UV-assisted surface modification of polyethersulfone (PES) membrane using TiO2 nanoparticles

  • Singh, Shruti;Karwa, Vinay;Marathe, K.V.
    • Membrane and Water Treatment
    • /
    • v.9 no.6
    • /
    • pp.393-403
    • /
    • 2018
  • In this research commercial polyethersulfone (PES) membrane was modified using $TiO_2$ nanoparticles (P-25 Degussa) and further irradiated using UV light to overcome the hydrophobicity and fouling nature of the membrane. Further the membranes were characterized using SEM and FTIR. Contact angle measurements study confirmed the hydrophilic tendency of the modified membrane by decreasing the contact angle from $73^{\circ}$ to $20.28^{\circ}$. The modified membranes showed higher flux and better anti-fouling properties as compared to the unmodified counterparts. The optimum conditions were found to be 0.5 wt% $TiO_2$ loading with 60 min membrane immersion and 10 min UV light illumination. The effect of different pH conditions of feed was analysed. Real wastewater filtration experiments also indicated better performance of modified membranes as opposed to neat PES membranes.

Electrochemical Characteristics of Hybrid Capacitor using Core-shell Structure of MCMB/Li4Ti5O12 Composite (Core-shell 구조의 MCMB/Li4Ti5O12 합성물을 사용한 하이브리드 커패시터의 전기화학적 특성)

  • Ko, Hyoung Shin;Choi, Jeong Eun;Lee, Jong Dae
    • Korean Chemical Engineering Research
    • /
    • v.52 no.1
    • /
    • pp.52-57
    • /
    • 2014
  • The MCMB-$Li_4Ti_5O_{12}$ with core-shell structure was prepared by sol-gel process to improve low cycle capability of MCMB in this study. The electrochemical characteristics were investigated for hybrid capacitor using MCMB-$Li_4Ti_5O_{12}$ as the negative electrode and $LiMn_2O_4$, Active carbon fiber as the positive electrode. The electrochemical behaviors of hybrid capacitor using organic electrolytes ($LiPF_6$, EC/DMC/EMC) were characterized by charge/discharge, cyclic voltammetry, cycle and impedance tests. The hybrid capacitor using MCMB-$Li_4Ti_5O_{12}/LiMn_2O_4$ electrodes had better capacitance than MCMB hybrid systems and was able to deliver a specific energy with 67 Wh/kg at a specific power of 781 W/kg.

The analysis for the HCl modification effect and formation of TiO2 on activated carbon fiber surface (활성탄소섬유 표면의 염산처리효과와 TiO2 형성에 관한 분석)

  • Oh, Won-Chun;Han, Sang-Bum;Bae, Jang-Soon
    • Analytical Science and Technology
    • /
    • v.20 no.4
    • /
    • pp.279-288
    • /
    • 2007
  • We have studied a method for the preparation of $ACF/TiO_2$ composites involving the penetrationof titanium n-butoxide (TNB) solution into activated carbon fiber. It was focused on the characterization of $TiO_2$ formed in prorous carbon was which increased with surface functional groups by hydrochloric acid treatment. The conversion of TNB to $TiO_2$ for the acid treatment effect must be important for the preparationof $ACF/TiO_2$ composites. From the characterization of surface properties, both the BET surface area and the total pore volume decreased as the distribution of $TiO_2$ on the activated carbon fiber surfaces after acid treatments.The changes in XRD pattern showed the typical anatase type on $ACF/TiO_2$ composite for the sample named FT, FT1 and FT2 treated with 0.05, 0.1 and 0.5 M, respectively. However, XRD patern of FT3 treated with 0.5M showed mixed amatase-rutile structure. According to the results of SEM micrographs, the titanium complexe particles were irregularly distributed around carbon. And some large clusters were found when an amount of acid treatment increased. The EDX results of $ACF/TiO_2$ composites showed the presence of C, O and P with strong Ti peaks. Finally, the excellent photocatalytic activity of the $ACF/TiO_2$ composites between relative concentration($c/c_o$) of MB (methylene blue) and UV irradiation time could be attributed to the both effects between photocatalysis of the formation of titania complexes and adsorptivity of the activated carbon fiber.

