 no.2
    • /
    • pp.107-114
    • /
    • 2021
  • Material Life Cycle Assessment (MLCA) was performed to analyze the environmental impact characteristics of the Mg2NiHx-5 wt% CaO hydrogen storage composites' manufacturing process. The MLCA was carried out by Gabi software. It was based on Eco-Indicator 99' (EI99) and CML 2001 methodology. The Mg2NiHx-5 wt% CaO composites were synthesized by Hydrogen Induced Mechanical Alloying (HIMA). The metallurgical, thermochemical characteristics of the composites were analyzed by using X-ray diffraction (XRD), scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), specific surface area analysis (Bruner-Emmett-Teller, BET), and thermogravimetric analysis (TGA). As a result of the CML 2001 methodology, the environmental impact was 78% for Global Warming Potential (GWP) and 22% for Eutrophication Potential (ETP). In addition, as a result of applying the EI 99' methodology, the acidification was the highest at 43%, and the ecotoxicity was 31%. Accordingly, the amount of electricity used in the manufacturing process may have an absolute effect on environmental pollution. Also, it is judged that the leading cause of Mg2NiHx-5 wt% CaO is the addition of CaO. Ultimately, it is necessary to research environmental factors by optimizing the process, shortening the manufacturing process time, and exploring eco-friendly alternative materials.

Microelectromechnical system 소자를 위한 박막형 2차 전지용 TEX>$SnO_2$ 음극 박막의 충, 방전 특성 평가

  • 윤영수;전은정;신영화;남상철;조원일
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 1999.07a
    • /
    • pp.50-50
    • /
    • 1999
  • 마이크로 공정을 이용한 초소형 정밀 기계는 공정 기술과 재료 기술의 발전에 의하여 더욱 소형화되고 있으며 특히 기능을 갖는 부분과 이 부분을 제어하는 주변회로의 on-chip화의 요구가 증가되기 시작하였다. 이와 같은 추세에 있어서의 문제점은 초소형 정밀기계 부품 소자의 구동을 위한 에너지원의 개발이다. 즉, 소자의 크기가 작아진 것에 부합되는 초소형의 전지가 필요하게 된 것이다. 따라서 보다 완전한 초소형 정밀 기계 및 마이크로 소자의 구현을 위하여 마이크로 소자와 혼성 (Hybrid) 되어 이용될 수 있는 고성능 및 초소형의 전지의 개발이 필수적이다. 초소형 전지의 구현을 위하여 Li계의 2차 전지를 선택하여 이를 박막화하고 반도체 공정을 도입할 수 있다. 이러한 전지를 박막형 2차 전지 또는 박막형 마이크로 전지(thin film Secondary Battery : TFSB or Thin Film Micro-Battery : TFMB)라 하며 이러한 2차 전지는 일반적인 벌크 전지와 동일하게 cathode/Electolyte/Anode의 구조를 갖는다. 박막의 특성상 전해질은 고상의 물질을 사용하는 것이 벌크형 2차 전지와 다른 점이다. TFSB의 성능은 주로 cathode에 의하여 결정되며 지금까지 많은 cathode 물질에 대한 연구 보고가 발표되고 있다. 반도체 공정을 이용한 TFMB의 제작시 무엇보다 중요한 점은 우수한 고상 전해질 및 anode 물질의 선택에 있다. 최근에 2차 전지를 위한 carbon계 anode를 대체할 수 있는 SnO에 대한 보고가 있는데 이는 한 개의 Sn 원자당 2개 이사의 Li가 반응하여 높은 용량을 갖는 전지의 제작이 가능하기 때문이다. Sno2의 anode는 매우 높은 충전용량을 갖는데 첫 번째 방전시에 Li2O를 생성하여 비가역적 반응을 나타내고 계속되는 충방전 동안 Li-Sn 합금이 생성되어 2차전지의 가역적 반응을 가능하게 한다. SnO2 는 대기중에서 Li 금속보다 안정하기 때문에 전지의 제작 공정 및 사용 면에서 매우 우수한 물질이지만 아직까지 SnO2 구조적 특성과 전지의 충, 방전 특성에 대한 관계의 규명을 위한 정확한 정설은 제시되고 있지 못하다. 본 연구에서는 TFSB anode 물질로써 SnOx박막을 상온에서 여러 전도성 콜렉터 위에 증착하여 그 충, 방전 특성을 보고하였다. 증착된 SnOx박막의 표면은 SEM, AFM으로 분석하였으며 구조의 분석은 XR와 Auger electron spectroscope로 하였다. 충, 방전 특성을 분석하기 위하여 리늄 foil을 대극과 참조 전극으로 하여 EC:DMC=1:1, 1M LiPF6 액체 전해질을 사용한 Half-Cell를 구성하여 100회 이상의 정전류 충, 방전 시험을 행하였다. Half-Cell test 결과 박막의 구조, 콜렉터의 종류 및 Sn/O비에 따라 서로 다른 충, 방전 거동을 나타내었다.

