The Structural and Dielectric Properties of the PZT/BST Heterolayered Thin Films with RF Power (RF Power에 따른 PZT/BST 이종층 박막의 구조 및 유전 특성)

  • Lee Sang-Chul;Nam Sung-Pil;Lee Sung-Gap;Lee Young-Hie
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.54 no.1
    • /
    • pp.13-17
    • /
    • 2005
  • The Pb(Zr/sub 0.52/Ti/sub 0.48/)O₃/(Ba/sub 0.6/Sr/sub 0.4/)TiO₃[PZT/BST] heterolayered thin films were deposited on Pt/Ti/SiO₂/Si substrates by using the RF sputtering method with different RF power. The PZT/BST heterolayered thin films had the tetragonal structure of the PZT phase and BST phase. Increasing the RF power. the intensity of the PZT (100), (110) peaks and BST (111) peaks were decreased and the intensity of the BST (100), (110) peaks were increased. The thickness ratio of the top layered BST thin film and the bottom layered PZT thin film was 2 to1. The atomic concentration of the Ba, Sr, Pb. Zr, Ti atoms were constant in the PZT thin films and BST thin films, respectively. The Pt atom was diffused to the PZT region in the PZT/BST heterolayered thin films deposited at condition of 60[W] RF power. Increasing the frequency, dielectric constant and loss of the PZT/BST heterolayered thin films were decreased. The dielectric constant and loss of the PZT/BST heterolayered thin films deposited with RF power of 90[W] were 406 and 3%, respectively.

Structural, Dielectric and Field-Induced Strain Properties of La-Modified Bi1/2Na1/2TiO3-BaTiO3-SrZrO3 Ceramics

  • Hussain, Ali;Maqbool, Adnan;Malik, Rizwan Ahmed;Zaman, Arif;Lee, Jae Hong;Song, Tae Kwon;Lee, Jae Hyun;Kim, Won Jeong;Kim, Myong Ho
    • Korean Journal of Materials Research
    • /
    • v.25 no.10
    • /
    • pp.566-570
    • /
    • 2015
  • $Bi_{0.5}Na_{0.5}TiO_3$ (BNT) based ceramics are considered potential lead-free alternatives for $Pb(Zr,Ti)O_3$(PZT) based ceramics in various applications such as sensors, actuators and transducers. However, BNT-based ceramics have lower electromechanical performance as compared with PZT based ceramics. Therefore, in this work, lead-free bulk $0.99[(Bi_{0.5}Na_{0.5})_{0.935}Ba_{0.065}]_{(1-x)}La_xTiO_3-0.01SrZO_3$ (BNBTLax-SZ, with x = 0, 0.01, 0.02) ceramics were synthesized by a conventional solid state reaction The crystal structure, dielectric response, degree of diffuseness and electric-field-induced strain properties were investigated as a function of different La concentrations. All samples were crystallized into a single phase perovskite structure. The temperature dependent dielectric response of La-modified BNBT-SZ ceramics showed lower dielectric response and improved field-induced strain response. The field induced strain increased from 0.17%_for pure BNBT-SZ to 0.38 % for 1 mol.% La-modified BNBT-SZ ceramics at an applied electric field of 6 kV/mm. These results show that La-modified BNBT-SZ ceramic system is expected to be a new candidate material for lead-free electronic devices.

Piezoelectric property of PZT ceramics by DC field and corona discharge poling (직류전계 및 corona방전에 따른 PZT 세라믹스의 분극과 압전특성)

  • Park, In-Cheol;Im, Jin-Ho;Lee, Jun-Hyeong;Jo, Sang-Hui
    • Korean Journal of Materials Research
    • /
    • v.5 no.2
    • /
    • pp.178-183
    • /
    • 1995
  • Piezoelectric properties of sintered specimen having a tetragonal phase of $Pb_{0.9888}Sr_{0.012}(Zr_{0.52}Ti_{0.48})O_{3}$ were comparatively studied with two different poling methodes, i.e., DC field and corona discharge technique. Internal stress of poled specimens by indentation fracture toughness was analyzed to evaluate degradation phenomenon. As the results, it was confirmed that corona discharge poling technique is practicable and has merits such as low-temperature poling, slow degradation and no electric breakdown comparing to DC field poling. However, corona discharge technique showed lower Kp value than DC field poling.

