• 제목/요약/키워드: 경화 깊이

검색결과 124건 처리시간 0.024초

표면 경화된 탄소강의 비틀림 피로강도에 미치는 조직의 경향 (The Effect of Structure on Torsional Fatigue Strength of Surface Hardened Carbon Steel)

  • 고준빈;김우강;원종호
    • 한국정밀공학회지
    • /
    • 제22권1호
    • /
    • pp.130-136
    • /
    • 2005
  • Induction hardening increases hardness near the surface where it's most needed, and leaves the surface in compression which improves fatigue life. Although case depth and chemical composition are same, the structure of induction hardened shaft affects the fatigue strength and life because of austenization during hardening. Therefore torsional fatigue tests of specimens from various structures, which are obtained by nomalizing, spheriodized annealing and tempering after quenching, were conducted on induction hardened automotive drive shafts with various case depths and loads applied in order to evalute the relation between structure and fatigue strength.

석면 건축자재의 비산 방지를 위한 침투성 경화제 침투 효과에 관한 연구 (A Study on Penetration Effect of Penetrating Hardener for Prevention of Scattering of Asbestos Building Materials)

  • 송태협;박지선;신현규
    • 한국건설순환자원학회논문집
    • /
    • 제6권4호
    • /
    • pp.324-330
    • /
    • 2018
  • 2007년 산업안전 보건법의 개정에 따라 우리나라도 유럽 및 일본과 같이 석면의 수입, 유통, 제조를 완전히 금지하였다. 이에 따라 현재의 석면의 문제는 기존에 시공된 석면 건축자재의 안전한 유지관리 및 친환경 해체, 그리고 폐기된 석면 건축자재의 안정적인 최종처리에 있다고 할 수 있다. 과거 우리나라는 매년 10만 톤의 석면을 사용하였으며, 이를 사용한 건축자재는 년간 100만 톤을 초과하였다. 이러한 석면 건축자재가 2006년까지 지속적으로 사용되었고, 이러한 자재는 향후 2044년까지 계속 유지될 것으로 환경부에서 예측한 바 있다. 석면 폐기물의 무해화 처리를 위한 사전 전처리 단계로 설치되어 있는 석면 건축자재에 침투성 경화제를 도포 하고, 해체 철거를 실시하면, 해체단계에서 석면의 비산을 억제하고, 무해화 단계에서 알칼리 공급 작용을 하여 무해화 처리 조건이 개선될 수 있다. 따라서 석면 건축자재에 침투성 경화제가 안정적으로 침투될 수 있어야 한다. 본 연구에서는 sodium silicate를 주성분으로 하는 침투성 경화제와 증류수의 희석 비율에 따른 침투 효과를 비교하고자 하였다. 시험결과 K성분의 침투에 따른 침투 깊이 평가가 가능할 것으로 판단되었으며, 증류수 희석 비율이 높을수록 침투효과는 커지는 것으로 나타났다. 본 연구를 통하여 중밀도 수준의 폐석면 건축자재의 무해화를 위한 사전 전처리 방법의 제시가 가능할 것으로 사료되며, 향후 화학적 무해화를 위한 사전 전처리를 효율적으로 하기 위해서는 침투성 경화제와 중류수의 혼합비율의 최적화가 가장 중요한 요소인 것으로 나타났다.

인천국제공항 줄눈콘크리트 슬래브의 초기재령 특성분석 (Analysis of Early-age Property of JPCP Slab of Incheon International Airport)

  • 썬런쥬안;정진훈;천성한;임진선
    • 한국방재학회:학술대회논문집
    • /
    • 한국방재학회 2007년도 정기총회 및 학술발표대회
    • /
    • pp.335-339
    • /
    • 2007
  • 줄눈콘크리트 슬래브의 초기 재령특성 분석을 위하여 인천국제공항 건설 현장에 설치된 슬래브에 온도와 습도를 측정 후 해석하였다. 성숙도 방법을 이용하여 결정한 콘크리트 슬래브의 초기경화시간은 콘크리트 타설 후부터 약 2시간 40분이었다. 콘크리트 슬래브 변형률의 변화는 초기경화 시간 이후부터 시작되었고, 이는 센서가 설치된 각 위치와 깊이에서 서로 다른 값을 나타냈다.

  • PDF

강재의 레이저 표면경화 공정제어를 위한 경화층깊이의 실시간 측정에 관한 연구 (A study on in-process measurement of hardening depth for LASER surface hardening process control)

  • 우현구;박영준;조형석;한유희
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 제어로봇시스템학회 1991년도 한국자동제어학술회의논문집(국내학술편); KOEX, Seoul; 22-24 Oct. 1991
    • /
    • pp.252-257
    • /
    • 1991
  • This paper proposed that the eddy-current measurement method can be used a means of in-process measuring the hardening depth in Laser surface treatment process. Also, this paper deal with the numerical analysis of magnetic flux distribution and experimental result of measurement. In Laser heat treatment process of steels, a thin layer of the substrate is rapidly heated to austenitizing temperature and subsequently cooled at a very fast rate due to the self-quenching by heat conduction into the bulk body, to produce a martensite structure which have low magnetic permeability. The eddy-current measurement method depends on the properties of material to be measured such as electric conductivity, magnetic permeability and geometry. In this paper, the hardening depth was measured by detecting relevant magnetic permeability changes caused by heat treatment of steels.

