• 제목/요약/키워드: $Mn-V_{2}O_{5}/TiO_2$

검색결과 62건 처리시간 0.029초

Metal-Organic Decomposition법에 의한 강유전성 $YMnO_3$ 박막의 제조 및 특성 (Preparation of Ferroelectric $YMnO_3$ Thin Films by Metal-Organic Decomposition Process and their Characterization)

  • 김제헌;강승구;김응수;김유택;심광보
    • 한국세라믹학회지
    • /
    • 제37권7호
    • /
    • pp.665-672
    • /
    • 2000
  • The ferroelectric YMnO3 thin films were prepared by MOD(metal-organic decomposition) method with Y- and Mn-acetylacetonate as starting materials. Thin films were grown on various substrates by spin-coating technique. The crystalline phases of the thin films were identified by X-ray diffractometer as a function of heat-treatment temperature, pH of coating solution and substrate. In addition, the effect of Mn/Y molar ratio(0.8~1.2) on the formation of hexagonal-YMnO3 phase was investigated. In forming highly c-axisoriented hexagonal-YMnO3 single phase, the Pt coated Si substrate was more effective than the bare Si substrate, and the optimum heat-treatment condition was at 82$0^{\circ}C$ for 30 min. Higher Mn/Y molar ratio within 0.8~1.2 and pH of YMnO3 precursor solution within 0.5~2.5 favored formation of ferroelectric hexagonal phase rather than orthorhombic phase. Leakage current density of the hexagonal-YMnO3 thin film formed on Pt(111)/TiO2/SiO2/Si substrate was low enough as 0.4~4.0$\times$10-8(A/$\textrm{cm}^2$) at 5 V and its remanent polarization(Pr), calculated from the P-E hysteresis loop, was 3 nC/$\textrm{cm}^2$.

  • PDF

Device and Piezoelectric Characteristics of Pb(Mn1/3Sb2/3) O3-PZT Ceramics for Piezoelectric Transformer

  • Sohn, Joon-Ho;Heo, Soo-Jeong;Sohn, Jeong-Ho;Lee, Joon-Hyung;Jung, Woo-Hwan;Kim, Dong-Bum;Cho, Sang-Hee
    • The Korean Journal of Ceramics
    • /
    • 제5권2호
    • /
    • pp.171-177
    • /
    • 1999
  • In the $(Pb_{1-x}M_x)[(Mn_{1/3}Sb_{2/3})_{0.05}Zr_yTi_{0.95-y}]O_3$ system, where M=Ca and Sr, the piezoelectric properties were evaluated to examine the possibility of application to piezoelectric transformer. A Rosen-type piezoelectric transformer was formed, then the electrical properties of voltage step-up ratio, frequency characteristics etc. were analysed. The morphotropic phase boundary was determined to be y=0.475 in $Pb[(Mn_{1/3}Sb_{2/3})_{0.05}Zr_yTi_{0.95-y}]O_3$ system and the piezoelectric properties of this composition was kp=0.59, Qm=1600 and $\varepsilon_r$=1150. Moreover, when 1-2 mol% of Sr are substituted, enhanced piezoelectric properties of kp=0.61, Qm=1600 and $\varepsilon_r$=1400 were shown. The temperature rising (ΔT) of a piezoelectric transformer with $Pb[Mn_{1/3}Sb_{2/3})_{0.05}Zr_{0.475}Ti_{0.475})]O_3 $ composition was $10^{\circ}C$, and the voltage step-up ratio was 500 when the output voltage was 4000V, whereas the ΔT was below $3^{\circ}C$ and the resonant frequency variation ($\Delta f_r$) as a function of load resistance was below 5% when the output voltage was 2000 V. These characteristics are superior to the properties of materials, which were substituted by Ca or without substitution.

