• 제목/요약/키워드: $\gamma2$ phase

검색결과 485건 처리시간 0.026초

고크롬 (α+γ) 2상강의 결정립 성장기구 (A study on the grain growth mechanism in dual-phase high Cr-steel)

  • 위명용
    • 열처리공학회지
    • /
    • 제11권4호
    • /
    • pp.324-332
    • /
    • 1998
  • The grain growth characteristics of dual-phase (${\alpha}+{\gamma}$) containing high Cr-steel have investigate using ${\alpha}$-, ${\gamma}$-single phases and (${\alpha}+{\gamma}$)dual-phase of 12%Cr Steel. The heat treatment has performed at $1000-1200^{\circ}C$ for 1-100hr. The results are as follows : 1) The grain growth rate in (${\alpha}+{\gamma}$) dual phase was substantially slower than that of single grain. 2) The relation between mean grain radius $\bar{{\gamma}}$ and annealing time t is, in general, described as following equation : $$(\bar{{\gamma}})^n-(\bar{{\gamma}_o})^n=K_n{\cdot}t{\cdots}{\cdots}(1)$$ i) In the case of single phase of high Cr steel, Eq.(1) is described as $(\bar{{\gamma}})^2-(\bar{{\gamma}_o})^2=K_2{\cdot}t$ and the grain growth is controlled by boundary migration. ii) In dual phase, the grain growth needs diffusion of alloying elements because the chemical composition of ${\alpha}$- and ${\gamma}$- phases differs from each other. When the volume fraction of ${\alpha}$-, ${\gamma}$-phase was almost equal and ${\gamma}$-phase in the case of 80 and $90%{\gamma}$. Eq.(1) is described as $(\bar{{\gamma}})^3-(\bar{{\gamma}_o})^3=K_3{\cdot}t$ because the grain growth is controlled by volume diffusion iii) In the case of ${\gamma}$-rich phase (80 and $90%{\gamma}$), the grain growth of minor phase (10 and $20%{\alpha}$) is described as $(\bar{{\gamma}})^4-(\bar{{\gamma}_o})^4=K_4{\cdot}t$ because the boundary diffusion is predominent rather than volume diffusion.

  • PDF

$L1_2$${\gamma}^{\prime}-Ni_3(Al,Ti)$ 규칙상 중에 불규칙 ${\gamma}$상의 석출거동에 관한 연구 (A Study on the Precipitation Behavior of Disordered ${\gamma}$ Phase in an $L1_2$ Ordered ${\gamma}^{\prime}-Ni_3(Al,Ti)$ Phase)

  • 한창석
    • 열처리공학회지
    • /
    • 제19권5호
    • /
    • pp.249-256
    • /
    • 2006
  • Structural studies have been performed on precipitation hardening found in $L1_2$ ordered ${\gamma}^{\prime}-Ni_3(Al,Ti)$ alloys using transmission electron microscopy. A uniform solid solution of ${\gamma}^{\prime}-L1_2$ ordered phase supersaturated with Ni can be obtained by solution annealing in a suitable temperature range. The ${\gamma}^{\prime}$ phase hardens appreciably by the fine precipitation of disordered ${\gamma}$. The shape of ${\gamma}$ precipitates formed during aging is initially spherical or round-cubic and grow into platelets as aging proceeds. High resolution electron microscopy revealed that the ${\gamma}$ precipitates are perfectly coherent with the matrix ${\gamma}^{\prime}$ as long as the ${\gamma}$-precipitates are plates. The loss of coherency initiates by the introduction of dislocations at the ${\gamma}/{\gamma}^{\prime}$ interface followed by the step formation at the dislocations. The ${\gamma}$ precipitates become globular after the loss of coherency. The strength of ${\gamma}^{\prime}-Ni_3(Al,Ti)$ increases over the temperature range of experiment by the precipitation of fine ${\gamma}$ particles. The peak temperature where a maximum strength was obtained shifted to higher temperature.

$\gamma$-TiAl 합금의 고온변형 및 Cavity 형성 연구 (A Study on the High Temperature Deformation and the Cavity Initiation of Gamma TiAl Alloy)

  • 김정한;하태권;장영원;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.172-175
    • /
    • 2001
  • The high temperature deformation behavior of two-phase gamma TiAl alloy has been investigated with the variation of temperature and ${\gamma}/{\alpha}_2$ volume fraction. For this purpose, a series of load relaxation tests and tensile tests have been conducted at temperature ranging from 800 to $1050^{\circ}C$. In the early stage of the deformation as in the load relaxation test experimental flow curves of the fine-grained TiAl alloy are well fitted with the combined curves of two processes (grain matrix deformation and dislocation climb) in the inelastic deformation theory. The evidence of grain boundary sliding has not been observed at this stage. However, when the amount of deformation is large (${\epsilon}{\approx}$ 0.8), flow curves significantly changes its shape indicating that grain boundary sliding also operates at this stage, which has been attributed to the occurrence of dynamic recrystallization during the deformation. With the increase in the volume fraction of ${\alpha}_2$-phase, the flow stress for grain matrix deformation increases since ${\alpha}_2$-Phase is considered as hard phase acting as barrier for dislocation movement. It is considered that cavity initiation is more probable to occur at ${\alpha}_2/{\gamma}$ interface rather than at ${\gamma}/{\gamma}$ interface.