  • PDF

Solidification Process of a Binary Mixture with Anisotropy of the Mushy Region (머시영역의 비등방성을 고려한 2성분혼합물의 응고과정)

  • 유호선
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.17 no.1
    • /
    • pp.162-171
    • /
    • 1993
  • This paper deals with the anisotropy of the mushy region during solidification process of a binary mixture. A theoretical model which specifies a permeability tensor in terms of pricipal values is proposed. Also, the governing equations are modified into convenient forms for the numerical analysis with the existing algorithm. Some test computations are performed for soeidification of aqueous ammonium chloride solution contained in a square cavity. Results show that not only the present model is capable of resolving fundamental characteristics of the tranport phenomena, but also the anisotropy significantly affects the interdendritic flow structure, i.e., double-diffusive convection and macrosegregation patterns.

Thermal and Mechanical Properties of Rapidly Solidified Zr-Ni-Cu-Al-Ti Alloy (급냉응고법으로 제조한 Zr-Ni-Cu-Al-Ti 합금의 열적, 기계적 성질)

  • Choe, Ik-Seok;Han, Tae-Gyo;Ji, Yong-Gwon;Im, Byeong-Mun;Kim, Yeong-Hwan;Kim, In-Bae
    • Korean Journal of Materials Research
    • /
    • v.11 no.3
    • /
    • pp.171-177
    • /
    • 2001
  • The thermal and mechanical properties of amorphous Z $r_{62-x}$N $i_{10}$C $u_{20}$A $l_{8}$ $Ti_{x}$ (x=3, 6, 9at%) alloys were investigated. The crystallization process was confirmed as amorphous longrightarrow amorphous + Z $r_2$A $l_3$+ Zr + (Ni,Ti) longrightarrow Z $r_2$Cu + Al + (Ni,Ti) for 3at%Ti, amorphous longrightarrow amorphous + Al longrightarrow $Al_2$Ti + NiZr + CuTi for 6at%Ti and amorphous longrightarrow amorphous + Zr + Al longrightarrow Zr + $Al_2$Zr + Al $Ti_3$+ CuTi for 9at%Ti. lickers hardness ( $H_{v}$ ) increased with increasing volume fraction( $V_{f}$ ) of pricipitates for all concerned compositions. Tensile fracture strength ($\sigma_{f}$ ) showed a maximum value 1219MPa at $V_{f}$ = 38% for 3at%Ti, 1203MPa at $V_{f}$ = 2% for 6at%Ti and 1350MPa at $V_{f}$ = 5% for 9at%Ti. The $\sigma_{f}$ was rapidly decreased after showing the maximum value. The $V_{f}$ corresponding to rapidly decreased $\sigma_{f}$ coincided with the $V_{f}$ transited from ductile to brittle fracture surface.ace.

