BLN-PZT 세라믹의 상전이 특성 (Phase Transition Characteristics of the BLN - PZT Ceramics.)

  • 류기원;이영종;배선기;이영회
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1994년도 춘계학술대회 논문집
    • /
    • pp.25-33
    • /
    • 1994
  • Temperature dependences of the remanent polarization $P_{\gamma}$/(T), effective birefringence ㅿn(T). dielectric constant K(T) and quadratic electro-optic coefficient R(T) of the two-stage sintered xBa(La$_{1/2}$Nb$_{1/2}$)O$_3$Pb$(Zr_{y}Ti_{1-y})O-{3}$(x=0.085, 0.09, 0.40$\leq$y$\leq$0.70)ceramics were investigated. Increasing the PbZrO$_3$ contents, the crystal structure of a specimen was varied from tetragonal and rhombohedral to cubic, and the phase transition was showed a diffuse phase transition(DPT) characteristics. Especially. in the compositions which located on the PE-FE phase boundary were showed a discrepancy between curie temperature and temperature range which a macroscopic polarization and a effective birefringence were disappeared.

  • PDF

새로운 파이로클로어의 합성 및 결정화학적 특징 (Synthesis and Crystal Chemistry of New Actinide Pyrochlores)

  • 장영남;채수천;배인국
    • 한국광물학회지
    • /
    • 제15권1호
    • /
    • pp.78-84
    • /
    • 2002
  • New pyrochlore-type phases($A_2$$B_2$$O_{7}$) were synthesized in the systems: CaO-C$eO_2$-T$iO_2$, CaO-$UO_2$(T$hO_2$)-Z$rO_2$, CaO-$UO_2$(T$hO_2$)-$Gd_2$$O_3$-T$iO_2$-Z$rO_2$, 및 CaO-T$hO_2$-S$nO_2$. The starting materials were pressed with the pressure of 200~400 MPa and sintered at 1500~ 155$0^{\circ}C$ for 4~8 hours in air and at 1300~ 135$0^{\circ}C$ for 5 ~50 hours under oxygen atmosphere. The products were characterized using XRD, SEM/EDS and TEM. In the bulk compositions of CaCe$Ti_2$$O_{7}$, CaTh$Zr_2$$O_{7}$,($Ca_{0.5}$ Gd$Th_{0.5}$)(ZrTi)$O_{7}$) ($Ca_{0.5}$Gd$Th_{0.5}$)(ZrTi)$O_{7}$, ($Ca_{0.5}$G$dU_{0.5}$)(ZrTi)$O_{7}$ and CaTh$Sn_2$$O_{7}$ , pyrochlore was the major phase, together with other oxide phase $of_2$$O_{7}$ fluorite structure. In the samples with target compositions CaU$Zr_2$$O_2$$Ca_{0.5}$ G$dU_{0.5}$)$Zr_2$T$iO_{7}$ pyrochlore was not identified, but a fluorite-structured phase was detected. The formation factor as the stable phase depended on crystal chemical characteristics of the actinide and lanthanide elements of the system concerned.