  • PDF

Comparison of Abnormal Grain Growth Behavior of Lead-Free (Na,K)NbO3-M(Cu,Nb)O3, (M = Ca, Sr, Ba) Piezoelectric Ceramics (비납계 (Na,K)NbO3-M(Cu,Nb)O3, (M = Ca, Sr, Ba) 압전 세라믹의 비정상 결정 성장 거동 비교)

  • Jung, Seungwoon;Lim, Ji-Ho;Jung, Han-Bo;Ji, Sung-Yub;Choi, Seunggon;Jeong, Dae-Yong
    • Korean Journal of Materials Research
    • /
    • v.30 no.7
    • /
    • pp.343-349
    • /
    • 2020
  • NKN [(Na,K)NbO3] is a candidate lead-free piezoelectric material to replace PZT [Pb(Zr,Ti)O3]. A single crystal has excellent piezoelectric-properties and its properties are dependent of the crystal orientation direction. However, it is hard to fabricate a single crystal with stoichiometrically stable composition due to volatilization of sodium during the growth process. To solve this problem, a solid solution composition is designed (Na,K)NbO3-Ba(Cu,Nb)O3 and solid state grain growth is studied for a sizable single crystal. Ceramic powders of (Na,K)NbO3-M(Cu,Nb)O3 (M = Ca, Sr, Ba) are synthesized and grain growth behavior is investigated for different temperatures and times. Average normal grain sizes of individual specimens, which are heat-treated at 1,125 ℃ for 10 h, are 6.9, 2.8, and 1.6 ㎛ for M = Ca, Sr, and Ba, respectively. Depending on M, the distortion of NKN structure can be altered. XRD results show that (NKN-CaCuN: shrunken orthorhombic; NKN-SrCuN: orthorhombic; NKN-BaCuN: cubic). For the sample heat-treated at 1,125 ℃ for 10 h, the maximum grain sizes of individual specimens are measured as 40, 5, and 4,000 ㎛ for M = Ca, Sr, and Ba, respectively. This abnormal grain size is related to the partial melting temperature (NKN-CaCuN: 960 ℃; NKN-SrCuN: 971 ℃; NKN-BaCuN: 945 ℃).

A Study on the Coloration of the $Nd_2O_3$ Containing Glass by X-ray Irradiation ($Nd_2O_3$ 함유 유리의 X-선조사에 따른 변색에 관한 연구)

  • 박용원;강원호
    • Journal of the Korean Ceramic Society
    • /
    • v.21 no.4
    • /
    • pp.373-381
    • /
    • 1984
  • The coloration of the $Nd_2O_3$ contained $R_2O-BaO-SrO-ZrO_2-SiO_2$ glass added the various amount of $CeO_2$ $MnO_2$, $Fe_2O_3$ and $As_2O_3$ alone or together by the irradiation of X-ray irradiation,. The glasses added $CeO_2$ in proportion to amount were more effective on preventing coloration by X-ray irradiation but the addition of $MnO_2$ produced different color according to the amount of addition. The addition of the $Fe_2O_3$, $TiO_2$ and $As_2O_3$ did not give much effects to the transmission changes of $Nd_2O_3$ contained glass by X-ray irradiation but the glass added $CeO_2$ , $Fe_2O_3$, $TiO_2$ together was most effective to prevent coloration and transmisson changes.

  • PDF

Effects of Sr on the Characteristics of PZT Ceramics Prepared by Hydrothermal Process (수열합성법에 의해 제조된 PZT의 특성에 미치는 Sr의 영향)

  • Yang, Beom-Seok;Shin, Chang-Yun;Won, Chang-Whan
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.11
    • /
    • pp.681-687
    • /
    • 2008
  • The sintering and electrical properties of the hydrothermal PSZT powders obtained by substituting 4, 6 and 8mol% Sr for Pb in PZT lattice structure were investigated. The lattice constant and particle size decreased in proportion to a quantity of Sr. The sintering properties of PSZT powders showed $7.754g/cm^3$ of sintered density and $4{\mu}m$ of grain size at sintering temperature of $1250^{\circ}C$. Curie temperature lowered gradually from $363.6^{\circ}C\;to\;319.2^{\circ}C$ and relative dielectric constants increased rapidly by a quantity of Sr. In comparison to PZT, moreover, the quality factor of PSZT was increased more than three times with increase of Sr mole ratio, and piezoelectric constant $(d_{31}\;and\;g_{31})$ was decreased. It was found that dielectric loss of PSZT was decreased by 0.574% which was half of PZT.

