• Title/Summary/Keyword: ${Zn_2}{SiO_4}$:Mn

Search Result 136, Processing Time 0.034 seconds

Synthesis of Zn2SiO4 : Mn Phosphor Particles by Spray-pyrolysis Method (분무 열 분해법을 이용한 Zn2SiO4 : Mn 나노 형광체의 광학적 특성에 관한 연구)

  • Nam, Sang-Hun;Kim, Myoung-Hwa;Lee, Sang-Duck;Boo, Jin-Hyo
    • Journal of the Korean Vacuum Society
    • /
    • v.19 no.1
    • /
    • pp.66-71
    • /
    • 2010
  • Spherical shape $Zn_2SiO_4:Mn$ phosphor particles with the mean particle size from submicron to micron sizes were prepared by ultrasonic spray pyrolysis method. A droplet separator was introduced to control the size distribution of the phosphor particles with spherical shape. The $Zn_2SiO_4:Mn$ phosphor particles with 2 mol% doping concentration of manganese have decay time and have photoluminescence intensities comparable with those of the latest commercial product prepared by the solid state reaction method. The size of the phosphor particles was decreased from 1 to 0.2 micrometers as the inorganic salt solution concentration was changed from 0 to 5 M. The phosphor particles prepared from the solutions above 0.5 M have photoluminescence intensities comparable with that of the latest commercial product.

Aging Characteristics of the Green Phosphors for PDP Application

  • Han, Bo-Yong;Yoo, Jae-Soo
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2005.07b
    • /
    • pp.1262-1265
    • /
    • 2005
  • The picture quality of a plasma display panel is very sensitive to the phosphor characteristics such as decay time, surface state, and even longevity of phosphor material in itself. In this work, material characteristics of $Zn_2SiO_4:Mn$, $Y_2O_3-coated$ $Zn_2SiO_4:Mn$, and $YBO_3:Tb$, which are dominant in commercial application, were examined for investigating the aging characteristics of green PDP phosphors. It was found that $Y_2O_3-coated$ $Zn_2SiO_4:Mn$ are easily degraded at high temperature. However, all the samples were very weak after vacuum annealing. The luminescence intensity was decreased by order of one magnitude.

  • PDF

Magnetic Loss of Mn-Zn Ferrite Cores Used for SMPS (SMPS용 Mn-Zn 페라이트 코어의 자기손실 특성)

  • 권태석;김성수
    • Journal of the Korean Magnetics Society
    • /
    • v.9 no.3
    • /
    • pp.149-153
    • /
    • 1999
  • Frequency and temperature dependence of magnetic loss has been investigated in Mn-Zn ferrites containing the sesistive temary compounds of $SiO_2-CaO-V_2O_5$. The Mn-Zn ferrite with the composition of $MnO:ZnO:Fe_2O_3=36:11:53$(by mol %) are prepared by self-propagating high-temperature synthesis. From the results of frequency dependence of core loss, it has been found that the hysteresis loss is dominant at low frequency and the eddy current loss becomes more dominant as the frequency increases. With the addition of resistive compound, the frequency dependence of core loss, it has been found that the hysteresis loss is dominant at low frequency and the eddy current loss becomes more dominant as the frequency increases. With the addition of resistive compound, the frequency region where the hysteresis loss is dominant becomes wide. The core-loss minimum occurs at about 4$0^{\circ}C$ in the specimens with the additive because of the reduction in eddy current loss.

  • PDF

Formation and Characterization of Green and Blue Phosphor Nano Powders (녹색과 청색 형광체 나노 분말의 합성 및 특성 평가)

  • Kwon, Oh Sung;You, Young Chul;Kim, Sang Min;Kim, Ki Do;Lim, Hyung Sup;Kim, Hee Taik
    • Applied Chemistry for Engineering
    • /
    • v.20 no.5
    • /
    • pp.565-569
    • /
    • 2009
  • Nano-sized green and blue phosphor powders were synthesized by liquid phase method to confirm the size and morphology. By using that process, the particle sizes of green and blue phosphor particles were 80 nm and 60 nm, respectively. The characteristic comparison of $Zn_2SiO_4$ : Mn and BAM : Eu was carried out and as a result, $Zn_2SiO_4$ : Mn powders showed an higher PL performance compared to BAM : Eu.