Electrodeposition of Ni-W/Al2O3 Nano-Composites and the Influence of Al2O3 Incorporation on Mechanical and Corrosion Resistance Behaviours

  • M. Ramaprakash;R. Nivethida;A. Muthukrishnan;A. Jerom Samraj;M. G. Neelavannan;N. Rajasekaran
    • Journal of Electrochemical Science and Technology
    • /
    • v.14 no.4
    • /
    • pp.377-387
    • /
    • 2023
  • Ni-W/Al2O3 nano-composites were electrodeposited on mild steel substrate for mechanical and corrosion resistance applications. This study focused on the preparation of Ni-W/Al2O3 nano-composite coating with various quantity of Al2O3 incorporations. The addition of Al2O3 in the electrolytes were varied from 1-10 g/L in electrolytes and the Al2O3 incorporation in Ni-W/Al2O3 nano-composite coatings were obtained from 1.82 to 13.86 wt.%. The incorporation of Al2O3 in Ni-W alloy matrix influenced the grain size, surface morphology and structural properties were observed. The distributions of Al2O3 particle in alloy matrix were confirmed using electron microscopy (FESEM and TEM) and EDAX mapping analysis. The crystal structure informations were studied using X-ray diffraction method and it confirms that the deposits having cubic crystal structure. The better corrosion rate (0.87 mpy) and microhardness (965 HV) properties were obtained for the Ni-W/Al2O3 nano-composite coating with 13.86 wt.% of Al2O3 incorporations.

Complex Permeability Analysis of NiCuZn Ferrites (NiCuZn 계 페라이트의 조성에 따른 복소투자율 변화 해석)

  • 남중희;오재희
    • Journal of the Korean Magnetics Society
    • /
    • v.6 no.6
    • /
    • pp.382-387
    • /
    • 1996
  • The characteristics of the complex permeability of ${(Ni_{x}Cu_{0.2}Zn_{0.8-x}O)}_{1-w}{(Fe_{2}O_{3})}_{1+w}$ with various Ni and $Co_{3}O_{4}$ contents were investigated in this work. It is found that the NiCuZn ferrites with $x{\geq}0.6$ have a relatively small peak width of the imaginary part of permeability $\mu$". The resonance frequency is increased as Ni content becomes higher, where the loss is low. The $\mu$" value decreases with increasing FezO, deficiency, but the resonance frequency($f_{\mu"max}$) is only slightly affected by $Fe_{2}O_{3}$ deficiency. In case of $Co_{3}O_{4}$ addition to the NiCuZn ferrites, the $f_{\mu"max}$ increases since the initial permeability decreases with the amount of $Co_{3}O_{4}$. It is concluded that the Ni content in the NiCuZn ferrite is a dominant factor for the total loss of these spinel ferrites.

  • PDF

Studies on the Development of a Microbial Cryoprotectant Formulation Using a W/O/W Multiple Emulsion System

  • Bae, Eun-Kyung;Cho, Young-Hee;Park, Ji-Yong
    • Journal of Microbiology and Biotechnology
    • /
    • v.14 no.4
    • /
    • pp.673-679
    • /
    • 2004
  • A microbial cryoprotectant formulation using a W/O/W multiple emulsion system was developed. The psychrotolerant microorganism, B4, isolated from soil in South Korea, was observed by the drop freezing method, in which the microorganism sample inhibited ice nucleation activity. The antifreeze activity was eliminated when the microorganism sample was treated with protease, indicating that the antifreeze activity was due to the presence of antifreeze protein. The result of the l6S rDNA sequencing indicated the B4 strain was most closely related to a species of the genus Bacillus. Culture broth of B4 strain (Bacillus sp.) and rapeseed oil containing 1 % polyglycerine polyricinolate (PGPR) were used as core and wall material, respectively. The most stable W/O emulsion was prepared at a core/oil ratio of 1:2. The highest W/O/W emulsion stability was achieved when the primary emulsion to external aqueous phase containing 0.5% caster oil polyoxyethylene ether $(COG25^{TM})$ ratio was 1:1. Microcrystalline cellulose showed better W/O/W emulsion stability than other polymer types. The viability of cells in a W/O/W emulsion was higher than free cells during storage at $37^\circ{C}$. An acidic pH and UV exposure decreased the viability of free cells, but cells in W/O/W emulsion were more stable under these conditions.

