• Title/Summary/Keyword: $B_4C/Al$ cermet

Search Result 3, Processing Time 0.012 seconds

Effects of Atmosphere during Al Infiltration on Properties of B4C/Al Cermets (B4C/Al 복합체 제조시 함침 분위기가 물성에 미치는 영향)

  • Lim, Kyoung-Ran;Kang, Deog-Il;Kim, Chang-Sam
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.11
    • /
    • pp.1069-1073
    • /
    • 2002
  • Properties of $B_4C/Al$ cermets were studied as a function of atmosphere during infiltration and post-heat treatment. The cermet A(infiltrated at $1100{\circ}C$/10 min under vacuum) had 19.4 wt% of Al but the cermet B(infiltratd at $1080{\circ}C$/10 min under a flowing argon) showed 14.4 wt% of Al. It indicated that the reaction between $B_4C$ and Al underwent slower under vacuum than under a flowing argon. The cermet B as infiltrated showed the density of 2.65 $g/cm^3$, the MOR of 503 MPa and the Young's Modulus of 237 GPa, but the post-heat treatment at $900{\circ}C$ for 8h under a flowing Ar gave rise to the cermet with the density of 2.65 $g/cm^3$, the MOR of 296 MPa, the Young's Modulus of 300 GPa. The cermet B showed better properties than the cermet A. Changes in compositions of the cermets by the post-heat treatment were observed qualitatively by XRD and SEM, the amount of Al was determined by analysis of its DSC curve.

Effect of Addition of Other Componene (B4C, Mn, TiB2, B) on TiC-Ni3Al Cermet (TiC-Ni3Al Cermet에 타성분(B4C, Mn, TiB2, B) 첨가의 영향)

  • 김지헌;이완재
    • Journal of Powder Materials
    • /
    • v.9 no.5
    • /
    • pp.352-358
    • /
    • 2002
  • The effects of boron or manganese added as $B_4C$, Mn, $TiB_2$, B on TiC-30vo1.%$Ni_3Al$ cermet sintered at 1380 and $1400^{\circ}C$ for 1 hour, were examined in relation with shrinkage, relative density, microstructure, lattice parameter, hardness and fracture toughness ($K_{IC}$). The results are summarized as follows: 1) The highest shrink-age showed about 30.5% in the specimen added B$_4$C and the maximum relative density was about 99% in the specimen added $TiB_2$; 2) The grains of TiC were grown during sintering and made the surrounding structure by adding boron and manganese. The largest grain size showed about $2.8\mutextrm{m}$ in the specimen with boron sintered at $1400^{\circ}C$;3) The lattice parameter of TiC was about $4.325\AA$ and $Ni_3Al$ about $3.592\AA$ by adding other elements; 4) The highest hardness was about $1100kgf/\textrm{mm}^2$ in the specimen with B4C; 5) The fracture toughness ($K_{IC}$) showed about $15MNm^{-3/2}$ in the specimen added $TiB_2$.