Volume 13 Issue 3
-
Lee, Phil-Woo 3
PDFThe object of this study was to investigate the effects on physical and mechanical properties of wood particle and sawdust board combined with wire net. Conventional forming, press-lam, and veneer comply boards combining one to four wire net sheets were made from wood particle and sawdust with different spacings (8, 10, 12, and 18 Mok) and different wire diameters (0.35, 0.50, and 0.80mm) composing wire net. They were compared and analyzed statistically with specific gravity, thickness swelling, length swelling, bending properties (modulus of rupture, modulus of elasticity, work to proportional limit, and total work), internal bonding strength, and screw holding strength between wood particle and sawdust boards. The results obtained at this study as cording to the discussions might be concluded as follows; 1. In specific gravity, both particle and sawdust boards by press-lam method were higher than by conventional forming and veneer comply method, and the boards containing more wire net sheets also showed higher value. But the wire net spacings(Mok) had no influence on specific gravity. In general, particle board showed higher specific gravity than sawdust board. Veneer comply board showed lowest specific gravity values. 2. Both particle and sawdust boards by press-lam method was slightly lower than by conventional forming and veneer comply method in thickness swelling. The sawdust board containing 8, 12. and 18 Mok wire net showed lower thickness swelling than the corresponding particle board, but both sawdust and particle boards containing the T8 and 10 Mok wire net showed higher and similar thickness swelling. 3. Both particle and sawdust boards containing wire net showed no difference in MOR and MOE of bending. Comply board was the highest and particle board showed slightly higher than sawdust board in MOR and MOE values. 4. In work to proportional limit and total work in bending, both particle and sawdust boards containing thicker wire diameter and more wire net sheets showed higher value. From these facts, it is conceivable that boards with thicker wire diameter and more wire net sheets show increasing resistance against external force. But there was no significant difference between particle and sawdust borads. 5. In resistance against delamination (internal bonding strength), both sawdust and particle boards containing wire net showed lower value than control, and also showed decreasing tendency with more number of wire net sheet composed. Particle board showed higher resistance against delamination than sawdust board. 6. In screw holding strength, sawdust board containing thicker wire diameter and more wire net sheets showed higher value, but particle board by press-lam method was higher than by conventional forming and veneer comply method. Screw holding strength of particle board was higher than that of sawdust board. -
Jung, Hee-Suk 27
PDFAir-drying tests were carried out on green taun (Pometia pinnata f glabra) for 25-mm and 50-mm thickness to elucidate drying characteristics on air-drying rate, time and defects in spring and air-drying calendar. The results of this study were as follows: 1. The air-dried lumber for 25-mm thickness from an initial average moisture content (MC) of$58.3{\pm}3.5$ percent reached 30 percent MC in 17 days, 25 percent MC in 24 days, 20 percent MC in 38 days and 15 percent MC in 84 days. 2. The air-dried lumber for 50-mm thickness from an initial average MC of$59.6{\pm}5.0$ percent reached 30 percent MC in 39 days, 25 percent MC in 55 days and 20 percent MC in 84 days. 3. Air-drying calendar that could be useful in estimating drying times for each month developed by the use of climatological data for Suwon. Total number of effective air-drying days during a year were 243.5 days and the major determinant of the effect air-drying days was temperature. 4. The air-drying rates for 25-mm and 50-mm coated lumber were slight1y slower than those of uncoated lumber. The number and total length of both end checks and surface checks for end coated lumber were less severe than those of uncoated lumber. -
Hong, Byung-Wha 34
PDFThe characteristics of Paulownia coreana wood used for sounding boards has been revealed through this study. The 80 specimens were selected from Paulownia coreana wood. The dynamic Young's modulus, the internal friction and resonant frequency of wood were measured by the method of making a rectangular bar resonate in the audio frequency range. The results obtained are summarized as follows: 1. The average values of the specific gravity, the dynamic Young's modulus and the internal friction concerning Paulownia coreana used for sounding boards are$0.252{\pm}0.022$ ,$(0.494{\pm}0.068){\times}10^{11}$ dyne/cm and$(7.89{\pm}1.692){\times}10^{-3}$ respectively. 2. The average values of resonant frequency, the velosity of sound, and K values are$504{\pm}24.298$ Hz,$5018{\pm}219.83$ m/s, and$(9.907{\pm}2.05){\times}10^{-4}$ respectively. 3. The dynamic Young's modulus of Paulownia coreana increases with the increase of the specific gravity, and that on the contrary the internal friction decreases. 4. The dynamic Young's modulus was abruptly decreased as the moisture content of wood specimens was increased up to the fiber saturation point, and the internal friction was linearly increased as the moisture content of wood specimens were increased. 5. The vibration properties of Paulownia coreana are that the dynamic Young's modulus is fairly high, the internal friction is low, and the ratio of Young's modulus to specific gravity shows large value. -