Effect of Excess MgO on Dielectric and Electrostrictive Properties of $0.99Pb(Mg_{1/3}Nb_{2/3})O_3-0.01Pb(Mn_{2/3}W_{1/3})O_3$ ($0.99Pb(Mg_{1/3}Nb_{2/3})O_3-0.01Pb(Mn_{2/3}W_{1/3})O_3$계의 유전 및 전왜 특성에 미치는 과잉 MgO의 영향)

  • 윤기현;김승연;남윤우;조용수;강동헌
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.8
    • /
    • pp.629-634
    • /
    • 1993
  • Dielectric and electrostrictive properties of 0.99Pb(Mg1/3Nb2/3)O3-0.01Pb(Mn2/3W1/3)O3 system using KCl-NaCl salts have been investigated as a function of the amount of excess MgO. For the specimens calcined at $700^{\circ}C$ for 1h and then sintered at 115$0^{\circ}C$ for 4h, the perovskite phase and the relative density were about 98% and 95%, respectively. With the addition of excess MgO up to 10mol%, the dielectric constant and the electrostrictive strain increased due to the increase of density and grain size, and these properties were degraded by the further addition of excess MgO. For the 10mol% excess MgO added specimen, the maximum electrostrictive strain, Xmax, and the electrostrictive coefficient, Q11, were 4.5$\times$10-4, 3.5$\times$10-2m4/C2, respectively. These results were correlated with the property of PMW and microstructure.

  • PDF

Evaluation or various vehicles and O/W Microemulsions of Flurbiprofen as Transdermal Delivery System (경피제제로서 수종의 플루비프로펜 Vehicle과 O/W 마이크로에멀젼의 평가)

  • Lee, Gye-Won;Jee, Ung-Kil
    • Journal of Pharmaceutical Investigation
    • /
    • v.28 no.3
    • /
    • pp.141-149
    • /
    • 1998
  • In order to reduce systemic side effects following administration, flurbiprofen was formulated as O/W microemulsion consisting of the surfactant, oil phase and aqueous phase. Particle size distribution, apparent viscosity, solubility and skin permeation of flurbiprofen in various vehicles and microemulsion were evaluated. The domain of O/W microemulsion s phase diagram had difference between oil types and the area of O/W microemulsion was wide distributed by adding to PG and cosurfactant than that of water alone. As increasing 10, 15 and 20% of Brij 97 content and 1, 2.5, 5% of oil content, the solubility of flurbiprofen in O/W microemulsions and various vehicles was $400{\sim}1,000$ and $10{\sim}500$ times higher than that of control. Also, apparent viscosity of soybean oil microemulsions was higher than that of IPM microemulsions and that of vehicle were increased as increasing vehicle content. Since skin permeation of flurbiprofen decreased as increasing viscosity, in each vehicle, it was not affected 2% ${\beta}-CD$ and decreased as increasing PG content and to 2, 5 and 10% of $HP-{\beta}-CD$. In O/W microemulsion, 5% soybean oil. 20% Brij 97 and 75% water(A-1) with high viscosity showed low skin penetration.

  • PDF

Microwave Synthesis of Titanium Silicalite-1 Using Solid Phase Precursors

  • Kim, K.Y.;Ahn, W.S.;Park, D.W.;Oh, J.H.;Lee, C.M.;Tai, W.P.
    • Bulletin of the Korean Chemical Society
    • /
    • v.25 no.5
    • /
    • pp.634-638
    • /
    • 2004
  • Titanium silicalite-1 (TS-1) molecular sieve was produced by microwave heating of amorphous titanium-containing solid precursors after impregnation with aqueous TPAOH solution. $SiO_2-TiO_2$ xerogel, sub-micron sized $SiO_2-TiO_2$ prepared by thermal plasma process, and Ti-containing mesoporous silica, Ti-HMS, were tested as the solid phase substrates. Highly crystalline product was obtained within 30 min. after microwave irradiation with yields over 90% using $SiO_2-TiO_2$ xerogel, which showed essentially identical physicochemical properties to TS-1 prepared by conventional hydrothermal method. Excellent catalytic activity was also obtained for 1-hexene epoxidation using $H_2O_2.\;SiO_2-TiO_2$ particles prepared by thermal plasma and Ti-HMS were found inferior as a substrate for TS-1, probably due to difficulties in wetting the surface uniformly with TPAOH.

