NANO-SIZED COMPOSITE MATERIALS WITH HIGH PERFORMANCE

  • Niihara, N.;Choa, H.Y.;Sekino, T.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 1996.11a
    • /
    • pp.6-6
    • /
    • 1996
  • Ceramic based nanocomposite, in which nano-sized ceramics and metals were dispersed within matrix grains and/or at grain boundaries, were successfully fabricated in the ceramic/cerarnic and ceramic/metal composite systems such as $Al_2O_3$/SiC, $Al_2O_3$/$Si_3N_4$, MgO/SiC, mullite/SiC, $Si_3N_4/SiC, $Si_3N_4$/B, $Al_2O_3$/W, $Al_2O_3$/Mo, $Al_2O_3$/Ni and $ZrO_2$/Mo systems. In these systems, the ceramiclceramic composites were fabricated from homogeneously mixed powders, powders with thin coatings of the second phases and amorphous precursor composite powders by usual powder metallurgical methods. The ceramiclmetal nanocomposites were prepared by combination of H2 reduction of metal oxides in the early stage of sinterings and usual powder metallurgical processes. The transmission electron microscopic observation for the $Al_2O_3$/SiC nanocomposite indicated that the second phases less than 70nm were mainly located within matrix grains and the larger particles were dispersed at the grain boundaries. The similar observation was also identified for other cerarnic/ceramic and ceramiclmetal nanocornposites. The striking findings in these nanocomposites were that mechanical properties were significantly improved by the nano-sized dispersion from 5 to 10 vol% even at high temperatures. For example, the improvement in hcture strength by 2 to 5 times and in creep resistance by 2 to 4 orders was observed not only for the ceramidceramic nanocomposites but also for the ceramiclmetal nanocomposites with only 5~01%se cond phase. The newly developed silicon nitride/boron nitride nanocomposites, in which nano-sized hexagonal BN particulates with low Young's modulus and fracture strength were dispersed mainly within matrix grains, gave also the strong improvement in fracture strength and thermal shock fracture resistance. In presentation, the process-rnicro/nanostructure-properties relationship will be presented in detail. The special emphasis will be placed on the understanding of the roles of nano-sized dispersions on mechanical properties.

  • PDF

Advanced SPS Systems and FGM Technolgy

  • Tokita, Masao
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2000.04a
    • /
    • pp.11-11
    • /
    • 2000
  • Large-size ceramic/metal bulk FGMs have been fabricated on a recently developed and the world's largest Spark Plasma Sintering(SPS) systems, As a part of the development program for practical production processes and machines for FGMs by SPS, the processes, mechanical properties, dimensional size and shape effects, and production machine systems were investigated. In the past, $ZrO_{2}$/TiAI, $ZrO_{2}$/Ni, $Al_{2}O_{3}$/Ti, WC/Co, WC/Co/Steel, A1/P, Polymide, Cu/Polymide, nano-composites, porous and other combinations of bulk FGMs have already been processed using SPS. However, most of the specimen sizes were small, in a range of 20 to 30mm in diameter. Recently disk-shape sintered compacts with diameters of 100 and 150 mm, and thickness of approximately 15 and 17 mm, $ZrO_{2}$(3Y)/ stainless steel FGMs were homogenous consolidated in a shorter sintering time, while maintaining high quality and repeatability by utilizing a temperature gradient sintering method. The SPS heating up and holding time totaled less than one hour. Therefore, the SPS process in expected to find increased use in the fabrication of large-size FGMs as a new industrial processing technology. This paper introduces SPS systems, the processing principles, features and the characteristies of ceramic/metal bulk FGM.

  • PDF

Mechanical Properties and Biocompatibility of Ti-Nb-Zr-Mo-CPP Biomaterial Fabricated by Spark Plasma Sintering (스파크플라즈마 소결에 의한 Ti-Nb-Zr-Mo-CPP 생체복합재의 기계적 성질 및 생체적합성)

  • Woo, Kee Do;Kim, Sang Mi;Kim, Dong Gun;Kim, Dae Young;Kang, Dong Soo
    • Korean Journal of Materials Research
    • /
    • v.23 no.2
    • /
    • pp.135-142
    • /
    • 2013
  • The Ti-6Al-4V extra low interstitial (ELI) alloy has been widely used as an orthopedic implant material because of its excellent mechanical properties and biocompatibility. However, it still has many problems, including a high elastic modulus and toxicity of the Al and V elements. Therefore, non-toxic biomaterials with a low elastic modulus need to be developed. A high energy mechanical milling (HEMM) process is introduced to improve the effect of sintering. Rapid sintering of spark plasma sintering (SPS) under pressure was used to make an ultra fine grain of Ti-25 wt.%Nb-7 wt.%Zr-10 wt.%Mo-(10 wt.%CPP) composites with bio-attractive elements for increasing strength. These composites were fabricated by SPS at $1000^{\circ}C$ at 60 MPa using HEMM powders. During the sintering process, $CaTiO_3$, TixOy, and CaO were formed because of the reaction between Ti and CPP. The effects of CPP content on the physical and mechanical properties of the sintered Ti-Nb-Zr-Mo-CPP composites were investigated. The biocompatibility and corrosion resistance of the Ti-Nb-Zr-Mo alloys were improved by the addition of CPP.