  • PDF

6Bi2O3.GeO2 조성 융액의 결정화 (Crystallization from The Melt of 6Bi2O3.GeO2 Composition)

  • 김호건;김명섭
    • 한국세라믹학회지
    • /
    • 제26권4호
    • /
    • pp.479-486
    • /
    • 1989
  • According to the phase diagram, 6Bi2O3.GeO2 composition melts congruently at 93$0^{\circ}C$ and forms a stable ${\gamma}$-6Bi2O3.GeO2 crystal phase below the melting point. But when the melt of this composition was cooled at a rate 1-15$0^{\circ}C$/min without tapping by a glass rod or impurity addition, a metastable $\delta$-6Bi2O3.GeO2 crystal phase was formed. It is due to that as the nucleation energy barrier of $\delta$-6Bi2O3.GeO2 crystals, which have more open and defective structure, is lower than that of ${\gamma}$-6Bi2O3.GeO2 crystals. When impurities or ${\gamma}$-6Bi2O3.GeO2 crystals existed in the melt, stable ${\gamma}$-6Bi2O3.GeO2 crystal phase was formed at various cooling rate. It is because of that the impurities or the ${\gamma}$-6Bi2O3.GeO2 crystals role as a seed crystal and as a result the nucleation energy barrier of ${\gamma}$-6Bi2O3.GeO2 crystals is lowered.

  • PDF

긍정, 부정 감정 유발 시각자극에 의한 감마-대역 신경동기화 증가 (Increased Gamma-band Neural Synchrony by Pleasant and Unpleasant Visual Stimuli)

  • 여동훈;최정우;김경환
    • 대한의용생체공학회:의공학회지
    • /
    • 제39권2호
    • /
    • pp.94-102
    • /
    • 2018
  • It is known that gamma-band activity (GBA) and phase synchrony (GBPS) are induced by emotional visual stimuli. However, the characteristics of GBA and GBPS according to different emotional states have not been identified. The purpose of this study is to investigate the changes in gamma-band neuronal synchronization induced by positive and negative emotional visual stimuli using electroencephalograms (EEGs). Thirteen healthy male subjects have participated in the experiment. The induced spectral power in gamma-band was the highest for negative stimuli, and the lowest for neutral stimuli in 300-2,000 ms after the stimulus onset. The inter-regional phase synchronization in gamma-band was increased in 500-2,000 ms, mainly between the bilateral frontal regions and the parieto-occipital regions. Larger number of significant connections were found by negative stimuli compared to positive ones. Judging from temporal and spatial characteristics of the gamma-band activity and phase synchrony increases, the results may imply that affective visual stimuli cause stronger memory encoding than non-emotional stimuli, and this effect is more significant for negative emotional stimuli than positive ones.

Control of Crystal Phase and Agglomeration of Iron Oxide Nanoparticles in Gas Phase Synthesis

  • Lee, Chang-Woo;Lee, Jai-Sung
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.424-425
    • /
    • 2006
  • The effects of reaction temperature and precursor concentration on the microstructure and magnetic properties of ${\gamma}-Fe_2O_3$ nanoparticles synthesized as final products of iron acetylacetonate in chemical vapor condensation (CVC) were investigated. Pure ${\gamma}-Fe_2O_3$ phase was obtained at temperature above $900^{\circ}C$ and crystallite size of ${\gamma}-Fe_2O_3$ nanoparticles decreased with lowering precursor concentration. Also, the coercivity decreases with decreasing crystallite size of nanopowder. The lowest coercivity was 7.8 Oe, which was obtained from the ${\gamma}-Fe_2O_3$ nanopowder sample synthesized at precursor concentration of 0.3M. Then, the crystallite size of ${\gamma}-Fe_2O_3$ nanoparticles was 8.8 nm.

  • PDF

화학센서용 다공성 ${\gamma}-Fe_2O_3$ 박막 제조 (Fabrication of ${\gamma}-Fe_2O_3$ Thin Film for Chemical Sensor Application)

  • 김범진;임일성;장건익
    • 센서학회지
    • /
    • 제8권2호
    • /
    • pp.171-176
    • /
    • 1999
  • PECVD법을 이용하여 $Al_2O_3$ 기판위에 증착된 $Fe_3O_4$박막의 상전이를 통하여 ${\gamma}-Fe_2O_3$ 박막을 제조하였다. ${\gamma}-Fe_2O_3$ 박막의 상전이는 주로 증착온도와 $Fe_3O_4$의 산화과정에 의해 유도되었다. $Fe_3O_4$ 상은 $200{\sim}300^{\circ}C$의 증착온도에서 in-situ로 얻을 수 있었다. 증착온도에 따른 상변화는 없었으며 $250^{\circ}C$에서 증착된 $Fe_3O_4$상이 가장 안정된 상을 나타내었다. ${\gamma}-Fe_3O_3$ 상은 $280{\sim}300^{\circ}C$의 온도범위에서 $Fe_3O_3$ 상을 산화시켜 유도하였다. $Fe_3O_4$ 상과 ${\gamma}-Fe_2O_3$ 상은 같은 spinel구조를 가지고 있으며 공존상으로서 존재함을 알 수 있었다. 또한, $Al_2O_3$에 산화된 ${\gamma}-Fe_2O_3$ 박막은 다공성의 미세구조를 나타내었다.

