• Title/Summary/Keyword: ${\alpha}$-FeMn

Search Result 110, Processing Time 0.024 seconds

$M\"{o}ssbauer$ studies of $NdFe_{10.7}TiM{0.3}(M\;=\;B,\;Ti)$ ($NdFe_{10.7}TiM{0.3}(M\;=\;B,\;Ti)$$M\"{o}ssbauer$ 연구)

  • 김철성;이용종;김윤배;김창석
    • Journal of the Korean Magnetics Society
    • /
    • v.5 no.1
    • /
    • pp.64-70
    • /
    • 1995
  • The authors have studied crystallographic and magrletic properties of $NdFe_{10.7}TiM_{0.3}(M=B,\;Ti)$ by X-ray diffraction, VSM magnetometer, and Mossbauer spectrometer. The Alloys were prepared by arc-melting under argon atmosphere. The $NdFe_{10.7}TiM_{0.3}$ has pure single phase, whereas the $NdFe_{10.7}Ti_{1.3}$ contains some $\alpha-Fe$, from powder X-ray diffractometry. The $NdFe_{10.7}TiM_{0.3}$ has the $ThMn_{12}$-type tetragonal structure with $a_{0}=8.587\;{\AA}\;and\;c_{0}=4.788\;{\AA}$. The Curie temperature ($T_c$) is $570{\pm}3\;K$ from $M\"{o}ssbauer$ spectroscopy performed at various temperatures ranging from 13 to 770 K. Each spectrum of below $T_c$ was fitted with five subspectra of Fe sites in the structure ($8i_{1},\;8i_{2},\;8j_{1},\;8j_{2}\;and\;8f$). The area fraction of the subspectra at room temperature are 16.4, 8.2, 14.8, 21.3 and 39.3 %, respectively. Magenetic hyperfine fields for the Fe sites decrease in the order, $H_{hf}(8i)>H_{hf}(8j)>H_{hf}(8f)$.

  • PDF

A Study on the Formation Mechanism of Microconstituents in Brazed Joint of Duplex Stainless Steel and Cr-Cu Alloy (2상 스테인리스강과 크롬동합금의 브레이징부 생성상의 생성기구에 관한 연구)

  • 김대업
    • Journal of Welding and Joining
    • /
    • v.19 no.5
    • /
    • pp.534-539
    • /
    • 2001
  • The formation mechanism of microconstituents in brazed joints of duplex stainless steel and Cr-Cu alloy which is an essential process of rocket engine manufacturing was investigated using Cu base insert metal. $SUS329J_3L$ and C18200 were used for base metal and AMS 4764 was used for insert metal. The brazing was carried out under various conditions. There were various phases in the joints, because of reaction between liquid insert metal and base metals. Since liquid insert metal reacts with duplex stainless steel, liquid Cu from insert metal infiltrated into the $\alpha/\beta$ interface of duplex stainless steel. Through the process of Cu infiltration, isolated stainless steel pieces come into the liquid insert metal. Since liquid insert metal reacts with Cr-Cu alloy. Cr precipitates from C18200 come into the liquid insert metal. With increment of bonding temperature and holding time, amounts and sizes of phases increased. but Cr-Mn compounds decreased at 1303k for 1.2ks and Mn-rich phases disappeared Fe-Cr compounds formed.

  • PDF

Wear Resistance Characteristics of Iron Weld Overlays by Composite Chromium Powders (복합 크롬 분말에 의한 철계 용접 오버레이의 내마모 특성)

  • 김종철;박경채;최창옥
    • Journal of Welding and Joining
    • /
    • v.19 no.5
    • /
    • pp.506-511
    • /
    • 2001
  • Weld overlay has been developed to improve the property of material surface which is used in the severe environment. Weld overlay is the process which uses an arc heat and welds different composition of alloy on the substrate for the improvements of heat resistance and wear resistance. Weld overlay has a lot of advantages which are high hardness, good processing efficiency, easy controlling of layer thickness, good quality and low cost. In this study, weld overlay was performed by MAG welding on the base metal(SS400) with filler metal which contain composite powders(Cr+C+Mn+Mo+NbC) and solid wire(JIS-YGW11). Characterization of hardness and wear resistance were analyzed by EDS, EPMA, XRD and observations of microstructure were performed to investigate characteristics of overlays. The experimental results of overlaid specimens manufactured with Cr+C+Mn+Mo+NbC powders were obtained as fellows. ${\alpha}-phase$, M(Fe, Cr)3C and NbC of overlays were increased with decreasing the wire feed rates and increasing powder feed rates. Also the hardness of overlays were increased and the specific wear were decreased.

