• 제목/요약/키워드: ${\varepsilon}$ 마르텐사이트

검색결과 20건 처리시간 0.016초

Fe-Mn 합금에서 열적 ${\varepsilon}$ 마르텐사이트와 변형유기 ${\varepsilon}$ 마르텐사이트 부피분율에 대한 진동감쇠능의 의존성 (Dependence of Damping Capacity on Volume Fractions of Thermal and Deformation-induced ${\varepsilon}$ Martensites in an Fe-Mn Alloy)

  • 전중환;홍권표;최종술
    • 열처리공학회지
    • /
    • 제15권6호
    • /
    • pp.272-278
    • /
    • 2002
  • The changes in damping capacity with volume fractions of thermal and deformation-induced ${\varepsilon}$ martensites were compared and analyzed in an Fe-23%-Mn alloy. The volume fraction of thermal ${\varepsilon}$ martensite increased with decreasing cooling temperature, whereas that of deformation-induced ${\varepsilon}$ martensite increased steeply up to 10%- of cold rolling and nearly saturated in further cold rolling. In the case of thermal ${\varepsilon}$ martensite, the damping capacity increased linearly with the increase in ${\varepsilon}$ martensite content. For the deformation-induced ${\varepsilon}$ martensite, however, the damping capacity increased continuously up to 70%- of ${\varepsilon}$ martensite, over which it decreased suddenly. TEM microstructures showed that the deterioration of damping capacity above 70%- of deformation-induced ${\varepsilon}$ martensite is ascribed to the introduction of perfect dislocations, which play a important role in inhibiting the movement of damping sources such as stacking fault boundaries inside ${\varepsilon}$ martensite, ${\varepsilon}$ martensite variant boundaries and ${\gamma}/{\varepsilon}$ interfaces.

Fe-Cr-Mn-X계 합금의 감쇠능 및 플라즈마이온질화 특성에 미치는 합금원소의 영향 [I 감쇠능] (The Effect of Alloy Elements on the Damping Capacity and Plasma Ion Nitriding Characteristic of Fe-Cr-Mn-X Alloys [I Damping Capacity])

  • 손동욱;정상훈;김재환;이종문;김익수;강창룡
    • 동력기계공학회지
    • /
    • 제9권1호
    • /
    • pp.70-75
    • /
    • 2005
  • The damping property of Fe-12Cr-22Mn-X alloys has been investigated to develop high damping and high strength alloy. Particularly, the effect of the phase of austenite, alpha and epsilon martensite, which constitute the structure of the alloys Fe-12Cr-22Mn-X alloys, on the damping capacity at room temperature has been investigated. Various fraction of these phases were formed depending on the alloy element and cold work degree. The damping capacity is strongly affected by ${\varepsilon}$ martensite while the other phase, such as ${\alpha}'$ martensite, actually exhibit little effect on damping capacity. In case of Fe-12Cr-22Mn-3Co alloy, the large volume fraction of ${\varepsilon}$ martensite formed at about 30% cold rolling, and in case of Fe-12Cr-22Mn-1Ti alloy, formed at about 20% cold rolling and showed the highest damping capacity. Damping capacity showed higher value in Fe-12Cr-22Mn-1Ti alloy than one in Fe-12Cr-22Mn-3Co alloy.

  • PDF

Fe-Al-Mn 합금의 진동감쇠능 및 인장성질에 미치는 미세조직의 영향 (Effect of Microstructure on the Damping Capacity and Tensile Properties of Fe-Al-Mn Alloys)

  • 손동욱;김재환;이종문;김익수;김한청;강창룡
    • 동력기계공학회지
    • /
    • 제8권4호
    • /
    • pp.31-37
    • /
    • 2004
  • The damping capacity and strength of Fe-2Al-26Mn alloys have been studied for the development of new materials with high strength and damping capacity. Particularly, the effect of ${\alpha}'\;and\;{\varepsilon}$ martensite phase, which constitutes the microstructure of cold rolled Fe-Al-Mn alloys, has been investigated in terms of the strength and damping capacity of the alloys. The damping capacity rises with increasing the degree of cold rolling and reveals the maximum value at 25% reduction. The damping capacity is strongly affected by the volume fraction of ${\varepsilon}$ martensite, while the other phases, such as ${\alpha}'$ martensite and austenite phase, actually exhibit little effect on damping capacity. Considering that tensile strength increases and elongation decreases with increasing the volume fraction of ${\alpha}'$ martensite, it is proved that tensile strength is mainly affected by the amount of ${\alpha}'$ martensite.

