• 제목/요약/키워드: ${\beta}-type$ titanium

검색결과 15건 처리시간 0.028초

DV-Xα 분자 궤도법을 이용한 고강도 타이타늄 합금 설계 (A Study on the Design of High-Stength Titanium Alloys Using DV-Xα Molecular Orbital Method)

  • 백민숙;윤동주;원대희;김병일
    • 대한금속재료학회지
    • /
    • 제49권9호
    • /
    • pp.739-745
    • /
    • 2011
  • Beta-type alloys are the most versatile class of titanium alloys. They offer the highest strength to weight ratios and very attractive combinations of strength, toughness, and fatigue resistance inlarge cross sections [1]. The present study was made to obtain useful information for the design of ${\beta}$-type titanium alloys with high-strength properties by using the $DV-X{\alpha}$ method. Employing two calculated parameters, the bond order (Bo) and the d-orbital energy level (Md) of alloying elements in ${\beta}$-type titanium alloy was introduced and used for prediction of mechanical properties. Thus, high-strength titanium alloys were designed by calculating the Md and Bo values of the previous and present titanium alloys.

Ti-Nb계 합금의 상변화가 기계적 성질에 미치는 영향 (Effects of phase changes on mechanical properties of Ti-Nb alloys)

  • 박효병
    • 대한치과기공학회지
    • /
    • 제27권1호
    • /
    • pp.9-17
    • /
    • 2005
  • The use of titanium alloys as biomaterials is increasing due to their superior biocompatibility and enhanced corrosion resistance compared to conventional stainless steels and cobalt-based alloys. Ti-6Al-4V ($\alpha+\beta$type) alloy instead of pure titanium ($\alpha$type) is being widely used as biomaterials has some characteristics such as high fatigue strength, tensile strength and corrosion resistance. But it has been reported recently that the vanadium element expresses cytotoxicity and the aluminium element is related with dementia of Alzheimer type and neurotoxicity. In order to overcome their detrimental effects, $\beta$-phase stabilizer Nb was chosen in the present study. This paper was described the influence of phase changes of Ti-Nb alloys on mechanical properties. Ti-3wt.%Nb($\alpha$type),Ti-20wt.%Nb($\alpha+\beta$type) and Ti-40wt.%Nb($\beta$type) alloys were melted by vacuum arc furnace. The specimens were homogenized at 1050$^{\circ}C$ for 24hr and were then hot rolled to 50% reduction. Each alloys were solution heat treated at $\beta$ zone and $\alpha+\beta$ zone after homogenization and then were aged. The mechanical properties of Ti alloys were analysed by hardness test, tensile test, elongation test and SEM test. The results can be summarized as follows: 1) The higher hardness value of $\alpha+\beta$type alloy was obtained compared to the, $\alpha,\beta$type alloys. 2) The aged treated showed better hardness compared to the solution heat treated, homogenized. 3) In the case of solution and aging treatment at $\beta$region, the $\alpha+\beta$type alloy showed the most highest tensile strength and $\beta$type alloy showed the best elongation.

  • PDF

타이타늄 중공마더빌렛 주조재의 열처리공정 최적화 연구 (Study for Heat Treatment Optimization of Titanium Hollow Casted Billet)

  • 윤창석;박양균;이형욱;이동근
    • 열처리공학회지
    • /
    • 제32권2호
    • /
    • pp.68-73
    • /
    • 2019
  • ${\alpha}$-titanium alloy has a relatively low heat treatment characteristic and it is mainly subjected to heat treatment for residual stress, recovery or dynamic recrystallization. In this study, commercially pure titanium hollow castings was fabricated by gravity casting. Heat treatments were carried out at $750^{\circ}C$, $850^{\circ}C$ and $950^{\circ}C$ to investigate the effect of post-heat treatment on microstructure and mechanical properties. Beta-transus temperature ($T_{\beta}$) was about $913^{\circ}C$, and equiaxed microstructure was shown at temperature below $T_{\beta}$ and lath-type microstructure at temperature above $T_{\beta}$. Microstructure and mechanical properties did not show any significant difference in the direction of solidification for titanium hollow billet, so it can be seen that it was a well-made material for extrusion process. The optimum heat treatment condition of hollow billet castings for the seamless tube production was $850^{\circ}C$, 4 hr, FC, indicating a combination of equiaxed microstructure and appropriate mechanical properties.

