Low Temperature Sintering and Microwave Dielectric Properties of 0.85CaWO4-0.15LnNbO4 (Ln = La, Sm) Ceramics

  • Kim, Su-Jung;Kim, Eung-Soo
    • Korean Journal of Materials Research
    • /
    • v.17 no.8
    • /
    • pp.442-446
    • /
    • 2007
  • Microwave dielectric properties of $0.85CaWO_4-0.15LnNbO_4$ (Ln = La, Sm) ceramics were investigated as a function of the sintering temperature and $Li_2WO_4$ content from 0.8 wt.% to 1.5 wt.%. A single phase with tetragonal scheelite structure was obtained at a given composition ranges. For the specimens with $Li_2WO_4$, the sintering temperature could be effectively reduced from $1150^{\circ}C$ to $900^{\circ}C$ due to the enhancement of sinterability. Dielectric constant (K) of the specimens with $LaNbO_4$ and $SmNbO_4$ was increased with the increase of sintering temperature and/or $Li_2WO_4$ content. However, K of the specimens with $LaNbO_4$ was higher than that of $SmNbO_4$ due to the larger dielectric polarizability $(\alpha)$ of $LaNbO_4$ ($18.08{\AA}$) than that of $SmNbO_4$ ($16.75{\AA}$). With an increase of $Li_2WO_4$ content, Qf value of the specimens with $SmNbO_4$ was decreased, while that of the specimens with $LaNbO_4$ was increased. Temperature coefficient of resonant frequency (TCF) was increased with the increase of $Li_2WO_4$ content.