• Title/Summary/Keyword: $Pb^{4+}$

Search Result 3,208, Processing Time 0.03 seconds

Effect of Pb Content on the Phase Transformation of Sputter-Deposited PZT Thin Film During RTA (PZT 박막의 급속열처리시 Pb 함량이 상변태에 미치는 영향)

  • 주재현;길덕신;주승기
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.10
    • /
    • pp.803-810
    • /
    • 1993
  • PbxZr0.4Ti0.6O3 thin films were prepared by reactive co-sputtering and annealed by RTA(Rapid Thermal Annealing) process. Effect of Pb content in PbxZr0.4Ti0.6O3 films on the phase transformation was intensively studied. It has been found out that depending on the Pb content as well as RTA temperature, crystal structure of PbxZr0.4Ti0.6O3 films change greatly. It turned out that transformation temperature for perovskite can be lowered and the width of transition temperature region was reduced by increasing Pb content in the film. And the lattice was expanded with increasing Pb content. With increasing RTA temperature, as-deposited phase was transformed into perovskite through three different transformation paths depending on Pb content. It was confirmed that activation energies for nucleation of perovskite structure are much larger than those of its growth.

  • PDF

Sol-Gel Template Synthesis and Phase Transitions of $PbZrO_3$ Nanotubes ($PbZrO_3$ 나노튜브의 졸-겔 형판 합성과 상전이)

  • Chang, Ki-Seog;Bu, Sang-Don
    • Journal of the Korea Institute of Military Science and Technology
    • /
    • v.8 no.4 s.23
    • /
    • pp.85-90
    • /
    • 2005
  • We report the phase transition temperatures of the $PbZrO_3$ perovskite nanotubes made by sol-gel template synthesis. The lead zirconate($PbZrO{_3}$) nanotubes were prepared with a chelate sol-gel of zirconium tetrabutoxide($Zr(OBu){_4}$) and leadacetate($Pb(OAc){_2}-3H_2O$). $Whatman^(r)$ anodisc membranes, with a 200nm pore size, served as the template. After removing the template in the 6M-NaOH solution, the $PbZrO{_3}$ nanotubes so far have shown an anomalous transition temperature, $123.6^{\circ}C$ as measured by DSC with a small particle size, 15.4nm determined by X-ray analysis with the aid of Scherrer's equation.

Quantum Dot Sensitized Solar Cell Using PbS/ZnO Nanowires (황화납/산화아연 나노선을 이용한 양자점 감응형 태양전지)

  • Kim, Woo-Seok;Yong, Ki-Jung
    • Clean Technology
    • /
    • v.16 no.4
    • /
    • pp.292-296
    • /
    • 2010
  • We fabricated quantum dot sensitized solar cells(QDSSC) using PbS as a sensitizer and measured the solar energy conversion efficiency. After growing ZnO nanowires on the substrate by low temperature ammonia solution reaction, PbS QDs were deposited on ZnO nanowires by SILAR(Successive ionic layer adsorption and reaction) method. The morphology and crystallinity of PbS/ZnO nanowires were studied by SEM and XRD. In this study, the maximum conversion efficiency of QDSSC using PbS was 0.075% at one sun, which was lower than that of QDSSC using other sensitizers. The reasons it showed relatively low efficiency are i) the probability of type-I band gap arrangement between ZnO and PbS, ii) disturbance of electron migration by the various-sized PbS band gap, iii) stability dip by the chemical reaction of PbS QDs with electrolyte. To solve these problems, researches about controlling the size distribution of PbS and new type electrolyte would be needed.

Effect of Excess PbO Addition on Sintering and Piezoelectric Characteristics in Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3 System (PbO 과잉량이 Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3계의 소결 및 압전특성에 미치는 영향)

  • 전구락;김정주;조상희;김도연
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.4
    • /
    • pp.568-574
    • /
    • 1989
  • Effect of PbO addition on sintering and piezoelectric properties at 0.45Pb(Ni1/3Nb2/3)O3-0.40PbTiO3-0.15PbZrO3 composition which is tetragonal phase was investigated. In this composition, Porosity and dielectric constant were increased with excess PbO addition, but Kp and d31 was not changed. These variation of physical properties could be interpreted as composition change of solid grains from tetragonal to MPB region due to amount of PbO-rich liquid changing.

  • PDF

SHRIMP U-Pb Zircon Ages of the Haeinsa Granite from Central Part of the Yeongnam Massif (영남육괴 중부에 분포하는 해인사화강암의 SHRIMP U-Pb 저어콘 연대)

  • Kim, Sunwoong;Choi, Jeongyun;Kim, Jin-Seop
    • The Journal of the Petrological Society of Korea
    • /
    • v.25 no.4
    • /
    • pp.401-407
    • /
    • 2016
  • The SHRIMP zircon U-Pb age dating was carried out for the age-unknown Haeinsa Granite located in the middle Yeongnam Massif. SHRIMP zircon U-Pb age determinations of 7 samples from the Haeinsa Granite in Geochang area show two age groups. Ages from 5 samples (M-3-1, H-1, 3, 5, 10) are $192.4{\pm}1.4{\sim}195.5{\pm}1.9Ma$, whereas ages from 2 samples (H-11 and 12) are $187.7{\pm}3.3Ma$ and $188.2{\pm}3.6Ma$, respectively.