  • PDF

역사시대에 분화한 백두산 화산재의 화학 성분 (Geochemical Composition of Volcanic Ash from Historical Eruptions of Mt. Baekdu, Korea)

  • 윤성효;고정선;장철우
    • 암석학회지
    • /
    • 제27권1호
    • /
    • pp.37-47
    • /
    • 2018
  • 백두산에서 역사시대에 분화한 화산재의 시료에 대하여 다양한 방법으로 주성분과 미량성분을 분석하였다. 화산재의 주성분 원소 함량은 $SiO_2$ 58.8~71.1 wt.%, $Al_2O_3$ 9.6~16.8 wt.%, ${Fe_2O_3}^T$ 4.5~6.9 wt.%, MgO 0.1~1.7 wt.%, CaO 0.3~1.6 wt.%, $Na_2O$ 5.2~6.3 wt.%, $K_2O$ 4.3~5.9 wt.% 그리고 $TiO_2$ 1.2 wt.%이하로 분석되었다. Ba, Cu, Cr. Co, Ni, Sr, V, Zn와 Zr을 포함하는 32개 미량원소가 분석되었는데, 이들 화산재는 일부 미량원소와 경희토류 원소의 부화정도에 따라 두 그룹(그룹 A, 그룹 B)으로 구분되며, 그룹 A에는 1천년 전의 밀레니엄 분화물, 1668년과 1903년 분화물이, 그룹 B에는 1702년 분화물이 해당된다. 중금속원소인 Cu, Co, Zn, Mn 등은 소량 함유되어 나타난다. 백두산 화산재는, 섭입대 기원의 일본 사쿠라지마 화산의 화산재와 비교하여, 미량성분원소 중 Y, Nb, Pb, U, Sc, V, Ni 그리고 Cu 함량은 낮게 나타나며, Zr, Ba, Hf, Cr, Co, Zn 그리고 희토류(Eu제외) 등은 높은 함량을 나타낸다.

ATO 처리후, 플라즈마 전해 산화 처리된 Ti-6Al-4V 합금의 표면 형태 (Surface Morphology of PEO-treated Ti-6Al-4V Alloy after Anodic Titanium Oxide Treatment)

  • Kim, Seung-Pyo;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2018년도 춘계학술대회 논문집
    • /
    • pp.75-75
    • /
    • 2018
  • Commercially pure titanium (CP-Ti) and Ti-6Al-4V alloys have been widely used in implant materials such as dental and orthopedic implants due to their corrosion resistance, biocompatibility, and good mechanical properties. However, surface modification of titanium and titanium alloys is necessary to improve osseointegration between implant surface and bone. Especially, when titanium oxide nanotubes are formed on the surface of titanium alloy, cell adhesion is greatly improved. In addition, plasma electrolytic oxide (PEO) coatings have a good safety for osseointegration and can easily and quickly form coatings of uniform thickness with various pore sizes. Recently, the effects of bone element such as magnesium, zinc, strontium, silicon, and manganese for bone regeneration are researching in dental implant field. The purpose of this study was researched on the surface morphology of PEO-treated Ti-6Al-4V alloy after anodic titanium oxide treatmentusing various instruments. Ti-6Al-4V ELI disks were used as specimens for nanotube formation and PEO-treatment. The solution for the nanotube formation experiment was 1 M $H_3PO_4$ + 0.8 wt. % NaF electrolyte was used. The applied potential was 30V for 1 hours. The PEO treatment was performed after removing the nanotubes by ultrasonics for 10 minutes. The PEO treatment after removal of the nanotubes was carried out in the $Ca(CH_3)_2{\cdot}H_2O+(CH_3COO)_2Mg{\cdot}4H_2O+Mn(CH_3COO)_2{\cdot}4H_2O+Zn(CH_3CO_2)_2Zn{\cdot}2H_2O+Sr(CH_2COO)_2{\cdot}0.5H_2O+C_3H_7CaO_6P$ and $Na_2SiO_3{\cdot}9H_2O$ electrolytes. And the PEO-treatment time and potential were 3 minutes at 280V. The morphology changes of the coatings on Ti-6Al-4V alloy surface were observed using FE-SEM, EDS, XRD, AFM, and scratch tester. The morphology of PEO-treated surface in 5 ion coating solution after nanotube removal showed formation or nano-sized mesh and micro-sized pores.