Machinable Ceramics Made by the Reaction Sintering of PSZ, Al2O3 and TiO2 (PSZ, Al2O3, TiO2를 반응소결하여 제조한 쾌삭(快削) 세라믹스)

  • Park, Jeong Hyun;Jung, Dong Sik;Lee, Won Jae;Kim, Il Soo
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.6
    • /
    • pp.581-585
    • /
    • 2012
  • Machinability is important in engineering applications, especially in the current micro-electronics industry. Most ceramic components have complex shapes and hence require machining generally with diamond tools, which incurs a high production cost. Recently, h-BN-containing machinable ceramics have been developed, but these materials are very expensive due to the high raw materials and production costs. Therefore, the development of low-cost machinable ceramics is necessary. In this study, inexpensive $Al_2TiO_5$ was studied as a replacement for h-BN. $Al_2O_3$, $TiO_2$ and partially stabilized $ZrO_2$(PSZ) powders were mixed with various mole ratios and were sintered at $1500^{\circ}C$ for 1 h. The density, hardness and strength were then measured. The phase analysis and microstructures were observed by XRD and SEM, respectively. The machinability of each specimen was tested by micro-hole machining. The results of this research showed that the produced composites could be used as low-cost machinable ceramics.

Microstructure and Mechanical Properties of Infiltrated Zirconia-Mullite Composite (침투된 지르코니아-뮬라이트 복합체의 미세구조 및 기계적 성질)

  • 손영권;이윤복;김영우;오기동;박홍채
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.2
    • /
    • pp.174-180
    • /
    • 2000
  • Y-TZP/mullite composites were prepared by the infiltration of Y-TZP precursor into partially reaction-sintered mullite. The addition of Y-TZP(~7.2 wt%) increased the bend strength(207 MPa), fracture toughness(4.6MPa.m1/2) and Vickers microhardness(853kg/$\textrm{mm}^2$) of the uninfiltrated mullite sintered at 162$0^{\circ}C$ for 10h by more than 75, 70 and 105%, respectively. Residual alumina-rich glass was observed at a mullite/mullite junction, due to the mullitization reaction of silica melt with crystalline $\alpha$-Al2O3 during a final sintering. Although ZrO2 inclusions improved the final sintered density of mullite they did not effectively prevent its grain growth.

  • PDF

Multifunctionality in Ceramic/Metal Nanocomposites

  • Sekino, Tohru;Kondo, Hiroki;Niihara, Koichi
    • Journal of Powder Materials
    • /
    • v.8 no.3
    • /
    • pp.186-191
    • /
    • 2001
  • Several fabrication processes, corresponding nanostructural features and multifunctionality as well has been investigated for oxide ceramic based nanocomposites with metal nanodispersion (i.e., ceramic/metal nanocomposites). Transition metal (Ni, Co, etc) dispersed alumina and zirconia based nanocomposites have been synthesized by reducing and hot-press sintering of ceramic and metal oxide mixtures prepared by several method. Improved fracture strength (1.1 and 1.9 GPa for $Al_2O_3/Ni$ and $ZrO_2/Ni$ nanocomposites, respectively) of these composites have been achieved according to their nanostructures. In addition, ferromagnetic characteristic has been kept. The variation of magnetization with an applied stress has found to be more sensitive as smaller as the magnetic metal dispersion is. This result thus suggests the possibility of fracture and/or stress sensing of the composites by simple magnetic measurement.

  • PDF

Effects of ceramic fillers on fracture resistance of barrier ribs of PDP

  • Baek, Se-Kyung;Kim, Yong-Seog
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2004.08a
    • /
    • pp.552-554
    • /
    • 2004
  • Barrier ribs of plasma display panel (PDP) are glass matrix composite reinforced with alumina particles. Mechanical properties of the ribs are very crucial for the improvement in reliability of the panel as the ribs might fracture during transportation and service. In this study, therefore, the effects of filler type and content on the mechanical properties of the ribs were investigated. The fillers used include $Al_2O_3$, $TiO_2$, $ZrO_2$ and fused silica. The content of the filler was changed from 0 to 40 vol.%. The mechanical properties of the ribs measured were hardness, Young's modulus, fracture toughness, and 3-point bending modulus. The fracture toughness evaluated by micro-Vicker's indentation of the composites, in general, was measured to increase with the content of the filler until the sintered density does not decrease significantly. The improvement, however, was dependent on the type of filler employed.

