Air Content, Workability and Bleeding Characteristics of Fresh Lightweight Aggregate Concrete (굳지 않은 경량골재 콘크리트의 공기량, 유동성 및 블리딩 특성)

  • Sim, Jae-Il;Yang, Keun-Hyeok
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.4
    • /
    • pp.559-566
    • /
    • 2010
  • Fifteen lightweight concrete mixes were tested to evaluate the effect of maximum size of coarse aggregate and the replacement level of natural sand on the various properties of fresh lightweight concrete. The different properties, such as water absorption against the elapsed time, pore size distribution and micro-structure of lightweight aggregates used, influencing on the workability of fresh concrete were also measured. Test results showed that the initial slump of lightweight concrete decreased with the increase of the replacement level of natural sand. The slump of all-lightweight concrete sharply decreased by around 80% of the initial slump after 30~60 minutes. The air content and bleeding rate of lightweight concrete were significantly affected by the replacement level of natural sand as well as the maximum size of coarse aggregates. Empirical equations recommended in ACI 211 and Korea concrete standard specifications underestimated the air content of the lightweight concrete, indicating that the underestimation increases with the decrease of the replacement level of natural sand. In addition, equations to predict the air content and bleeding rate of lightweight concrete were proposed based on the test results.

ALGORITHMS FOR AGGREGATE INTERLOCK CONSTITUTIVE BEHAVIOR AT R/C CRACKS (철근콘크리트 균열에서의 골재맞물림 거동에 대한 해석연구)

  • 최기봉;황철성
    • Magazine of the Korea Concrete Institute
    • /
    • v.1 no.2
    • /
    • pp.113-120
    • /
    • 1989
  • 이 논문에서는 철근콘크리트 균열에서의 활동전단변형에대해 골재맞물림에 따라 수반되는 저항응력을 예측할 수 있는 해석방법들이 개발되어졌다. 이러한 방법들은 거의 정확하게 실험결과들을 예측하였으며 초기 균열폭, 콘크리트 압축강도, 최대 골재크기, 그리고 균열틈에 따라 수반되는 구속력에 의해 영향을 받는 골재맞물림 거동에 대한 해석연구를 위해 사용되어졌다.

Fundamental Properties of Porous Concrete According to the Sizes of Aggregate (골재 크기에 따른 포러스콘크리트의 기초물성에 관한 실험적 연구)

  • 김무한;백용관;강석표;김용로;김재환
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.5
    • /
    • pp.438-446
    • /
    • 2001
  • Recently, porous concrete has been used for the purpose of decreasing the load of earth environment. It consists solely of cement, water and uniform-sized coarse aggregate. And its fundamental properties will be considerably affected by the physical properties of aggregate because the aggregate occupies for the most part in its mix proportion. For such a reason, this study was carried out to investigate the influence of the sizes and kinds of aggregate for the fundamental properties of porous concrete. It showed that the fundamental properties of porous concrete were the similar value in all sizes of aggregate except in the case of using the 2.5∼5㎜ aggregate and were varied according to the kinds of aggregate. In particular, compressive strength of porous concrete using 2.5∼5㎜ aggregate was more higher than that using other aggregate, and its void ratio and coefficient of permeability was lower. And the maintenance capacity of permeability of porous concrete was varied by the sizes and the kinds of aggregate. In particular, it was greatly decreased in case of using the 2.5∼5㎜ aggregate. And unlike dynamic modulus of elasticity of ordinary concrete, that of porous concrete was very high value in early ages and was slowly increased after that time.

Influence of Specimen Geometries on the Compressive Strength of Lightweight Aggregate Concrete (경량골재 콘크리트의 압축강도에 대한 시험체 기하학적 특성의 영향)

