• Title/Summary/Keyword: $B_2O_3$ substitution

Search Result 107, Processing Time 0.025 seconds

Piezoelectric and Electro-induced Strain Properties of $(Pb_{1-2x/3}Bi_x)[(Ni_{1/3}Nb_{2/3})_{0.4}(Ti_{0.6}Zr_{0.4})_{0.6}]O_3$Ceramics with the Substitution of $Bi_2O_3$ ($Bi_2O_3$치환에 따른 $(Pb_{1-2x/3}Bi_x)[(Ni_{1/3}Nb_{2/3})_{0.4}(Ti_{0.6}Zr_{0.4})_{0.6}]O_3$ 세라믹스의 압전 및 전계유기 왜형 특성)

  • 윤현상;정회승;임인호;윤광희;김준한;박창엽
    • Electrical & Electronic Materials
    • /
    • v.10 no.5
    • /
    • pp.434-439
    • /
    • 1997
  • It this paper, the piezoelectric and electro-induced strain properties of (P $b_{1-}$2x/3/B $i_{x}$ )[N $i_{1}$3/N $b_{2}$3/)$_{0.4}$( $Ti_{0.6}$Z $r_{0.4}$)$_{0.6}$] $O_3$ceramics (x=0, 0.005, 0.02) were investigated with the substitution of B $i^{3+}$, and the feasibility of the application for bimorph actuator was evaluated by measuring the dynamic properties of the piezoelectric bimorph fabricated with above ceramics. Dielectric constant was enhanced with the increase of B $i^{3+}$ substitution, and appeared the maximum value of 5032 at x=0.01 composition. Increasing the substitution of B $i^{3+}$, the electromechanical coefficient( $k_{p}$ , $k_{31}$ ) was increased up to the substitution of 0.5 mol% B $i^{3+}$, showed the value of 0.656, 0.439, respectively. The piezoelectric constant( $d_{33}$ $d_{31}$ ) had the highest value of 344, 825 with the substitution of 0.5 mol% B $i^{3+}$. The strain, generated by 60 Hz AC electric field, had the largest value of 1200($\times$10$^{-6}$ $\Delta$1/1) in the composition with the substitution of 0.5 mol% B $i^{3+}$. The dynamic properties of the bimorph actuator, fabricated with the composition substitution of 0.5 mol% B $i^{3+}$, showed the largest value of 325 $\mu$m at $\pm$150 V square pulse. square pulse.are pulse..

  • PDF

Physical Properties and Hydroxyapatite Formation of Low Alkali Containing Bioglass (저농도 알칼리 생체유리의 물성 및 Hydroxyapatite 형성)

  • 김용수;김철영
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.12
    • /
    • pp.1521-1528
    • /
    • 1994
  • To improve mechanical strength of bioglass, it is considered to use the glass as a coating material to alumina, but the difference in thermal expansion coefficient between two materials is too high to make a good coating. The aim of the present study, therefore, is to find out proper glass composition matching its thermal expansion coefficient to that of alumina without losing biocompatibility. In the present work, various glasses were prepared by substituting B2O3 and CaO for Na2O in the glass system of 55.1%SiO2-2.6%P2O5-20.1%Na2O-13.3%CaO-8.9%CaF2 (in mole%), and the thermal expansion property and reaction property in tris-buffer solution for the resulting glasses were measured. The thermal expansion coefficient of the glass was decreased with the substitution of B2O3 for Na2O, and it became close to that of alumina in the glass in which 8 mole% of CaO was substituted for Na2O. Hydroxyapatite formation was enhanced and silica rich layer thickness was decreased with B2O3 substitution for Na2O. CaO substitution for Na2O didn't deteriorated the hydroxyapatite development.

  • PDF

Improvement of $^{4}I_{11/2}{\to}^{4}I_{13/2}$ Transition Rate and Thermal Stabilities in $Er^{3+}-Doped\;TeO_2-B_2O_3\;(GeO_2)-ZnO-K_2O$ Glasses

