Kim, Jun-Il;Park, Sun-Min;Roh, Kwang Chul;Lee, Jae-Won
Bulletin of the Korean Chemical Society
/
제34권9호
/
pp.2573-2576
/
2013
Rate capability and cyclability of $LiMn_2O_4$ should be improved in order to use it as a cathode material of lithium-ion batteries for hybrid-electric-vehicles (HEV). To enhance the rate capability and cyclability of $LiMn_2O_4$, it was coated with $MnV_2O_6$ by a sol-gel method. A $V_2O_5$ sol was prepared by a melt-quenching method and the $LiMn_2O_4$ coated with the sol was heat-treated to obtain the $MnV_2O_6$ coating layer. Crystal structure and morphology of the samples were examined by X-ray diffraction, SEM and TEM. The electrochemical performances, including cyclability at $60^{\circ}C$, and rate capability of the bare and the coated $LiMn_2O_4$ were measured and compared. Overall, $MnV_2O_6$ coating on $LiMn_2O_4$ improves the cyclability at high temperature and rate capability at room temperature at the cost of discharge capacity. The improvement in cyclability at high temperature and the enhanced rate capability is believed to come from the reduced contact between the electrode, and electrolyte and higher electric conductivity of the coating layer. However, a dramatic decrease in discharge capacity would make it impractical to increase the coating amount above 3 wt %.
산소 과전압이 낮은 $MnO_2$를 촉매로 사용하여 반도체 산화물계의 산소선택성 전극을 제조하고 산화물 코팅층의 미세구조와 전기화학적 특성을 분석하였다. Ti 기판에 열분해 법을 이용하여 $MnO_2$ 피막을 형성하였고, 또한 binder를 이용한 코팅 방법을 이용하여 Ti, Fb 기판에 $MnO_2$ 피막층을 형성하였다. 450$^{\circ}C$에서 1시간 열분해하여 약 1 ${\mu}m$의 $MnO_2$ 피막층을 형성 시켰으나 Ti 기판과의 접착력이 약하여 피막자체에 대한 전기화학적 특성은 관찰할 수 없었다. PVDF : $MnO_2$의 함량비가 1:1에서 1:6 까지는 DMF의 함량에 무관하게 전극 특성이 나타나지 않았지만 20:1 이상의 조성에서는 균일한 C-V 특성을 나타냈고, 산소 발생 과전압도 약 1.4V 정도로 감소되었다. 그러나 Ti 기판의 경우 열분해법을 이용하여 제조된 전극과 같이 낮은 기판과의 접착력 때문에 $MnO_2$ 피막층의 촉매효과가 현저하게 감소하였다.
고출력 전기화학 캐패시터를 위한 전극제조공정으로 screen printing과 doctor blade법이 연구되었다. Screen printing에 의해서 제작된 비정질 $MnO_2$전극으로 측정된 CV (cyclic voltammogram)는 이상적인 캐패시터에 가까운 특성을 보여주었다. 50mV/s의 scan rate에서의 CV로부터 계산된 비용량은 $140{\mu}m,\;24{\mu}m,\; 3{\mu}m$의 전극두께에 대해서 각각 5.8F/g과, 81.8F/g, 172.0F/g의 값을 나타내었다. Screen printing전극에서의 $MnO_2$활물질의 이용율을 $100\%$로 하였을 때, paste와 doctor blade법의 이용율은 각각 $3.4\%$와 $47.6\%$이었다. Screen printing은 고출력 응용을 위한 얇은 전극의 코팅 방법으로 우수한 특성을 보였다.
