DOI QR코드

DOI QR Code

Analytical Method for Determination of Microstructure of SBR and SBR Content in Blended Rubber Composites Using Pyrolytic Technique

  • Received : 2022.11.28
  • Accepted : 2022.12.03
  • Published : 2022.12.31

Abstract

Styrene-butadiene rubber(SBR) is a copolymer of styrene and butadiene. It is composed of 1,2-unit, 1,4-unit, and styrene, and its properties are dependent on its microstructure. In general, rubber composites contain a single rubber or a blended rubber. Similarly, SBR is used by mixing with natural rubber(NR) and butadiene rubber(BR). The composition of a rubber article affects its physical and chemical properties. Herein, an analytical method for determining the microstructure of SBR using via pyrolysis is introduced. Pyrolysis-gas chromatography/mass spectrometry is widely used to analyze the microstructure of polymeric materials. The microstructure of SBR can be determined by analyzing the principal pyrolysis products formed from SBR, such as 4-vinylcyclohexene, styrene, 2-phenylpropene, 3-phenylcyclopentene, and 4-phenylcyclohexene. An analytical method for determining the composition of SBR/NR, SBR/BR, and SBR/NR/BR blends via pyrolysis is introduced. The composition of blended rubber can be determined by analyzing the principal pyrolysis products formed from each rubber component.

Keywords

Acknowledgement

이 연구는 2020년도 산업통상자원부 및 산업기술평가관리원(KEIT) 연구비 지원에 의한 연구임(과제번호 20010851).

