Volume 42 Issue 2
-
Kim, Hyun-Bae;Park, Joo-Saeng;Hong, Jung-Pyo;Oh, Jung-Kwon;Lee, Jun-Jae 89
Energy consumption statistics in 2005 from the Korea Energy Management Corporation show that building energy usage was about 24.2% of total domestic energy consumption, and 64% of total building energy usage was consumed by residential buildings. Thus, about 10% of total domestic energy consumption is due to the heating of residential buildings. Building energy can be calculated by the configuration of the building envelope and the rate of infiltration (the volume of the infiltration of outdoor air and the leakage of indoor air), and by doing so, the annual energy usage for heating and cooling. Therefore, air-tightness is an important factor in building energy conservation. This investigate air infiltration and various factors that decrease it in timber frame buildings and suggest ways to improve air-tightness for several structural types. Timber frame buildings can be classified into light frame, post and beam, and log house. Post and beam includes Han-ok (a Korean traditional building). Six light frame buildings, three post and beam buildings, one Korean traditional Han-ok and a log house were selected as specimens. Blower door tests were performed following ASTM E779-03. The light frame buildings showed the highest air-tightness, followed by post and beam structures, and last, log houses. -
Lee, Nam-Ho;Zhao, Xue-Feng;Shin, Ik-Hyun;Lee, Chang-Jin 101
In this study the effect of heartwood-coating (HCO), vapor-dam (VD), bark-remaining (BR) and bark-remaining-coating (BRC) treatments on the air circulating oven-drying characteristics of Japanese larch hollowed round-post was evaluated. The drying times of the hollowed round-posts for control, VD, HCO and BR specimens were 72, 168, 204 and 240 hours, respectively, from the initial MC to about 8% MC, which was recommended as the indoor in-use MC. The temperature in the hole of the VD specimen was lower than that of wood and the difference between air temperature in the hole and wood temperature became large during drying period. The vapor pressure of air in the hole was higher than that of inside wood for all specimens except VD specimen. The surface checks on all specimens were observed in increasing order of BR, BRC, UC, HCO and VD specimens. -
The depth effect on bending strength of Japanese larch structural lumber was investigated by using the published data of two different depth lumbers with the same length. Depth effect parameters were derived from Weibull's weakest link theory and compared to the results from other researches. Depth effect on bending strength was significant for No.1 and No.3 lumber, but not insignificant for No.2 lumber. Calculated value of the depth effect adjustment factors was 0.21, 0.11 and 0.22 by lumber grade, respectively. These results were similar to those results from previous researches and supported depth effect on bending strength of lumber. An apparent depth adjustment factor has been proposed to 0.2 in the literatures. Based on this study, depth adjustment factor was considered to 0.2 as a conservative optimum design value that should be incorporated in domestic building code (KBC) for structural lumber.
-
Park, Byung-Dae;Um, In Chul;Lee, Sun-Young;Dufresne, Alain 119
This work undertook to prepare nanofibers of cellulose nanofibrils (CNF)/polyvinyl alcohol (PVA) composite by electrospinning, and characterize the electrospun composite nanofibers. Different contents of CNFs isolated from hardwood bleached kraft pulp (HW-BKP) by 2,2,6,6-tetramethylpiperidine-1-oxy radical (TEMPO)-mediated oxidation were suspended in aqueous polyvinyl alcohol (PVA) solution, and then electrospun into CNF/PVA composite nanofibers. The morphology and dimension of CNFs were characterized by transmission electron microscopy (TEM), which revealed that CNFs were fibrillated form with the diameter of about$7.07{\pm}0.99$ nm. Morphology of the electrospun nanofiber observed by field-emission scanning electron microscopy (FE-SEM) showed that uniform CNF/PVA composite nanofibers were manufactured at 1~3% CNF contents while many beads were observed at 5% CNF level. Both the viscosity of CNF/PVA solution and diameter of the electrospun nanofiber decreased with an increase in CNF content. The diameter and its distribution of the electrospun nanofibers helped explain the differences observed in their morphology. These results show that the electrospinning method was successful in preparing uniform CNF/PVA nanofibers, indicating a great potential for manufacturing consistent and reliable cellulose-based nanofibrils for scaffolds in future applications. -
Nondestructive evaluation (NDE) method by using a resonance frequency mode was carried out for ceramics made from particle boards with different phenol resin impregnation ratios (30, 40, 50, 60%) at carbonizing temperature of
$800^{\circ}C$ . The material for ceramics was Miscanthus sinensis var. purpurascens board. Dynamic modulus of elasticity increased with increasing impregnation ratio. There was a close relationship of dynamic modulus of elasticity and static bending modulus of elasticity to modulus of rupture (MOR). However, the result indicated that correlation coefficient is higher in dynamic modulus of elasticity to MOR than that in static modulus of elasticity to MOR. Therefore, the dynamic modulus of elasticity using resonance frequency by free vibration mode is more useful as a nondestructive evaluation method for predicting the MOR of ceramics made from Miscanthus sinensis var. purpurascens particle boards by different phenol resin impregnation ratios. -
Stem and root of Lindera erythrocarpa were described and compared in the wood anatomical aspects. Root wood appeared to differ from stem wood in the qualitative features of growth ring boundary, extraneous materials in vessel element and ray parenchyma cell, outline of ray, and sheath cell. In the quantitative features, there were differences between these two tissues in vessels per square millimeter, tangential diameter of vessel lumina, length of vessel element, and width of ray. These wood anatomical differences between stem above ground and root below ground were thought to be attributed to their different growth environments.