  • PDF

Enhanced Mechanical Properties and Thermal Stability of CrAlN Coatings by Interlayer Deposition (중간층 증착에 의한 CrAlN 코팅의 기계적 물성 및 내열성 향상에 관한 연구)

  • Kim, Hoe-Geun;Ra, Jeong-Hyeon;Song, Myeon-Gyu;Lee, Sang-Yul
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.100-100
    • /
    • 2016
  • 물리기상증착방법 (Physical vapor deposition)에 의하여 합성된 천이금속 질화물 박막은 경도, 내마모성 등 절삭공구의 성능을 향상시키며, Ti-Al-N, Ti-Zr-N, Zr-Al-N, Cr-Si-N 등의 3원계 경질 박막에 대한 연구가 지속적으로 이루어지고 있다. 이중에서도 CrAlN 코팅은 높은 경도, 낮은 표면 조도 등의 우수한 기계적 특성 이외에 고온에서 안정한 합금상 형성으로 인하여 우수한 내열성을 보유하여 공구 코팅으로의 적용 가능성이 크다. 그러나 최근 공구사용 환경의 가혹화로 인하여 코팅의 내마모성 및 내열성 등의 물성 향상을 통한 공구의 수명 향상이 필요시 되고 있으며, 코팅에 적합한 중간층을 합성함으로써 공구 코팅으로의 적용 가능성을 높이는 연구들이 진행되고 있다. 본 연구에서는 CrAlN 코팅의 물성을 향상시키기 위해 CrAlN 코팅과 WC-Co 6wt.% 모재 사이에 CrN, CrZrN, CrN/CrZrSiN 등의 다양한 중간층을 합성하였으며, 중간층을 포함한 모든 코팅의 두께는 $3{\mu}m$ 로 제어하였다. 합성된 코팅의 미세조직, 경도 및 탄성계수, 내모성을 분석하기 위해 field emission scanning electron microscopy(FE-SEM), nano-indentation, ball-on-disk 마모시험기 및 ${\alpha}-step$을 사용하였다. 코팅의 내열성을 확인하기 위해 코팅을 furnace에 넣어 공기중에서 500, 600, 700, 800, 900, $1,000^{\circ}C$로 30분 동안 annealing 한 후에 nano-indentation을 사용하여 경도를 측정하였다. CrAlN 코팅을 나노 인덴테이션으로 분석한 결과, 모든 코팅의 경도(35.5-36.2 GPa)와 탄성계수(424.3-429.2 GPa)는 중간층의 종류에 상관없이 비슷한 값을 보인 것으로 확인됐다. 그러나, 코팅의 마찰계수는 중간층의 종류에 따라 다른 값을 보였으며, CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅의 마찰계수는 0.34로 CrZrN 중간층을 증착한 CrAlN 코팅의 마찰계수(0.41)에 비해 낮은 값을 보였다. 또한, 코팅의 마모율 및 마모폭도 비슷한 경향을 보인 것으로 보아, CrN/CrZrSiN 중간층을 합성한 CrAlN 코팅의 내마모성이 상대적으로 우수한 것으로 판단된다. 이것은 중간층의 H/E ratio가 코팅의 내마모성에 미치는 영향에 의한 결과로 사료된다. H/E ratio는 파단시의 최대 탄성 변형율로써, 모재/중간층/코팅의 H/E ratio 구배에 따라 코팅 내의 응력의 완화 정도가 변하게 된다. WC 모재 (H/E=0.040)와 CrAlN 코팅(H/E=0.089) 사이에서 CrN, CrZrSiN 중간층의 H/E ratio 는 각각 0.076, 0.083 으로 모재/중간층/코팅의 H/E ratio 구배가 점차 증가함을 확인 할 수 있었고, 일정 응력이 지속적으로 가해지면서 진행되는 마모시험중에 CrN과 CrZrSiN 중간층이 WC와 CrAlN 코팅 사이에서 코팅 내부의 응력구배를 완화시키는 역할을 함으로써 CrAlN 코팅의 내마모성이 향상된 것으로 판단된다. 모든 코팅을 열처리 후 경도 분석결과, CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅은 $1,000^{\circ}C$까지 약 28GPa의 높은 경도를 유지한 것으로 확인 되었고, 이는 CrZrSiN 중간층 내에 존재하는 $SiN_x$ 비정질상의 우수한 내산화성에 의한 결과로 판단된다.