Lee, Choon-Taek;Kang, Dae-Hun;Chung, Doo-Jin;Lee, Yong-Dae;Joe, Jae-Myung 41
PDFIn near future about 500,000 hectares of Japanese larch and pitch pine need thinning to improve crop-tree spacing and reasonable species composition in Korea. Although thinned trees show very little high quality wood, in fact, all the sawed products are suitable for construction and farming materials. Studies on the utilization of thinned small-diameter trees have been implemented in order to increase lumber yield and display the skeleton of farm buildings. The results obtained in this study were summarized as follows: 1. According to Korean Conifers Log Grading System, log grade 3 was 87.4 percent in Japanese larch bolts and 95.8 percent in pitch pine bolts from thinned trees. The ability to identify defects was essential for grading logs. 2. Cutting diagrams of sawing were developed for 1-sided sawing, 2-sided sawing and 3-sided sawing by small end diameter class of bolt and cutting sizes also were found to use effectively lumber with wane. 3. Lumber recovery of Pitch pine was a little higher than that of Japanese larch. The maximum lumber yields of pitch pine by sawing patterns were 87.2 percent for 1-sided sawing, 80.8 percent for 2-sided sawing an 64.1 percent for 3-sided sawing, up yield compared with 58.1 percent for 4-sided sawing. The lumber yield of 1, 2 and 3-sided sawing significantly was higher value than that of 4-sided sawing. 4. Lumber was inspected and graded. Lumber quality of diameter class 12cm was a little better than that of diameter class 8cm, but 90 percent of lumber in diameter c1ass 16cm fell into grade 3. The lumber grade was classified by Korean standard grades of confiers lumber. 5. Lumber from 1, 2 and 3-sided sawing was used to build the skeleton of a farm house ($53m^2$ ) and greenhouse ($60m^2$ ) in order to display more efficient use of small diameter trees from thinning 6. Total volume of timber for building a farm house was$8.1m^3$ of imported timber. Timber of$7m^3$ , 70 percent of total volume would be substituted imported timber for domestic timber. -
Ahn, Won-Yung;Shin, Dong-So;Choi, Don-Ha 49
PDFThe effects of pre-treatments, the hot water extraction of wood meal and the addition of chemical ($CaCl_2$ ) to wood-cement water system on the properties of wood-cement composite such as modulus of rupture (MOR), modulus of elasticity (MOE), water sorption ratio and swelling ratio of resulting boards were studied in this experiment. The wood meals through 0.83mm(20 mesh) and retained on 0.42mm(35 mesh) screen were prepared from Pinus densiflora S. at Z. and Larix leptolepsis G. For hot water extraction, 500 grams of wood meal for each species were heated to boiling with 1,500ml of distilled water in 2-liter beaker for 6 hours. Every 2 hours, the wood meals were washed with boiling distil1ed water and reheated to boiling again. After 6 hours boiling, the boiled wood particles were collected by pouring this particles on 200 mesh screen. The collected particles then washed twice with hot distilled water and dried for 24 hours in an oven at$109{\pm}20^{\circ}C$ . A mixture of 663.4 grams of cement with 331.7 grams of wood meal based on oven-dry weight were dry-mixed in a plastic vessel. The mixture was kneaded with 497.6ml of distilled water in the ratio of 1.5ml of water to a gram of wood meal. To add calcium chloride to the mixture as an accelerator,$CaCl_2$ 4% solution by weight per volume, was added to pine-or larch-cement board in the ratio of 3% to cement weight. To set wood-cement board, this mixture was clamped at 30cm${\times}$ 30cm, in thickness of 1.5cm for 3 days at room temperature, declamped and then placed at open condition for 17 days. The target density was 1.0. The four specimens sized to 5cm in width and 28cm in length were used for MOR and MOE test for each treatment. After MOR test, the tested specimens were cut to the size of 5cm${\times}$ 5cm for water sorption and swelling test. The twenty specimens used to measure the water sorption ratio (soaking 24 hours) and ten of these were used for swelling ratio measurement The results obtained were as follows: 1) Larch was not suitable for wood-cement boards because larch-cement board developed no strength, but pine showed 97.9kg/$cm^2$ by hot water extraction. 2) To increase MOR, hot water extraction was more effective than the addition of$CaCl_2$ in pine and larch because the$CaCl_2$ addition was seemed to speed up the ratio of cement hydration without reacting with the wood substances. 3) The water sorption ratio was lowered by the addition of$CaCl_2$ to wood-cement system because the chemical additive accelerated the rate of cement hydration. 4) In pine-cement board, the swelling ratio from 0.37 to 0.42 percent was observed in length and the swelling ratio from 0.88 to 2.0 percent in thickness. As a rule, the swelling ratio of wood-cement board was very low and the swelling ratio in thickness was higher than in length.