Volume 15 Issue 3
-
Park, Byung-Dae;Park, Sang-Jin 1
PDFThis study was carried out to investigate the variations of dimension and exterior shape of vessel elements, morphology of spiral thickening and ray-vessel pit in korean diffuse-porous woods (56 species, 18 families), The tangential pore diameter and vessel element length was increased, whereas the pore number per unit area($1mm^2$ ) was decreased from pith outwards. The tangential pore diameter was decreased but the length of vessel element was not changed from earlywood to latewood within an annual ring. However, the dimensional variations of vessel element was not able to be recognized among relative positions in peripheral variation. The exterior shape of vessel element could be classified into four types; Type 1 is without tail, Type 2 with ligulate tail, Type 3 with broad taper tail and Type 4 with the very short length between perforations. The distribution frequency of Type 2 and 3 was relatively high in comparision with the others. According to the prominence, distribution position and branched shape, the spiral thickenings could be divided into five types. The spiral thickenings occurred 52% in the species observed. Thus it was doubtful to consider the simple presence of spiral thickening as diagnostic index in diffuse-porous woods. The morphology of ray-vessel pit could be grouped as reticulate, scalariform, oval, linear and coalescent type. Most of species examined showed oval and linear type. -
Lee, Jae-Ki;Park, Sang-Jin 14
PDFThis study was carried out to investigate the anatomical characteristics, the radial and axial variation of the cell dimension and bulk density for four bamboo species used as the major material of bamboo products in Korea; Phyllostachys(P.bambusoides, P.edulis, P.nigra var.henonis, and Pnigra). The results obtained were summarized as follows; 1) In the outer part of culm, the mophological difference of cell diameter and distribution were not acknowledged. However, gum-like substance was occurred In the epidermis, hypodermis, cortex and metaxylem vessel of P.nigra, while it was occured only in the metaxylem vessel of P.edulis. 2) The protoxylem vessel in the central zone of culm-wall could be in the two types; the first type consisted of 4-5 small cell pieces occurred in P.edulis and P.nigra var. henonis, the second type of 1-2 large cell pieces in P.bambusoides and P.nigra. And transition of cell diameter from the vascular bundle sheath to the ground tissue was gradually enlarged in P.nigra and P.edulis but abruptly in P.bambusoides and P.nigra var. henonis. 3) Thin-wall tyloses were well developed in the outer and central zone of culm-wall in four species. 4) Compared with the central part of culm-wall, the number of parenchyma cells and the amount of the vascular bundle sheaths per unit area were a few in the inner part. The inner part nearest to the pith cavity was consisted of thick-well parenchyma cell. 5) The dimensional variations of metaxylem vessel and parenchyma cell in the radial direction were decreased from the inner part to the epidermis in all species observed. 6) The fiber length was the maximum in the central zone and its diameter was increased from the inner part to the outer part. In the axial variation. fiber length was slightly increased from the base and then decresed slowly toward the top, and its diameter was reverse. 7) The axial variation of the bulk density was continuously increased from the base toward the top and its radial variation was rapidly increased from the inner part to the epidermis. -
Lee, Phil-Woo;Kim, Hyun-Joong 24
PDFThis study was executed to investigate scanning electron microscopic characteristics of Korean Rhus lacquer coats. With the unrefined coat, distilled water, sodium hydroxide, acetic acid, ethyl alcohol, cold-check test, and accelerated weathering were performed after refining treatment. These treated lacquer coats were discussed through observation by scanning electron microscope and the obtained results were summarized as follows: 1. Compared with unrefined coat, the refined coat of Korean Rhus lacquer showed more even surface with regular distribution of dispression. 2. Korean Rhus lacquer coat heated at$120^{\circ}C$ for 3 hours revealed no observable difference irrespective of refining and unrefining. 3. Korean Rhus lacquer coat treated by distilled water, sodium hydroxide, acetic acid. ethyl alcohol, cold-check test. and ultraviolet radiation showed significant characteristics compared with untreated coat. Especially. large deformation and checkings were observed by cold-check test and ultraviolet radiation respectively. 4. The Korean Rhus lacquer coat radiated by ultraviolet ray showed 0.11 duller and 1.41 brighter than non-radiated coat through color difference calculator. -
Lee, Sang-Pill;Lee, Jong-Yoon 34
PDFThis study was performed to find out the types of linkage of carbohydrates in wood cell walls. To study the structure of linkage of carbohydrates in wood cell walls, we have attempted to find out the method holocellulose preparation and optimum condition of enzyme hydrolysis in holocellulose, and fractionate oligosaccharide with products that hydrolized partly by acetolysis and deacetylation in holocellulose. We have achieved four results. These results as follow; 1. At first. we reacted in wood meal$NaClO_2$ 1g per lignin lg for one hour and then the same of quantity$NaClO_2$ for four hours. Through these experiments, we have developed new holocellulose preparation method which had low loss of carbohydrates and high effect of the delignification. 2. The optimum condition of enzyme hydrolysis of holocellulose which had lignin was 0.005M sodium acetate buffer (pH 5.0). We have achieved 7.2% reducing sugar through the procedure that reactioned 0.01g holocellulose putting enzyme 0.03g for 72 hours. It may be supposed that 5.5% of lignin contained in holocellulose prevented enzyme contaction from holocellulose and so this lignin has resulted in the low efficiency of enzyme hydrolysis. 3. We did not fractionated from oligosaccharides which were preparated by the method of acetolysis and deacetylation in holocellulose. The reason is that holocellulose having a lot of lignin prevented prefectly partial hydrolysis from the method of acetolysis and deacetylation. 4. We attempted analysis of six standard substances through HPLC apparatus having sugar pak 1 column which we have changed flow rate and the column temperature variably. These six standard substances were D-glucose, D-mannose, D-xylose, D-galactose and L-rhamnose, L-arabinose, But sugar pak 1 column was not fitted analysis of four substances because D-galactose, D-mannose, D-xylose, L-rhamnose were agreement with elution time. And so, we could not analize four standard substances with sugar pak 1 column. -
