Microstructure and Microwave Dielectric Properties of (1-x)Mg4Ta2O9-xTiO2(x=0\sim0.9) Ceramics ((1-x)Mg4Ta2O9-xTiO2(x=0\sim0.9)세라믹스의 미세구조와 마이크로파 유전 특성)

  • 김재식;최의선;이문기;류기원;이영희
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.8
    • /
    • pp.840-845
    • /
    • 2004
  • The microstructure and microwave dielectric properties of $(1-x){Mg}_4{Ta}_2{O}_9-xTi{O}_2(x=0\sim0.9)$ ceramics were investigated. The specimens were prepared by the conventional mixed oxide method with sintering temperature of 140$0^{\circ}C$∼150$0^{\circ}C$. To improve the quality factor and the temperature coefficient of resonant frequency,$ Ti{O}_2(\varepsilon\Gamma=100, Q\times f_\Gamma=40,000 GHz,\ta_f= +450 ppm\diagup^{\circ}C $ was added in ${Mg}_4{Ta}_2{O}_9$ceramics. The dielectric and structural properties were investigated. According to the XRD patterns, $(1-x){Mg}_4{Ta}_2{O}_9-xTi{O}_2(x=0\sim0.9)$ ceramics had the ${Mg}_4{Ta}_2{O}_9$ phase(hexagonal) and ${MgTi}_2{O}_5$phase(orthorhombic). The dielectric constant($\varepsilon_r$). quality($Qtimes{f}_r$${\tau}_f$) of the $(1-x){Mg}_4{Ta}_2{O}_9-xTi{O}_2(x=0\sim0.9)$ ceramics were 8.12∼18.59, 18,750∼186,410 GHz and -36.02∼+3.46 ppm/$^{\circ}C$, respectively.