  • The formation and thermal properties of the $BaO_2$ and $TiO_2$ mixtures were prepared by mechanical alloying method was investigated by X-ray diffractometry (XRD), scanning electron microscopy (SEM), and thermogravimetric/differential thermal analysis (TG/DTA). The rotating speed of 750 rpm shows more effects on the formation of $BaTiO_3$ single phase. The internal strain calculated using Williamson-Hall method was $4.27{\times}10^{-3}$ for the mixture milled for 300 min, the crystallite size was calculated using the Scherrer method decreased with milling time. The $BaTiO_3$ crystal improved crystallinity was formed by thermal annealing at a temperature of $600^{\circ}C$ for 1 h for the mixture milled for 300 min.

  • PDF

다결정 $Fe_{1+X}Eu_{1-X}O_{3}$의 결정구조 연구 (The Crystallograpic Study of Polycrystalline $Fe_{1+X}Eu_{1-X}O_{3}$)

  • 김정기;서정철;한은주
    • 한국자기학회지
    • /
    • 제3권2호
    • /
    • pp.101-107
    • /
    • 1993
  • 다결정 $Fe_{1+X}Eu_{1-X}O_{3}$(x=-0.06, 0.0, 0.1, 0.2, 0.3과 0.4)의 결정구조를 X-선 회절과 $M\"{o}ssbauer$ 분광학 방법에 의해서 연구하였다. X-선 회절선과 $M\"{o}ssbauer$ 분광 스펙트럼 분석 결과 $-0.06{\leq}x{\leq}0.0\;과\;0.2{\leq}x{\leq}0.3$ 영역의 시료에서는 각각 orthoferrite와 garnet 단일 결정상을 나타낸다. 그러나, $0.0의 영역의 시료에서는 각각 garnet-orthoferrite와 garnet-trigonal의 두 결정상만이 우세하게 나타나는데, 이때 x가 증가함에 따라 orthoferrite 결정상에서 garnet 결정상을 거쳐서 trigonal 결정상으로 변환하는 경향을 보인다. $M\"{o}ssbauer$ 분광학 분석은 garnet 구조의 d-site에 vacancy가 존재함을 나타내며, 이는 X-선 회절선의 강도 변화와도 연관 지울수 있다.

  • PDF

분무열분해법을 이용하여 M3MgSi2O8:Eu2+ (M=Ca, Sr, Ba) 형광체 분말의 VUV 특성 최적화 (Optimization of VUV Characteristics of M3MgSi2O8:Eu2+ (M=Ca, Sr, Ba) Phosphor by Spray Pyrolysis)

  • 정유리;정경열
    • 한국분말재료학회지
    • /
    • 제15권5호
    • /
    • pp.399-404
    • /
    • 2008
  • Spray pyrolysis was applied to prepare $M_{3}MgSi_{2}O_{8}:Eu^{2+}$ (M=Ca, Sr, Ba) blue phosphor powder. The library of a Ca-Sr-Ba ternary system was obtained by a combinatorial method combined with the spray pyrolysis in order to optimize the luminescent property under vacuum ultraviolet (VUV) excitation. 10 potential compositions were chosen from the first screening. The emission shifted to longer wavelength as Ca became a dominant element and the emission intensity was greatly reduced in the composition region at which Ba is dominant element. On the base of the first screening result, the second fine tuning was carried out in order to optimize the luminescence intensity under VUV excitation. The optimal composition for the highest luminescence intensity was $(Ca_{1.7},\;Sr_{0.3},\;Ba_{1.0})Si_{2}O_{8}:Eu^{2+}$ which had the color coordinate of (0.152, 0.072) and about 64% emission intensity of $BaMgAl_{10}O_{17}$ (BAM) phosphor.

Investigation of thermal annealing effects on the optical transparency and luminescent characteristics of Eu-doped Y2O3 thin films

  • Chung, Myun Hwa;Kim, Joo Han
    • Journal of Ceramic Processing Research
    • /
    • 제20권4호
    • /
    • pp.431-435
    • /
    • 2019
  • The thermal annealing effects on the optical transparency and luminescent characteristics of the Eu-doped Y2O3 thin films have been investigated. The as-deposited Y2O3:Eu films exhibited an optical band gap of 5.78 eV with a transparency of 89 % at a wavelength of 550 nm. As the annealing temperature increased from 1000 to 1300 ℃, the optical band gap and transparency of the films decreased from 5.77 to 4.91 eV and from 86.8 to 64.5 % at 550 nm, respectively. The crystalline quality of the films was improved with increasing annealing temperature. The annealed Y2O3:Eu films emitted a red-color photoluminescence (PL) with the highest emission peak near 612 nm. The PL intensity was increased with increasing annealing temperature to 1200 ℃, resulting from the improvement in the crystalline quality of the films. The PL intensity was decreased with further increasing temperature above 1200 ℃ due to the formation of Y2SiO5 phase by the reaction of the film with the quartz substrate.