  • PDF

Effect of Alloying Element Addition on the Microstructure and Wear Properties of Die-casting ADC12 Alloy (ADC12 다이캐스팅 합금의 미세조직 및 기계적 특성에 미치는 개량 원소 첨가의 영향)

  • Kang, Y.J.;Yoon, S.I.;Kim, D.H.;Lee, K.A.
    • Transactions of Materials Processing
    • /
    • v.28 no.1
    • /
    • pp.34-42
    • /
    • 2019
  • In this study, various alloying elements (Cr, Sr, Ca, Cd) were added to improve the mechanical properties of ADC12 fabricated by a die casting process. The effect of alloying elements on the microstructure and mechanical properties were investigated. The phase analysis results of the modified ADC12 alloy with conventional ADC12 alloy, showed the similar characteristics of Al matrix, Si phase, $CuAl_2$ phase and the Fe intermetallic phase. As a result of the microstructure observation, the secondary dendrite arm spacing (SDAS) was shown to have decreased after the addition of the alloying elements. The eutectic Si phase, which existed as flake form in the conventional ADC12 alloy, was modified finely as a fiber form in the modified ADC12 alloy. It was observed that the $CuAl_2$ phase as the strengthening phase was relatively finely distributed in the modified ADC12 alloy. The Fe intermetallic appeared as a Chinese script shaped $Al_6$ (Mn,Fe) which is detrimental to mechanical properties in conventional ADC12 alloy. On the other hand, in the modified ADC12 alloy, polyhedral ${\alpha}-Al_{15}Si_2$ $(Fe,Mn,Cr)_3$ was observed. The tensile properties were improved in the modified ADC12 alloy. The yield strength and tensile strength increased by 12.4% and 10.0%, respectively, in the modified ADC12 alloy, and the elongation was also seen to have been increased. As a result of the pin on disk wear test, the wear resistance properties were also improved by up to about 7% in the modified ADC12 alloy. It is noted that the wear deformation microstructures were also observed, and it was found that the fine eutectic Si and strengthening phases greatly improved abrasion resistance.

Preparations and characteristics of the ceramic balls for heavy metals absorption and antibacterial activities in the drinking water (음용수중의 중금속흡착과 항균성용 세라믹 볼의 제조 및 특성평가)

  • Park, Chun-Won;Park, Ra-Young;Park, Sun-Min
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.15 no.6
    • /
    • pp.263-268
    • /
    • 2005
  • The ceramic balls impregnated with $20{\sim}40nm$ sized Ag colloid were examined for heavy metals absorption and antibacterial activities in the drinking water. The preparation conditions of ceramic ball that the porosity was excellent were as follows: starting material: 85 wt% $Ca_{10}(PO_4)_6(OH)_2$, binder: 5 wt% PVA and 15 wt% ${\alpha}-Ca_3(PO_4)_2$, heating temperature: $1000^{\circ}C$, duration: 3 hrs. The ceramic balls obtained under these conditions showed specific surface area of $110m^2/g$, pore size of $120{\mu}m$ and porosity of 80%. Also, as the results of a performance test on a rate of adsorbing and removing heavy metals in the drinking water by using the.AAS, heavy metals such as Zn, Mn, Fe and Cu were removed to the extent that their content became 0.03mg/l or lower after 1 day and they showed an excellent bactericidal activity that all coliforms were killed after 3 hrs.