Ti-Nb계 합금의 세포독성에 관한 연구 (A study on cytotoxicity of Ti-Nb alloys)

  • 박효병
    • 대한치과기공학회지
    • /
    • 제25권1호
    • /
    • pp.89-94
    • /
    • 2003
  • The use of titanium alloys as biomaterials is increasing due to their superior biocompatibility and enhanced corrosion resistance compared to conventional stainless steels and cobalt-based alloys. Ti-6Al-4V ($\alpha+\beta$type) alloy instead of pure titanium ($\alpha$type) is being widely used as biomaterials has some characteristics such as high fatigue strength, tensile strength and corrosion resistance. It also has similar characteristics to Ti in inducing bony ingrowth. But it has been reported recently that the vanadium element expresses cytotoxicity and carcinogenicity and the aluminium element is related with dementia of Alzheimer type and neurotoxicity. In order to overcome their detrimental effects, $\beta$-phase stabilizer Nb was chosen in the present study. CP-Ti(ASTM grade 2), Ti-3wt.%Nb($\alpha$type), Ti-20wt.%Nb ($\alpha+\beta$type) and Ti-40 wt.%Nb($\beta$type) alloys were melted by vacuum arc furnace. Biocompatibility of Ti-Nb alloys was evaluated by cytotoxicity test. The results can be summarized as follows: 1. For the cytotoxicity test, Ti-Nb alloys showed excellent biocompatibility compared to CP-Ti(ASTM grade 2), 316L STS and Co-Cr alloys.

  • PDF

양극산화 표면처리한 티타늄 임플랜트를 난소절제한 백서 경골에 매식 후 주위 골형성에 관한 연구 (THE BONE FORMATION AROUND ANODIC OXIDIZED TITANIUM IMPLANTS IN THE TINBIAE OF OVARECTOMIZED RATS)

  • 박성환;정석영;이재열;김규천;신상훈
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • 제34권3호
    • /
    • pp.306-318
    • /
    • 2008
  • Anodic spark deposition method(ASD) surface treated titanium implant possesses a considerable osteoconductive potential that promoting a high level of implant osseointegration in normal bone. The purpose of this study was to observe the ASD implant's osseointegration in the osteoporosis-induced animal model. Twenty four rats, 10 weeks of age, were ovarectomized and 5 weeks later divided into two groups : ASD implant group and control implant group. Titanium screw implants (diameter; 2.0 mm, length, 3.5 mm; pitch-height, 0.4 mm) were designed for this study. Experimental implants were ASD treated and no treatment on control implants. ASD implants and control implants were placed in to left tibiae of rats. The rats were sacrificed at different time interval(1, 2, 4 and 8 weeks after implantation) for histopathologic observation and immunohisto-chemistrical observation, with collagen type Ⅰ, fibronectin, integrin ${\alpha}_2{\beta}_1$ and integrin ${\alpha}_5{\beta}_1$ antibodies. The results obtained from this study were as follow: 1. Histopathologic findings, overall tissue response and the pattern of bone formation in both groups were similar. In ASD group, more newly formed bone was seen at 1 week and 2weeks than control group. 2. The levels of type Ⅰ collagen and fibronectin expression were the most abundant at 2weeks and decreased gradually in both groups. Fibronectin and type Ⅰ collagen expression in ASD group were stronger than control group but no significance. 3. The levels of integrin ${\alpha}_2{\beta}_1$ and Integrin ${\alpha}_5{\beta}_1$ expression were most abundant at 2 weeks and decreased gradually in both groups. No significant difference was observed in both groups. From this results, anodic oxidized titanium implants were more advantages in early stage of bone formation than control group, but have no significance in tissue responses and late bone formations. It could be stated that although anodic oxidized titanium implant possesses considerable osteoconductive potential but in osteoporotic bone condition dental implant procedure should performed after improving or treating the osteoporotic bone condition.