  • PDF

CeMnO3가 치환된 저온소결 PMW-PNN-PZT 세라믹스의 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of Low Temperature Sintering PMW-PNN-PZT Substituted with CeMnO3)

  • 김용진;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제28권3호
    • /
    • pp.160-164
    • /
    • 2015
  • In this study, $(1-x)Pb(Mg_{1/2}W_{1/2})_{0.03}(Ni_{1/3}Nb_{2/3})_{0.09}(Zr_{0.5}Ti_{0.5})_{0.88}O_3+xCeMnO_3$ (x= 0~0.02) ceramics were prepared by Columbite precursor method. The phase structure, ferroelectric and piezoelectric properties were systematically investigated. It was found that PMW-PNN-PZT possessed superior electrical properties due to its composition close to the MPB (morphotropic phase boundary). Coercive electric field of 10.05 [kV/cm] and density of 7.88 [$g/cm^3$] were obtained when the substitution amount of $CeMnO_3$ is x=0.02. In contrast, specimens with x=0.01 showed the mechanical quality factor($Q_m$) of 1,091 and the electromechanical coupling factor($k_p$) of 0.613.

SL 온도특성을 가지는 적층 칩 세라믹 캐패시터용 유전체의 유전 및 전기적 특성 (Dielectric and Electric Properties of Mutilayer Ceramic Capacitor with SL Temperature Characteristics)

  • 윤중락;이상원;김민기;이경민
    • 한국전기전자재료학회논문지
    • /
    • 제21권7호
    • /
    • pp.645-651
    • /
    • 2008
  • To reduce noise in high frequency and distortion of signal, the composition of $(Ca_{0.7}Sr_{0.3})(Zr_{0.97}Ti_{0.03})O_3$ and $(Ba_{0.2}Ca_{0.4}Sr_{0.4})TiO_3$ was developed. The composition was not solid solution, but mixtures of various phases composed of Ca, Sr, Zr, Ti and Ba oxides. The dielectric constant increased, the quality factor and the insulation resistance decreased with $(Ba_{0.2}Ca_{0.4}Sr_{0.4})TiO_3$ content. The composition of $0.4(Ba_{0.2}Ca_{0.4}Sr_{0.4})TiO_3$ satisfied the electric characteristics and the temperature coefficient of dielectric constant (TCC). In addition, the glass frit and $MnO_2$ also affected the electric characteristics. From the result of the best fit simulation, $MnO_2$ 0.3 mol%, the glass frit 0.6 wt% showed the insulation resistance $906{\Omega}{\cdot}F$, the quality factor 821, and the dielectric constant 92. With the selected composition, MLCC capacitors sized $4.5{\times}3.2{\times}2.5mm$ were manufactured with 105 layered of the dielectric thickness $16{\mu}m$ using Ni inner electrode, They represented the capacitance $98{\sim}102$ nF, the quality factor 1,200 and the insulation resistance $1,500{\Omega}{\cdot}F$. Also, they had high break-down voltage with $107{\sim}115V/{\mu}m$, and satisfied the SL TCC characteristics.

입도분포에 따른 하상퇴적물의 지구화학적 분산 및 부화 (Geochemical Dispersion and Enrichment of Fluvial Sediments Depending on the Particla Size Distribution)

  • 이현구
    • 자원환경지질
    • /
    • 제32권3호
    • /
    • pp.247-260
    • /
    • 1999
  • Geochermical characteristics of the fluvial sediments deprnding on particle size distribution size were investigated in the respect of majir, minor and rare eath element chemisitry. Ratios of $Al_{2}O_{3}/Na_{2}O$ and $K_{2}O/Na_{2}O$ of the sediments show the homogeneous valus, and partly positive correlation with $SiO_{2}/Al_{2}O_{3}$, respecively. Characteristics of minor element ratios (V/Ni, Cr/V, Ni/Co and Zr/Hf)are within the lower and narrow range. Thesesuggested that sediment sources may be acidic to intermediate granitic rock, and may be explained by simple weathering and sedimentation. With increasing SiO2 contents, concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, CaO and MgO decreased, but those of $K_{2}O$ and $Na_{2}O$ increased, Concentrations of Ba, Be, Cs, Cu, Li, Ni, Sr, V and Zr show comparatively normal negative and some positive trends. Compared with the mean composition of granite, concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, MnO, CaO and MgO in the sediments of the study area were highly enriced. Among some minor and rare earth elements, concentrations of As, Cd, Cu, and V were enriched, but those of Be, Ce, Rb, Sc, Sr and Zn were depleted when compared with average composition of granite. By decreasing of particle size fractions, SiO2, Rb and Sr conterts decreased, but concentrations of $Al_{2}O_{3}$, $Fe_{2}O_{3}$, CaO, MgO, $TiO_{2}$, MgO, $P_{2}O_{5}$, Be, Cu, Hf, Pb, V and Zr increased. From the correlations between particle size fractions and element concenreations, some elements of $Fe_{2}O_{3}$, CaO, MgO, $P_{2}O_{5}$, Cu, Ni, Zn and Zr showed typical trends in the secondary contramination sediments. These trends are typically shown under 100 mesh fractions. It indicates that the fraction of minus 100 mesh is the optimum size fraction for geochemical and environmental survey.