Effect of Thermo-Mechanical Treatment on the Damping Capacity of Alloy with Deformation Induced Martensite Transformation (가공유기 마르텐사이트 변태를 갖는 합금의 감쇠능에 미치는 가공열처리의 영향)

  • Han, Hyun-Sung;Kang, Chang-Yong
    • Korean Journal of Materials Research
    • /
    • v.29 no.3
    • /
    • pp.160-166
    • /
    • 2019
  • This study investigates the effect of thermo-mechanical treatment on the damping capacity of the Fe-20Mn-12Cr-3Ni-3Si alloy with deformation induced martensite transformation. Dislocation, ${\alpha}^{\prime}$ and ${\varepsilon}-martensite$ are formed, and the grain size is refined by deformation and thermo-mechanical treatment. With an increasing number cycles in the thermo-mechanical treatment, the volume fraction of ${\varepsilon}-martensite$ increases and then decreases, whereas dislocation and ${\alpha}^{\prime}-martensite$ increases, and the grain size is refined. In thermo-mechanical treated specimens with five cycles, more than 10 % of the volume fraction of ${\varepsilon}-martensite$ and less than 3 % of the volume fraction of ${\alpha}^{\prime}-martensite$ are attained. Damping capacity decreases by thermo-mechanical treatment and with an increasing number of cycles of thermo-mechanical treatment, and this result shows an opposite tendency for general metal with deformation induced martensite transformation. The damping capacity of the thermo-mechanical treated damping alloy with deformation induced martensite transformation greatly affect the formation of dislocation, grain refining and ${\alpha}^{\prime}-martensite$ and then ${\varepsilon}-martensite$ formation by thermo-mechanical treatment.

Effect of Sc, Sr Elements on Eutectic Mg2Si Modification and Castability of Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe Casting Alloy (주조용 Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe 합금의 공정 Mg2Si 개량과 주조특성에 미치는 Sc, Sr 첨가원소의 영향)

  • Kim, Heon-Joo
    • Journal of Korea Foundry Society
    • /
    • v.35 no.6
    • /
    • pp.147-154
    • /
    • 2015
  • The effects of Sc and Sr elements on the modification of the eutectic $Mg_2Si$ phase and the castability were investigated in the Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe alloy. Measurements of the cooling curve and microstructure observations were performed to analyze the additional effects of Sc and Sr minor elements during the solidification process. A prominent effect found on the modification of the eutectic $Mg_2Si$ phase with additions of the Sr and Sc elements. Here, a fine eutectic $Mg_2Si$ phase and a decrease in the growth temperature of the eutectic $Mg_2Si$ phase were evident with an addition of Sc element up to 0.2 wt%. The growth temperature of the eutectic $Mg_2Si$ phase decreased and the effect on the modification of the eutectic $Mg_2Si$ phase increased with the addition of Sr element up to 0.02 wt%. The addition of 0.02wt%Sr had the strongest effect on the modification of the eutectic $Mg_2Si$ phase, and the resulting microstructure of the eutectic $Mg_2Si$ phase was found to have a fibrous morphology with a decreased aspect ratio and an increased modification ratio. Fluidity and shrinkage tests were conducted to evaluate the castability of the alloy. The addition of 0.02wt%Sr effectively increased the fluidity of the alloy, while an addition of Sc did not show any effect compared to when nothing was added. The maximum filling length was recorded for 0.01wt%TiB-0.02wt%Sr owing to the effect of the fine ${\alpha}$-Al grains. The macro-shrinkage ratio decreased, while the micro-shrinkage ratio increased with the addition of various eutectic modifiers. The highest ratio of micro-shrinkage was recorded for the 0.02wt%Sr condition. However, the total shrinkage ratio was nearly identical regardless of the amounts added in this study.

