• Title/Summary/Keyword: $\alpha$-$Fe_{2}O_{3}$

Search Result 331, Processing Time 0.029 seconds

The Influence of $O_2$ Partial Pressure on Soft Magnetic Properties of As-deposited Fe-Sm-O Thin Films (산소분압에 따른 Fe-Sm-O계 박막의 연자기적 성질)

  • Yoon, T.S.;Cho, W.S.;Koo, E.S.;Li, Ying;Park, J.B.;Kim, C.O.
    • Korean Journal of Materials Research
    • /
    • v.10 no.11
    • /
    • pp.755-759
    • /
    • 2000
  • The influence of $O_2$partial presure on saturation magnetization, coercivity and effective permeability(0.5~100MHz) of as-deposited Fe-Sm-O thin films, which were fabricated by RF magnetron reactive sputtering method, were investigated. The nanocrystalline Fe(sub)83.4Sm(sub)3.4O(sub)13.2 thin film fabricated at $O_2$partial pressure of 5% exhibits the best magnetic softness with saturation magnetization of 18kG, coercivity of 0.82 Oe and effective permeability about 2,600 at 0.5~100MHz. $\alpha$-Fe grain size is decreased with increasing $O_2$partial pressure. In case of $O_2$partial pressure of 10%, it is observed that FeO compound is formed and soft magnetic properties are decreased. The electrical resistivity of Fe-Sm-O thin films were increased with increasing $O_2$partial pressure, the electrical resistivity of Fe(sub)83.4Sm(sub)3.4O(sub)13.2 thin film with the best soft magnetic properties was 130 $\mu$$\Omega$cm. Therefore, It is assumed that the good soft magnetic properties of Fe(sub)83.4Sm(sub)3.4O(sub)13.2 thin film results from high electrical resistivity and decreasing $\alpha$-Fe grain size due to precipitation of Sm-Oxide phase.

  • PDF

Growth of Zn0.4Fe2.6O4 Thin Films using Pulsed Laser Deposition and their Crystal Structural and Magnetic Properties (Pulsed Laser Deposition을 이용한 Zn0.4Fe2.6O4 박막의 합성과 그 결정성 및 자기적 특성의 연구)

  • Jang, A.N.;Song, J.H.;Park, C.Y.
    • Journal of the Korean Magnetics Society
    • /
    • v.21 no.3
    • /
    • pp.88-92
    • /
    • 2011
  • We grew $Zn_{0.4}Fe_{2.6}O_4$ thin films using Pulsed Laser Deposition and studied their crystal structure and magnetical characteristics as a function of growth temperature ($T_g$). For the film with $T_g=300^{\circ}C$, X-ray reflections from ${\alpha}-Fe_2O_3$ and ZnO were observed. However, when $T_g$ was increased from 300 to $500^{\circ}C$, crystal structure of inverse spinel was stabilized with the crystal orientation of $Zn_{0.4}Fe_{2.6}O_4(111)/Al_2O_3(0001)$ without any detection of ${\alpha}-Fe_2O_3$ and ZnO phases. The surface morphology shows flattening behavior with increasing $T_g$ from 300 to $500^{\circ}C$. These observations indicate that Zn is substituted into tetrahedron A-site of the inverse-spinel $Fe_3O_4$. M-H curves exhibit clear ferromagnetism for the sample with $T_g=500^{\circ}C$ whereas no ferromagnetism is observed for the film with $T_g=300^{\circ}C$.

The Dispersion Stability of $\alpha-Fe_2O_3$ Particulate Soil in the Anionic/Nonionic Mixed Surfactant Solution (음/비이온계 혼합계면활성제 용액에서 $\alpha-Fe_2O_3$ 입자의 분산안정성)

  • 정선영;강인숙
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.28 no.6
    • /
    • pp.854-861
    • /
    • 2004
  • To estimate dispersion stability of particles in anionic and nonionic surfactant mixed solution, suspending power was examined as functions of duration time of suspension, ionic and nonionic surfactant mixed ratio, surfactant concentration, kinds of electrolyte, ionic strength and mole numbers of oxyethylene additions to nonionic surfactant using $\alpha$-Fe$_2$O$_3$ particle as the model of particulate soil. The suspending power of anionic and nonionic surfactant mixed solution was relatively higher than that of anionic and nonionic surfactant single solution regardless of solution concentration. The suspending power was gradually decreased with increasing duration time of suspension. In the absence of electrolyte, the effect of surfactant concentration on suspending power was small but in solution with electrolyte, suspending power was lowest at 1 % surfactant concentration. With 1${\times}$10$^{-3}$ ionic strength and polyanionic electrolyte in solution, the suspending power was high but effects of oxyethylene mole number to nonionic surfactant on suspending power was small. Generally the suspending power was gradually increased with decreasing the particle size. Hence the suspending power was inversely related to the particle size.

