Charcoal Properties and Temperature Change of a Kiln's Inner and Outer Walls in Carbonization Process Using an Improved Kiln (개량형탄화로를 이용한 제탄과정 중 탄화로 내·외벽 온도변화 및 목탄 특성)

  • Kwon, Gu-Joong;Kwon, Sung-Min;Jang, Jae-Hyuk;Hwang, Won-Joung;Kim, Nam-Hun
    • Journal of the Korean Wood Science and Technology
    • /
    • v.39 no.3
    • /
    • pp.230-237
    • /
    • 2011
  • The study was performed to investigate the characteristics of charcoal and temperature change of a kiln's inner and outer walls in carbonization process using improved kiln. In this kiln system, carbonization process was completed in eight days. In the kiln, the ignition temperature was kept about $720^{\circ}C$. And then the temperature were increased gradually prior to be refined. Finally, the temperature in refining process was reached to maximum point, $1,000^{\circ}C$. In the chimney, the temperature was increased gradually from $90^{\circ}C$ at ignition to $750^{\circ}C$ at refining. The temperature change of the kiln wall resembles a temperature change progress curve during a carbonization process. The highest temperature of the kiln wall that appeared by a carbonization process was around $500^{\circ}C$. As a result of having measured an inner wall and the outer wall of the kiln using an infrared thermography camera, it was judged with there being considerable latent heat on kiln wall and ceiling. Fixed carbon contented of charcoal was 85.9~89.9%. Refining degree of charcoal, hardness, calorific value and pH were l, 12, 7,047~7,456 kcal/kg, 9.0~9.9, respectively. The yield of wood charcoal was 13.8%, and compared to conventional kiln's yield increased 1.5%.