  • Epitaxial (La, Sr)$CoO_3/Pb(Zr,\;Ti)O_3/(La,\;Sr)CoO_3$by pulsed laser deposition for ferroelectric field effect transistor. Epitaxial $LaCoO_3/Pb(Zr,\;Ti)O_3/(La,\;Sr)CoO_3$ heterostructures exhibited 70$\mu C/cm^2$ and 17 $\mu C/cm^2$at a positively and negatively poled states, respectively. On the other hand, epitaxial (La, Sr)$CoO_3/Pb(Zr,\;Ti)O_3/LaCoO_3$heterostructures show the remnant polarization states opposite to the $LaCoO_3/Pb(Zr,\;Ti)O_3/(La,\;Sr)CoO_3$ heterostructures. This indicates that the interface between (La, Sr)$CoO_3$ (LSCO) and $Pb(Zr, Ti)O_3(PZT)$ layers affects the asymmetric polarization remanence through electrochemical nature. The resistivity of $LaCoO_3$ (LCO) layer was found to be dependent on an ambient oxygen, primarily the ambient oxygen pressure during deposition. The resistivity of the LCO layer varied in the range of 0.1-100 $\Omega$cm. It is suggested that, with an appropriate resistivity of the LCO layer, the LCO/PZT/LSCO heterostructure can be used as the ferroelectric field effect transistor.

  • PDF

알칼리족 금속이 첨가된 LaCoO3 산화물에서 메틸 오렌지의 광촉매분해 반응 (Photocatalytic Decomposition of Methyl Orange over Alkali Metal Doped LaCoO3 Oxides)

  • 홍성수
    • Korean Chemical Engineering Research
    • /
    • 제55권5호
    • /
    • pp.718-722
    • /
    • 2017
  • 마이크로파 공정으로 제조된 순수한 $LaCoO_3$와 금속이온이 첨가된 $LaCoO_3$ 페롭스카이트 산화물에서 메틸오렌지의 광촉매 분해반응의 활성을 조사하였다. 순수한 $LaCoO_3$와 세슘 이온이 첨가된 $LaCoO_3$ 산화물들은 제조법과 무관하게 페롭스카이트 구조를 보여주었다. UV-Vis DRS 결과에 의하면 모든 촉매들은 가시광 영역에서 흡수스펙트럼을 나타내었다. 화학흡착된 산소종은 메틸오렌지의 광촉매 분해반응에서 중요한 역할을 하였으며, 화학흡착된 산소의 비율이 높을수록 더 높은 광촉매 활성을 보여주었다.

Citrate Sol-Gel법에 의한 Perovskite형 복합 산화물 LaBO3(B = Mn, Fe, Co)의 생성 및 환원 반응성 (Reactivity and Preparation of Perovskite-Type Mixed Oxides LaBO3(B = Mn, Fe, Co) by Citrate Sol-Gel Method)

  • 황호순;박일현
    • 대한화학회지
    • /
    • 제38권4호
    • /
    • pp.276-282
    • /
    • 1994
  • Citrate sol-gel법을 이용하여 perovskite형 복합산화물 LaBO$_3$(B = Mn, Fe, Co)을 공기 중 $850^{\circ}C$에서 24시간 동안 소성하여 제조하였다. X-선 회절분석(XRD)과 TPR결과에 의하면 이들 산화물의 결정구조와 산소화학양론은 LaMnO$_{3.16}$(a = 5.507, c = 13.329 $\AA$, hexagonal), LaFeO$_{3.17}$(a = 5.554, b = 5.555, c = 7.863 $\AA$, orthorhomibic), LaCoO$_{3.0}$(a = 5.436, c = 13.095 $\AA$, hexagonal)으로 수소 분위기(300torr)에서의 TPR결과에 의하면 이들 산화물은 2단계 환원반응으로 반응이 진행되며, 열적안정성은 LaMnO$_3$ > LaFeO$_3$ > LaCoO$_3$순으로 나타났고, 반응속도론적 결과 역시 LaCoO$_3$의 활성화에너지 값이 가장 낮음을 보였다.

  • PDF

$\textrm{LaCoO}_{3}/\textrm{Pb(Zr,Ti)O}_{3}/\textrm{(La,Sr)CoO}_{3}$다층구조에서의 강유전체 전계효과에 의한 LaCoO$_{3}$의 전항변조 (Resistance Modulation of $\textrm{LaCoO}_{3}$ by Ferroelectric Field Effect in $\textrm{LaCoO}_{3}/\textrm{Pb(Zr,Ti)O}_{3}/\textrm{(La,Sr)CoO}_{3}$ Heterostructures)