High Temperature Oxidation of ${Fe_3}Al-4Cr$ Alloys (${Fe_3}Al-4Cr$ 합금의 고온산화)

  • Kim, Gi-Young;Lee, Dong-Bok
    • Korean Journal of Materials Research
    • /
    • v.11 no.1
    • /
    • pp.34-38
    • /
    • 2001
  • Intermetallics of Fe-28%Al($Fe_3Al$) and Fe-28%Al-4%Cr($Fe_3Al-4Cr$) were oxidized at 1073, 1273 and 1473k in air for up to 17 days. The oxidation resistance of$Fe_3Al-4Cr$ was basically similar to or better than that of $Fe_3Al$. The oxide scales formed on $Fe_3Al$ consisted essentially of pure ${\alpha}-AL_2O_3$, while those formed on $Fe_3Al-4Cr$ consisted of ${\alpha}-AL_2O_3$ having dissolved iron and chromium ions. The preferential outward diffusion of substrate elements to form the outer oxide layer led to the formation of Kirkendall voids at the oxide-matrix interface. The scales formed on $Fe_3Al(-4Cr)$ were thin and dense up to 1273K, but they spalled easily at 1473K, accompanied by more weight gains.

  • PDF

Mössbauer Studied of Multiferroic Bi2/3La1/3FeO3 Nanoparticles (Multiferroic Bi2/3La1/3FeO3 나노입자의 Mössbauer 연구)

  • Lee, Seung-Wha
    • Journal of the Korean Magnetics Society
    • /
    • v.16 no.1
    • /
    • pp.28-33
    • /
    • 2006
  • La substituted perovskite $BiFeO_3$ have been prepared by a sol-gel method. Magnetic and structural properties of the powders were characterized with Mossbauer spectroscopy, XRD, SEM, and TG-DTA. The crystal structure is found to be a rhombohedrally distorted perovskite structure with the lattice constant $\alpha=3.985{\AA}\;and\;\alpha=89.5^{\circ}.\;Bi_{2/3}La_{1/3}FeO_3$ powders that were annealed at and above $600^{\circ}C$ have a single-phase perovskite structure. However, powders annealed at $900^{\circ}C$ have a typical perovskite structure with small amount of $Bi_2O_3$ phase. The Neel temperature of $Bi_{2/3}La_{1/3}FeO_3$ is found to be $680\pm3K$. The isomer shift value at room temperature is found to be 0.27 mm/s relative to the Fe metal, which is consistent with high-spin $Fe^{3+}$ charge states. Debye temperature far$Bi_{2/3}La_{1/3}FeO_3$ is found to be $305\pm5K$. The average hyperfine field $H_{hf}(T)$ of the $Bi_{2/3}La_{1/3}FeO_3$, shows a temperature dependence of $[H_{hf}(T)-H_{hf}(0)]/H_{hf}(0)=-0.42(T/T_N)^{3/2}-0.13(T/T_N)^{5/2}$ for $T/T_N<0.7$ indicative of spin-wave excitation.

Preparation and Magnetic Properties of Amorphous Spinel Ferrite (비정질 Spinel Ferrite의 제조와 그 자기적 특성)

  • 김태옥;김창곤
    • Journal of the Korean Magnetics Society
    • /
    • v.2 no.1
    • /
    • pp.29-36
    • /
    • 1992
  • The fundamental research about the amorphous ferrite, which is expected as the important material for electronic and information imdustry in future, was carried out in this work. Because the ferromagnetic amorphous ferrites reported recently are very inferior in magnetic properties than the crystalline ferrites, the development of the more ferromagnetic amorphous ferrites is required. In order to obtain the fundamental data for the preparation of amorphous ferrites, the hand-made twin-roller quenching apparatus was used for rapid quenching. Investigation on amorphous ferrite in the system $CaO-Bi_{2}O_{3}-Fe_{2}O_{3}$ has been carried out in the composition of 10-50 mole% CaO, 10-50 mole% $Bi_{2}O_{3}$, 40-70 mole% $Fe_{2}O_{3}$. Large magnetization values were obtained near the composition of the mixture of $BiFeO_{3}$ and $CaFe_{4}O_{7}$. Especially, an amorphous ${(CaO)}_{20}{(Bi_{2}O_{3})_{15}{(Fe_{2}O_{3})}_{65}$ specimen has a magmetization value of about 21.84 emu/g at 0K(10 kOe). Fe $M\"{o}ssbauer$ absorption spectrum indicates that this specimen is compsed of two amorphous phases, antiferromagnetic phase($\alpha$-phase) and ferromagnetic phase($\beta$-phase). Crystallization of this amorphous ferrite was happened in steps-$550^{\circ}C$ and $775^{\circ}C$, then observed crystal phases were perovskite phase of $BiFeO_{3}$ and $Fe_{2}O_{3}$ phase.