The effects of oxygen partial pressure on $SrTiO_3$ films with $RuO_2$ bottom electrode ($SrTiO_3/RuO_2$ 박막 형성시 플라즈마 가스 주입비의 영향)

  • 박치선;김상훈;마재평
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.8 no.2
    • /
    • pp.286-291
    • /
    • 1998
  • $SrTiO_3$[ST] thin films were fabricated on $RuO_2$bottom electrodes by RF magnetron sputtering with various $Ar/O_2$ratio in sputtering gas. As the content of oxygen increases, the leakage current of ST films measured at $10^5$ V/cm decreases from $2.0{\times}10^{-6}A/{\textrm}{cm}^2(Ar/O_2=10/0)$ to $3.8{\times}10^{-7}A/{\textrm}cm^2(Ar/O_2=5/5)$, and the dielectric constant of ST films increases from $70(Ar/O_2=10/0)$ to $190(Ar/O_2=5/5)$. The improvement of electrical properties of ST films is mainly due to the structural modification of ST films such as better crystallinity, smooth surface morphology with the increase of oxygen content in the sputtering gas.

  • PDF

H2S tolerance effects of Ce0.8Sm0.2O2-δ modification on Sr0.92Y0.08Ti1-xNixO3-δ anode in solid oxide fuel cells

  • Kim, Kab In;Kim, Hee Su;Kim, Hyung Soon;Yun, Jeong Woo
    • Journal of Industrial and Engineering Chemistry
    • /
    • v.68
    • /
    • pp.187-195
    • /
    • 2018
  • $Sr_{0.92}Y_{0.08}Ti_{1-x}Ni_xO_{3-{\delta}}$ (SYTN) was investigated in the presence of $H_2S$ containing fuels to assess the feasibility of employing oxide materials as alternative anodes. Aliovalent substitution of $Ni^{2+}$ into $Ti^{4+}$ increased the ionic conductivity of perovskite, leading to improved electrochemical performance of the SYTN anode. The maximum power densities were 32.4 and $45.3mW/cm^2$ in $H_2$ at $900^{\circ}C$ for the SYT anode and the SYTN anode, respectively. However, the maximum power densities in 300 ppm of $H_2S$ decreased by 7% and by 46% in the SYT and the SYTN anodes, respectively. To enhance the sulfur tolerance and to improve the electrochemical properties, the surface of SYTN anode was modified with samarium doped ceria (SDC) using the sol-gel coating method. For the SDC-modified SYTN anode, the cell performance was mostly recovered in the pure $H_2$ condition after 500-ppm $H_2S$ exposure in contrast to the irreversible cell performance degradation exhibited in the unmodified SYTN anode.

Effects of SrTiO3-Modification on the Dielectric and Electromechanical Strain Properties of Lead-Free Bi1/2Na1/2TiO3-BiAlO3 Piezoceramics (Bi1/2Na1/2TiO3-BiAlO3 무연 압전 세라믹스의 유전 및 전기 기계적 변형 특성에 대한 SrTiO3 첨가 효과)

  • Lee, Sang Sub;Lee, Chang-Heon;Duong, Trang An;Kim, Dong Hyeok;Kim, Byeong Woo;Han, Hyoung-Su;Lee, Jae-Shin
    • Korean Journal of Materials Research
    • /
    • v.31 no.10
    • /
    • pp.562-568
    • /
    • 2021
  • (Bi1/2Na1/2)TiO3 (BNT)-based ceramics are considered promising candidates for actuator application owing to their excellent electromechanical strain properties However, to obtain large strain properties, there remain several issues such as thermal stability and high operating fields. Therefore, this study investigates a reduction of operating field in (0.98-x)Bi1/2Na1/2TiO3-0.02 BiAlO3-xSrTiO3 (BNT-2BA-100xST, x = 0.20, 0.21, 0.22, 0.23, and 0.24) via analyses of the microstructure, crystal structure, dielectric, polarization, ferroelectric and electromechanical strain properties. The average grain size of BNT-${\underline{2}}$BA-100xST ceramics decreases with increasing ST content. Results of polarization and electromechanical strain properties indicate that a ferroelectric to relaxor state transition is induced by ST modification. As a consequence, a large electromechanical strain of 592 pm/V is obtained at a relatively low electric field of 4 kV/mm in 22 mol% ST-modified BNT-2BA ceramics. We believe that the materials synthesized in this study are promising candidates for actuator applications.

Thermal properties of the surface-modified Inconel 617 (표면 처리에 따른 Inconel 617 합금의 고온 특성)

  • Cho, Hyun;Bang, Kwang-Hyun;Lee, Byeong-Woo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.19 no.6
    • /
    • pp.298-304
    • /
    • 2009
  • The effect of the surface treatments on the high temperature properties of the Inconel 617, one of the promising candidate alloys for high temperature heat-transport system, has been studied. Various surface modification methods including a rapid thermal process(RTP), a hydrothermal treatment, and a physical vapor deposition($2{\mu}m$ thick TiAlN film by an arc discharge) were applied to the Inconel 617. The morphological and the structural properties of the surface-modified Inconel 617 samples after heat treatment at $1000^{\circ}C$ in the air were compared to find out whether inhomogeneous formation of $Cr_2O_3$ crust at the surface region was suppressed or not. TiAlN-coated Inconel 617 showed homogeneous microstructure and the lowest wear loss compared to bare, RTP- and hydrothermally-treated Inconel 617 by suppressing the $Cr_2O_3$ crust formation.

