• Title/Summary/Keyword: $Bi_{2}Sr_{2}CuO_{x}$ thin film

Search Result 20, Processing Time 0.029 seconds

Epitaxy Growth of the Thin Films Fabricated by Layer by Layer Method (Layer by Layer 법으로 제작한 박막의 에피택셜 성장)

  • Kim, Tae-Gon;Cheon, Min-Woo;Yang, Sung-Ho;Park, Yong-Pil;Park, No-Bong;Lee, Hee-Kab
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.529-530
    • /
    • 2006
  • $Bi_2Sr_2CuO_x$ thin films have been fabricated by atomic layer-by-layer deposition using the ion beam sputtering method. During the deposition, 10 and 90 wt%-ozone/oxygen mixture gas of typical pressure of $1{\sim}9{\times}10^{-5}\;Torr$ are supplied with ultraviolet light irradiation for oxidation. XRD and RHEED investigations reveal out that a buffer layer with some different compositions is formed at the early deposition stage of less than 10 units cell and then Bi-2201 oriented along the c-axis is grown.

  • PDF

Characteristics of Bi2212 Thin Film Fabricated by Layer-by-Layer Deposition at an Ultra Low Growth rate (초저속 순차증착으로 제작한 Bi2212 박막의 특성)

  • Lee, Hee-Kab;Park, Yong-Pil;Cheon, Min-Woo
    • Proceedings of the KIEE Conference
    • /
    • 2002.11a
    • /
    • pp.119-121
    • /
    • 2002
  • $Bi_2Sr_2CuO_x$ thin films were fabricated by atomic layer-by-layer deposition using an ion beam sputtering method, 10 wt% and 90 wt% ozone mixed with oxygen were used with ultraviolet light irradiation to assist oxidation. At early stages of the atomic layer by layer deposition, two dimensional epitaxial growth which covers the substrate surface would be suppressed by the stress and strain caused by the lattice misfit, then three dimensional growth takes place. Since Cu element is the most difficult to oxidize, only Sr and Bi react with each other predominantly, and forms a buffer layer on the substrate in an amorphous-like structure, which is changed to $SrBi_2O_4$ by in-situ anneal.

  • PDF

Fabrication Condition for Single Phase of Bi-superconductor Thin Film

  • Ahn, Joon-Ho;Park, Yong-Pil;Wang, Jong-Bae
    • Transactions on Electrical and Electronic Materials
    • /
    • v.2 no.4
    • /
    • pp.11-14
    • /
    • 2001
  • Phase intergrowth in BSCCO thin films has been Investigated. It turfed out from XRD analyses of these phases that molar fraction of each constituent phase in the intergrowth thin film can be exhibited as a function of substrate temperature and ozone pressure. Super- conducting behavior of the intergrowth thin aim Is also discussed.

  • PDF

Preparation of Bi2O3-PbO-SrO-CaO Coating Sol for Wiring and Superconductivity and Its properties

  • Jung, Jee-Sung;Iwasaki, Mitusnobo;Park, Won-Kyu
    • Korean Journal of Materials Research
    • /
    • v.17 no.3
    • /
    • pp.147-151
    • /
    • 2007
  • Cu-free multi-component sol, of which final oxide composition becomes $Bi_{1.9}Pb{0.35}SrCaO,\;Bi_{1.8}Pb_{0.2}SrCaO\;and\;Bi_{1.5}SrCaO$, respectively, was prepared through sol-gel route and coated on a bare Cu substrate. Starting materials were metal-alkoxides as follows.; [$Bi(OC_{2}H_{5})_{3}\;Pb(O^{1}C_{3}H_{7})_{2},\;Sr(O^{i}C_{3}H_{7})_{2},\;Ca(OC_{2}H_{5})_{2}$] as a reagent grade. Transparent light yellowish sol was obtained in the case of $Bi_{1.9}Pb_{0.35}SrCaO\;and\;Bi_{1.8}Pb_{0.2}SrCaO$ composition and $Bi_{1.5}SrCaO$ composition's sol was light greenish. Each sol was repeatedly dip-coated on Cu substrate four times and pre-heated at $400^{\circ}C$ and finally heat-treated in the range of $740{\sim}900^{\circ}C$. In the results, crystalline phases confirmed by XRD were (2201) orthorhombic and monoclinic phases. However, only $Bi_{1.9}Pb_{0.35}SrCaO_{x}$ composition showed pseudo-superconductive behavior after heat-treatment at $900^{\circ}C$ for 12 seconds and then onset temperature was 77 K, even though it did not exhibit zero resistance below Tc.