References

  1. S.-S. Choi and H.-M. Kwon, "Analytical method for determination of butadiene and styrene contents of styrene-butadiene rubber vulcanizates without pretreatment using pyrolysis-gas chromatography/mass spectrometry", Polym. Test, 38, 87 (2014).
  2. S.-S. Choi, "Influence of silane coupling agent on pyrolysis pattern of styrene-butadiene rubber in filled rubber compounds", Bull. Korean Chem. Soc., 22, 1145 (2001).
  3. S.-S. Choi, "Characteristics of the pyrolysis patterns of styrene-butadiene rubbers with differing microstructure", J. Anal. Appl. Pyrolysis, 62, 319 (2002).
  4. S.-S. Choi and H.-M. Kwon, "Characterization of pyrolysis products formed from styrene-1,2-unit heterosequence of styrene-butadiene copolymer", J. Anal. Appl. Pyrolysis, 99, 1 (2013).
  5. S.-S. Choi and H.-M. Kwon, "Analytical method for determination of microstructures of solution styrene-butadiene copolymers using 2-phenylpropene/styrene ratio of pyrolysis products", Polym. Test, 44, 153 (2015).
  6. S.-S. Choi, Y. Kim, and H.-M. Kwon, "Microstructural analysis and cis-trans isomerization of BR and SBR vulcanizates reinforced with silica and carbon black using NMR and IR", RSC Adv., 4, 31113 (2014).
  7. S.-S. Choi, Y. Kim, and H.-M. Kwon, "Analytical considerations for determination of the microstructures of sulfur-cured solution styrene-butadiene rubbers", Polym. Int., 66, 803 (2017).
  8. N. J. Morrison and M. Porter, "Temperature effects on the stability of intermediates and crosslinks in sulfur vulcanization", Rubber Chem. Technol., 57, 63 (1984).
  9. S.-S. Choi and G. Cho, "Influence of 1,2-unit contents on retraction behaviors of SBR vulcanizates", J. Appl. Polym. Sci., 102, 4707 (2006).
  10. S.-S. Choi and J.-C. Kim, "Thermal aging behaviors of weather resistant rubber composites of EPDM, IIR, and BIIR", Elast. Comp., 47, 148 (2012).
  11. S.-S. Choi and J.-C. Kim, "Influence of the 1,2-unit content of SBR and filler systems on thermal aging behaviors of SBR composites", J. Ind. Eng. Chem, 13, 950 (2007).
  12. Y. Kim and S.-S. Choi, "Microstructural analysis of SBR blends using infrared spectroscopy", Elast. Comp., 49, 103 (2014).
  13. X. Liu, S. Zhao, X. Zhang, X. Li, and Y. Bai, "Preparation, structure, and properties of solution-polymerized styrene-butadiene rubber with functionalized end-groups and its silica-filled composites", Polymer, 55, 1964 (2014).
  14. J. Zhang, H. Chen, Y. Zhou, C. Ke, and H. Lu, "Compatibility of waste rubber powder/polystyrene blends by the addition of styrene grafted styrene butadiene rubber copolymer: effect on morphology and properties", Polym. Bull., 70, 2829 (2013).
  15. C. B. B. Luna, E. M. Araujo, D. D. Siqueira, D. D. S. Morais, E. A. S. Filho, and M. V. L. Fook, "Incorporation of a recycled rubber compound from the shoe industry in polystyrene: effect of SBS compatibilizer content", J. Elastomers Plast., 52, 3 (2019).
  16. K.-H. Kim, J.-Y. Lee, J.-M. Choi, H.-J. Kim, B. Seo, B.-S. Kim, G.-H. Kwag, H.-J. Paik, and W. Kim, "Synthesis of ionic elastomers based on styrene-butadiene rubber containing methacrylic acid", Elast. Compos., 48, 46 (2013).
  17. S. Khoee and M. Sorkhi, "Microstructure analysis of brominated styrene-butadiene rubber", Polym. E ng. Sci., 47, 87 (2007).
  18. 권혁민, "SBR 열분해 생성물의 특성 연구", 세종대학교 석사학위논문, 2014.
  19. S. R. Shield, G. N. Ghebremeskel, and C. Hendrix, "Pyrolysis-GC/MS and TGA as tools for characterizing blends of SBR and NBR", Rubber Chem. Technol., 74, 803 (2001).
  20. R. P. Lattimer, K. M. Schur, W. Windig, and H. L. C. Meuzelaar, "Quantitative analysis of rubber triblends by pyrolysis-mass spectrometry", J. Anal. Appl. Pyrolysis, 8, 95 (1985).
  21. E. Grieco, M. Bernardi, and G. Baldi, "Styrene-butadiene rubber pyrolysis: products, kinetics, modelling", J. Anal. Appl. Pyrolysis, 82, 304 (2008).
  22. S.-S. Choi and H.-M. Kwon, "Considering factors on determination of microstructures of SBR vulcanizates using pyrolytic analysis", Polym. Test., 89, 106572 (2020).
  23. S. C. Moldoveanu, "Analytical pyrolysis of natural organic polymers", 1st ed., p.26, Elsevier, Amsterdam, 1998.
  24. C. Watanabe, K. Sato, A. Hosaka, H. Ohtani, and S. Tsuge, "Development of a multifunctional pyrolyzer for evolved gas analysis, thermal desorption, and/or pyrolysis-GC of polymeric materials", Am. Lab., 33, 14 (2001).
  25. Y. Pico and D. Barcelo, "Pyrolysis gas chromatography-mass spectrometry in environmental analysis: focus on organic matter and microplastics", Trends Anal. Chem., 130, 115964 (2020).
  26. K. L. Sobeih, M. Baron, and J. Gonzalez-Rodriguez, "Recent trends and developments in pyrolysis-gas chromatography", J. Chromatogr. A, 1186, 51 (2008).
  27. A. Lourenco, "The influence of heartwood on kraft delignification of Eucalyptus globulus wood", PhD Thesis, Universidade Tecnica de Lisboa, 2012.
  28. N. W. Bower and C. J. K. Blanchet, "Analytical pyrolysis-chromatography: something old, something new", J. Chem. Educ., 87, 467 (2010).
  29. M. R. Grimbley, R. S. Lehrle, R. J. Williams, and D. M. Bate, "An enclosed Curie point pyrolysis-GC technique for studying the oxidative or thermal degradation of polymers and volatile oligomeric oils", Polym. Degrad. Stab., 48, 143 (1995).
  30. C. Peres, C. Viallon, and J.-L. Berdague, "Curie point pyrolysis-mass spectrometry applied to rapid characterization of cheeses", J. Anal. Appl. Pyrolysis, 65, 161 (2002).
  31. K. Kuroda and D. R. Dimmel, "Effect of pyrofoil composition on pyrolysis of lignin", J. Anal. Appl. Pyrolysis, 62, 259 (2002).
  32. S. Buco, M. Moragues, P. Doumenq, A. Noor, and G. Mille, "Analysis of polycyclic aromatic hydrocarbons in contaminated soil by Curie point pyrolysis coupled to gas chromatography-mass spectrometry, an alternative to conventional methods", J. Chromatogr. A, 1026, 223 (2004).
  33. T. S. Radhakrishnan and M. Ramarao, "Thermal decomposition of polybutadienes by pyrolysis gas chromatography", J. Polym. Sci. Polym. Chem. Ed., 19, 3197 (1981).
  34. J. Hacaloglu, T. Ersen, N. Ertugrul, M. M. Fares, and S. Suzer, "Pyrolysis mass spectrometric analysis of styrene-butadiene block and random copolymers", Eur. Polym. J., 33, 199 (1997).
  35. S.-S. Choi, "Characteristics of pyrolysis patterns of polybutadienes with different microstructures", J. Anal. Appl. Pyrolysis, 57, 249 (2001).
  36. M. Guaita, "Thermal degradation of polystyrene", Br. Polym. J., 18, 226 (1986).
  37. Y. S. Lee, W.-K. Lee, S.-G. Cho, I. Kim, and C.-S. Ha, "Quantitative analysis of unknown compositions in ternary polymer blends: a model study on NR/SBR/BR system", J. Anal. Appl. Pyrolysis, 78, 85 (2007).
  38. Z. Yang, G. Fan, Y. Ma, C. Gong, and H. Xu, "A novel quantitative method for analyzing binary rubber blends with characteristics ion by pyrolysis/GC/MS", Am. Lab., 40, 24 (2008).
  39. G. R. Cotten and L. J. Murphy, "Mixing of carbon black with rubber. VI. Analysis of NR/SBR blends", Rubber Chem. Technol., 61, 609 (1988).
  40. D. S. Huh, J. S. Kim, K. J. Kim, B. K. Ahn, S. K. Suh, and O. K. Han, "Study on analysis of vulcanized rubber by pyrolysis-gas chromatography (I) (vulcanizates of NR, BR, and SBR)", J. Korea Ins. Rubber Ind., 22, 11 (1987).
  41. A. Krishen and R. G. Tucker, "Quantitative determination of the polymeric constituents in compounded cured stocks by Curie-point pyrolysis-gas chromatography", Anal. Chem., 46, 29 (1974).
  42. E. Chae and S.-S. Choi, "Building calibration curve for PyGC/MS analysis of SBR/BR blend rubber compounds", Elast. Compos., 55, 281 (2020).