Dielectric and piezoelectric properties of (1-x)$(Na_{0.5}K_{0.5})NbO_3$ - $x(Ba_{(1-y)}Sr_y)TiO_3$ ceramics ((1-x)$(Na_{0.5}K_{0.5})NbO_3$ - $x(Ba_{(1-y)}Sr_y)TiO_3$의 유전 및 압전 특성)

  • Kim, Mi-Ro;Song, Hyun-Cheol;Choi, Ji-Won;Cho, Young-Soo;Kim, Hyun-Jai;Yoon, Seok-Jin
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.59-59
    • /
    • 2008
  • Pb(Zr,Ti)$O_3$(PZT)는 현재 가장 우수한 압전특성을 가진 압전 재료로써, 압전효과와 역압전효과를 이용한 압전 액추에이터, 압전 트랜스듀서, 센서, 레조네이터 등의 활동에 대한 연구과 활발하게 이루어 지고 있다. 그러나 압전성이 우수한 PZT 세라믹스들은 Pb 성분이 포함되어 있기 때문에 환경오염뿐 아니라, 경제적인 측면에서도 많은 문제점을 가지고 있어 최근에는 유해원소인 Pb를 포함하지 않는 친환경 압전 세라믹스에 관한 연구가 활발히 진행되고 있다. (Na, K)$NbO_3$은 뛰어난 특성을 가지고 있어 Pb를 기본조성으로 하는 압전세라믹스를 대체할 수 있는 대표적인 물질중의 하나로 알려져 있다. 그러나, potassium의 수분과의 반응성과, 소결시 휘발로 인해 높은 소결밀도의 NKN을 제조하기 어렵다. 이러한 단점을 보안하기 위해 Hot pressing, Hot forging, SPS 등 여러가지 방법을 이용하여 연구가 수행되고 있지만, 고가의 제조공정을 이용해야만 한다. 본 연구에서는 $BaSrTiO_3$의 새로운 고용체를 추가시켜 기본 NKN 조성보다 소결밀도, 유전 및 압전특성을 향상시키고자 하였다.

  • PDF

Performance Characteristics of Anode-Supported Tubular Solid Oxide Fuel Cell (연료극 지지체식 원통형 고체산화물 연료전지의 성능 특성)

  • Song Rak-Hyun;Song Keun-Suk
    • Korean Journal of Materials Research
    • /
    • v.14 no.5
    • /
    • pp.368-373
    • /
    • 2004
  • To improve the conventional cathode-supported tubular solid oxide fuel cell (SOFC) from the viewpoint of low cell power density, expensive fabrication process and high operation temperature, the anode-supported tubular solid oxide fuel cell was investigated. The anode tube of Ni-8mol% $Y_2$O$_3$-stabilized $ZrO_2$ (8YSZ) was manufactured by extrusion process, and, the electrolyte of 8YSZ and the multi-layered cathode of $LaSrMnO_3$(LSM)ILSM-YSZ composite/$LaSrCoFeO_3$ were coated on the surface of the anode tube by slurry dip coating process, subsequently. Their cell performances were examined under gases of humidified hydrogen with 3% water and air. In the thermal cycle condition of heating and cooling rates with $3.33^{\circ}C$/min, the anode-supported tubular cell showed an excellent resistance as compared with the electrolyte-supported planar cell. The optimum hydrogen flow rate was evaluated and the air preheating increased the cell performance due to the increased gas temperature inside the cell. In long-term stability test, the single cell indicated a stable performance of 300 mA/$\textrm{cm}^2$ at 0.85 V for 255 hr.

Geochemical and Nd-Sr Isotope Studies for Foliated Granitoids and Mylonitized Gneisses from the Myeongho Area in Northeast Yecheon Shear Zone (예천전단대 북동부 명호지역 엽리상 화강암류와 압쇄 편마암류에 대한 지구화학 및 Nd-Sr 동위원소 연구)