EFFECTS OF PROTEIN LEVEL AND EXTRUSION PROCESSING OF SOYBEAN MEAL ON THE PERFORMANCE OF GROWING PIGS

  • Paik, I.K.;Um, J.S.;Lee, S.H.;Chung, M.S.
    • Asian-Australasian Journal of Animal Sciences
    • /
    • 제8권2호
    • /
    • pp.129-133
    • /
    • 1995
  • A feeding trial was conducted to evaluate the effects of crude protein concentration (44% vs 48%) and extrusion processing of soybean meal (SBM) on the performance of weanling and growing pigs. One hundred and ninety two (96 pigs of each sex) 3 way crossed (Landrace ${\times}$ Hampshire ${\times}$ Duroc) weaned pigs were allotted to 12 pens each of 16 pigs (8 pigs of each sex). Three pens were assigned to each of the 4 treatment; $T_1$; 44% SBM diet, $T_2$; extruded 44% SBM diet, $T_3$; 48% SBM diet and $T_4$; extruded 48% SBM diet. The 44% SBM diet was formulated to have 18% CP for the starter phase (5-10 wk of age) and 15% CP for the grower phase (10-15 wk of age). The other treatments used equivalent amount of each SBM, replacing the 44% SBM. Chemical assay showed that extrusion processing generally decreased amino acid content especially total lysine and available lysine. Extrusion increased Hunterlab color +a value and decreased the urease activity index. The body weight gains for the $T_3$ and $T_4$ pigs were significantly(p < 0.05) greater than for those on $T_1$ and $T_2$ for the starter phase, but not the grower phase. Extrusion processing did not improve weight gain. Feed intake for the overall period was significantly(p < 0.05) different among treatments. The feed conversion ratios were not significantly different among treatments. An economic analysis showed that the high protein (48%) SBM diet was more cost effective than the low protein(44%) SBM diet, for the starter phase.

Effects on G2/M Phase Cell Cycle Distribution and Aneuploidy Formation of Exposure to a 60 Hz Electromagnetic Field in Combination with Ionizing Radiation or Hydrogen Peroxide in L132 Nontumorigenic Human Lung Epithelial Cells

  • Jin, Hee;Yoon, Hye Eun;Lee, Jae-Seon;Kim, Jae-Kyung;Myung, Sung Ho;Lee, Yun-Sil
    • The Korean Journal of Physiology and Pharmacology
    • /
    • 제19권2호
    • /
    • pp.119-124
    • /
    • 2015
  • The aim of the present study was to assess whether exposure to the combination of an extremely low frequency magnetic field (ELF-MF; 60 Hz, 1 mT or 2 mT) with a stress factor, such as ionizing radiation (IR) or $H_2O_2$, results in genomic instability in non-tumorigenic human lung epithelial L132 cells. To this end, the percentages of G2/M-arrested cells and aneuploid cells were examined. Exposure to 0.5 Gy IR or 0.05 mM $H_2O_2$ for 9 h resulted in the highest levels of aneuploidy; however, no cells were observed in the subG1 phase, which indicated the absence of apoptotic cell death. Exposure to an ELF-MF alone (1 mT or 2 mT) did not affect the percentages of G2/M-arrested cells, aneuploid cells, or the populations of cells in the subG1 phase. Moreover, when cells were exposed to a 1 mT or 2 mT ELF-MF in combination with IR (0.5 Gy) or $H_2O_2$ (0.05 mM), the ELF-MF did not further increase the percentages of G2/M-arrested cells or aneuploid cells. These results suggest that ELF-MFs alone do not induce either G2/M arrest or aneuploidy, even when administered in combination with different stressors.

(Na,K)NbO3계 무연 압전체에서 Cu2O 첨가물의 농도 변화에 따른 미세구조 및 전기적 특성 평가 (Evaluation of Microstructure and Electrical Properties in (Na,K)NbO3-Based Pb-free Piezoelectrics Doped with Various Cu2O Concentration)

  • 이윤기;류성림;권순용
    • 한국전기전자재료학회논문지
    • /
    • 제24권11호
    • /
    • pp.870-875
    • /
    • 2011
  • The $(Na_{0.52}K_{0.44})(Nb_{0.9}Sb_{0.06})O_3-0.04dLiTaO_3$ (NKNS-LT) ceramics with various $Cu_2O$ concentration were prepared by the conventional solid state reaction method. The $Cu_2O$ content was varied in the range of 0.1~0.4 wt%. The effects of Cu on microstructure, crystallographic phase transition, and piezoelectric properties were investigated. The material with perovskite structure had a tetragonal phase (T1) when $Cu_2O$ concentration was less than 0.3 wt% and it transformed to another tetragonal phase (T2) when the $Cu_2O$ amount was greater than 0.3 wt%. The phase boundary between T1 and T2 phases appeared at around 0.3 wt% of $Cu_2O$ concentration. The piezoelectric properties were shown the maximum values at the composition of the phase boundary. The electro-mechanical coupling factor ($k_p$) was 0.42 and the piezoelectric charge constant ($d_{33}$) was 245 pC/N at the 0.3 wt% of $Cu_2O$ concentration.