-
Park, Han-Saem;Ham, Youngseok;Ahn, Hee-Hoon;Shin, Keum;Kim, Yeong-Suk;Kim, Tae-Jong 149
Termites are wood pests that cause vast economic damage every year. They digest both cellulose and starch, but the enzymes for starch digestion have not been well characterized. We obtained complete amino acid sequence information on the KME1${\alpha}$ -amylase from Reticulitermes speratus KMT1 through analysis of total mRNA sequences. The KME1 enzyme has two${\alpha}$ -amylase domains and is 68% identical to the${\alpha}$ -amylase from Blattellager manica, its closest relative in the GenBank database. Some unique features of its conserved region and its distant evolutionary relationship to other insect${\alpha}$ -amylases suggest that KME1 is a new type of${\alpha}$ -amylase. -
Son, Dong Won;Kang, Mee Ran;Hwang, Won Joung;Lee, Hyun Mi;Park, Sang Bum 157
This study was conducted to examine the functionality of the fire retardant treated wood. The hygroscopic property, leaching resistance, metal corrosive efficacy and gas toxicity of retardant treated wood were analyzed. Sodium silicate was penetrated to the wood for making fire retardant treated wood. The subsequent treatment agents such as boric acid, ammonium borate, di-ammonium phosphate were treated after sodium silicate treatment due to fixation. As results for the test, the leaching resist was improved by subsequent treatment. The fire retardant combination such as sodium silicate, boric acid and di-ammonium phosphate showed high hygroscopic property, metal corrosive efficacy. The gas toxicity was also satisfied KS standard. -
Lee, Min;Park, Sang-Bum;Lee, Sang-Min;Son, Dong-Won 163
Environmental issues about indoor air quality have been increased and focused on volatile organic compounds (VOCs) caused cancer, asthma, and skin disease. Reducing VOCs has been attempted in many different methods such as using environmentally friendly materials and air cleaner or purifier. Charcoal is well known material for absorbing VOCs. Therefore, carbonized board from medium density fiberboard has been developed. We assumed that the source of carbonized boards can be any type of wood-based panels. In this study, carbonized boards were manufactured from oriented strand board (OSB) at 400, 600, 800, and$1000^{\circ}C$ . Each carbonized OSB (c-OSB) was evaluated and determined physiomechanical characteristics such as exterior defects, dimensional shrinkage, modulus of elasticity, and bending strength. No external defects were observed on c-OSBs at all carbonizing conditions. As carbonizing temperature increased, less porosity between carbonized wood fibers was observed by SEM analysis. The higher rate of dimensional shrinkage was observed on c-OSB at$1000^{\circ}C$ (66%) than c-OSB at 400, 600, and$800^{\circ}C$ (47%, 58%, and 63%, respectively). The densities of c-OSBs were lower than original OSB, but there was no significant different among the c-OSBs. The bending strength of c-OSB increased 1.58 MPa (c-OSB at$400^{\circ}C$ ) to 8.03 MPa (c-OSB at$1000^{\circ}C$ ) as carbonization temperature increased. Carbonization temperature above$800^{\circ}C$ yielded higher bonding strength than that of gypsum board (4.6 MPa). In conclusion, c-OSB may be used in sealing and wall for decorating purpose without additional artwork compare to c-MDF which has smooth surface. -
Extraction is a necessary element in the bioconversion of lignocellulosics to fuels and chemicals. Although various forms of chemical pretreatment of cellulosic materials have been proposed, their effectiveness varies depending on the treatment conditions and substrate. In this study, mixed hardwood (MH) and loblolly pine (LP) were pretreated with dilute acid in a 100 mL accelerated solvent extraction (ASE) at the predetermined optimal conditions: temperature:
$170^{\circ}C$ , acid concentration: 0.5% (w/v), and reaction time: 2~64 min. This method was highly effective for extracting the hemicellulose fraction. Total xmg (defined as the sum of xylose, mannose, and galactose) can be extracted from milled MH and LP through pressurized dilute acid treatment in maximum yields of 12.6 g/L and 15.3 g/L, respectively, representing 60.5% and 70.4% of the maximum possible yields, respectively. The crystallinity index increased upon pretreatment, reflecting the removal of the amorphous portion of biomass. The crystalline structure of the cellulose in the biomass, however, was not changed by the ASE extraction process. -
