In this study, three types of Ti3AlC2 MAX phase powders with different oxygen contents were synthesized using a calcium reduction deoxidation process, and their effects on phase purity and the electrical conductivity of Ti3C2Tx MXene were quantitatively evaluated. Titanium powders with initial oxygen contents of 880, 4,800, and 8,800 ppm were sintered at 1,450℃ for 5 hours under Ar atmosphere, yielding MAX phase powders with final oxygen contents of 4,300, 8,030, and 15,100 ppm, respectively. XRD analysis and Rietveld quantification revealed Ti3AlC2 phase fractions of 85.9, 90.8, and 98.0 wt. % for HI-MAX, MID-MAX, and LO-MAX samples, confirming that lower oxygen content promotes higher phase purity. TiO2 peaks were additionally detected in HI-MAX, indicating that excess oxygen accelerates impurity phase formation during sintering. MXene fabricated from LO-MAX exhibited a highly ordered restacked structure, whereas MXene fabricated from HI-MAX exhibited a more disordered stacking structure. The electrical conductivity of Ti3C2Tx MXene films fabricated via LiF/HCl etching was 3,150, 6,350, and 13,140 S/cm for HI-MAX, MID-MAX, and LO-MAX derived samples, respectively, showing a clear improvement with decreasing oxygen content. This is attributed to residual TiC and TiO2 impurities impeding charge transport within the MXene after etching. These results demonstrate that controlling the oxygen content of the precursor titanium powder is a critical factor for fabricating high-quality Ti3C2Tx MXene.