1055SiV steel, developed for bearing raceways, is a medium-carbon steel alloyed with Vanadium as a microalloying element to improve mechanical properties and fatigue resistance [1]. However, its high hardness leads to difficulties in machining. This study aimed to retain the enhanced properties while optimizing heat treatment conditions to reduce the hardness to a machinable level and significantly shorten the time required for spheroidization. In tests conducted on ring-shaped outer race forgings for wheel hub bearings, the initial microstructure was observed as a mixture of pearlite and proeutectoid ferrite [2-5]. Subcritical annealing was applied at 680℃, 700℃, and 720℃, temperatures below the A1 transformation point (738℃, Fig. 1). Prior to this, to remove proeutectoid ferrite, the specimens were held at 820℃, above the A3 point (763℃, Fig. 1), for 30 minutes, followed by quenching and furnace cooling. Applying newly designed spheroidizing cycles at 680℃ and 720℃ reduced the process time by 44% to under 10 hours, while achieving uniform hardness of approximately 170 HV. Microstructural analysis revealed a fully spheroidized matrix containing ribbon- and rod-shaped carbides, which are expected to improve machinability [6]. This study presents a practical improvement strategy by correlating heat treatment conditions with the resulting microstructure and mechanical properties of 1055SiV steel.