인체 유방암 세포에서 과다발현 시킨 Cyclin D2의 영향에 대한 연구 (Effect of Cyclin D2 on Cell Proliferation in T-47D Breast Cancer Cells)

  • 김현준;이근수;전상학;공구
    • 한국환경성돌연변이발암원학회지
    • /
    • 제24권1호
    • /
    • pp.1-9
    • /
    • 2004
  • Three D-type cyelins (D1, D2, and D3) are expressed in G1 phase of the cell cyele and have been implicated in cell transformation and neoplasia in human and mouse. Cyclin D1 overexpression or amplification was described in various human cancers. However, there is controversy about the role of cyclin D2 in cell cyele progression and human carcinogenesis. Specially, loss of cyelin D2 is involved in a vital tumor suppressor function in normal breast tissue, and that its loss may be related to tumorigenesis. The author examined to effect over-expression of cyclin D2 on the cell proliferation, apoptosis, and cell cycle using cyclin D2 transfected stable T47D breast cancer cells to investigate whether cyclinD2 functions as a positive regulator or negative regulator in cell proliferation. Overexpression of cyclin D2 led to the suppression of cell growth in cyclin D2 transfected T47D in both in its expression level and a time dependent manner with up to 50% reduction of cell growth at 72 hours. Therefore, the authors performed the cell cycle phase analysis using the flow cytometry to investigate the effect of cyclin D2 on the cell cycle phase in cyclin D2 transfected stable T47D cells. The flow cytometry analysis revealed increased sub G0 phase in cyclin D2 transfeted cells up to 23% at 72 hours. To confirm these results induced by overexpression of cyclinD2, the apoptotic bodies were counted in control and cyclin D2 transfected T47 cells. There are markedly increases of apoptotic bodies in cyclin D2-transfected cells up to 18%. These results suggested that Cyclin D2 suppresses the cell proliferation in breast cancers cells via the induction of apotosis.

  • PDF

${NH}_{3}$ 분위기에서 급속열처리에 의한 TiN/${TiSi}_{2}$ 이중구조막의 특성에 대한 고찰 (A Study on the Properties of TiN/${TiSi}_{2}$ Bilayer by a Rapid Thermal Anneal in ${NH}_{3}$ Ambient)

  • 이철진;성영권
    • 대한전기학회논문지
    • /
    • 제41권8호
    • /
    • pp.869-874
    • /
    • 1992
  • The physical and electrical properties of TiN/TiSiS12T bilayer were studied. The TiN/TiSiS12T bilayer was formed by rapid thermal anneal in NHS13T ambient after the Ti film was deposited on silicon substrate. The Ti film reacts with NHS13T gas to make a TiN layer at the surface and reacts with silicon to make a TiSiS12T layer at the interface respectively. It was found that the formation of TiN/TiSiS12T bilayer depends on RTA temperature. In this experiment, competitive reaction for TiN/TiSiS12T bilayer occured above $600^{\circ}C$. Ti-rich TiNS1xT layer and Ti-rich TiSiS1xT layer and Ti-rich TiSiS1xT layer were formed at $600^{\circ}C$. stable structure TiN layer TiSiS12T layer which has CS149T phase and CS154T phase were formed at $700^{\circ}C$. Both stable TiN layer and CS154T phase TiSiS12T layer were formed at 80$0^{\circ}C$. The thickness of TiN/TiSiS12T bilayer was increased as the thickness of deposited Ti film increased.