  • 김선웅;이재찬
    • 한국재료학회지
    • /
    • 제7권12호
    • /
    • pp.1058-1062
    • /
    • 1997
  • 강유전체 전계효과를 관찰하기 위해 LaCoO$_{3}$/Pb(Zr, Ti)O$_{3}$(La, Sr)CoO$_{3}$ 다층구조를 LcOo$_{3}$가 기판 위에 pulsed laser deposition(PLD)법으로 에피택셜하게 성장시켰다. 이러한 다층구조에서는 전도성 채널층으로 Si대신 반도성 LaCoO$_{3}$가 사용 되었다. LaCoO$_{3}$(LCO)의 비저항은 산소 분위기에 의하여 변화되었는데 특히 증착시 산소 분위기에 의존함을 보였다. LCO의 비저항은 0.1-100Ωcm범위에서 변화되었다. LCO층에 유도되는 강유전체 전계효과는 Pb(Zr, Ti)O$_{3}$(PZT)의 분극 상태에 따른 LCO의 저항 변화를 측정함으로써 관찰되었는데 1020$\AA$ 두께를 가진 LCO층에서는 4%의 저항 변화를 얻었으며 680$\AA$의 LCO에서는 9%의 증가된 저항 변화를 얻었다. DC 바이어스(-5V)를 가한 후에는 저항 변화가 45%까지 증가하였다. 이러한 결과는 적당한 비저항을 갖는 LCO를 사용한 LCO/PZT/LSCO다층구조가 강유전체 전계효과 트랜지스터로 사용될 수 있다는 가능성을 제시하고 있다.

  • PDF

$La_xCe_{1-x}Co_yCu_{1-y}O_{3-{\alpha}}$ Perovskite촉매의 선택적 CO 산화반응에 관한 연구 (Study on the Selective CO Oxidation Using $La_xCe_{1-x}Co_yCu_{1-y}O_{3-{\alpha}}$ Perovskite Catalysts)

  • 강대규;이영일;손정민
    • 한국수소및신에너지학회논문집
    • /
    • 제18권1호
    • /
    • pp.32-39
    • /
    • 2007
  • CO oxidation and selective CO oxidation of $La_xCe_{1-x}Co_yCu_{1-y}O_{3-{\alpha}}$ perovskite(x=1, 0.9, 0.7. 0.5; y=1, 0.9, 0.7, 0.5) were investigated. For CO oxidation, catalytic activities were studied according to different preparation conditions such as pH and calcination temperature. The influence of the change of the $O_2$ concentration for selective CO oxidation was studied, too. The substitution of Ce for La improved the catalytic activity for CO oxidation and selective CO oxidation and best activity was observed for $La_{0.7}Ce_{0.3}CoO_3$ prepared at pH 11 and calcined at $600^{\circ}C$. The temperature of 90% CO conversion for CO oxidation using $La_{0.7}Ce_{0.3}CoO_3$ was $230^{\circ}C$. In contrast to the enhancement effect by Ce substitution, the partial substitution of Cu for Co in $LaCo_yCu_{1-y}O_{3-{\alpha}}$ decreased catalytic activities for CO oxidation reaction compared to that using $LaCoO_3$. For selective CO oxidation, the best CO conversion was 66% at $230^{\circ}C$ for $La_{0.7}Ce_{0.3}CoO_3$. The CO conversion of $La_{0.7}Ce_{0.3}CoO_3$ was greatly increased from 66% to 91% as increasing $O_2$ concentration from 1% to 2%.

과량의 니켈 첨가로 합성된 NiO와 Co3O4가 도핑된 La(CoNi)O3 페로브스 카이트의 알칼리용액에서 산소환원 및 발생반응 특성 (Characterization of NiO and Co3O4-Doped La(CoNi)O3 Perovskite Catalysts Synthesized from Excess Ni for Oxygen Reduction and Evolution Reaction in Alkaline Solution)

  • 버링;임형렬;이홍기;박경세;심중표
    • 한국수소및신에너지학회논문집
    • /
    • 제32권1호
    • /
    • pp.41-52
    • /
    • 2021
  • NiO and Co3O4-doped porous La(CoNi)O3 perovskite oxides were prepared from excess Ni addition by a hydrothermal method using porous silica template, and characterized as bifunctional catalysts for oxygen reduction reaction (ORR) and oxygen evolution reaction (OER) for Zn-air rechargeable batteries in alkaline solution. Excess Ni induced to form NiO and Co3O4 in La(CoNi)O3 particles. The NiO and Co3O4-doped porous La(CoNi)O3 showed high specific surface area, up to nine times of conventionally synthesized perovskite oxide, and abundant pore volume with similar structure. Extra added Ni was partially substituted for Co as B site of ABO3 perovskite structure and formed to NiO and Co3O4 which was highly dispersed in particles. Excess Ni in La(CoNi)O3 catalysts increased OER performance (259 mA/㎠ at 2.4 V) in alkaline solution, although the activities (211 mA/㎠ at 0.5 V) for ORR were not changed with the content of excess Ni. La(CoNi)O3 with excess Ni showed very stable cyclability and low capacity fading rate (0.38 & 0.07 ㎶/hour for ORR & OER) until 300 hours (~70 cycles) but more excess content of Ni in La(CoNi)O3 gave negative effect to cyclability.