  • Cho, Doo-Hee;Choi, Yong-Gyu;Kim, Kyong-Hon
    • ETRI Journal
    • /
    • v.23 no.4
    • /
    • pp.151-157
    • /
    • 2001
  • Spectroscopic and thermal analysis indicates that tellurite glasses doped with $B_2O_3$ and $GeO_2$ are promising candidate host materials for wide-band erbium doped fiber amplifier (EDFA) with a high 980 nm pump efficiency. In this study, we measured the thermal stabilities and the emission cross-sections for $Er^{3+}:^{4}I_{13/2}\;{\to}\;^{4}I_{15/2}$ transition in this tellurite glass system. We also determined the Judd-Ofelt parameters and calculated the radiative transition rates and the multiphonon relaxation rates in this glass system. The 15 mol% substitution of $B_2O_3$ for $TeO_2$ in the $Er^{3+}-doped\;75TeO_2-20ZnO-5K_2O$ glass raised the multiphonon relaxation rate for $^4I_{11/2}\;{\to}\;^4I_{13/2}$ transition from 4960 $s^{-1}$ to 24700 $s^{-1}$, but shortened the lifetime of the $^4I_{13/2}$ level by 14 % and reduced the emission cross-section for the $^4I_{13/2}\;{\to}\;^4I_{15/2}$ transition by 11%. The 15 mol% $GeO_2$ substitution in the same glass system also reduced the emission cross-section but increased the lifetime by 7%. However, the multiphonon relaxation rate for $^4I_{11/2}{\to}^4I_{13/2}$ transition was raised merely by 1000 $s^{-1}$. Therefore, a mixed substitution of $B_2O_3$ and $GeO_2$ for $TeO_2$ was concluded to be suitable for the 980 nm pump efficiency and the fluorescence efficiency of $^4I_{13/2}{\to}^4I_{15/2}$ transition in $Er^{3+}-doped$ tellurite glasses.

  • PDF

A Stud on the Catalytic Removal of Nitric Oxide (질소산화물의 촉매반응에 의한 저감기술에 관한 연구)

  • 홍성수;박종원;정덕영;박대원;조경목;오광중
    • Journal of Korean Society for Atmospheric Environment
    • /
    • v.14 no.1
    • /
    • pp.25-33
    • /
    • 1998
  • We have studied the reduction of NO by propane over perovskite-type oxides prepared by malic acid method. The catalysts were modified to enhance the activity by substitution by substitution of metal into A or B site of perovskite oxides. In addition, the reaction conditions, such as temperature, $O_2$ concentration, space velocity have been studed. In the $LaCoO_3$ type catalyst, the partial substitution of Ba, Sr into A site enhanced the catalytic activity in the reduction of NO. In the $La_{0.6}Sr_{0.4}Co_{1-x}Fe_xO_3(x=0 \sim 1.9)$ catalyst, the partial substitution of Fe into B site enhanced the conversion of NO, but excess amount of Fe decreased the conversion of NO. The surface area and catalytic activity of perovskite catalysts prepared by malic acid method showed higher values than those of solid reaction method. In the $La_{0.6}Sr_{0.4}Co_{1-x}Fe_xO_3$ catalyst, the conversion of NO increased with increasing $O_2$ concentration and contact time. The introduction of water into reactant feed decreased the catalytic activity.

  • PDF

A study on Dielectric and Electrical Properties using PMN Ceramics with $La_{2}O_{3}$ substitution ($La_{2}O_{3}$ 치환된 PMN계 세라믹스의 유전 및 전기적특성에 관한 연구)

  • Ji, S.H.;Kim, B.S.;Lee, N.H.;Lee, H.K.;Kim, Y.H.;Lee, D.C.
    • Proceedings of the KIEE Conference
    • /
    • 1996.07c
    • /
    • pp.1621-1623
    • /
    • 1996
  • The dielectric and polarizable properties of 0.85Pb$Mg_{1/3}Nb_{2/3}$)$O_3$-$0.125PbTiO_3$-$0.25BaTiO_3$ Ceramics have been investigated as a addition of the amount of $La_{2}O_{3}$($0{\leq}x{\geq}0.05$). The Temperature-dependant electrostictive characteristics of 0.85PMN-0.125PT-0.25BT relaxor ferroelectic system were improved by enhencing the extent of the diffuse phase transition(DPT). This was achieved using PMN-PT-BTceramics by the partial substitution of La at the Pb site. The curie temperature and the maximum dielectic permittivity decreased by substituting $La_{2}O_{3}$ and the electic field-related hysteresis phenomena decreased with increasing $La_{2}O_{3}$ substitution amount. It is showed decreasing in induced strain for electric field with increasing $La_{2}O_{3}$ substitution.