  • Sim, Jae-Il;Yang, Keun-Hyeok
    • Journal of the Korea Concrete Institute
    • /
    • v.24 no.3
    • /
    • pp.333-340
    • /
    • 2012
  • The current study prepared 9 laboratorial concrete mixes and 3 ready-mixed concrete batches to examine the size and shape effects in compression failure of lightweight aggregate concrete (LWC). The concrete mixes were classified into three groups: normal-weight, all-lightweight and sand-lightweight concrete groups. For each concrete mix, the aspect ratio of circular or square specimens was 1.0 and 2.0. The lateral dimension of specimens varied between 50 and 150 mm for each laboratorial concrete mix, whereas it ranged from 50 to 400 mm with an incremental variation of 50 mm for each ready-mixed concrete batch. Test observations revealed that the crack propagation and width of the localized failure zone developed in lightweight concrete specimens were considerably different than those of normal-weight concrete (NWC). In LWC specimens, the cracks mainly passed through the coarse aggregate particles and the crack distribution performance was very poor. As a result, a stronger size effect was developed in LWC than in NWC. Especially, this trend was more notable in specimens with aspect ratio of 2.0 than in specimens with that of 1.0. The prediction model derived by Kim et al. overestimated the size effect of LWC when lateral dimension of specimen is above 150 mm. On the other hand, the modification factors specified in ASTM and CEB-FIP provisions, which are used to compensate for the shape effect of specimen on compressive strength, were still conservative in LWC.

Effects of Aggregate Size and Steel Fiber Volume Fraction on Compressive Behaviors of High-Strength Concrete (골재크기 및 섬유혼입률에 따른 강섬유 보강 고강도 콘크리트의 압축거동)

  • Ahn, Kyung-Lim;Jang, Seok-Joon;Jang, Sang-Hyeok;Yun, Hyun-Do
    • Journal of the Korea Concrete Institute
    • /
    • v.27 no.3
    • /
    • pp.229-236
    • /
    • 2015
  • This paper describes the effect of aggregate size on compressive behavior of high-strength steel fiber reinforced concrete. The Specified compression strength is 60 MPa and the range of fiber volume fraction is 0~2%. The main variable is the aggregate size, which was used for the aggregate size of 8 and 20 mm. So, ten concrete mixtures were prepared and tested to evaluate the fresh and hardened properties of SFRC at curing ages (7, 14, 28, 56 and 91 days), respectively. Items estimated in this study are the fresh properties (air contents, slump), hardened properties (compressive strength, modulus of elasticity, post-peak response and compressive toughness). As a result, the aggregate size has little effect on the compressive strength and modulus of elasticity. On the other hand, the ductile behavior was shown after post peak and the compressive toughness was increasing as decreasing the aggregate size. These effects are clearly represented in the fiber volume fraction 2%, which are the point appeared fiber ball. It is considered that the decreasing the aggregate size has effect on the fiber dispersibility.

Effect of a Aggregate Moisture Content on Aggregate Gradation Analysis (비 절건상태 골재의 함수비가 골재입도분석 결과에 미치는 영향)

  • Kim, Nam-ho;Ji, Hyeong-jun;Yang, Hong-seok;Jeon, Sun-je
    • Journal of Practical Engineering Education
    • /
    • v.13 no.3
    • /
    • pp.559-566
    • /
    • 2021
  • The aggregate gradation analysis is a study that evaluates the accuracy of a specific purpose for the aggregate gradation analysis results essential for construction-related major education. This study is to evaluate the effect of aggregate moisture content on aggregate gradation analysis. The change in the moisture content of the aggregate stored in the asphalt plant cold bin and stock piles was monitored for one year, and based on the results, a sample of aggregate with different moisture content was produced. The gradation curve for each aggregate sample was analyzed to evaluate the effect of aggregate moisture content on aggregate gradation analysis. As a result of the gradation evaluation, it was confirmed that as the moisture content increased, the particle size error for particles less than 5 mm increased in the gradation analysis of the oven-dried aggregate, and this error increased as the particle size decreased. In addition, for aggregate particles of 5 mm or more, it was confirmed that the error in gradation analysis rapidly decreased due to the increase in the moisture content. An analysis was performed on the effect of the error in gradation analysis on the management of hot-bin aggregates in asphalt plants. As a result of the analysis, it was found that the minimum aggregate size of the first hot-bin in a general asphalt plant was 2.38 mm or more, so the maximum gradation error due to the non oven-dry aggregate was less than 2%. Therefore, it seems possible to use the results of the gradation analysis of cold bin non oven-dry aggregate for quality management of asphalt mixture production.

