  • The films of the vanadium tungsten oxide, $V_{1.85}W_{0.15}O_5$, were grown on Pt/Ti/$SiO_2$/Si substrate by RF sputtering method. It was found that film crystallinity, dielectric properties, and TCR properties were strongly dependent upon the thin film thickness. As increasing of $V_{1.85}W_{0.15}O_5$ thickness, the grain size, morphology, and crystallinity increased. The dielectric constants of $V_{1.85}W_{0.15}O_5$ thin films deposited at 150nm were 71.11, with a dielectric loss of 0.015, respectively. Also, The $V_{1.85}W_{0.15}O_5$ thin films showed good TCR values of -3.45%/K.

  • PDF

비냉각 적외선 검출기용 $V_{1.85}W_{0.15}O_5$ 박막의 구조적, 전기적 특성 (Structural and Electrical Properties of $V_{1.85}W_{0.15}O_5$ Thin Films for the Uncooled Infrared Detector)

  • 남성필;류기원;이성갑;배선기;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.237-238
    • /
    • 2008
  • The films of Vanadium tungsten oxide, $V_{1.85}W_{0.15}O_5$, were grown on Pt/Ti/$SiO_2$/Si substrate by RF sputtering method. The $V_{1.85}W_{0.15}O_5$ thin films deposited on Pt/Ti/$SiO_2$/Si substrates by RF sputtering method exhibited fairly good TCR and dielectric properties. It was found that film crystallinity, dielectric properties, and TCR properties were strongly dependent upon the annealing temperature. The dielectric constants of the $V_{1.85}W_{0.15}O_5$ thin films annealed at $300^{\circ}C$ were 55, with a dielectric loss of 1.435, respectively. Also, the TCR values of the $V_{1.85}W_{0.15}O_5$ thin films annealed at $300^{\circ}C$ were about -3.6%/K.

  • PDF

텅스텐을 첨가한 $V_{2-x}W_xO_5$ 박막의 전기적 특성 (Electrical properties of $V_{2-x}W_xO_5$ thin film doped Tungsten contents)

  • 남성필;노현지;이성갑;배선기;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2009년도 제40회 하계학술대회
    • /
    • pp.1322_1323
    • /
    • 2009
  • The $V_{1.85}W_{0.15}O_5$ thin films deposited on Pt/Ti/$SiO_2$/Si substrates by RF sputtering method exhibited fairly good TCR and dielectric properties. It was found that film crystallinity, dielectric properties, and TCR properties were strongly dependent upon the annealing temperature. The dielectric constants of the $V_{1.85}W_{0.15}O_5$ thin films annealed at $400^{\circ}C$ were 38.11, with a dielectric loss of 1%, respectively. Also, the TCR values of the $V_{1.85}W_{0.15}O_5$ thin films annealed at $400^{\circ}C$ were about -3.45%/K.

  • PDF

텅스텐 첨가에 따른 $V_{2-n}W_nO_5$ 박막의 구조적, 전기적 특성 (Electrical and Structural Properties of $V_{2-n}W_nO_5$ Thin Films as a function of Tungsten Contents)

  • 남성필;이성갑;배선기;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2008년도 Techno-Fair 및 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.117-118
    • /
    • 2008
  • The $V_{1.85}W_{0.15}O_5$ thin films deposited on Pt/Ti/$SiO_2$/Si substrates by RF sputtering method exhibited fairly good TCR and dielectric properties. It was found that film crystallinity, dielectric properties, and TCR properties were strongly dependent upon the annealing temperature. The dielectric constants of the $V_{1.85}W_{0.15}O_5$ thin films annealed at $400^{\circ}C$ were 38.11, with a dielectric loss of 1%, respectively. Also, the TCR values of the $V_{1.85}W_{0.15}O_5$ thin films annealed at $400^{\circ}C$ were about -3.45%/K.