졸-겔(sol-gel) 방법을 이용하여 스피넬(spinel) 구조를 가지는 $LiNi_xMn_{2-x}O_4$ 박막을 x = 0.9까지 합성하였다. 니켈 치환된 박막은 작은 x 값에서는 cubic 구조가 유지되지만, $x{\geq}0.6$ 범위에서는 tetragonal 구조로 상전이가 일어남이 발견되었다. 이와 같은 cubic-tetragonal 상전이는 low-spin $(t_{2g}^6,e_g^1)$ 상태를 가지는 $N^{3+}(d^7)$ 이온이 팔면체 자리를 차지하게 됨으로써 나타나는 Jahn-Teller 효과에 의한 것으로 해석된다. 이와 같은 Ni 이온들은 +3 및 +2의 원자가를 가지고 존재함이 X-ray photoelectron spectroscopy 분석을 통하여 확인되었다. $LiNi_xMn_{2-x}O_4$ 박막들에 대하여 가시광선-자외선 영역에서 spectroscopic ellipsometry(SE)를 이용하여 광학적 성질을 조사하였고, 그 결과 분석을 통하여 화합물 전자구조에 대하여 고찰하였다. SE 측정된 유전함수 스펙트럼은 주로 전하이동(charge-transfer, CT) 전이(transition)에 의한 넓은 에너지 영역을 가지는 1.9, 2.3, $2.8{\sim}3.0$, $3.4{sim}3.6eV$ 근처의 흡수구조 들로 이루어져 있는데, $O^{2-}$에서 $Mn^{4+}$ 이온의 $t_{2g}$ (1.9 eV)와 $e_g$$(2.8{\sim}3.0\;eV)$로의 전이 즉, $O^{2-}(2p){\rightarrow}Mn^{4+}(3d)$ 및 $O^{2-}$에서 $Mn^{3+}$ 이온의 $t_{2g}$ (2.3 eV)와 $e_g$ ($3.4{\sim}3.6$ eV)로의 전이 즉, $O^{2-}(2p){\rightarrow}Mn^{3+}(3d)$ 등에 의한 것으로 해석된다. 또한, 1.6, 1.8, 1.9 eV 부근에서 관측된 좁은 에너지 영역의 흡수구조 들은 팔면체 $Mn^{3+}$ 이온 내에서의 d-d 결정장(crystal-field) 전이에 의한 것으로 해석된다. 이러한 흡수구조는 Ni 치환량이 증가함에 따라 그 강도가 감소한다. x = 0.6의 경우 $e_g$ 상태와 관련된 CT 전이구조 들이 $t_{2g}$ 상태와 관련된 전이구조 들에 비하여 큰 폭으로 감소하는데 이것은 Jahn-Teller 효과에 의해서 격자상수가 tetragonal 구조로 확장됨에 따라 $e_g$ 상태와 $O^{2-}(2p)$ 상태 간의 파동함수 중첩이 감소한 것에 기인하는 것으로 해석된다.
비철금속 습식 제련용 고효율 장수명의 양극을 개발하기 위해서 산소 과전압이 낮은 $MnO_{2}$를 촉매로 사용하여 반도체 산화물계의 산소선택성 전극을 제조하고 산화물 coating층의 미세구조와 전기화학적 특성을 분석하였다. PVDF : $MnO_{2}$의 함량비플 1 : 1 에서 1 : 40까지 정량적으로 변화시켰고, 용제의 점도에 지배적인 영향을 미치는 DMF의 함량을 각각의 고정된 PVDF : $MnO_{2}$의 함량비에서 변화시켜 용제를 제조하였으며 4% $HNO_{3}$ 용액에 세척된 Pb전극을 1.5 mm/sec 의 속도로 5회 dipping 하였다. PVDF : $MnO_{2}$ = 1 : 6인 경우 PVDF의 양이 증가하고 DMF의 양이 감소할수록 피막층이 두꺼워지고 PVDF : DMF = 4 : 96인 경우 pb 전극의 피막층이 얇기 때문에 박리현상이 일어났으며 이는 산화물 용제의 낮은 점도 때문인 것으로 판단된다. 또한 PVDF : DMF = 10 : 90의 경우는 5회 dipping 하여 약 $150{\mu}m$의 피막층을 형성하였다. PVDF : Mn02의 함량비가 1:1에서 1:6 까지는 DMF의 함량에 무관하게 전극 특성이 나타나지 않았지만 $MnO_{2}$의 양이 상대적으로 증가하면 cycle 이 증가하더라도 거의 일정한 전류 값을 갖고$MnO_2$와 PVDF의 비가 20:1 이상의 조성에서는 균일한 CV 특성을 나타냈다 이는 $MnO_{2}$가 효과적으로 촉매 작용을 한 것으로 판단되며 anodic polarization에 의한 산소 발생 과전압도 약 1.4V 정도로 감소되었다.