  • PDF

Effects of Substituting B2O3 for P2O5 on the Structure and Properties of P2O5-SnO2 Glass Systems (P2O5-SnO2계 유리에서 P2O5를 B2O3로 치환첨가 시 구조와 물성에 미치는 영향)

  • Choi, Byung-Hyun;Ji, Mi-Jung;An, Yong-Tae;Ko, Young-Soo;Lee, Young-Hun
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.8
    • /
    • pp.459-463
    • /
    • 2008
  • $P_2O_5-SnO_2$ system $0.5SnO_2-xP_2O_5-(0.5-x)B_2O_3$(x=0.1, 0.2, 0.3, 0.4, 0.5) glasses have been prepared for Pb-free low temperature glass frit. A investigation about the effect of $B_2O_3$ substitution on properties of $P_2O_5$ glasses, including glass structure properties, thermal properties, and mechanical properties was presented. Substance that is responsible for in moisture absorption existing circumstances supposes by phosphate, and excess moisture tolerance that state funeral's structure is improved breaking does not affect in state funeral bond that only most single bond remains, and can know that does not suffer big impact in boric oxide anomaly present state. This phenomenon estimates that connect with structure change. It is thought according to link this result the phosphoric acid happened structural change. $B_2O_3$ displacement quantity 0.3 mole put out $BO_4$ structures, but above 0.3 mole it changed with the case $BO_3$ structure which it displaces.

The Effect of Ta-substitution on the Bi-O Bonding and the Electrical Properties of $Bi_4$$Ti_3$$O_{12}$ Thin Films ($Bi_4$$Ti_3$$O_{12}$ 박막에서 Bi-O 결합과 전기 물성에 대한 Ta 치환의 영향)

  • 고태경;한규석;윤영섭
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.6
    • /
    • pp.558-567
    • /
    • 2001
  • 본 연구에서는 알콕사이드를 전구물질로 하는 졸겔공정을 이용하여 Bi 과잉 12 mol%의 조성인 B $i_4$ $Ti_3$ $O_{12}$ 박막과 B $i_4$ $Ti_{3-x}$T $a_{x}$ $O_{12}$(x=0.1, 0.2, 0.3) 박막을 제조하였다. XPS 분석에 따르면 Ta 치환 x=0.2에서 Bi 4f의 photoemission 곡선이 낮은 결합에너지로 이동하였고 피크 강도가 감소하는 현상이 관측되었다. 이는 x=0.1과 0.2 사이에서 Bi-O 결합이 길어져 인장상태 하에 있었음을 나타내었다. B $i_4$ $Ti_3$ $O_{12}$(BIT) 박막의 유전상수와 유전손실은 100 kHz에서 340, 0.05이었고, B $i_4$ $Ti_{3-x}$T $a_{x}$ $O_{12}$ 박막에서 이들 값은 x=0.1에서 가장 높았으며, 각각 480, 0.13이었다. B $i_4$ $Ti_3$ $O_{12}$ 박막의 잔류분극과 항전계는 1.24$\mu$C/$ extrm{cm}^2$, 31.4 kV/cm 이었으나, Ta 치환 x=0.2에서 이들 값은 각각 19.7$\mu$C/$\textrm{cm}^2$, 49.5 kV/cm 에 이르렀다. 또한, B $i_4$ $Ti_3$ $O_{12}$ 박막의 누설전류 밀도는 ~$10^{-6}$ A/$\textrm{cm}^2$ 정도이었으며, Ta 치환은 누설전류를 감소시켜 Ta 치환 x=0.2 이상에서 BIT 박막에 비해 한 차수 정도 낮아졌다. Ta 치환에 따른 B $i_4$ $Ti_3$ $O_{12}$ 전기 물성에서 변화는 Bi-O 결합에서 관측된 인장상태로의 전이와 연관성이 있었으며, 덧붙여 치환에서 생성된 전자에 의한 정공보상이 이에 영향을 끼쳤다. 정공보상이 이에 영향을 끼쳤다.끼쳤다.