  • PDF

Fe-Mn계 합금에서 응력유기 ${\varepsilon}$ 마르텐사이트의 양에 미치는 열처리 온도의 영향 (Effect of Heat Treatment Temperature on Amount of Stress-Induced ${\varepsilon}$ Martensite in an Fe-Mn Baesd Alloy)

  • 지광구;한준현;장우양
    • 열처리공학회지
    • /
    • 제17권6호
    • /
    • pp.342-345
    • /
    • 2004
  • In this work, a new method of measuring volume fraction of deformation-induced ${\varepsilon}$ martensite is proposed using endothermic heat on reverse transformation. As grain size increases, the amount of ${\varepsilon}$ martensite forming on cooling increases. However, with a decrease in grain size, more ${\varepsilon}$ is induced by deformation, improving shape memory effect.

저방사화 Fe-Cr-Mn계 스테인리스강의 미세 조직 특성 및 부식 저항성에 미치는 Mn 및 W의 영향

  • 이정훈;박용수;김영식;류우석;홍준화
    • 한국원자력학회:학술대회논문집
    • /
    • 한국원자력학회 1996년도 춘계학술발표회논문집(3)
    • /
    • pp.335-340
    • /
    • 1996
  • 핵융합로 제1벽 재료의 후보재로 고려되는 Fe-Cr-Mn계 스테인리스강을 진공 용해하여 이 합금의 미세 조직 및 기계적 성질 그리고 부식 특성에 미치는 Mn, W의 첨가 효과 및 소둔 열처리 온도의 효과에 대하여 실험하였다. 미세 조직 분석은 광학 현미경 관찰, XRD분석 등으로 행하였으며, 기계적 시험으로는 상온 인장 시험, 경도 시험 및 충격 시험을 행하였다. 그리고 부식 시험으로는 부식 환경을 염산과 황산으로 나누어 각 환경에서의 양극 분극 시험을 행하였다. Mn함량이 증가할수록 오스테나이트상이 증가하고 있으나, $\alpha$'마르텐사이트는 급격히 감소하는 대신$\varepsilon$마르텐사이트는 Mn함량이 20%일 때 최대간을 보인 뒤 감소하고 있다. Mn함량이 증가할 수록 또한 소둔 온도가 상승할수록 항복 강도, 인장 강도 및 경도는 감소하였으며 연신율은 증가하였다. 이러한 결과는 합금 중의 오스테나이트 및 마르텐사이트 조직의 함량과 밀접한 관련이 있는 것으로 판단된다. 한편 합금 중의 Mn함량이 증가할수록 부식 환경에 관계없이 부식 저항성의 변화는 크지 않은 것으로 나타났다. 그러나 W함량이 증가하면 환경에 관계없이 임계 전류 밀도를 감소시키나, 부동태 전류 밀도는 HCI환경에서는 감소시키고 H$_2$SO$_4$환경에서는 오히려 증가시키는 상반된 효과가 나타났다.

  • PDF

Fe-Mn 계 합금에서 비부피 차를 이용한 ${\varepsilon}$ 마르텐사이트의 부피분율 측정 (Measurement of Volume Fraction of ${\varepsilon}$ Martensite using Specific Volume Difference in Fe-Mn Based Alloys)

  • 지광구;한준현;장우양
    • 열처리공학회지
    • /
    • 제16권4호
    • /
    • pp.211-215
    • /
    • 2003
  • In this work, a new way of measuring the volume fraction of e martensite in Fe-based alloys has been proposed. Since the specific volume of ${\varepsilon}$ martensite, depending on alloy composition, is smaller than that of austenite i.e ${\gamma}$ phase, volume expansion takes place during ${\varepsilon}{\rightarrow}{\gamma}$ reverse transformation. As the amount of the volume expansion is proportional to the product of specific volume difference times the volume fraction of ${\varepsilon}$ martensite, the volume fraction of ${\varepsilon}$ martensite can be calculated by measuring the volume expansion and the specific volume difference. Such a relationship was confirmed in Fe-21Mn and Fe-32Mn-6Si alloys which undergo ${\gamma}{\rightarrow}{\varepsilon}$ martensitic transformation on cooling and by cold rolling, respectively. It was also found that the former has isotropic ${\varepsilon}$ martensite while the latter has anisotropic ${\varepsilon}$ martensite.