For the structure determination of D-(+)-sucrose, which consists of
${\alpha}$ -D-(+)-glucose and${\beta}$ -D-(+)-fructose, it was acetylated with acetic anhydride and triethyl amine, pyridine, zinc chloride, and sodium acetate as catalysts. The acetylated D-(+)-sucrose was acid-hydrolyzed using sulfuric acid and sodium chloride in methanolic solution. The structures of the reaction products were determined by$^1H$ -NMR and$^{13}C$ -NMR spectra. The yield of the acetylation indicated the high value in zinc chloride as 70% in zinc chloride catalyst. The acid-hydrolyzed product of the acetylated D-(+)-sucrose, 2,3,4,6,1',3',4',6'-octa-O-acetyl-D-(+)-sucrose, gave 2,3,4,6-tetra-O-acetyl-${\beta}$ -D-(+)-glucose and it suggests that the acetylated D-(+)-sucrose was rearranged through the formation of oxonium ion by mutarotation in the 2,3,4,6-tetra-O-acetyl-${\alpha}$ -D-(+)-glucose moiety and through the ring opening in the 1',3',4',6'-tetra-O-acetyl-${\beta}$ -D-(+)-fructose moiety. -
Lee, Hyun-Mi;Hwang, Won-Joung;Lee, Dong-Heub;Kim, Hong Sik 193
Residual performance of old architectural wood which has been damaged was measured using Nondestructive Evaluation (NDE). The wood Pole Tester was used to assess ultrasonic velocity inside wood and drill resistance was determined using an IML-resistograph. For ultrasonic measurements squared timber and circular timber's measurements were separately conducted with 1,300 m/s as the standard ultrasonic velocity. The standard wood samples divided into two parts; a non-sound area (below the standard), and a sound area (above the standard). Furthermore, schematization of wood was compared with results naked eye observation. The drilling resistance test was performed for both length and thickness direction in wood. The internal of the drilling was set at 30 cm (length direction), 5 cm (width direction) and 30cm (thickness direction). A non-sound area was defined as that 1) amplitude is below 20% and 2) carbonization and deterioration are related. -
This study was carried out to investigate the feasibility and usefulness of a commercial synthetic adsorbent, Diaion HP 20, for the isolation of proanthocyanidins (PAs) from hot water extract (HWE) prepared from Pinus radiata bark. Most ultraviolet (UV) absorbing materials in HWE were adsorbed onto Diaion HP 20 and easily recovered by simple ethanol (EtOH) washing. More than 50% of the UV absorbing materials were adsorbed within 20 minutes, and the adsorption equilibrium was reached within 3 h. The recovered materials from Diaion HP 20 were mostly composed of PAs, but some monomeric flavonoids such as taxifolin and unidentified hydrophobic materials were also adsorbed. The impurities such as carbohydrates and inorganic materials contained in HWE were mostly removed by Diaion HP 20. The adsorption ability of the UV absorbing materials onto Diaion HP 20 was almost the same as the first cycle even after 14 times of repeating cycles of adsorption and desorption. The radical scavenging ability of the recovered materials from the adsorbent was slightly higher than that of the pure PAs prepared by Sephadex LH 20 from the same HWE.
-
Hwang, Won-Joung;Lee, Hyun-Mi;Park, Young-Ran;Lee, Dong-Heub 214
The deterioration in wood by the brown-rot fungus (Fomitopsispalustris) and the white-rot fungus (Trametesversicolor) were measured using ultrasonic velocity. Those were used for the decay exposure and 4 wood species of wood as the test specimens, Pinusdensiflora, Larixkaempferi, Pinuskoraiensis and Pinusrigida, were chosen with both the brown- and white-rot culture petridish during 12 weeks. After 12 weeks, the decrease rate of ultrasonic velocity was measured at 10~15%. In both brown- and white-rot exposure experiments, P. rigida showed significant decrease in ultrasonic velocity (20%), L. kaempferi on the other hand did not show decrease in ultrasonic velocity. After the fungal exposure experiment, the inside of specimens was investigated by computer tomography (C/T). After C/T investigation, bending tests were performed.