Nb 함량에 따른 Ti-Nb계 합금의 내식성에 대한 연구 (A study on corrosion resistance of Ti-Nb alloys by Nb contents)

  • 박근형
    • 대한치과기공학회지
    • /
    • 제28권1호
    • /
    • pp.61-66
    • /
    • 2006
  • Titanium alloys have been used for dental materials due to it's very good biocompatibility. Ti-6Al-4V alloy instead of pure titanium is being widely used as biomaterials has some characteristics such as high fatigue strength, tensile strength and corrosion resistance. But it has been reported recently that the vanadium element expresses cytotoxicity and carcinogenicity and the aluminium element is related with dementia of Alzheimer type and neurotoxicity. The Ti-Nb alloys has designed and examined corrosion resistance. Ti-3wt.%Nb($\alpha$type), Ti-20wt.%Nb(${\alpha}+{\beta}$type) and Ti-40wt.%Nb($\beta$type) alloys were melted by vacuum arc furnace. The corrosion resistance of Ti alloys was evaluated by potentiodynamic polarization test in the solution of 0.9% NaCl and 5% HCl. The results can be summarized as follows: 1) For the corrosion test in the solution of 0.9% NaCl and 5% HCl, the corrosion behaviour of Ti-Nb alloys was similar to ASTM grade 2 CP Ti. 2) The corrosion resistance of Ti-20Nb alloy was better than that of CP-Ti, Ti-3Nb, Ti-40Nb alloy in 0.9% NaCl and 5% HCl, solutions.

  • PDF

A TISSUE RESPONSE TO THE TITANIUM ALLOY (Ti-13Zr-6Nb) IN VIVO

  • Kim Chang-Su;Lee Seok-Hyung;Shin Sang-Wan;Suh Kyu-Won;Ryu Jae-Jun
    • 대한치과보철학회지
    • /
    • 제42권6호
    • /
    • pp.619-627
    • /
    • 2004
  • Statement of problem. Mechanisms of tissue-implant interaction and the effect of the implant surface on the behavior of cells has not yet been clarified. Purpose. This study was performed to investigate the tissue reaction to the titanium alloy submerged into rat peritoneum in vivo. Materials and methods. Titanium alloys (titanium-13Zirconium-6Niobium) were inserted inside the peritoneal cavity of Sprague Dawley rats. After 3 months, the tissue formed around the inserted titanium alloys were examined with a light-microscope. Tissue reaction around the material was analyzed by confocal microscopy to evaluate their biocompatibility in a living body. Results. In in vivo study, foreign body type multinucleated giant cells were found in the fibrous tissue formed as a reaction to the foreign material (4 in 20 cases), but the inflammatory reaction was very weak. After experiment, the contaminants of biomaterials was removed from living tissue. In confocal microscopy, we observed that the staining of vinculin and actin showed mixed appearance. In a few cases, we found that the staining of vinculin and beta-catenin showed the prominent appearance. Conclusion. We found that titanium-13Zirconium-6Niobium alloy was an excellent biomaterial.

TiAl-Nb 합금의 고온상변태와 일방향응고에 관한 연구 (Study on High Temperature Phase Transformation and Directional Solidification of TiAl-Nb Alloy)

  • 박종문;장호승;김성웅;김승언;손지하;오명훈
    • 열처리공학회지
    • /
    • 제29권5호
    • /
    • pp.227-233
    • /
    • 2016
  • Phase transformation phenomenon at high temperature was investigated by using designed TiAl-Nb alloys with addition of the ${\beta}$ stabilizer. Examination of dendritic morphologies in arc-melted button ingot could reveal the crystallography of the primary solidification phase. It was found that the addition of ${\beta}$ stabilizer(Nb) shifted the high temperature region of the binary Ti-Al phase diagram to the high Al composition side so that ${\beta}$ phase forms as a primary crystal even at higher Al composition compared with the binary Ti-Al system. The ${\beta}$ was found to be the primary solidification phase for alloys with Al content less than about 52 at.%. The composition of ${\beta}$ solidification in Ti-Al-Nb ternary system could be determined from the partial liquidus projection which was constructed by observing the microstructure of arc-melted buttons. The Ti-46Al-(6, 8)Nb composition was selected for ${\beta}$ solidification and the directional solidification was performed by a floating zone-type DS apparatus at the growth rate 30 mm/hr respectively.