Metal-Dinitrosyl Complexes(III) : Synthesis and Structural Study of Homo-, Hetero-dinuclear Molybdenum and Tungsten Complexes, $[Cl(phen)(NO)_2M({\mu}-pyz)M'(NO)_2(phen)Cl][ClO_4]_2 $(phen = 1,10-phenanthroline, pyz = pyrazine) (금속-디니트로실 착물 (제 3 보) : 몰리브덴과 텅스텐의 호모 및 헤테로 이핵 착물, $[Cl(phen)(NO)_2M({\mu}-pyz)M'(NO)_2(phen)Cl][ClO_4]_2 (phen=1,10-phenanthroline,\;pyz=pyrazine)$의 합성 및 구조에 대한 연구)

  • Sang-Oh Oh;Seong-Jong Mo
    • Journal of the Korean Chemical Society
    • /
    • v.37 no.7
    • /
    • pp.655-661
    • /
    • 1993
  • The neutral monomeric compounds $[Mo(NO)_2Cl_2(phen)]$ and $[W(NO)_2Cl_2(phen)]$ (phen= 1,10-phenanthroline) have been prepared by reactions of polymeric compounds $[{Mo(NO)_2Cl_2}n],\;[{W(NO)_2Cl_2}n]$ with chelate ligands. Additions of one equivalent of silver(I) perchlorate to these cis-dinitrosyl compounds in acetone solution produce $[Mo(NO)_2(phen)(S)Cl][ClO_4]\;and\;[W(NO)_2(phen)(S)Cl][ClO_4]$ (S = acetone). The homo- and hetero-dinuclear complexes, $[Cl(phen)(NO)_2M(pyz)M'(NO)_2(phen)Cl][ClO_4]_2$ (M = Mo, W) and $[Cl(phen)(NO)_2M(pyz)M'(NO)_2(phen)Cl][C1O_4]_2$ (M = Mo, M' = W) have been prepared by these monocationic complexes with pyrazine ligand respectively. These complexes characterized by elemental analysis, $1^H-\;and\;^{13}C-NMR$, infrared, and UV-visible spectroscopy are reported. The spectral data indicate that homo- and hetero-dinuclear complexes were symmetrical structures of $C_{2v}$.

  • PDF

Deposition of SiO2 Thin Film for the Core of Planar Light-Wave-Guide by Transformer Coupled Plasma Chemical-Vapor-Deposition (TCP-CVD 장비를 활용한 광도파로용 Core-SiO2 증착)

  • Kim, Chang-Jo;Shin, Paik-Kyun
    • Journal of the Korean Vacuum Society
    • /
    • v.19 no.3
    • /
    • pp.230-235
    • /
    • 2010
  • In this paper, we controlled the deposition rate and reflective index with process conditions that are TCP power, gas flow ratio and bias for optical properties of $SiO_2$ thin film using TCP-CVD equipment. We obtained a excellent $SiO_2$ thin film which has a excellent uniformity (<1 [%]), deposition rate (0.28 [${\mu}m$/ min]) and reflective index (1.4610-1.4621) within 4" wafer with process conditions ($SiH_4:O_2$=50 : 100 [sccm], TCP power 1 [kW], bias 200 [W]) at [$300^{\circ}C$].

A Study on the Dielectric Properties of the Pb($Mg_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-Pb($Ni_\frac{1}{2}W_\frac{1}{2}$)$O_3$ Ceramics (Pb($Mg_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-Pb($Ni_\frac{1}{2}W_\frac{1}{2}$)$O_3$세라믹의 유전특성에 관한 연구)

  • 유남산;류기원;이성갑;이영희
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1990.10a
    • /
    • pp.65-67
    • /
    • 1990
  • In this study, (0.80-x)Pb($Mg_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-Pb($Ni_\frac{1}{2}W_\frac{1}{2}$)$O_3$ 0.05$\leq$x$\leq$0.20) ceramics were fabricated by the mixed oxide method, the sintering temperature and time were 950∼1200[$^{\circ}C$], 2[hr], respectively. The dielectric and structural properties with composition and sintering temperature were investigated for the application as multilayer ceramic capacitors. Dielectric constant of 0.70PMN-0.2PT-0.10PNW composition with repeated calcination was increased rapidly. Increasing the Pb($Mg_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-Pb($Ni_\frac{1}{2}W_\frac{1}{2}$)$O_3$ contents from 0.05 to 0.20 [mol], phase transition temperature was shifted from 68 to 2[$^{\circ}C$] and dielectric constant was decreased while sintered density was increased. In the specimens containing 0.10, 0.15[mol] of PNW, dielectri constants at room temperature were exhibited the highest values 11199, 10114, respectively. Resistivity of specimens were $10^{10}$$10^{12}$($\Omega$.m) and there was no dependence on sintering temperature and composition.