Electrical Properties and Phase Transition Behavior of Lead-Free BaTiO3-Modified Bi1/2Na1/2TiO3-SrTiO3 Piezoelectric Ceramics (BaTiO3 첨가에 따른 Bi1/2Na1/2TiO3-SrTiO3 무연 압전 세라믹스의 전기적 특성 및 상전이 거동 연구)

  • Kang, Yubin;Park, Jae Young;Devita, Mukhllishah Aisyah;Duong, Trang An;Ahn, Chang Won;Kim, Byeong Woo;Han, Hyoung-Su;Lee, Jae-Shin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.35 no.5
    • /
    • pp.516-521
    • /
    • 2022
  • We investigated the microstructure, crystal structure, dielectric, and elecromechanical strain properties of lead-free BaTiO3 (BT)-modified (Bi1/2Na1/2)TiO3-SrTiO3 (BNT-ST) piezoelectric ceramics. Samples were prepared by a conventional ceramic processing route. Temperature dependent dielectric properties confirmed that a phase transition from a nonergodic relaxor to an ergodic relaxor was induced when the BT concentration reached 1.5 mol%, interestingly, where the average grain size reached a maximum value of 4.5 ㎛. At the same time, enhanced electromechanical strain (Smax/Emax = 600 pm/V) was obtained. It is suggested that the induced ferroelectric-relaxor phase transition by the BT modification is responsible for the enhancement of electromechanical strain in 1.5 mol% BT-modified BNT-ST ceramics.

Effects of Bi(Mg1/2Sn1/2)O3 Modification on the Dielectric and Piezoelectric Properties of Bi1/2(Na0.8K0.2)1/2TiO3 Ceramics (Bi1/2(Na0.8K0.2)1/2TiO3 세라믹스의 유전 및 압전 특성에 대한 Bi(Mg1/2Sn1/2)O3 변성 효과)

  • Pham, Ky Nam;Dinh, Thi Hinh;Lee, Hyun-Young;Kong, Young-Min;Lee, Jae-Shin
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.3
    • /
    • pp.266-271
    • /
    • 2012
  • The effect of $Bi(Mg_{1/2}Sn_{1/2})O_3$ (BMS) modification on the crystal structure, ferroelectric and piezoelectric properties of $Bi_{1/2}(Na_{0.8}K_{0.2})_{1/2}TiO_3$ (BNKT) ceramics has been investigated. The BMS-substitution induced a transition from a ferroelectric (FE) tetragonal to a nonpolar pseudocubic phase, leading to degradations in the remnant polarization, coercive field, and piezoelectric coefficient $d_{33}$. However, the electric-field-induced strain was significantly enhanced by the BMS substitution-induced phase transition and reached a highest value of $S_{max}/E_{max}$ = 633 pm/V under an applied electric field of 6 kV/mm when the BMS content reached 6 mol%. The abnormal enhancement in strain was attributed to the field-induced transition of the pseudocubic symmetry to other asymmetrical structure, which was not clarified in this work.

Surface modification of $TiO_2$ by atmospheric pressure plasma

  • Jo, Sang-Jin;Jeong, Chung-Gyeong;Bu, Jin-Hyo
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.08a
    • /
    • pp.96-96
    • /
    • 2010
  • To improve surface wettability, each sample was treated by atmospheric pressure plasma (APP) using dielectric barrier discharge (DBD) system. Argon and oxygen gases were used for treatment gas to modify the $TiO_2$ surface by APP with RF power range from 50 to 200 W. Water contact angle was decreased from $20^{\circ}$ to $10^{\circ}$ with argon only. However, water contact angle was decreased from $20^{\circ}$ to < $1^{\circ}$ with mixture of argon and oxygen. Water contact angle with $O_2$ plasma was lower than water contact angle with Ar plasma at the same RF power. It seems to be increasing the polar force of $TiO_2$ surface. Also, analysis result of X-ray photoelectron spectra (XPS) shows the increase of intensity of O1s shoulder peak, resulting in increasing of surface wettability by APP. Moreover, each water contact angle increased according to increase past time. However, contact angle increase with plasma treatment was lower than without plasma treatment. Additionally, the efficiency of $TiO_2$ photocatalyst was improved by plasma surface-treatment through the degradation experiment of phenol

  • PDF