A series of 20 wt % $(NH_4)_2SO_4$ and 3 wt % $Al_2O_3$ surface treatments were applied to $Li[Li_{0.2}Mn_{0.54}Co_{0.13}Ni_{0.13}]O_2$ substrates. The $Li[Li_{0.2}Mn_{0.54}Co_{0.13}Ni_{0.13}]O_2$ substrates were synthesized using a co-precipitation method. Sample (a) was left pristine and variations of the 20 wt % $(NH_4)_2SO_4$ and 3 wt % $Al_2O_3$ were applied to samples (b), (c) and (d). XRD was used to verify the space group of the samples as R$\bar{3}$m. Additional morphology and particle size data were obtained using SEM imagery. The $Al_2O_3$ coating layers of sample (b) and (d) were confirmed by TEM images and EDS mapping of the SEM images. 2032-type coin cells were fabricated in a glove box in order to investigate their electrochemical properties. The cells were charged and discharged at room temperature ($25^{\circ}C$) between 2.0V and 4.8V during the first cycle. The cells were then charged and discharged between 2.0V and 4.6V in subsequent cycles. Sample (d) exhibited lower irreversible capacity loss (ICL) in the first charge-discharge cycle as compared to sample (c). Sample (d) also had a higher discharge capacity of ~250 mAh/g during the first and second charge-discharge cycles when compared with sample (c). The rate capability of the $Al_2O_3$-coated sample (b) and (d) was lower when compared with sample (a) and (c). Sample (d), coated with $Al_2O_3$ after the surface treatment with $(NH_4)_2SO_4$, showed an improvement in cycle performance as well as an enhancement of discharge capacity. The thermal stability of sample (d) was higher than that of the sample (c) as the result of DSC.
The interface between the surface of a cathode material and the electrolyte gives rise to surface reactions such as solid electrolyte interface (SEI) and chemical side reactions. These reactions lead to increased surface resistance and charge transfer resistance. It is consequently necessary to improve the electrochemical characteristics by suppressing these reactions. In order to suppress unnecessary surface reactions, we coated cathode material using polypropylene (PP). The PP coating layer effectively reduced the SEI film that is generated after a 4.3 V initial charging process. By mitigating the formation of the SEI film, the PP-coated Li[(Ni0.6Co0.1Mn0.3)0.36(Ni0.80Co0.15Al0.05)0.64)]O2(NCS) electrode provided enhanced transport of Li+ ions due to reduced SEI resistance (RSEI) and charge transfer resistance (Rct). The initial charge and discharge efficiency of the PP-coated NCS electrode was 96.2 % at a current density of 17 mA/g in a voltage range of 3.0 ~ 4.3 V, whereas the efficiency of the NCS electrode was only 94.7 %. The presence of the protective PP layer on the cathode improved the thermal stability by reducing the generated heat, and this was confirmed via DSC analysis by an increased exothermic peak.
