• Title/Summary/Keyword: (Fe, Co)/Zeolite Catalyst

Search Result 6, Processing Time 0.021 seconds

Hydroxylation of Phenol over (Fe, Co)/Zeolite Catalysts for the Selective Synthesis of Catechol (카테콜의 선택적 합성을 위한(Fe, Co)/Zeolites 촉매상에서 페놀의 수산화 반응)

  • Park, Jung-Nam;Shin, Chae-Ho;Baeg, Jin-Ook;Lee, Chul Wee
    • Korean Chemical Engineering Research
    • /
    • v.44 no.4
    • /
    • pp.387-392
    • /
    • 2006
  • (Fe, Co)/zeolite catalysts such as (Fe, Co)/NaY, (Fe, Co)/NaBeta and (Fe, Co)/HUSY were prepared by ion-exchange method and their catalytic performance was examined in the hydroxylation of phenol with $H_2O_2$ for the production of catechol. The (Fe, Co)/NaBeta catalyst showed its best performance at reaction temperature=$70^{\circ}C$, molar ratio of phenol/$H_2O_2=3$, weight ratio of phenol/catalyst=50 and weight ratio of solvent (water)/phenol=6 as 20% of phenol conversion, 77% of the selectivity for the hydroxylation, 70% of the selectivity for catechol, and 2.5 of the formation ratio of catechol/hydroquinone. The (Fe, Co)/zeolite catalysts showed the reproducible activities without deactivation after repeated regeneration. The fresh and used(Fe, Co)/zeolites were characterized by XRD, UV-VIS DRS, and XPS and their catalytic performance was discussed based on these characterization results.

Synthesis and Characterization of Fe-Co/mesoHZSM-5 : Effect of Desilication Agent and Iron-cobalt Composition

  • Jimmy, Jimmy;Roesyadi, Achmad;Suprapto, Suprapto;Kurniawansyah, Firman
    • Korean Chemical Engineering Research
    • /
    • v.58 no.1
    • /
    • pp.163-169
    • /
    • 2020
  • Synthesis of Fe-Co/meso-HZSM5 catalyst, intended to be applied in Fischer-Tropsch (FT) reaction was investigated. The study emphasized the effect of desilication agents, NaOH and KOH, on the catalyst materials properties. Impregnation composition of active metal (Fe and Co) was also examined. HZSM-5, converted from ammonium ZSM-5 through calcination, was treated with NaOH and KOH for desilication, followed by impregnation with 10% metal loading. Fe composition in the initial mixture was varied at 10-50% from total composition. After impregnation, reduction was applied by flowing hydrogen gas at 400 ℃ for 10 hours. The use of KOH solution induced greater mesoporous volumes; however, it had a detrimental effect on zeolite crystal structure. NaOH solutions, on the other hand, increased mesopore area as high as 100%, indicated from surface area increase from 266.28 m2/g of HZSM-5, to 526.03 m2/g of NaOH-desilicated HZSM-5. In addition, the application of NaOH solution increased pore volume from 0.14 cc/g to 0.486 cc/g. Further, more Fe-Co alloys and less oxide of iron (Fe2O3) as well cobalt (Co3O4) had been commonly observed in the produced catalysts. The largest Fe-Co alloys could be found in 50Fe-50Co/HZSM-5

Effect of Steam-Treated Zeolite BEA Catalyst in NH3-SCR Reaction (NH3-SCR 반응에서 스팀 처리된 zeolite BEA 촉매의 영향)

  • Park, Ji Hye;Cho, Gwang Hee;Hwang, Ra Hyun;Baek, Jeong Hun;Yi, Kwang Bok
    • Clean Technology
    • /
    • v.26 no.2
    • /
    • pp.145-150
    • /
    • 2020
  • Nitrous oxide (N2O) is one of the six greenhouse gases, and it is essential to reduce N2O by showing a global warming potential (GWP) equivalent to 310 times that of carbon dioxide (CO2). Selective catalytic reduction (SCR) is a technology that converts ammonia into harmless N2 and H2O by using ammonia as a reducing agent to remove NOx, one of the air pollutants; the process also produces high denitrification efficiency. In this study, the Fe-BEA catalyst was steam-treated at 100 ℃ for 2 h before Fe ion exchange in the fixed bed reactor in order to investigate the effect of the steam-treated Fe-BEA catalyst on the NH3-SCR reaction. NH3-SCR reaction test of synthesized catalysts was performed at WHSV = 180 h-1, 370 to 400 ℃ in the fixed bed reactor. The Fe-BEA(100) catalyst steam-treated at 100 ℃ showed a somewhat higher activity than the Fe-BEA catalyst at 370 to 390 ℃. The catalysts were characterized by BET, ICP, NH3-TPD, H2-TPR, and 27Al MAS NMR in order to determine the cause affecting NH3-SCR activity. The H2-TPR result confirmed that the Fe-BEA(100) catalyst had a higher reduction of isolated Fe3+ than the Fe-BEA catalyst, and that the steam treatment increased the amount of isolated Fe3+ as an active species, thus increasing the activity.