Mechanical Properties of Lightweight Aggregate Concrete according to the Substitution Rate of Natural Sand and Maximum Aggregate Size (천연모래 치환율과 경량 굵은 골재 최대 크기에 따른 경량 골재 콘크리트의 역학적 특성)

  • Sim, Jae-Il;Yang, Keun-Hyeok
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.5
    • /
    • pp.551-558
    • /
    • 2011
  • The effect of the maximum aggregate size and substitution rate of natural sand on the mechanical properties of concrete is evaluated using 15 lightweight aggregate concrete mixes. For mechanical properties of concrete, compressive strength increase with respect to age, tensile resistance, elastic modulus, rupture modulus, and stress-strain relationship were measured. The experimental data were compared with the design equations specified in ACI 318-08, EC2, and/or CEB-FIP code provisions and empirical equations proposed by Slate et al., Yang et al., and Wang et al. The test results showed that compressive strength of lightweight concrete decreased with increase in maximum aggregate size and amount of lightweight fine aggregates. The parameters to predict the compressive strength development could be empirically formulated as a function of specific gravity of coarse aggregates and substitution rate of natural sand. The measured rupture modulus and tensile strength of concrete were commonly less than the prediction values obtained from code provisions or empirical equations, which can be attributed to the tensile resistance of lightweight aggregate concrete being significantly affected by its density as well as compressive strength.

Study on the Properties of Porous Concrete According to the Aggregate Shape and Size (골재 입형 및 크기에 따른 포러스 콘크리트의 특성에 관한 연구)

  • Lim, Seo-Hyung;Kang, Hyun-Sik;Jee, Nam-Yong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.9 no.3
    • /
    • pp.93-100
    • /
    • 2005
  • The purpose of this study is to investigate the physical properties of porous concrete according to the aggregate shape and size which is produced by con crusher and impact crusher. For this purpose, the selected test variables were the aggregate size and shape, the ratio of water to cement and the ratio of paste to aggregate. The results of this study showed that its economic performance and physical properties were improved using the aggregate made by impact crusher. The coefficient of permeability and compressive strength of porous concrete had a close correlationship with the void ratio, and it was suggested as a function of void ratio.

An Analysis of the Shear Strength of Reinforced Concrete Beams with Recycled Coarse Aggregates (순환굵은골재 철근 콘크리트 보의 전단강도 분석)

  • Ji, Sang-Kyu;Yun, Hyun-Do;Song, Seon-Hwa;Choi, Ki-Sun;You, Young-Chan;Kim, Keung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.11a
    • /
    • pp.851-854
    • /
    • 2008
  • Using the recycled aggregate not only saves landfill space but also reduces the demand for extraction of natural raw material for new construction activity. However few investigations have been carried out to study the shear behaviors of RC beams with recycled aggregates such as low absorption of recycled aggregate and full-scale specimens. In this study, six reinforced concrete beams were tested to evaluate the effects of shear strength, and shear behavior on the replacement level (0, 30, 60, and 100%) of recycled coarse aggregate and different amounts of shear reinforcement. The results showed that the beams with recycled coarse aggregates present the similar shear strength and deflections as the beam with natural aggregate on an equal amount of shear reinforcement. the reinforced concrete beams with recycled coarse aggregates present the Influence of shear span-to-depth ratio, effective depth, tension reinforcement ratio and compressive strength as the beams with natural aggregate. Shear strength were compared with the provisions in current code (KCI2007) and the equation proposed by Zsutty. The KCI equations were conservative and subsequently can be used for the shear design of recycled aggregate concrete beam.

  • PDF

Fine Aggregates Size Effect on Rheological Behavior of Mortar (잔골재 입자 크기에 따른 모르타르의 레올로지 거동 특성)

  • Lee, Jin Hyun;Kim, Jae Hong;Kim, Myeong Kyu
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.16 no.8
    • /
    • pp.5636-5645
    • /
    • 2015
  • Physical characteristics of aggregates affect the workability and strength of mortar and concrete, which include their fineness ratio, particle size distribution and water absorption. The workability of construction materials decreases if the incorporated fine aggregates show improper size distribution of their particles. This study shows the particle size effect on the rheological behavior of mortar and provides basic information for evaluating its workability. A mini-slump flow test was adopted to evaluate the workability of mortar. In addition, its plastic viscosity and yield stress were measured using a rheometer for building materials. The sand samples were prepared by sieving river sand and sorting out with their particle sizes. As a result, it was observed that the fines less than 0.7 mm increases the yield stress and plastic viscosity of the mortar samples. If the fines are less than 0.34 mm, the water absorption of the fines dominates change on the workability.