  • PDF

Tailored Powder Composites by Freeze Drying, Electrophoretic Deposition and Sintering

  • Olevsky, Eugene A.;Wang, Xuan
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.287-288
    • /
    • 2006
  • Two approaches for the fabrication of tailored powder composites with specially distributed pore-grain structure and chemical composition are investigated. Electrophoretic Deposition (EPD) followed by microwave sintering is employed to obtain functionally graded materials (FGM) by in-situ controlling the deposition bath suspension composition. $Al_2O_3/ZrO_2$ and zeolite FGM are successfully synthesized using this technique. In order to fabricate an aligned porous structure, unidirectional freezing followed by freeze drying and sintering is employed. By controlling the temperature gradient during freezing of powder slurry, a unidirectional ice-ceramic structure is obtained. The frozen specimen is then subjected to freeze drying to sublimate the ice. The obtained capillary-porous ceramic specimen is consolidated by sintering. The sintering of the graded structure is modeled by the continuum theory of sintering.

  • PDF

Designing Materials for Hard Tissue Replacement

  • Nath, Shekhar;Basu, Bikramjit
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.1
    • /
    • pp.1-29
    • /
    • 2008
  • In last two decades, an impressive progress has been recorded in terms of developing new materials or refining existing material composition/microstructure in order to obtain better performance in biomedical applications. The success of such efforts clearly demands better understanding of various concepts, e.g. biocompatibility, host response, cell-biomaterial interaction. In this article, we review the fundamental understanding that is required with respect to biomaterials development, as well as various materials and their properties, which are relevant in applications, such as hard tissue replacement. A major emphasize has been placed to present various design aspects, in terms of materials processing, of ceramics and polymer based biocomposites, Among the bioceramic composites, the research results obtained with Hydroxyapatite (HAp)-based biomaterials with metallic (Ti) or ceramic (Mullite) reinforcements as well as $SiO_2-MgO-Al_2O_3-K_2O-B_2O_3-F$ glass ceramics and stabilized $ZrO_2$ based bioinert ceramics are summarized. The physical as well as tribological properties of Polyethylene (PE) based hybrid biocomposites are discussed to illustrate the concept on how can the physical/wear properties be enhanced along with biocompatibility due to combined addition of bioinert and bioactive ceramic to a bioinert polymeric matrix. The tribological and corrosion properties of some important orthopedic metallic alloys based on Ti or Co-Cr-Mo are also illustrated. At the close, the future perspective on orthopedic biomaterials development and some unresolved issues are presented.

Mechanical Properties and Bio-Compatibility of Ti-Nb-Zr-HA Biomaterial Fabricated by Rapid Sintering Using HEMM Powders (고에너지 밀링분말과 급속소결을 이용한 Ti-Nb-Zr-HA 생체복합재의 기계적 성질 및 생체적합성)

  • Park, Sang-Hoon;Woo, Kee-Do;Kim, Sang-Hyuk;Lee, Seung-Min;Kim, Ji-Young;Ko, Hye-Rim;Kim, Sang-Mi
    • Korean Journal of Materials Research
    • /
    • v.21 no.7
    • /
    • pp.384-390
    • /
    • 2011
  • Ti-6Al-4V ELI (Extra Low Interstitial) alloy has been widely used as an alternative to bone due to its excellent biocompatibility. However, it still has many problems, including a high elastic modulus and toxicity. Therefore, nontoxic biomaterials with a low elastic modulus should be developed. However, the fabrication of a uniform coating is challenging. Moreover, the coating layer on Ti and Ti alloy substrates can be peeled off after implantation. To overcome these problems, it is necessary to produce bulk Ti and Ti alloy with hydroxyapatite (HA) composites. In this study, Ti, Nb, and Zr powders, which are biocompatible elements, were milled in a mixing machine (24h) and by planetary mechanical ball milling (1h, 4h, and 6h), respectively. Ti-35%Nb-7%Zr and Ti-35%Nb-7%Zr-10%HA composites were fabricated by spark plasma sintering (SPS) at $1000^{\circ}C$ under 70MPa using mixed and milled powders. The effects of HA addition and milling time on the biocompatibility and physical and mechanical properties of the Ti-35%Nb-7%Zr-(10%HA) alloys have been investigated. $Ti_2O$, CaO, $CaTiO_3$, and $Ti_xP_y$ phases were formed by chemical reaction during sintering. Vickers hardness of the sintered composites increases with increased milling time and by the addition of HA. The biocompatibilty of the HA added Ti-Nb-Zr alloys was improved, but the sintering ability was decreased.