  • PDF

Catalytic Combustion of Benzene over Perovskite-type Oxides Prepared Using Malic Acid Method (능금산법으로 제조된 페롭스카이트형 산화물에서 벤젠의 촉매연소반응)

  • Jung, Won-Young;Hong, Seong-Soo
    • Clean Technology
    • /
    • v.18 no.3
    • /
    • pp.259-264
    • /
    • 2012
  • Perovskite-type oxides were successfully prepared using malic acid method, characterized by TG/DTA, XRD, XPS, TEM and $H_2$-TPR and their catalytic activities for the combustion of benzene were determined. Almost of catalyst showed perovskite crystalline phase and 15-70 nm particle size. The $LaMnO_3$ catalysts showed the highest activity and the conversion reaches almost 100% at $350^{\circ}C$. The catalysts were modified to enhance the activity through substitution of metal into the A or B site of the perovskite oxides. In the $LaMnO_3$-type catalyst, the partial substitution of Sr into site the A-site enhanced the catalytic activity in the benzene combustion. In addition, the partial substitution of Co or Cu into site the B-site also enhanced the catalytic activity and the catalytic activity was in the order of Co > Cu > Fe in the $LaMn_{1-x}B_xO_3$ (B = Co, Fe, Cu) type catalyst.

CEMS Study of Ferrite Films M0.2Fe2.8O4 (M =Mn, Ni, Cu) (페라이트 박막 M0.2Fe2.8O4(M=Mn, Ni, Cu)의 Mössbauer 분광학적 연구)

  • Park, Jae Yun;Kim, Kwang Joo
    • Journal of the Korean Magnetics Society
    • /
    • v.24 no.2
    • /
    • pp.46-50
    • /
    • 2014
  • The crystallographic properties and cationic distribution of $M_{0.2}Fe_{2.8}O_4$ (M =Mn, Ni, Cu) and $Fe_3O_4$ thin films prepared by sol-gel method have been investigated by X-ray diffraction (XRD) and conversion electron M$\ddot{o}$ssbauer spectroscopy (CEMS). The ionic valence, preferred site, and hyperfine field of Fe ions of the ferrites could be obtained by analyzing the CEMS spectra. The $M_{0.2}Fe_{2.8}O_4$ films were found to maintain cubic spinel structure as in $Fe_3O_4$ with the lattice constant slightly decreased for Ni substitution and increased for Mn and Cu substitution from that of $Fe_3O_4$. Analyses on the CEMS data indicate that $Mn^{2+}$ and $Ni^{2+}$ ions substitute octahedral $Fe^{2+}$ sites mostly, while $Cu^{2+}$ ions substitute both the octahedral and tetrahedral sites. The observed intensity ratio $A_B/A_A$ of the CEMS subspectra of the samples exhibited difference from the theoretical value. It is interpreted as due to the effect of the M substitution for A and B on the Debye temperature of the site. The relative line-broadening of the B-site CEMS subspectra can be explained by the dispersion of magnetic hyperfine fields due to random distribution of M cations in the B sites.

The Study on Phase Transition Pressure of Donor doped Pb(Zr0.52Ti0.48)O3 Ceramics with Diamond Anvil Cell (다이아몬드 엔빌 셀을 이용한 Donor doped Pb(Zr0.52Ti0.48)O3 세라믹스의 상전이 압력 연구)

  • Cho, Kyung-Ho;Ko, Young-Ho;Seo, Chang-Eui;Kim, Kwang-Joo
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.5
    • /
    • pp.471-478
    • /
    • 2011
  • Investigations of crystal structure and phase transition of $Pb(Zr_{0.52}Ti_{0.48})O_3$ ceramics doped with A-site substitution impurity (La, Nd) or B-site substitution impurity (Sb, Nb) at 2 mol% concentration were carried out. X-ray diffraction patterns of impurities doped $Pb(Zr_{0.52}Ti_{0.48})O_3$ ceramics have been measured at pressures up to ~5 GPa with diamond anvil cell and synchrotron radiation. The patterns were obtained at room temperature using methanol-ethanol mixture as pressure-transmitting media. In order to refine the crystal structure, Rietveld analysis has been performed. The structures of impurities doped $Pb(Zr_{0.52}Ti_{0.48})O_3$ ceramics are tetragonal in space group P4mm at ambient pressure and are transformed into a cubic phase in space group Pm$\bar{3}$m as the pressure increases. In this study, when A-site substitution donor $La^{3+}$ or $Nd^{3+}$ ion was added to $Pb(Zr_{0.52}Ti_{0.48})O_3$ ceramics, the phase transition phenomena showed up at the pressure of 2.5~4.6 GPa, but when B-site substitution donor $Nb^{5+}$ or $Sb^{5+}$ ion was added to it, the phase transition appeared at relatively lower pressure of 1.7~2.6 GPa.