Removal of Cu(II) and Pb(II) by Solid-Phase Extractant Prepared by Immobilizing D2EHPA with Polysulfone (D2EHPA를 Polysulfone으로 고정화하여 제조한 고체상 추출제에 의한 Cu(II)와 Pb(II)의 제거)

  • Kam, Sang-Kyu;Jeon, Jin-Woo;Lee, Min-Gyu
    • Journal of Environmental Science International
    • /
    • v.23 no.11
    • /
    • pp.1843-1850
    • /
    • 2014
  • PS-D2EHPA beads were prepared by immobilizing di-2-ethylhexyl-phosphoric acid (D2EHPA) with polysulfone (PSf). The removal experiments of Cu(II) and Pb(II) by the prepared PS-D2EHPA beads were conducted batchwise. The removal efficiency of Cu(II) and Pb(II) by PS-D2EHPA beads was increased with increasing pH of solution. The removal rate of Cu(II) and Pb(II) was well described by the pseudo-second-order kinetic model. The maximum removal capacity of Cu(II) and Pb(II) obtained from Langmuir isotherm were 2.58 mg/g and 12.63 mg/g, respectively. External mass transfer coefficients for the removal of Cu(II) and Pb(II) by PS-D2EHPA beads were obtained $0.61{\times}10^{-2}{\sim}5.87{\times}10^{-2}/min$ and $1.55{\times}10^{-2}{\sim}8.53{\times}10^{-2}/min$, respectively and diffusion coefficients were obtained $1.32{\times}10^{-4}{\sim}3.98{\times}10^{-4}cm^2/min$ and $1.80{\times}10^{-4}{\sim}2.28{\times}10^{-4}cm^2/min$, respectively.

Variations of Reaction Sequence with Precusor Mixing Methods in the Formation of $Pb(Zn_{0.6}Mg_{0.4})_{1/3}Nb_{2/3}O_3$[PZMN] ($Pb(Zn_{0.6}Mg_{0.4})_{1/3}Nb_{2/3}O_3$[PZMN] 합성시 전구체 혼합방법에 따른 반응 경로변화)

  • 김봉철;김정주;김남경;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.5
    • /
    • pp.458-464
    • /
    • 1998
  • Variations of reaction sequence of $Pb(Zn_{0.6}Mg_{0.4})_{1/3}Nb_{2/3}O_3$[PZMN] with precusor mixing methods were ex-amined using X-ray diffraction and dielectric characteristics. In the present study three different types of precursor mixing methods (oxide mixing PbO+$ZnNb_2O_6+MgNb_2O_6$[Zn+MN] and PbO+(Zn,Mg)$Nb_2O_6$[ZMN] precursor mixing) were adopted. When the oxide mixing method was used for the PZMN synthesis a Zn-rich perovskite phase and pyrochlore phase were formed. Compared with PbO+ZN+MN precursor mixing method the PbO-ZMN precursor led to a lowering of the formation temperature for perovskite sin-gle phase. These variation of composition and formation temperature of the perovskite phase were dis-cussed in terms of the difference in the solid-reaction requence between these three different types of pre-cursor mixing.

  • PDF

Microstructure and Dielectric Properties in $30Pb(Mg_{1/3}Nb_{2/3})O_3-20PbTiO_3-50Pb(Mg_{1/2}W_{1/2})O_3$ Ceramics with Excess MgO Addition (MgO가 과잉첨가된 $30Pb(Mg_{1/3}Nb_{2/3})O_3-20PbTiO_3-50Pb(Mg_{1/2}W_{1/2})O_3$계 세라믹스의 미세구조와 유전특성)

  • 길영배;이응상
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.1
    • /
    • pp.31-36
    • /
    • 1997
  • The effects of 0 to 10mol% excess MgO addition on the microstructure and dielectric properties in 30Pb(Mg1/3Nb2/3)O3-20PbTiO3-50Pb(Mg1/2W1/2)O3 ternary system were investigated. Samples were prepared by mixed oxide and precursor methods to compare the role of excess MgO. Excess MgO enhanced grain growth and increased dielectric constant. The dielectric constant and tesmperature dependence of dielectric constant of the sample sintered at 100$0^{\circ}C$ with 5mol% MgO were above 5,000 and +25% to -50% from - 55$^{\circ}C$ to 1$25^{\circ}C$, respectively. For these specimens the phases percent were mainly perovskite and Pb2WO5, which was confirmed by XRD analysis. Also the amount of cubic pyrochlore Pb3Nb4O13 and PbWO4 were de-creased with sintering temperature and MgO addition. BSE image showed the chemical inhomogeneous dis-tribution. Crystal phase formed at each sintering temperature and the chemical inhomogeneous distribution caused the decrease of the temperature dependence of dielectric constant.

  • PDF