A Study on the Epitaxial Growth of Superconducting Thin Film (초전도 박막의 에피택셜 성장에 관한 연구)

  • Lee, Hee-Kab;Park, Yong-Pil;Kim, Gwi-Yeol
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.05c
    • /
    • pp.208-211
    • /
    • 2002
  • $Bi_2Sr_2CuO_x$(Bi-2201) thin films were fabricated by atomic layer-by-layer deposition using an ion beam sputtering method. 10 wt% and 90 wt% ozone mixed with oxygen were used with ultraviolet light irradiation to assist oxidation. At early stages of the atomic layer by layer deposition, two dimensional epitaxial growth which covers the substrate surface would be suppressed by the stress and strain caused by the lattice misfit, then three dimensional growth takes place. Since Cu element is the most difficult to oxidize, only Sr and Bi react with each other predominantly, and forms a buffer layer on the substrate in an amorphous-like structure, which is changed to $SrBi_2O_4$ by in-situ anneal.

  • PDF

Characteristics of BSCCO Thin Film by Layer-by-layer Deposition (순차 스퍼터 법에 의한 BSCCO 박막의 특성)

  • Lee, Hee-Kab;Park, Yong-Pil;Kim, Gwi-Yeol;Oh, Geum-Gon;Choi, Woon-Shik;Cho, Choon-Nam
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.281-283
    • /
    • 2001
  • $Bi_{2}Sr_{2}CuO_{x}$(Bi-2201) thin films were fabricated by atomic layer-by-layer deposition using an ion bearn sputtering method. 10 wt% and 90 wt% ozone mixed with oxygen were used with ultraviolet light irradiation to assist oxidation. At early stages of the atomic layer by layer deposition. two dimensional epitaxial growth which covers the substrate surface would be suppressed by the stress and strain caused by the lattice misfit. then three dimensional growth takes place. Since Cu element is the most difficult to oxidize. only Sr and Bi react with each other predominantly. and forms a buffer layer on the substrate in an amorphous-like structure. which is changed to $SrBi_{2}O_{4}$ by in-situ anneal.

  • PDF

Characteristics of BSCCO Thin Film by Layer-by-layer Deposition (순차 스퍼터 법에 의한 BSCCO 박막의 특성)

  • 이희갑;박용필;김귀열;오금곤;최운식;조춘남
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.281-283
    • /
    • 2001
  • Bi$_2$Sr$_2$CuO$\_$x/(Bi-2201) thin films were fabricated layer-by-layer deposition using an ion beam sputtering method. 10 wt% and 90 wt% ozone mixed with oxygen were used ultraviolet light irradiation to assist oxidation. At early stages of the atomic layer by layer deposition, two dimensional epitaxial growth which covers the substrate surface would be suppressed by the stress and strain caused by the lattice misfit, then three dimensional growth takes place. Since Cu element is the most difficult to oxidize, only Sr and Bi react with each other predominantly, and forms a buffer layer on the substrate in an amorphous-like structure, which is changed to SrBi$_2$O$_4$ by in-situ anneal.

  • PDF

Epitaxial Growth of BSCCO Thin film Fabricated by Layer-by-layer Sputtering

  • Yang, Sung-Ho;Park, Yong-Pil;Lee, Hee-Kab
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.212-217
    • /
    • 2000
  • Bi$_2$Sr$_2$CuO$_{x}$(Bi-2201) thin films have been fabricated by atomic layer-by-layer deposition using ion beam sputtering(IBS) process. During the deposition, 14 wt%-ozone/oxygen mixture gas of typical pressure of 5.0$\times$10$^{-5}$ Torr is supplied with ultraviolet light irradiation for oxidation. XRD and RHEED investigations reveal that a buffer layer with compositions different from Bi-2201 is formed at the early deposition stage of less than 10 units cell and then Bi-2201 oriented along the c-axis is grown.n.

  • PDF

Fabrication Condition for Single Phase of BSCCO Thin Film

  • An, In-Soon;Chun, Min-Woo;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.327-330
    • /
    • 2001
  • Phase intergrowth in BSCCO thin films have been investigated. It turned out from XRD analyses of these phases that molar fraction of each constituent phase in the intergrowth thin film can be exhibited as a function of substrate temperature and ozone pressure. Superconducting behavior of the intergrowth thin film is also discussed.

  • PDF

A Study on the Resistivity-Temperature Characteristic of the Bi-Superconducting Thin Films Fabricated by using the Bon Beam Sputtering Method (이온 빔 스퍼링 법으로 제작한 Bismuth계 초전도 박막의 저항률-온도특성에 관한 연구)

  • Cheon, Min-Woo;Park, No-Bong;Yang, Sung-Ho;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.1218-1221
    • /
    • 2004
  • Bi2212 superconducting thin films fabricated by using the ion Beam Sputtering Method. As a result, although the composition of Bi2212 was set up, the phase of Bi2201, Bi2212 and Bi2223 was formed. The formation area of these stable phases is indicated as inclined line in the direction of the right lower end from the Arrhenius plot of the substrate temperature-oxidation gas pressure, and are distributed in very small area. The activation energy for the phase transformation from the Bi2201 to the Bi2212 is estimated in terms of the Avrami equation.

  • PDF