압력용기 클래드 보수용 전해니켈도금 인자 관계 연구

Variables of Electrolytic Nickel Plating for RPV Cladding Repair

  • 김민수 (한국원자력연구원, 안전재료기술개발부) ;
  • 황성식 (한국원자력연구원, 안전재료기술개발부) ;
  • 김동진 (한국원자력연구원, 안전재료기술개발부) ;
  • 이동복 (성균관대학교 신소재공학과)
  • 투고 : 2019.08.07
  • 심사 : 2019.08.27
  • 발행 : 2019.08.30

초록

Pure nickel with a thickness of 1 mm was plated on type 304 stainless steels and low alloy steels (JIS G3131 SPHC) by electrolytic plating method in a circulating plating bath. Plating performance, mechanical properties, and surface characteristics were evaluated in terms of pretreatment process, anode material, pH, current density, and flow rate of the plating solution. Addition of hydrochloric acid during pre-treatment process improved the adhesion performance of plating. To improve plating efficiency, it is desirable to use S-nickel rather than electrolytic nickel. The use of S-nickel was also confirmed to be desirable for maintaining the pH and concentration of the plated solution. The defect of the plating using S-nickel anode produced pit on the surface. However, it is believed that proper control can be obtained by increasing the flow rate. Internal stress and hardness values of electrolytic nickel plating according to current density need to be carried out with further studies.

키워드

참고문헌

  1. M.-J. Kim, D. J. Kim, J. S. Kim, H. P. Kim, and S. S. Hwang, Proc. 2013 ASME Pressure Vessels and Piping Division Conf., PVP2013-97857 (2013).
  2. D. -J. Kim, M. J. Kim, J. S. Kim, and H. P. Kim, Surf. Coat. Technol., 202, 2519 (2008). https://doi.org/10.1016/j.surfcoat.2007.09.027
  3. ASME Code Case N-840, 2013 ASME boiler and pressure vessel code (2013).
  4. KAERI report, CR-271, Process technology development of Ni electroplating in steam generator tube (2006).
  5. ASME BPVC-IX-2013, Qualification standard for welding, brazing, and fusing procedures, welders; brazers; and welding, brazing, and fusing operators, ASME International (2013).