The Changes of Biologically Functional Compounds and Antioxidant Activities in Ecklonia cava with Blanching Times (데침조건에 따른 감태의 생리활성 성분 및 항산화 활성의 변화)

  • Kim, Jin-Ah;Lee, Jong-Mee
    • Journal of the Korean Society of Food Culture
    • /
    • v.19 no.4
    • /
    • pp.369-377
    • /
    • 2004
  • This study was performed to investigate the change of biologically functional compounds and antioxidant activities in Ecklonia cava with blanching times. As biologically functional compounds, the contents of minerals(K, Ca, Na, Mg, Fe, Cu, Mn and Zn), vitamins($vitamin\;C,\;{\beta}-carotene\;and\;{\alpha}-tocopherol$) and total polyphenol were analyzed. And antioxidant activity was determined through free radicals(DPPH radical, superoxide anion radical, hydroxyl radical and hydrogen peroxide) scavenging activity and linoleic acid peroxidation inhibitory activity. As the blanching time increased, the contents of minerals, vitamin C, ${\beta}-carotene$ and total polyphenol were decreased however ${\alpha}-tocopherol$ was not affected by blanching time, and antioxidant activities were decreased with blanching time.

The Effect of Oxygen and Chlorine Dioxide during Pulp Bleaching - The Effect of Hydroxyl Radical and Metal Ion - (펄프 표백시 산소와 이산화염소의 영향 - 수산기 라디칼의 생성과 금속이온의 영향-)

  • Yoon, Byung-Ho;Jo, Byoung-Muk;Lee, Myoung-Ku
    • Journal of Forest and Environmental Science
    • /
    • v.13 no.1
    • /
    • pp.153-165
    • /
    • 1997
  • Hydroxyl radicals were detected and their qualitative yields were estimated by using chemiluminescence method and $\gamma$-irradiation technique in oxygen or chlorine dioxide radicals bleaching conditions. The correlation of hydroxyl radical formation and lignin model(Apocynol) or carbohydrate model($\alpha$-D-glucopyranose and methyl-$\beta$-D-glucopyranoside) degradation was studied in the presence of metal ion or without metal ion. The results showed that the presence of metal ions efficiently affected the formation of hydroxyl radicals in oxygen bleaching process, in the order of $Cu^{2+}$ > $Mn^{2+}$ > $Mg^{2+}$ > $Fe^{2+}$, and these metal gave also rise to the degradation of carbohydrate. But it was found that the addition of $100{\mu}m\;Mg^{2+}$ gave an efficient protection against carbohydrate degradation and suppressed the hydroxyl radical formation under oxygen bleaching conditions. And the presence of $Cu^{2+}$ had a detrimental effect on the stability of carbohydrates, whereas the addition of $3{\mu}m\;Mn^{2+}$ surprisingly had a small protective effect on methyl--$\beta$-D-glucopyranoside. In the $ClO_2$ radical bleaching conditions the hydroxyl radical expected to generate from water or substrates was not detected in the presence of metals.

  • PDF

Effect of Dimension Control of Piezoelectric Layer on the Performance of Magnetoelectric Laminate Composite

  • Cho, Kyung-Hoon
    • Korean Journal of Materials Research
    • /
    • v.28 no.11
    • /
    • pp.611-614
    • /
    • 2018
  • Laminate composites composed of $0.95Pb(Zr_{0.52}Ti_{0.48})O_3-0.05Pb(Mn_{1/3}Sb_{2/3})O_3$ piezoelectric ceramic and Fe-Si-B based magnetostrictive amorphous alloy are fabricated, and the effect of control of the areal dimensions and the thickness of the piezoelectric layer on the magnetoelectric(ME) properties of the laminate composites is studied. As the aspect ratio of the piezoelectric layer and the magnetostrictive layer increases, the maximum value of the ME voltage coefficient(${\alpha}_{ME}$) increases and the intensity of the DC magnetic field at which the maximum ${\alpha}_{ME}$ value appears decreases. Moreover, as the thickness of the piezoelectric layer decreases, ${\alpha}_{ME}$ tends to increase. The ME composites exhibit ${\alpha}_{ME}$ values higher than $1Vcm^{-1}Oe^{-1}$ even at the non-resonance frequency of 1 kHz. This study shows that, apart from the inherent characteristics of the piezoelectric composition, small thicknesses and high aspect ratios of the piezoelectric layer are important dimensional determinants for achieving high ME performance of the piezoelectric-magnetostrictive laminate composite.