Lee, Phil-Woo;Suh, Jin-Suk 44
PDFIn order to study the effect of sawdustboard combined with plastic chips, 0.5mm($T_1$ ), 1mm($T_2$ ), 1.4mm($T_3$ ) thick nylon fiber. polypropylene rope fiber(RP), and 0.23mm thick moth-proof polypropylene net fiber(NP) were cut into 0.5, 1, 2cm long plastic chips. Thereafter, sawdustboard combined with plastic chips prepared as the above and plastic non-combined sawdustboard(control) were manufactured into 3 types of one-, two-, and three layer with 5 or 10% combination level. By the discussions and results at this study, the significant conclusions of mechanical and physical properties were summarized as follows: 1. The MORs were shown in the order of 3 layer> 2 layer> 1 layer among plastic non-combined boards, and$T_3$ <$T_2$ <$T_1$ < RP (NP(5%) < NP(l0%) among plastic combined boards. In 2cm long plastic chip in 1 layer board, the highest strength through all the composition was recognized. 1 layer board showing the lower strength with 0.5cm plastic chip rendered to the bending strength improvement by 2 or 3 layer board composition. On the other hand, 2 or 3 layer combined with 1, 2cm long polypropylene net fiber chips incurred MOR's conspicuous decrease requiring optimum plastic chip combined level and consideration to combined type. 2. MOE in plastic non-combined 3 layer board exhibited sandwich construction effect by higher resin content application to surface layer in the order of 3layer>1layer>2layer with the highest stiffness of the board combined with polypropylene chip, while nylon chip-combined board had little difference from plastic non-combined board. In relevant to length and layer effect, 3 layer board combined with the 0.5cm long polypropylene net fiber chip in 5% and 10% combined level presented 34-43% and 44-76% stiffness increase against plastic non-combined board(control), respectively. Moreover, in 1 layer board, 30% stiffness increase with 10% against 5% combined level in the 1 and 2cm long polypropylene net fiber chip was obtained. 3. Stress at proportional limit(Spl) showing the fiber relationship (r: 0.81-0.97) between MOR presented in the order of 1 layer<2 layer<3 layer in plastic non-combined board. Correspondingly, combined effect by layer and plastic chip length was similar to MOR's. 4. Differently from previous properties(MOR, MOE, Spl). work to maximum load(Wml) of 2 layer board approached to that of 3 layer board. Conforming the above phenomenon. 2 layer combined with 0.5cm long polypropylene net fiber chip kept the greater work than 1 layer. The polypropylene combined board superior to nylon -and plastic non - combined board seemed to have greater anti - failing capacity. 5. Internal bond strength(IB), in contrast to MOR's tendency. showed in the order of T1Kim, Jong-Man 56
PDFPlywoods used for construction as a decorative interior material are inflammable and can make fire accidents, causing destruction of human life and property. Therefore, it is indeed required to make fire-retardant treated plywood. In this study, 3.7mm yellow meranti plywoods were soaked in 18% boric acid solutions and tap water by hot-cold bath for 1/2, 2/2, 4/2, 6/2 hours and redrying of treated plywoods was carried out by press drying at the platen temperature of 110, 130, 160,$180^{\circ}C$ and then it was conducted to investigate solution absorption, drying rates, dynamic young's modulus. specific gravity and fire-retardant factors such as burning point, flame spread length. flame exhausted time, back side carbonized area and weight loss by treating time, treating solutions and platen temperature. The results are as follows; 1. When plywood was impregnated with the hot bath temperature of$70^{\circ}C$ for 1. 2, 4, 6 hours and the cold bath temperature of$15^{\circ}C$ for 2 hours respectively, retentions of boric acid were 1.565, l.597, 1.643, 1.709kg/$(30cm)^3$ and all of them exceeded the minimum retention [1.125kg/$(30cm)^3$ ] even in the shortest treatment. 2. In hot-cold bath method for 1/2 hours, the drying rates of treated plywood remarkably increased with the extension of platen temperature of 110, 130, 160,$180^{\circ}C$ and the values of boric acid treated plywood were 5.900, 10.196, 45.42, 54.958m.c%/min and the values of water treated plywood were 6.014, 12.373, 46.520, 55.730m.c%/min and drying rates of water treated plywood were faster than those of boric acid treated plywood. 3. The values of boric acid treated plywoods in dynamic young's modulus were widely higher than those of water treated plywoods. And it can be observed that there were highly significant differences for treating time between dynamic young's modulus, and the values of boric acid plywoods increased with the extension of treating time but on the contrary water treated plywoods were decreased values with prolonged time 4. It was observed that there were highly significant differences for platen temperature between dynamic young's modulus. When the values of water treated plywoods in dyna nic young's modulus were abruptly decreased according to the rise of platen temperature. boric acid treated plywoods showed rather increased values at$160^{\circ}C$ of platen temperature. And in 2- way interactions, there were also highly significant for dynamic young's modulus between treating time x treating solutions and platen temperature x treating solutions. 5. Correlation coefficients of fire-retardant factors were shown in table 5. It could be recognized that there were close correlations between the treating solutions and burning point, flame spread length, back side carbonized area, flame exhausted time and weight loss, but there was no correlation between fire-retardant factors and treating time and platen temperature. 6. From table 6, it can be observed that there were highly significant differences for burning point, flame spread length, flame exhausted time, back side carbonized area, weight loss between treating solutions. And in 2-way interactions, there were highly significant for burning point, flame spread length, weight loss between treating time$\times$ treating solutions.