The Effect of Heat treating Conditions on Wear Characteristics of High Speed Steel by Powder Metallurgy (분말고속도공구강의 미끄럼마모특성에 미치는 열처리조건의 영향)

  • 이한영;노정균;배종수;김용진
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2000.06a
    • /
    • pp.48-53
    • /
    • 2000
  • The effects of added elements, such as Co or Nb, on wear properties of high speed steel by powder metallurgy(PM-HSS) had been evaluated in previous paper. The wear properties of materials, in fact, have been a]so influenced by heat-treating conditions. In this paper, the effects of heat-treating conditions on wear properties of PM-HSS have been evaluated. The wear tests have been performed as same conditions as previous paper using PM-HSS(5%Co-1%Nb) heat-treated under different quenching and tempering temperature. The result of this paper shows that wear resistance of PM-HSS is improved with relatively high quenching temperature. However tempering temperature is not sensitve to the wear resistance in range of high quenching temperature. It may be deduced by the fact that the shear strength of matrix by strengthening mechanisms of quenching aging in addition to dispersion-hardening is improved.

  • PDF

Analysis of Rolling Contact Surface on PM-High Speed Steel by X-ray Diffraction (구름접촉을 하는 분말고속도공구강의 X선을 이용한 표면성상해석)

  • 이한영;김용진;배종수
    • Tribology and Lubricants
    • /
    • v.19 no.1
    • /
    • pp.1-8
    • /
    • 2003
  • Recently, PM-high speed steel(PM-HSS) has reportedly been a good alternative material for rolling mill because of its superior performance to conventional HSS. This paper has been aimed to investigate the possibility for application to rolling contact element for PM-HSS by X-ray diffraction technique. The X-ray elastic constant for PH-HSS has been found by X-ray diffraction during the four-point bending test. Residual stress and half-value breadth on the contact surface during rolling contact fatigue process by X-ray diffraction have also been measured. The result of this study shows that the application of X-ray diffraction technique to PM-HSS could be as possible alternative material as conventional HSS. Half-value breadth on rolling contact surface by X-ray diffraction is not changed during rolling contact fatigue process. On the other hand, the residual stress is changed. This suggests that dislocation reaction has been hardly occurred in rolling contact, depending on super-saturated carbon in PM-HSS.

The Effects of Cobait on Wear and Friction Characteristics of PM-HSS (분말고속도공구강의 마찰마모특성에 미치는 Co의 영향)

  • 이한영;백금주;김용진;배종수;홍성현
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1998.04a
    • /
    • pp.108-114
    • /
    • 1998
  • The mechanical characteristics of the high speed steel by powder metallurgy process(PM-HSS) has been reported to improve with several alloying constituents, such as high carbon, vanadium and cobalt. In this paper, sliding wear test has been conducted using a pin-on-disc machine for three PM-HSS which contains 0%, 5% and 12% cobalt respectively, in order to evaluate the effect of cobalt on wear properties of PM-HSS. The results of this study showed that the wear resistance of PM-HSS has been increased by the addition of cobalt on the range of experimental friction velocities. When compared with the effect of addition of cobalt, the wear resistance of PM-HSS with 5% cobalt has been found to be superior to that of PM-HSS with 12% cobalt.

  • PDF

The Effects of Cobalt on Wear and Friction Characteristics of High Speed Steel by Powder Metallurgy (분말고속도공구강의 마찰마모특성에 미치는 Co의 영향)

  • 이한영;배종수;김용진
    • Tribology and Lubricants
    • /
    • v.15 no.2
    • /
    • pp.156-163
    • /
    • 1999
  • The mechanical characteristics of the high speed steel by Powder metallurgy Process (PM-HSS) has been reported to improve with several alloying constituents, such as high carbon, vanadium and cobalt. In this paper, sliding wear test has been conducted using a pin-on-disc machine for three PM-HSS which contains 0%, 5% and 12% cobalt respectively, in order to evaluate the effect of cobalt on wear properties of PM-HSS. The results of this study showed that the wear resistance of PM-HSS has been increased by the addition of cobalt on the range of experimental friction velocities. When compared with the effect of addition of cobalt, the wear resistance of PM-HSS with 5% cobalt has been found to be superior to that of PM-HSS with 12% cobalt.

Investigation of Effect of Hot Rolling Oil of on Rolling with HSS Roll (고속도공구강롤을 적용한 열간유압연 사용특성 연구)

  • 유재희;황상무;김철희
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1997.10a
    • /
    • pp.115-118
    • /
    • 1997
  • Recently, hot rolling oil lubrication technology is required to face with the new environments such as the rapid introduction of high wear resistent high speed steel roll the development of continuous hot rolling technology. In the hot strip mill, according to rolling and quality required conditions are constrict, Roll material of hot rolling finishing stand is changing Hi-Cr Roll to High Speed Steel [HSS] Roll. The problem of HSS Roll of roll force and strip scale defects are increasing in hot strip mill, So we have tested HSS Roll in hot rolling simulator as rolling condition, rolling speed, draft, hot oil concentration. To reduce roll force and prevent scale defects. We get some merit rolling force, rolling torque, roll wear reduction, roll and strip surface roughness and hot rolling critical oil concentration 0.4%. Finally we are going to investigate the effect of hot rolling oil of on rolling with HSS Roll.