Fe-17%Mn 합금의 진동감쇠능에 미치는 ε 마르텐사이트 함량과 진폭변형율의 영향 (Effect of ε Martensite Content and Strain Amplitude on Damping Capacity of Fe-17%Mn Alloy)

  • 전중환;이영국;최종술
    • 열처리공학회지
    • /
    • 제9권2호
    • /
    • pp.112-120
    • /
    • 1996
  • The effects of ${\varepsilon}$ martensite content and strain amplitude on damping capacity of an Fe-17%Mn alloy have been studied to establish damping mechanism of Fe-Mn system corresponding to the magnitude of strain amplitude. In a range of $1{\times}10^{-4}{\sim}3{\times}10^{-4}$ strain amplitude, the damping capacity is linearly proportional to the ${\varepsilon}$ martensite content, which suggests that stacking faults and ${\varepsilon}$ martensite variant boundaries are the principal damping sources. In the range of $4{\times}10^{-4}{\sim}6{\times}10^{-4}$ strain amplitude, however, a maximum damping capacity is observed around 68 vol.% ${\varepsilon}$. This behavior is very similar to dependence of relative area of ${\gamma}/{\varepsilon}$ interface on ${\varepsilon}$ martensite content. This means that in this strain range, ${\gamma}/{\varepsilon}$ interface acts as damping source in addition to the stacking faults and variant boundaries in Fe-17%Mn alloy.

  • PDF

Fe-Mn 합금의 γ→ε 마르텐사이트변태에 필요한 구동력 (Driving Forces for γ→ε Martensitic Transformation of Fe-Mn Alloys)

  • 이영국;최종술
    • 열처리공학회지
    • /
    • 제9권4호
    • /
    • pp.243-251
    • /
    • 1996
  • Dilatometric experiment and thermodynamic calculation have been performed to determine $M_s$, $A_s$ and driving forces for ${\gamma}{\rightarrow}{\varepsilon}$ martensitic transformation of Fe-Mn alloys. The transformation temperatures($M_s$, $A_s$, $T_o) were decreased with increasing manganese content and were newly formulated as a function of manganese content. Driving force for ${\gamma}{\rightarrow}{\varepsilon}$ martensitic transformation was increased from -75J/mole to -105J/mole with increasing manganese content from 15wt.% to 25wt.%. Transformation temperature hysteresis($A_s-M_s$) was also increased from 50K to 80K with increasing mangenese content from 15wt.% to 25wt.%. The small driving force(-75J/mole~-105J/mole) and small ${\Delta}T$(50K~80K) for ${\gamma}{\rightarrow}{\varepsilon}$ martensitic transformation indicated that Fe-Mn alloys behave like thermoelastic martensitic alloys : We would like to call them semi-thermoelastic martensitic alloys.

  • PDF

진동제어에 의한 정밀기기의 고성능화를 위한 고강도 및 고감쇠능 합금개발 (Development of Alloy with High Strength and Damping Capacity for High-Performance of Precision Devices by Vibration Control)

  • 강창룡;김익수
    • 한국해양공학회지
    • /
    • 제22권6호
    • /
    • pp.46-51
    • /
    • 2008
  • The effect of the addition of Co and N and subzero treatment on tensile strength and damping capacity was investigated in Fe-Cr-Mn alloy. Austenite was transformed into martensite by cold rollins increasing the degree of cold rollins led to an increase in the volume fraction of martensite. The damping capacity linearly increased with increasing volume fraction of ${\varepsilon}$ martensite in cold rolled specimens and subzero treated specimens after cold rolling. The volume fraction of ${\varepsilon}$ martensite, tensile strength and damping capacity was also increased by the addition of Co, while this treatment decreased the elongation. However, the volume fraction of ${\varepsilon}$ martensite, elongation and damping capacity were reduced by the addition of N, although the tensile strength increased. Tensile strength and damping capacity werealso increased by subzero treatment, while elongation decreased.

Fe-26Mn-2Al 합금의 진동 감쇠능에 미치는 결정립 크기의 영향 (The Effect of grain size on the damping capacity of Fe-26Mn-2Al alloy)

  • 강창룡;엄정호;김효종;성장현
    • 동력기계공학회지
    • /
    • 제11권1호
    • /
    • pp.115-120
    • /
    • 2007
  • The effect of grain size on the damping capacity of Fe-26Mn-2Al alloy studied in this paper has been investigated after changing the microstructure by cold rolling and changing grain size. Micro structures in Fe-26Mn-2Al at room temperature consist of a large quantity of austenite and a small quantity of ${\varepsilon}\;and\;{\alpha}'$ martensite. And ${\varepsilon}\;and\;{\alpha}'$ martensite was increased by increasing the degree of cold rolling. The content of deformation induced martensite was increased with increasing the degree of cold rolling. Damping capacity was linearly increased with increasing ${\varepsilon}$ martensite content, which suggests that stacking faults and ${\varepsilon}$ martensite variant boundaries are the principle damping sources. With increasing the grain size in Fe-26Mn-2Al alloy, the damping capacity was increased due to increasing the volume fraction of ${\varepsilon}$ martensite by decrement in stability of austenite phase. With decreasing the grain size, the content of deformation induced martensite was decreased and the damping capacity was decreased.

  • PDF