Hydrothermal Synthesis of LaCO3OH and Ln3+-doped LaCO3OH Powders under Ambient Pressure and Their Transformation to La2O2CO3 and La2O3

  • Lee, Min-Ho;Jung, Woo-Sik
    • Bulletin of the Korean Chemical Society
    • /
    • 제34권12호
    • /
    • pp.3609-3614
    • /
    • 2013
  • Orthorhombic and hexagonal lanthanum(III) hydroxycarbonate ($LaCO_3OH$) and $Ln^{3+}$-doped $LaCO_3OH$ ($LaCO_3OH:Ln^{3+}$, where Ln = Ce, Eu, Tb, and Ho) powders were prepared by a hydrothermal reaction under ambient pressure and characterized by thermogravimetry, powder X-ray diffraction, infrared and luminescence spectroscopy, and field-emission scanning electron microscopy. The polymorph of $LaCO_3OH$ depended on the reaction temperature, inorganic salt additive, species of $Ln^{3+}$ dopant, and solvent. The calcination of orthorhombic $LaCO_3OH:Ln^{3+}$ (2 mol %) powers at $600^{\circ}C$ yielded a mixture of hexagonal and monoclinic $La_2O_2CO_3:Ln^{3+}$ powders. The relative quantity of the latter increased with decreasing ionic radius of the $Ln^{3+}$ dopant ion and increasing doping concentrations. On the other hand, the calcination of hexagonal $LaCO_3OH:Ln^{3+}$ (2 mol %) powders at $600^{\circ}C$ resulted in a pure hexagonal $La_2O_2CO_3:Ln^{3+}$ powder, regardless of the species of $Ln^{3+}$ ions (Ln = Ce, Eu, and Tb). The luminescence spectra of $LaCO_3OH:Ln^{3+}$ and $La_2O_2CO_3:Ln^{3+}$ were measured to examine the effect of their polymorph on the spectra.

고체산화물 연료전지용 (La, Sr)$MnO_3$ 양극에 대한 Co 첨가효과 (Effect of Co Dopant on the (La, Sr)$MnO_3$ Cathode for Solid Oxide Fuel Cell)

  • 김재동;김구대;이기태
    • 한국세라믹학회지
    • /
    • 제37권6호
    • /
    • pp.612-616
    • /
    • 2000
  • The effect of Co dopant on the (La, Sr)MnO3 cathode was investigated. La2Zr2O7 and SrZrO3 were formed as the reaction products between YSZ and LSMC. The reactivity of LSMC with YSZ increased with increasing Co content. However, the cathodic polarization resistance decreased with increasing Co doping. Therefore, doping Co at Mn site in the (La, Sr)MnO3 cathode was effective on controlling the polarization resistance of the cathode. The polarization property of LSMC-YSZ composite(60 wt%: 40 wt%) cathode was better than that of LSMC single cathode.

  • PDF

(La,Sr)CoO₃/Pb(Zr,Ti)O₃/(La,Sr)CoO₃박막 캐패시터의 비대칭성의 전극 의존성 (Electrode Dependence of Asymmetric Behavior of (La,Sr)CoO₃/Pb(Zr,Ti)O₃/(La,Sr)CoO₃ Thin Film Capacitors)

  • 최치홍;이재찬;박배호;노태원
    • 한국세라믹학회지
    • /
    • 제35권7호
    • /
    • pp.647-647
    • /
    • 1998
  • 비대칭적인 전극 구조를 가지는 Pb(Zr,Ti)$O_3$(PZT) 박막의 비대칭적인 스위칭 특성을 연구하기 위해 Pulsed Laser Deposituin(PLD)방법으로 $LaAlO_3$ 기판 위에 (La,Sr)$CoO_3$/Pb(Zr,Ti)$O_3$/(La,Sr)$CoO_3$(LSCO) 다층구조를 성장시켰다. PZT 박막 캐시터의 전극이 모두 같은 조성일 때, 즉 $(La_0.5Sr_0.5)CoO_3$(LSCO)일 때 PZT 박막의 이력곡선은 대칭성을 보여주고 있다. 그러나 산화물 전극의 조성이 변할 때 PZT 박막 캐패시터는 비대칭성을 보여주고 있다. $LaCoO_3(LCO)$를 상층 전극, $La_0.5,Sr_0.5)CoO_3$(LSCO)를 하층 전극으로 사용하였을 때 이력 곡선은 음의 방향으로 분극된 상태가 불안정 하여 음의 잔류 분극의 완화 현상을 보여준다. 반면 상층 전극이 LSCO, 하층 전극이 LCO인 PZT 박막 캐패시터는 양의 방향의 분극 상태가 불안정하여 양의 잔류 분극이 완화현상을 보여준다. 이러한 이력 곡선의 완화 현상은 LCO/PZT 계면에서의 전자 밴드 구조의 변형에 의한 내부 전계의 형성 때문이라 생각할 수 있다. 내부 전계는 LCO/PZT와 LSCO/PZT 계면에서의 전자 밴드 구조의 변형에 의한 내부 전계의 형성 때문이라 생각할 수 있다.내부 전계는 LCO/PZT 계면에서의 인가된 전압 강하 차이에 의해 발생되며 전압 강하는 각각의 계면에서 0.6V와 -0.12V의 크기를 갖는다.