Commercially pure titanium (CP-Ti) and Ti-6Al-4V alloys have been widely used in implant materials such as dental and orthopedic implants due to their corrosion resistance, biocompatibility, and good mechanical properties. However, surface modification of titanium and titanium alloys is necessary to improve osseointegration between implant surface and bone. Especially, when titanium oxide nanotubes are formed on the surface of titanium alloy, cell adhesion is greatly improved. In addition, plasma electrolytic oxide (PEO) coatings have a good safety for osseointegration and can easily and quickly form coatings of uniform thickness with various pore sizes. Recently, the effects of bone element such as magnesium, zinc, strontium, silicon, and manganese for bone regeneration are researching in dental implant field. The purpose of this study was researched on the surface morphology of PEO-treated Ti-6Al-4V alloy after anodic titanium oxide treatmentusing various instruments. Ti-6Al-4V ELI disks were used as specimens for nanotube formation and PEO-treatment. The solution for the nanotube formation experiment was 1 M $H_3PO_4$ + 0.8 wt. % NaF electrolyte was used. The applied potential was 30V for 1 hours. The PEO treatment was performed after removing the nanotubes by ultrasonics for 10 minutes. The PEO treatment after removal of the nanotubes was carried out in the $Ca(CH_3)_2{\cdot}H_2O+(CH_3COO)_2Mg{\cdot}4H_2O+Mn(CH_3COO)_2{\cdot}4H_2O+Zn(CH_3CO_2)_2Zn{\cdot}2H_2O+Sr(CH_2COO)_2{\cdot}0.5H_2O+C_3H_7CaO_6P$ and $Na_2SiO_3{\cdot}9H_2O$ electrolytes. And the PEO-treatment time and potential were 3 minutes at 280V. The morphology changes of the coatings on Ti-6Al-4V alloy surface were observed using FE-SEM, EDS, XRD, AFM, and scratch tester. The morphology of PEO-treated surface in 5 ion coating solution after nanotube removal showed formation or nano-sized mesh and micro-sized pores.
Development of biodegradable implants for treatment of complex bone fractures has recently become one of the priority areas in biomedical materials research. Multifunctional corrosion resistant and bioactive coatings containing hydroxyapatite $Ca_{10}(PO_4)_6(OH)_2$ and magnesium oxide MgO were obtained on Mg-Mn-Ce magnesium alloy by plasma electrolytic oxidation. The phase and elemental composition, morphology, and anticorrosion properties of the coatings were investigated by scanning electron microscopy, energy dispersive spectroscopy, potentiodynamic polarization, and electrochemical impedance spectroscopy. The PEO-layers were post-treated using superdispersed polytetrafluoroethylene powder. The duplex treatment considerably reduced the corrosion rate (>4 orders of magnitude) of the magnesium alloy. The use of composite coatings in inducing bioactivity and controlling the corrosion degradation of resorbable Mg implants are considered promising. We also applied the plasma electrolytic oxidation method for the formation of the composite bioinert coatings on the titanium nickelide surface in order to improve its electrochemical properties and to change the morphological structure. It was shown that formed coatings significantly reduced the quantity of nickel ions released into the organism.
연료극 지지체 평관형 고체산화물 연료전지(SOFC)의 셀 전력밀도를 증가시키기 위하여 압출법에 의하여 제조하고 그 특성을 연구하였다. 연료극 지지체로써 Ni/YSZ($8mol\%$ yttria stabilized zirconia) cermet는 기공율 $50.6\%,\;0.23{\mu}m$의 기공크기를 나타내었다. 지지체에서의 Ni의 분포는 균일하였으며 전자전도 경로로써의 Ni의 연결성은 양호하였다. 지지체에 YSZ전해질과 복합 공기극층인 $LSM((La_{0.85}Sr_{0.15})_{0.9}MnO_3)/YSZ$ 복합층, LSM, LSCF $(La_{0.6}Sr_{0.4}Co_{0.2}Fe_{0.8}O_3)$층이 슬러리 디핑법에 의하여 코팅 및 소결된 연료극 지지체식 평관형 고체산화물 연료전지 단위전지의 성능은 $800^{\circ}C$에서 $300mW/cm^2(0.6V,\;500mA/cm^2)$의 성능을 나타내었다. 임피던스 분석에 의하여 평관형 셀의 전기화학적 분극저항을 평가하고 연료측의 가습에 따라 분극저항이 감소되어 성능이 향상됨을 알 수 있었다 슬러리 디핑법으로 LSM이 코팅된 SUS430 금속연결재를 $Ar+10\%\;H_2$에서 소결하였으며, $750^{\circ}C$에서 면저항의 측정할 결과, 초기에는 $148m{\Omega}cm^2$를 나타내었으며, 450시간 경과 후에 $43m{\Omega}cm^2$의 낮은 면저항을 유지하였다. 반면에 동일한 조건으로 LSM이 코팅된 Fecralloy는 높은 면저항을 나타내었다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.