  • PDF

미세석출상을 포함하는 $L1_2$형 규칙 $Ni_3Al$의 변형조직에 관한 연구 (A Study on the Deformation Induced Microstructure $L1_2$-ordered $Ni_3Al$ Containing Fine Precipitates)

  • 한창석;이준
    • 열처리공학회지
    • /
    • 제21권5호
    • /
    • pp.251-258
    • /
    • 2008
  • A transmission electron microscope investigation has been performed on the morphology of dislocations in deformed ${\gamma}^{\prime}-Ni_3(Al,Ti)$ alloys containing fine dispersion of disordered ${\gamma}$ particles. Superlattice dislocations dissociate into fourfold Shockley partial dislocations in a uniform supersaturated solid solution of the ${\gamma}^{\prime}$ phase. Dislocations are attracted into the disordered ${\gamma}$ phase and dissociate further in the particles. At any stage of aging, dislocations cut through the particles and the Orowan bypassing process does not occur even in the over-aged stage of this alloy system. The work necessary to pull the dislocation away from the disordered particles into the ordered matrix should mainly contribute to increase the strength of the ${\gamma}^{\prime}$ phase containing fine dispersion of the disordered ${\gamma}$ phase.

일방향 응고된 Cu-Al-Ni 합금의 변태특성에 미치는 열처리 영향 (Influence of Heat Treatment on Transformation Characteristics in an Unidirectionally Solidified Cu-Al-Ni Alloy)

  • 박윤규;장우양
    • 열처리공학회지
    • /
    • 제16권2호
    • /
    • pp.90-96
    • /
    • 2003
  • The effect of betatizing temperature on microstructure and transformation characteristics in a Cu-AI-Ni based pseudoelastic alloy fabricated by heated mold continuous casting by using metallography, XRD and calorimetry. The microstructure of cast rod betatized at $600^{\circ}C$ revealed a ${\beta}_1$ parent phase and a ${\gamma}_2$ phase precipitated along the casting direction. When the cast rod was betatized at the elevated temperature above $600^{\circ}C$, the ${\gamma}_2$ phase is completely dissolved into the matrix so that the volume fraction of the ${\gamma}_2$ phase was decreased. The parent phase was stabilized by betatizing at $600^{\circ}C$. However, the ${\beta}_1$ parent phase was transformed to both ${{\beta}_1}^{\prime}$ and ${{\gamma}_1}^{\prime}$ martensites with increasing betatizing temperatures above $600^{\circ}C$, while $M_s$ and $A_s$ temperatures were decreased. The stress-strain curves for compression test were not same with betatizing temperature; the stress-strain curves of the specimen betatized at $600^{\circ}C$ and $700^{\circ}C$ were linear but those of the specimen betatized at $800^{\circ}C$ and $900^{\circ}C$ were not linear.

고 망간강 2상 혼합조직의 열적 안정성에 관한 연구 (A Study on the Thermal Stability of Duplex High Mn-Steel Structure)

  • 위명용
    • 열처리공학회지
    • /
    • 제5권1호
    • /
    • pp.13-22
    • /
    • 1992
  • The thermal stability of duplex high Mn-steel structure have been investigated using 15%Mn~1.0~2.4%C steels which are composed of ${\gamma}$-and ${\theta}$-phases in the range of temperature from 900 to $1100^{\circ}C$, and time from 50 to 300h. The results are as follows ; 1) The grain growth in single-phase region proceeds by grain boundary migration and the relation between mean radius $\bar{r}$ and annealing time t is described as follows ; $\bar{r}^2-{\bar{r}_0}^2=k_0{\cdot}t$ 2) The grain growth of duplex, (${\gamma}+{\theta}$), strucrure is slower than that single phase because the chemical composition of ${\gamma}$-and ${\theta}$-phases differs esch others. 3) The grain of (${\gamma}+{\theta}$) duplex structure grow slowly in a mode of Ostwald ripening. Because grain boundaries of ${\gamma}$-phase migrate under a restriction of pinning by ${\theta}$-phases. 4) In the duplex structures. the dispersed structures change to the dual-structures, as the volume fraction of the dispersed second-phase increase. Consequently, the growth-law, which is controlled by boundary-diffusion change to that of the volume diffusion-mechanism.

  • PDF