  • Kim, Sung-Won;Lee, Chang-Yun;Ryu, In-Chang
    • Economic and Environmental Geology
    • /
    • v.41 no.3
    • /
    • pp.299-314
    • /
    • 2008
  • The NE-trending Honam shear zone is a broad, dextral strike-slip fault zone between the southern margin of the Okcheon Belt and the Precambrian Yeongnam Massif in South Korea and is parallel to the trend of Sinian deformation that is conspicuous in Far East Asia. In this paper, we report geochemical and isotopic(Sr and Nd) data of mylonitic quartz-muscovite Precambrian gneisses and surrounding foliated hornblende-biotite granitoids near the Myeongho area in the Yecheon Shear Zone, a representative segment of the Honam Shear Zone. Foliated hornblende-biotite granitoids commonly plot in the granodiorite field($SiO_2=61.9-67.1\;wt%$ and $Na_2O+K_2O=5.21-6.99\;wt%$) on $SiO_2$ vs. $Na_2O+K_2O$ discrimination diagram, whereas quartz-muscovite Precambrian orthogneisses plot in the granite field. The foliated hornblende-biotite granitoids are mostly calcic and calc-alkalic and are dominantly magnesian in a modified alkali-lime index(MALI) and Fe# [$=FeO_{total}(FeO_{total}+MgO)$] versus $SiO_2$ diagrams, which correspond with geochemical characteristics of Cordilleran Mesozoic batholiths. The foliated hornblende-biotite granitoids have molar ratios of $Al_2O_3/(CaO+Na_2O+K_2O)$ ranging from 0.89 to 1.10 and are metaluminous to weakly peraluminous, indicating I type. In contrast, Paleoproterozoic orthogneisses have peraluminous compositions, with molar ratios of $Al_2O_3/(CaO+Na_2O+K_2O)$ ranging from 1.11 to 1.22. On trace element spider diagrams normalized to the primitive mantle, the large ion lithophile element(LILE) enrichments(Rb, Ba, Th and U) and negative Ta-Nb-P-Ti anomalies of foliated hornblende-biotite granitoids and mylonitized quartz-muscovite gneisses in the Yecheon Shear Zone are features common to subduction-related granitoids and are also found in granitoids from a crustal source derived from the arc crust of active continental margin. ${\varepsilon}_{Nd}(T)$ and initial Sr-ratio ratios of foliated hornblende-biotite granitoids with suggest the involvement of upper crust-derived melts in granitoid petrogenesis. Foliated hornblende-biotite granitoids in the study area, together with the Yeongju Batholith, show not changing contents of specific elements(Ti, P, Zr, V and Y) from shear zone to the area near the shear zone. These results suggest that no volume changes and geochemical alterations in fluid-rich foliated hornblende-biotite granitoids may occur during deformation, which mass transfer by fluid flow into the shear zone is equal to the mass transfer out of the shear zone.

Fabrication and Performance of Anode-Supported Flat Tubular Solid Oxide Fuel Cell Unit Bundle (연료극 지지체식 평관형 고체산화물 연료전지 단위 번들의 제조 및 성능)

  • Lim, Tak-Hyoung;Kim, Gwan-Yeong;Park, Jae-Layng;Lee, Seung-Bok;Shin, Dong-Ryul;Song, Rak-Hyun
    • Journal of the Korean Electrochemical Society
    • /
    • v.10 no.4
    • /
    • pp.283-287
    • /
    • 2007
  • KIER has been developing the anode-supported flat tubular solid oxide fuel cell unit bundle for the intermediate temperature($700{\sim}800^{\circ}C$) operation. Anode-supported flat tubular cells have Ni/YSZ cermet anode support, 8 moi.% $Y_2O_3$ stabilized $ZrO_2(YSZ)$ thin electrolyte, and cathode multi-layer composed of Sr-doped $LaSrMnO_3(LSM)$, LSM-YSZ composite, and $LaSrCoFeO_3(LSCF)$. The prepared anode-supported flat tubular cell was joined with ferritic stainless steel cap by induction brazing process. Current collection for the cathode was achieved by winding Ag wire and $La_{0.6}Sr_{0.4}CoO_3(LSCo)$ paste, while current collection for the anode was achieved by using Ni wire and felt. For making stack, the prepared anode-supported flat tubular cells with effective electrode area of $90\;cm^2$ connected in series with 12 unit bundles, in which unit bundle consists of two cells connected in parallel. The performance of unit bundle in 3% humidified $H_2$ and air at $800^{\circ}C$ shows maximum power density of $0.39\;W/cm^2$ (@ 0.7V). Through these experiments, we obtained basic technology of the anode-supported flat tubular cell and established the proprietary concept of the anode-supported flat tubular cell unit bundle.