Pechini법에 의한 Ga2O3:Eu3+ 형광체 분말의 제조 (Preparation of Ga2O3:Eu3+ Phosphor by Pechini Method)

  • 박인용;이종원;김선태
    • 한국재료학회지
    • /
    • 제12권7호
    • /
    • pp.517-521
    • /
    • 2002
  • Europium-activated $Ga_2$$O_3$ phosphor powders were prepared by Pechini method from the mixed aqueous solutions of gallium(III) nitrate, europium(III) nitrate, ethylene glycol and citric acid. The phase formation process and particle shape of the powders obtained were investigated by means of TG/DTA, XRD and SEM. It was found that the powders were amorphous or ${\gamma}$-$Ga_2$$O_3$-like phase up to $500^{\circ}C$ and then transformed into $\beta$- $Ga_2$$O_3$ phase above $600 ^{\circ}C$. The powders calcined below $1000^{\circ}C$ were spherical and nanometer-sized. Photoluminescence spectra measured at room temperature showed that the highest luminescence intensity was obtained for the sample synthesized under the conditions of 2 mol% Eu concentration and heat treatment at $1000^{\circ}C$.

Yttria Stabilized Cubic Zirconia(YSCZ) 단결정의 결정성장과 Color Centers (Crystal Growth and Color Centers of Yttria Stabilized Cubic Zirconia(YSCZ) Single Crystals)

  • 정대식;오근호
    • 한국세라믹학회지
    • /
    • 제29권11호
    • /
    • pp.851-854
    • /
    • 1992
  • It was grown ZrO2:10 mol% Y2O3 single crystals doped with 1 wt% of rare earth metal ion (Ce, Pr, Nd, Er, Eu) by Skull Method. Grown crystals showed Ce:orange-red, Pr:golden-yellow, Nd:lilac, Er:pink, Eu:light pink due to dopant effect. It was examined color centers in light absorption pattern of visible region (λ= 300~700 nm); in as grown samples, absorption by Ce4+, (Pr4+, Pr3+), Nd3+, Er3+, Eu3+ ions were important, and in samples after vacuum annealing, decrease of absorption by Pr4+ ion and increase of absorption by Pr3+ ion was important, and absorption by Ce3+, Eu2+ was important due to reduction of activator.

  • PDF

수열합성에 의해 제조된 YVO4:Eu3+ 형광체의 발광특성 (Luminescent Properties of YVO4:Eu3+ Phosphor by Using Hydrothermal Synthesis)

  • 문영민;최성호;정하균;임상호
    • 한국재료학회지
    • /
    • 제18권10호
    • /
    • pp.511-514
    • /
    • 2008
  • We have synthesized $Eu^{3+}$-doped $YVO_4$ phosphors by using a hydrothermal method and investigated their luminescent properties. Aqueous solutions of $Y_2O_3,\;V_2O_5,\;Eu_2O_3$, and nitric acid with various pH values were used as the precursors. The crystallinity, surface condition, and emission characteristics were examined using XRD, FT-IR, and photo-excited spectrometer. $Eu^{3+}$ incorporation followed by the efficient red emission strongly depends on the acidity of solution media. The emission intensity becomes stronger as the pH values increase to 7 and then gradually decreases. This phenomenon might be related to the hydroxyl quenching effect, which is induced by surface bound OH-groups.

Eu 첨가에 따른 PZT 박막의 유전 특성 (Dielectric properties of Eu-doped PZT thin films)

  • 손영훈;김경태;김창일;장의구;이병기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.155-158
    • /
    • 2002
  • Eu-doped lead zirconium titanate $Pb_{1.1}(Zr_{0.3}Ti_{0.7})O_{3}$ thin films on the Pt/Ti/$SiO_2$/Si substrates prepared by a metalorganic decomposition (MOD) method. The effect on the structural and electrical properties of the films measured according to Eu content. Eu-doping altered significantly the dielectric and ferroelectric properties. The remanent polarization and coercive field decreased with increasing the concentration of Eu content. The dielectric constant and dielectric loss of the film decreased with increasing Eu contents. The 3 mol% of Eu-doped PZT thin film showed large remanent polarization and the fatigue characteristic of the film did not change up to $10^9$ switching cycles.