Ti 합금의 피로 특성 고찰 (Study for Fatigue Crack Propagation Behavior of Ti-alloy)

  • 정화일;조규종
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 추계학술대회 논문집
    • /
    • pp.786-789
    • /
    • 1997
  • Ti-6Al-4V has been used widely in biomedical field. But because of its toxicity, the ${\beta}$ stabilizing element, V, in Ti-6Al-4V has been replaced by Nb, Ta. Ti-10Ta-10Nb has been developed for biomedical applications. The fatigue crack propagation behavior of Ti-alloy(Ti-10Ta-10Nb) was investigated, in comparison with that of pure Ti. In order to better understand the fundamental fatigue behavior of Ti-10Ta-10Nb, rotating bending fatigue tests have been carried out. Ti-10Ta-10Nb has a better fatigue strength than pure Ti. In this paper, fatigue life has been predicted with Nisitani's equation of the fatigue crack propagation that can be established by measuring fatigue crack growth rates.

  • PDF

백서 태자 두개관세포에서 Ti-8Ta-3Nb 합금의 생체적합성 (Biocompatibility of Ti-8Ta-3Nb alloy with fetal rat calvarial cells)

  • 조인구;최득철;김영준;이경구;이도재
    • Journal of Periodontal and Implant Science
    • /
    • 제36권4호
    • /
    • pp.849-861
    • /
    • 2006
  • 타이타늄은 기계적 특성이 우수하고 생체적합성이 뛰어나 의료용 장비의 주 재료로 사용되고 있으며 타이타늄 보다 기계적 특성이 더 우수한 타이타늄 합금들(주로 Ti-6Al-4V와 Ti-6Al-7Nb 합금)도 개발되어 치과와 의료용 임플란트로 사용되고 있다. 그러나 타이타늄 합금 성분들 중 알루미늄 (aluminum)과 바나디움(vanadium)은 인체에 노출되면 세포손상과 신경계에 문제를 일으킬 수 있다. 따라서 인체에 독성이 없으면서 기계적 성질과 생체적합성이 우수한 타이타늄 합금의 개발이 필요하다. 최근 인체에 독성이 없는 성분들이 함유된 새로운 ${\beta}$ - 형태의 타이타늄 합금들이 개발되고 있는데, ${\beta}$ - 타이타늄 합금은 그 기계적 성질이 기존의 ${\alpha}+{\beta}$ 타이타늄 합금에 비해 우수하다고 알려져 있다. 최근 새로운 ${\beta}$ - 타이타늄 합금이 전남대학교 부설 타이타늄 연구소에서 개발되었다. 이 연구는 새로 개발된 ${\beta}$ - 타이타늄 합금의 생채 적합성을 세포 증식도, 알카리 인산 분해 효소 활성과 유전자 증폭을 통해 알아보고자 하였다. 그 결과는 다음과 같다; 1. Titanium-6aluminum-4vanadium (Ti-6Al-4V) 합금 표면애서의 세포 증식율은 Titanium-Titanium8Tantalum-3Niobium (Ti-8Ta-3Nb) 합금과 순수 타이타늄 표면에 비해 유의하게 낮았다(p<0.00l). Ti-8Ta-3Nb 합금 표면에서의 증식도는 순수 타이타늄 표면과 유사하였다. 2. Ti-8Ta-3Nb 합금과 순수 타이타늄에서 배양된 세포이 알카리 인산 분해 효소의 활성도는 Ti-6Al-4V 합금에서의 것보다 유의하게 높았다 (p<0.001). 3. 유전자 증폭 분석 결과, Ti-8Ta-3Nb 합금과 순수 타이타늄에서 collagen type I과 bone sialoprotein mRNA 가 유사한 수준으로 발현되었다. 이상의 결과는 생체 적합성 측면에서 Ti-8Ta-3Nb 합금과 순수 타이타늄의 차이가 없음을 보여주며 따라서 Ti-8Ta-3Nb 합금이 의학 및 치의학 영역에서 새로운 임프란트 재료로 사용될 수 있음을 의미한다.