A Review of Domestic Research Trends of Fischer-Tropsch for the Production of Light Hydrocarbons and Middle Distillates From Syngas (합성가스로부터 경질탄화수소 및 중산유분을 생산하기 위한 Fischer-Tropsch의 국내연구동향)

  • Kim, Jin-Ho;Kim, Hyo-Sik;Kim, Ji-Hyeon;Ryu, Jae-Hong;Kang, Suk-Hwan;Park, Myung-June
    • Korean Chemical Engineering Research
    • /
    • v.57 no.4
    • /
    • pp.565-574
    • /
    • 2019
  • Fischer-Tropsch synthesis process is a typical method for synthesizing hydrocarbons from syngas and is mainly known as iron (Fe) and cobalt (Co) catalysts. Currently, some technologies such as CTL (Coal to Liquid) and GTL (Gas to Liquid) are operated on a commercial scale depending on the products, but the research to produce light hydrocarbons and middle distillates directly has not been commercialized. Therefore, in this study, domestic studies for direct production of light hydrocarbons and middle distillates are summarized and the effect of catalyst preparation, promoter addition, zeolite combination on product selectivity is investigated.

Desulfurization of Sulfur Compounds in City-gas using Metal Salt Impregnated Zeolite (금속이온이 담지 된 제올라이트를 이용한 도시가스 내 부취제 제거)

  • Song, Hirn-Ill;Ko, Chang Hyun;Kim, Jae Chang;Kim, Jong-Nam
    • Korean Chemical Engineering Research
    • /
    • v.45 no.2
    • /
    • pp.143-148
    • /
    • 2007
  • In hydrogen production for fuel cell by reforming city-gas, sulfur compounds, odorant in city-gas, are detrimental to reforming catalyst and fuel cell electrodes. We prepared metal salt impregnated ${\beta}-zeolite(BEA)$ to remove sulfur compound in city-gas by adsorption. The sulfur breakthrough adsorption capacity was changed depending on the concentration and species of metal salt. $AgNO_3$ impregnated BEA showed the highest sulfur breakthrough capacity among adsorbents used in this experiment(41.1 mg/g). But metal salt impregnated BEA such as $Ni(NO_3)_2/BEA$, $Fe(NO_3_)_3/BEA$, $Co(NO_3)_2/BEA$ showed a certain amount of sulfur adsorption capacity comparable to $AgNO_3/BEA$. Adsorption temperature effect, desorption study, and x-ray photoelectron spectroscopy analysis revealed that the dominant interaction between metal impregnated adsorbent and sulfur compounds was not chemisorption but physisorption.

Dimethyl Carbonate Synthesis by Methanol Oxidative Carbonylation (메탄올 산화 카르보닐화에 의한 디메틸카보네이트 합성)

  • Nam, Jeong-Kwang;Cho, Deug-Hee;Suh, Jeong-Kwon;Kim, Seong-Bo
    • Korean Chemical Engineering Research
    • /
    • v.49 no.5
    • /
    • pp.530-534
    • /
    • 2011
  • The synthesis of dimethyl carbonate by liquid phase oxidative carbonylation of methanol was studied under batch reaction system. Reaction factors such as effect on various metals, anion containing in copper catalyst, temperature, carbon monoxide and oxygen molar ratio and copper content were investigated. In particular $CuCl_2{\cdot}2H_2O$ showed the excellent of the methanol conversion 65.2%, DMC selectivity 96.6% reaction condition under 1.0 g, $150^{\circ}C$, MeOH/CO/$O_2$=0.2/0.215/0.05 (molar ratio). $CuCl_2$ led to corrosion of the reactor. Thus, a new catalyst system using supports was investigated to resolve these corrosion problem. Influence on various supports were examined and copper catalyst supported on zeolite Y showed the most excellent activity on the formation of dimethyl carbonate. The amount of Fe dissolved during the reaction using ICP-AES (Inductively Coupled Plasma-Atomic Emission Spectrometer) was compared with catalysts, calcined Cu/zeolite Y showed the lower value below 5% than $CuCl_2-2H_2O$.