  • PDF

SKull법에 의한 Colored Cubic Zirconia(CCZ)단결정 성장 (Colored Cubic Zirconia(CCZ) Single Crystal Growth by Skull Method)

  • 김석호;최종건;정대식;오근호
    • 한국세라믹학회지
    • /
    • 제25권5호
    • /
    • pp.443-448
    • /
    • 1988
  • Colored Cubic Zircona(CCZ) single crystals were grown by the skull melting method. The grown crystals were doped with up to 0.1wt% transition (Cu, Ni, Co, Ti, Fe, Mo, Cr, V, Mn) metal ions on ZrO2-Y2O3(9.5~10mol%) and their Optical transmission spectra(λ=300~800nm)data were obtained. Various colors were pronounced due to dopant effects in the grown Crystals.

  • PDF

초음파 전동기용 0.125PMN-0.435PT-0.44PZ 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Properties of 0.125PMN-0.435PT-0.44PZ Ceramics for Ultrasonic footer Applications)

  • 김진수
    • 센서학회지
    • /
    • 제6권5호
    • /
    • pp.392-399
    • /
    • 1997
  • 본 연구에서는 $0.125Pb(Mg_{1/2}Nb_{2/3})O_{3}-0.435PbTiO_{3}-0.44PbZrO_{3}$의 조성을 갖는 hard계 압전 재료에 0.5 wt%의 $MnO_{2}$를 첨가하였으며, 이 시편으로 초음파 전동기를 제작하고자, 소결 온도에 따른 시편의 유전 및 압전특성에 대하여 연구하였다. 실험 결과, $1270^{\circ}C$의 소결 온도에서 다음과 같이 가장 우수한 압전특성을 나타냈다. 즉 시편의 밀도는 $7.72\;g/cm^{3}$ 유전상수는 570, 유전손실은 0.82 %f, 잔류분극 Pr은 $19.18{\mu}C/cm^{2}$ 항전계 Ec는 9.63 kW/cm, 전기기계 결합계수 kp는 55.1%, 기계적 품질계수 Qm은 886이 되었다. 또한 $1270^{\circ}C$ 에서 소결된 시편의 유전상수 및 유전손실을 주파수 변화와 온도 변화에 따라 조사하였다.

  • PDF

PAN-PZT계 세라믹스를 이용한 적층형압전변압기의 특성 (Characteristics of A Multilayer Piezoelectric Transformer Using PAN-PZT Ceramics)

  • 박타리;이동균;최지원;신용덕;김현재;고태국;윤석진
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.143-146
    • /
    • 2002
  • The characteristics of a multilayer piezoelectric transformer were investigated using 0.05Pb(A $l_{0.5}$N $b_{0.5}$) $O_3$-0.95Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$+0.9wt%N $b_2$ $O_{5}$+0.5wt%Mn $O_2$+0.04wt% $V_2$ $O_{5}$ ceramics. The multilayer piezoelectric trans formers were developed for voltage step-up. The multilayer ceramic technology was applied in piezoelectric transformer. The electrical characteristics of the piezoelectric transformer (33x8.5x1mm) has the efficiency of above 85%, step-up ratio of 70 under the 130 kΩ load, and driving frequency of 93.5kHz, respectively.ctively.y.y.

  • PDF