  • PDF

′YAG 레이저에 의한 표면경화강의 레이저 경화와 마멸특성 (Laser hardening and Wear Characteristics of Surfaces hardening steel by YAG LASER)

  • 옥철호;서영백;조연상;배효준;박흥식;전태옥
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1999년도 제30회 추계학술대회
    • /
    • pp.63-70
    • /
    • 1999
  • Surface hardening of plain carbon steel (SM45C) by Laser are usually much finer and stronger than those of the base metals. The present study was under taken to investigate the wear resistance and a processing parameters such as, power density, pulse width, defocusing distance, and molten depth for surface modification of plain carbon steel. The wear test was carried out under experimental condition using the wear test device, and in which the annular surfaces of wear test specimens as well as mating specimen of alumina ceramics($Al_2O_3$) was rubbed in dry sliding condition. It is shown that molten depth and width depend on defocusing distance. The wear loss on variation of sliding speed was much in lower speed range below 0.2m/sec and in higher speed range above 0.7m/sec, but wear loss was little in intermediate speed range. It depends on oxidation speed and wear speed.

  • PDF

탄소 표면경화처리 구름베어링의 유효 경화 깊이에 대한 고찰 (Study on Effective Case Depth for Case Hardened Rolling Bearings)

  • 이한영
    • Tribology and Lubricants
    • /
    • 제32권1호
    • /
    • pp.18-23
    • /
    • 2016
  • The effective case depth for case-hardened rolling bearing has been discussed. For this purpose, rolling contact fatigue tests for ball bearings built with inner race of various hardness values were conducted until L10 calculating rating life using a bearing life test machine under radial loading. Then, the distribution of residual stress below the inner raceway, which depended on the hardness value, was measured by X-ray diffraction. As a result, the linear relationship was established between the hardness value of the inner race and the theoretical shear stress evaluated at the depth where the residual stress disappeared below the inner raceway. Based on the relationship, it could be found that the factor of safety in bearing manufacturer’s rules for the effective case depth of case hardened rolling bearings was set higher. However, it could be also found that the hardness values at the depth where the maximum shearing stress acted below the raceway surface in a tapered roller bearing hardened by the carburizing process, were not sufficient for preventing plastic deformation under the basic dynamic load rating. Consequently, further efforts were still required to reduce or to disperse the contact load on the material design of a rolling bearing in order to prolong its life.

고주파표면경화한 SM45C 강에서 유교경화층깊이가 피로거동에 미치는 영향 (A Study on Fatigue Behavior according to Effective Case Depth in Induction Case Hardened SM45C Steel)

  • 오세욱;호정원;박원조
    • 한국해양공학회지
    • /
    • 제5권1호
    • /
    • pp.71-80
    • /
    • 1991
  • This paper reveals the effect of the effective case depth(ECD) on the fatigue behavior of a high-frequency induction hardened SM45C in rotated bending fatigue test. In addition, the effects of fracture modes(surface origin type, inner origin type) on it are discussed. The fatigue limit of the induction hardened steel is remarkably increased compared with that of base metal. In addition, the fatigue limit is linearly increased as the effective casedepth grows deep in the region of this experiment (ECD/R;0.23-0.49). The S-N curve and fracture mode in the induction case hardened steel are classified into two kinds, as a result : N$_{f}$<10$^{5}$ ;surface origin type fracture(at high stress), N$_{f}$>10$^{5}$ ; in ner origin type fracture(at low stress). In case of inner origin type fracture; as the effective case depth(ECD) gets deep, the fatigue limit is increased by the reason that the fracture origin moves toward center; in reverse, is decreased by reason that the compressive residual stress gets low. As a result, the increasing effect of the former is much bigger than the decreasing effect of the latter, and the fatigue limit is increased as the ECD gets deep.eep.

  • PDF

레이저빔 크기변화에 따른 광조형수지의 경화특성 (Cure Properties in Photopolymer for Stereolithography according to Variance of Laser Beam Size)

  • 이은덕;심재형;백인환
    • 한국정밀공학회지
    • /
    • 제20권2호
    • /
    • pp.76-84
    • /
    • 2003
  • Stereolithography is the technique using a laser beam to cure a liquid resin, a photopolymer, with three dimensional computer-aided design (CAD) data. The build parameters of stereolithography such as beam size, scan velocity. hatch spacing, layer thickness and etc. are determined by the accuracy of prototype, the build time and the cured properties of the resin. In particular, beam size is important processing parameter fur the other parameters. Therefore, this study observed the cured property to beam size. For this purpose, according to hatch spacing and beam size, the cure width and depth were measured on single cured line. Also, the cure width and depth were measured at single cured layer As a result of experiments. cure depth which varied from 0.23mm to 0.34mm was directly proportioned to beam radius. on the other hand, cure width which varied from 0.42mm to 1.07mm was inversely proportioned to beam radius. Surface roughness varied from 1.12 to 2.23 m for the ratio of hatch spacing to beam radius.