  • PDF

Fabrication and densification of magnetic α-Fe/Al2O3 nanocomposite by mechanical alloying (기계적합금화에 의한 α-Fe/Al2O3 자성 나노복합재료의 제조 및 치밀화)

  • Lee, Chung-Hyo;Kim, Han-Woong
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.23 no.6
    • /
    • pp.314-319
    • /
    • 2013
  • Fabrication of nanocomposite material for the $Fe_2O_3-Al$ system by mechanical alloying (MA) has been investigated at room temperature. It is found that ${\alpha}-Fe/Al_2O_3$ nanocomposite powders in which $Al_2O_3$ is dispersed in ${\alpha}-Fe$ matrix are obtained by mechanical alloying of $Fe_2O_3$ with Al for 5 hours. The change in magnetization and coercivity also reflects the details of the solid state reduction process of hematite by pure metal of Al during mechanical alloying. Densification of the MA powders was performed in a spark plasma sintering (SPS) machine using graphite dies at $1000^{\circ}C$ and $1100^{\circ}C$ under 60 MPa. Shrinkage change after SPS of MA'ed sample for 5 hrs was significant above $700^{\circ}C$ and gradually increased with increasing temperature up to $1100^{\circ}C$. X-ray diffraction result shows that the average grain size of ${\alpha}-Fe$ in ${\alpha}-Fe/Al_2O_3$ nanocomposite sintered at $1100^{\circ}C$ is in the range of 180 nm. It can be also seen that the coercivity (Hc) of SPS sample sintered at $1000^{\circ}C$ is still high value of 88 Oe, suggesting that the grain growth of magnetic ${\alpha}-Fe$ phase during SPS process tend to be suppressed.

Particle Refinement and Nano-structure Formation of Gas Atomized Al-14wt.%Ni-14 wt.%Mm Alloy Powder by Mechanical Milling (가스 분사된 Al-14wt.%Ni-14wt.%Mm 합금 분말의 기계적 밀링에 의한 입자 미세화와 나노조직 형성)

  • 홍순직;이윤석;천병선
    • Journal of Powder Materials
    • /
    • v.10 no.1
    • /
    • pp.26-33
    • /
    • 2003
  • Al-l4wt.%Ni-l4wt.% Mm(Mm=misch metal) alloy powders rapidly solidified by the gas atomization method were subjected to mechanical milling(MM). The morphology, microstructure and hardness of the powders were investigated as a function of milling time using scanning electron microscopy(SEM), transmission electron microscopy(TEM) and Vickers microhardness tester. Microstructural evolution in gas-atomized Al-l4wt.%Ni-l4wt.% Mm(Mm=misch metal) alloy powders was studied during mechanical milling. It was noted that the as-solidified particle size of $200\mutextrm{m}$ decreases during the first 48 hours and then increases up to 72 hours of milling due to cold bonding and subsequently there was continuous refinement to $20\mutextrm{m}$ on milling to 200 hours. Two microstructurally different zones, Zone A, which is fine microstructure area and Zone B, which has the structure of the as-solidified powder, were observed. The average thickness of the Zone A layer increased from about 10 to $15\mutextrm{m}$ in the powder milled for 24 hours. Increasing the milling time to 72 hours resulted in the formation of a thicker and more uniform Zone A layer, whose thickness increased to about $30~50\mutextrm{m}$. The TEM micrograph of ball milled powder for 200 hours shows formation of nano-particles, less than 20 nm in size, embedded in an Al matrix.