  • PDF

Two-Phase Magnet in the Co/Co2MnSn System

  • Kim, Tae-Wan;Yim, Hye-In;Lee, Hyun-Yong;Lee, Kyoung-Il
    • Journal of Magnetics
    • /
    • 제16권1호
    • /
    • pp.10-14
    • /
    • 2011
  • This study reports on Co/$Co_2$MnSn two-phase magnets. The Co/$Co_2$MnSn two-phase magnet has Co precipitates in a $Co_2MnSn$ Heusler alloy matrix, in which the two phases are exchange-coupled at the phase boundary. The as-casted Co/$Co_2$MnSn system, which has Co-Mn solid solution precipitates in a $Co_2$MnSn Heusler alloy matrix, showed that the Co solid solution precipitates are crystallographically coherent and there is exchange coupling at the phase boundary. To form pure Co precipitates by removal of Mn solute atoms in Co-Mn solid solution, annealing was carried out 48 hours at $870^{\circ}C$. After annealing, the low $T_c$ and low magnetization phase of the Co-Mn solid solution became a high $T_c$ and high magnetization phase of hexagonal Co.

바이폴라 델타 구동 GMSK에 대한 복조 (The Demodulation for Bipolar Delta Driven GMSK)

  • 방승철
    • 한국통신학회논문지
    • /
    • 제38B권10호
    • /
    • pp.824-831
    • /
    • 2013
  • 델타 구동 GMSK는 바이폴라 델타 신호로 가우시안 펄스를 생성하고 $+T_b/2$$-T_b/2$ 사이의 차분 신호로 위상변조하는 방식이다. 이러한 방식에 대한 복조는 기존의 GMSK와는 다르게 설계해야 한다. 본 논문에서는 인접한 비트 간의 위상 변화를 검출하고 위상 영역을 경판정한 다음에 상태 전이로 이진 데이터를 복원하는 방식을 설계하였다. AWGN 채널에 대한 전산모의실험 결과, 이진 데이터의 런 랭스에 의한 비트 오율의 영향이 확인되었으며, 이론적인 코히어런트 복조의 BER과 비교해서 $BT_b$=0.3에 대하여 2[dB] 정도의 성능 저하가 있는 것으로 분석되었다.

분극된 <001> 방위 Pb(Mg1/3Nb2/3)O3-PbTiO3 단결정의 유전 특성 및 상전이 (Dielectric Properties and Phase Transformation of Poled <001>-Oriented Pb(Mg1/3Nb2/3)O3-PbTiO3 Single Crystals)

  • 이은구;이재갑
    • 한국재료학회지
    • /
    • 제22권7호
    • /
    • pp.342-345
    • /
    • 2012
  • The dielectric properties and phase transformation of poled <001>-oriented $Pb(Mg_{1/3}Nb_{2/3})O_3-x%PbTiO_3$(PMN-x%PT) single crystals with compositions of x = 20, 30, and 35 mole% are investigated for orientations both parallel and perpendicular to the [001] poling direction. An electric-field-induced monoclinic phase was observed for the initial poled PMN-30PT and PMN-35PT samples by means of high-resolution synchrotron x-ray diffraction. The monoclinic phase appears from $-25^{\circ}C$ to $100^{\circ}C$ and from $-25^{\circ}C$ to $80^{\circ}C$ for the PMN-30PT and PMN-35PT samples, respectively. The dielectric constant (${\varepsilon}$)-temperature (T) characteristics above the Curie temperature were found to be described by the equation$(1/{\varepsilon}-1/{\varepsilon}_m)^{1/n}=(T-T_m)/C$, where ${\varepsilon}_m$ is the maximum dielectric constant and $T_m$ is the temperature giving ${\varepsilon}_m$, and n and C are constants that change with the composition. The value of n was found to be 1.82 and 1.38 for 20PT and 35PT, respectively. The results of mesh scans and the temperature-dependence of the dielectric constant demonstrate that the initial monoclinic phase changes to a single domain tetragonal phase and a to paraelectric cubic phase. In the ferroelectric tetragonal phase with a single domain state, the dielectric constant measured perpendicular to the poling direction was dramatically higher than that measured in the parallel direction. A large dielectric constant implies easier polarization rotation away from the polar axis. This enhancement is believed to be related to dielectric softening close to the morphotropic phase boundary.