  • PDF

Failure analysis of powder compacting punches made of powder metallurgy high speed steels (분말고속도공구강으로 만든 분말성형펀치의 손상분석)

  • 홍성현
    • Journal of Powder Materials
    • /
    • v.7 no.2
    • /
    • pp.78-84
    • /
    • 2000
  • P/M high speed steels(1.28% C, 4.20% Cr, 6.40% W, 5.00% Mo, 3.10% V, bal. Fe) from two different venders were applied to powder compacting punch. The test results show that failure lifes were very different between two punches. These were no difference in volume fraction and mean size of carbides(MC or M6C) but non-metallic inclusions in two punches. Small amount of non-metallic inclusion in the punch did not greatly affect impact energy and transverse rupture strength (TRS). But, fatigue life was drastically decreased by non-metallic inclusions. These results show that fatigue failure was initated around non-metallic inclusion by cyclic load and the fatigue life was greatly affected by the presence of non-metallic inclusions in the punch.

  • PDF

Life and Mechanical Properties of Hot Former Die for Bearing Race using P/M High Speed Steel (분말고속도공구강을 활용한 베어링 레이스 열간 단조 금형의 수명 및 기계적 특성)

  • Hong, Seong-Hyeon;Bae, Jong-Soo
    • Journal of Powder Materials
    • /
    • v.14 no.6
    • /
    • pp.367-371
    • /
    • 2007
  • P/M high speed steel (1.26% C, 4.42% Cr, 6.54% W, 4.92% Mo, 3.21 % V, 8.77% Co, bal. Fe) was applied to hot former die. It showed that the die life became 2.7 times higher than that of cast/wrought SKH 55 tool steel which is commercially used. The increase of die life was corresponding to the improved hardness and transverse rupture strength of PM high speed steel due to the finer grain and carbide as well as the uniform carbide distribution. The P/M high speed steel with the promoted die life could be an alternative to the conventional SKH55.

Three Point Bending Fatigue Property with Heat Treatment Condition in a Powder Metallurgical High Speed Steel JYPS-23 (분말고속도공구강 JYPS-23에서 열처리조건에 따른 3점 굽힘피로특성)

  • 홍성현;배종수;김용진
    • Journal of Powder Materials
    • /
    • v.7 no.3
    • /
    • pp.131-136
    • /
    • 2000
  • The effect of tempering temperature on the three point bending fatigue behavior of a P/M high speed steel JYPS-23 (1.28% C, 4.20% Cr, 6.40% W, 5.00% Mo, 3.10% V, bal. Fe) was investigated. The number of cycles to failure of the specimen austenitized at $1175^{\circ}C$ drastically increased with increasing tempering temperature. As tempering temperature increased from 500 to $620^{\circ}C$, the volume fraction and average size of carbides (MC or M6C) did not significantly changed, while hardness decreased drastically. The reduced hardness is due to the softening of matrix, which increased the resistance of the fatigue crack propagation. For a practical application, powder compacting test were also conducted with the P/M high speed steel punches tempered at 500, 580, and $620^{\circ}C$. The number of compacting cycles to failure of the punches also increased with increasing tempering temperature.

  • PDF

Sliding Wear Characteristics of High Speed Steel by Powder Metallurgy under several Testing Temperature (분말고속도공구강의 작동온도에 따른 미끄럼마모특성해석)

  • 이한영;노정균;배종수;김용진
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2001.06a
    • /
    • pp.135-140
    • /
    • 2001
  • In metal cutting at the tool-chip interface, friction generates considerable amount of heat. Thus, tile .knowledge of wear properties or the cutting tool material in high temperature has been known as one of tile important factors in need of clarification. The authors presented the wear properties of 5%V-5%Co-1%Nb high speed steel, fabricated by powder metallurgy, in room temperature in a previous article. The objective of this paper is to clarify tile effects of temperature ell its wear properties. Wear tests in sliding conditions under various temperatures have been conducted. The results indicate that tile wear properties of tile tool material in high temperature as well as in room temperature are excellent. It may be deduced that the oxide layer formed on the vol-n surface at high temperature is stable enough to prevent wear due to tile high temperature strength of its matrix.

  • PDF

The Effects of Niobium on Sliding Wear Characteristics of High Speed Steel by Powder Metallurgy (분말고속도공구강의 미끄럼마모특성에 미치는 Nb의 영향)

  • 이한영;배종수;김용진
    • Tribology and Lubricants
    • /
    • v.16 no.3
    • /
    • pp.194-200
    • /
    • 2000
  • In order to evaluate the effect of Nb on wear properties of high speed steel(HSS) by powder metallurgy, niobium-alloyed HSS have been prepared by adding 0%, 1%, 3% and 5%Nb to HSS of 6%W-5%Mo-4 %Cr-5%V-5%Co. Sliding wear tests were conducted at various sliding speed conditions under the constant pressure using a pin-on-disc type machine. The results of this study show that the wear resistance of HSS by powder metallurgy was increased by the addition of Nb within the range of sliding speed used in this experimental study. However, the amount of Nb did not improve the wear resistance. It may be due to the thermal stability of carbide and high temperature properties of the matrix containing Nb comparing to that without Nb.