  • PDF

Solution Processed Porous Fe2O3 Thin Films for Solar-Driven Water Splitting

  • Suryawanshi, Mahesh P.;Kim, Seonghyeop;Ghorpade, Uma V.;Suryawanshi, Umesh P.;Jang, Jun Sung;Gang, Myeng Gil;Kim, Jin Hyeok;Moon, Jong Ha
    • Korean Journal of Materials Research
    • /
    • v.27 no.11
    • /
    • pp.631-635
    • /
    • 2017
  • We report facile solution processing of mesoporous hematite (${\alpha}-Fe_2O_3$) thin films for high efficiency solar-driven water splitting. $Fe_2O_3$ thin films were prepared on fluorine doped tin oxide(FTO) conducting substrates by spin coating of a precursor solution followed by annealing at $550^{\circ}C$ for 30 min. in air ambient. Specifically, the precursor solution was prepared by dissolving non-toxic $FeCl_3$ as an Fe source in highly versatile dimethyl sulfoxide(DMSO) as a solvent. The as-deposited and annealed thin films were characterized for their morphological, structural and optical properties using field-emission scanning electron microscopy(FE-SEM), X-ray diffraction(XRD), X-ray photoelectron spectroscopy(XPS) and UV-Vis absorption spectroscopy. The photoelectrochemical performance of the precursor (${\alpha}-FeOOH$) and annealed (${\alpha}-Fe_2O_3$) films were characterized and it was found that the ${\alpha}-Fe_2O_3$ film exhibited an increased photocurrent density of ${\sim}0.78mA/cm^2$ at 1.23 V vs. RHE, which is about 3.4 times higher than that of the ${\alpha}-FeOOH$ films ($0.23mA/cm^2$ at 1.23 V vs. RHE). The improved performance can be attributed to the improved crystallinity and porosity of ${\alpha}-Fe_2O_3$ thin films after annealing treatment at higher temperatures. Detailed electrical characterization was further carried out to elucidate the enhanced PEC performance of ${\alpha}-Fe_2O_3$ thin films.

Conduction Band Model of the System ${\alpha}-Fe_2O_3$-CdO at Extrinsic Region (외성영역에서 ${\alpha}-Fe_2O_3$-CdO 계의 전도띠 모델)

  • Keu Hong Kim;Seok Ho Yun;Young Sik Kwon;Jae Shi Choi
    • Journal of the Korean Chemical Society
    • /
    • v.31 no.5
    • /
    • pp.406-412
    • /
    • 1987
  • The electrical conductivities of ${\alpha}-Fe_2O_3$ containing 2.5 and 5.0mol% of cadmium were measured from 300 to $900^{\circ}C$ under oxygen pressures of 10$^{-7}$ to 10$^{-1}$ atmosphere. Plots of log ${\sigma}$ vs. 10$^3$/T show the extrinsic conductivity at oxygen pressure higher than $5{\times}10$^{-2}$atm. The transition points appear at about 550$^{\circ}$C and the activation energies are 1.34 eV for the intrinsic region and 0.50 eV for the extrinsic region on 5mol% Cd-doped ${\alpha}-Fe_2O_3$. The extrinsic conductivity disappears at oxygen partial pressures lower than $5{\times}10$^{-2}$ atm, and the intrinsic conductivity predominates. The electrical conductivities decrease with increasing mol% of cadmium doped. The predominant defect of ${\alpha}-Fe_2O_3$ doped with Cd is believed to be Fe${2+}$ interstitial for the intrinsic, however, oxygen vacancy predominates for the extrinsic region. The electrical conduction mechanisms are proposed and the conduction band model is suggested for the extrinsic region.

  • PDF