  • PDF

Photoluminescent Properties of Eu(III) in the Composite Heterocyclic Ligands/Crown Ether Systems

  • Liu, Hong Guo;Jang, Ki-Wan;Feng, Xu Sheng;Kim, Chang-Dae;Yoo, Young-Jae;Lee, Yong-Ill
    • Bulletin of the Korean Chemical Society
    • /
    • 제26권12호
    • /
    • pp.1969-1974
    • /
    • 2005
  • Composite systems of $Eu(phen)_2Cl_3{(H_2O)}_2$, Eu(DN-bpy)$(phen)Cl_3{(H_2O)}_2$ and Eu(DB-bpy)$(phen)Cl_3{(H_2O)}_2$ (DNbpy: $4,4^\prime$-Dinonyl-$2,2^\prime$-dipyridyl; DB-bpy: $4,4^\prime$-Di-tert-butyl-$2,2^\prime$-dipyridyl) with crown ethers of Benzo-15-crown-5 (B15C5), Benzo-18-crown-6 (B18C6), 18-crown-6 (18C6), Dibenzo-18-crown-6 (DB18C6) and Dibenzo-24-crown-8 (DB24C8) were fabricated successfully and characterized by using photoluminescent spectroscopy and luminescent lifetime measurements. All composites formed show high luminescence mainly in red region. It was found that the heterocyclic ligands such as phen, DN-bpy and DB-bpy as well as the crown ethers have great influences on the photoluminescent properties of $Eu^{3+}$ ion. The environment around $Eu^{3+}$ ion in the composite systems changes greatly,presumably the variation of the first coordination sphere. The $Eu^{3+}$ ion occupies higher symmetrical environment and in more than one kind of symmetrical site in the composite systems studied in this work.

Synthesis and Photoluminescence Properties of $BaSiO_3:RE^{3+}$ (RE=Eu, Sm) Phosphor Powers

  • 조신호;최동화
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제45회 하계 정기학술대회 초록집
    • /
    • pp.180-180
    • /
    • 2013
  • 희토류 이온이 치환 고용된 실리케이트계 형광체는 자외선으로 여기될 때 높은 발광 효율을 나타내기 때문에 광전 소자, 레이저, 형광램프에 응용할 수 있는 발광 재료로 상당한 관심이 집중되고 있다. 본 연구에서는 고상반응법을 사용하여 초기 물질 (99.99% 순도), (99.99%), (99.9%), (99.9%)을 화학 정량으로 준비하여 활성제 이온 Eu3+와 Sm3+의 함량비를 0, 0.01, 0.05, 0.10, 0.20 mol로 변화시켜 BaSiO3:RE3+ (RE=Eu, Sm) 형광체를 제조하여 그것의 발광과 흡광 특성을 조사하였다. Eu3+ 이온이 도핑된 BaSiO3 형광체의 경우에, 발광 스펙트럼은 모든 시료에서 전이에 의한 발광 스펙트럼을 보였으며, 특히 j=2에서 가장 강한 적색 형광이 피크 620 nm에서 관측되었다. 상대적으로 발광 세기가 약한 595 nm 에 정점을 갖는 주황색 발광과 705 nm 에 피크를 갖는 적색 발광 스펙트럼이 관측되었다. Eu3+ 이온의 함량비가 0.15 mol 일 때 세 영역의 발광 스펙트럼의 세기는 최대값을 나타내었다. 주흡광 스펙트럼은 Eu3+ 이온의 함량비에 관계없이 397 nm에서 관측되었다. Sm3+ 이온이 도핑된 BaSiO3 형광체의 경우에, 모든 시료는 Sm3+ 이온의 함량비에 관계없이 전이에 의한 발광 스펙트럼을 보여주고 있으며, 특히 j=7/2에서 가장 강한 주황색 형광이 피크 603 nm에서 관측되었다. 상대적으로 발광 세기가 약한 567 nm에 정점을 갖는 황색 발광과 651 nm에 피크를 갖는 적색 발광 스펙트럼이 관측되었다. Sm3+ 이온의 함량비가 0.05 mol 일 때 세 종류의 발광 스펙트럼의 세기는 최대값을 나타내었다. Sm3+ 이온의 함량비가 더욱 증가함에 따라 모든 발광 스펙트럼의 세기는 순차적으로 감소하였는데, 이 현상은 농도 소광 현상에 기인함을 알 수 있었다. 주 흡광 스펙트럼은 Sm3+ 이온의 함량비에 관계없이 406 nm에서 관측되었으며, 이밖에도 상대적으로 세기가 약한 흡광 스펙트럼이 237 nm, 377 nm와 476 nm에서 관측되었다.