• 제목/요약/키워드: $NiSO_4/CeO_2-ZrO_2$ catalyst

검색결과 2건 처리시간 0.016초

Physicochemical and Catalytic Properties of NiSO4/CeO2-ZrO2 Catalyst Promoted with CeO2 for Acid Catalysis

  • Sohn, Jong-Rack;Shin, Dong-Cheol
    • Bulletin of the Korean Chemical Society
    • /
    • 제28권8호
    • /
    • pp.1265-1272
    • /
    • 2007
  • A solid acid catalyst, NiSO4/CeO2-ZrO2 was prepared simply by promoting ZrO2 with CeO2 and supporting nickel sulfate on CeO2-ZrO2. The support of NiSO4 on ZrO2 shifted the phase transition of ZrO2 from amorphous to tetragonal to higher temperatures because of the interaction between NiSO4 and ZrO2. The surface area of 10-NiSO4/1-CeO2-ZrO2 promoted with CeO2 and calcined at 600 oC was very high (83 m2/g) compared to that of unpromoted 10-NiSO4/ZrO2 (45 m2/g). This high surface area of 10-NiSO4/1-CeO2-ZrO2 was due to the promoting effect of CeO2 which makes zirconia a stable tetragonal phase as confirmed by XRD. The role of CeO2 was to form a thermally stable solid solution with zirconia and consequently to give high surface area and acidity of the sample, and high thermal stability of the surface sulfate species. 10-NiSO4/1- CeO2-ZrO2 containing 1 mol% CeO2 and 10 wt% NiSO4, and calcined at 600 oC exhibited maximum catalytic activities for both reactions, 2-propanol dehydration and cumene dealkylation.

CeO2-Promoted Highly Active Catalyst, NiSO4/CeO2-ZrO2 for Ethylene Dimerization

  • Pae, Young-Il;Shin, Dong-Cheol;Sohn, Jong-Rack
    • Bulletin of the Korean Chemical Society
    • /
    • 제27권12호
    • /
    • pp.1989-1996
    • /
    • 2006
  • The $NiSO_4/CeO_2-ZrO_2 $catalysts containing different nickel sulfate and $CeO_2$ contents were prepared by the impregnation method, where support, $CeO_2-ZrO_2$was prepared by the coprecipitation method using a mixed aqueous solution of zirconium oxychloride and cerium nitrate solution followed by adding an aqueous ammonia solution. No diffraction line of nickel sulfate was observed up to 20 wt %, indicating good dispersion of nickel sulfate on the surface of $CeO_2-ZrO_2$. The addition of nickel sulfate (or $CeO_2$) to $ZrO_2$ shifted the phase transition of $ZrO_2$ from amorphous to tetragonal to higher temperatures because of the interaction between nickel sulfate (or $CeO_2$) and $ZrO_2$. A catalyst (10-$NiSO_4/1-CeO_2-ZrO_2$) containing 10 wt % $NiSO_4$ and 1 mole % $CeO_2$, and calcined at $600{^{\circ}C}$ exhibited a maximum catalytic activity for ethylene dimerization. The catalytic activities were correlated with the acidity of catalysts measured by the ammonia chemisorption method. The role of $CeO_2$was to form a thermally stable solid solution with zirconia and consequently to give high surface area, thermal stability and acidity of the sample.