Effects of different surface treatments on the shear bond strength of veneering ceramic materials to zirconia

  • Abdullah, Adil Othman (School and Hospital of Stomatology, China Medical University) ;
  • Hui, Yu (School of Environmental and Chemical Engineering, Dalian University) ;
  • Sun, Xudong (School of Environmental and Chemical Engineering, Dalian University) ;
  • Pollington, Sarah (School of Clinical Dentistry, the University of Sheffield) ;
  • Muhammed, Fenik Kaml (School and Hospital of Stomatology, China Medical University) ;
  • Liu, Yi (School and Hospital of Stomatology, China Medical University)
  • Received : 2018.08.24
  • Accepted : 2019.02.15
  • Published : 2019.02.28

Abstract

PURPOSE. To evaluate and compare the effect of different materials and techniques on the shear bond strength of veneering ceramic materials to zirconia. MATERIALS AND METHODS. 136 sintered zirconia cubes were prepared and randomly divided into four study groups according to corresponding methods of surface treatment and materials: GLN (grinding followed by laser scanning using Noritake Cerabien ZR), SLN (sandblasting followed by laser scanning using Noritake Cerabien ZR), GLV (grinding followed by laser scanning using VITA VM 9), and SLV (sandblasting followed by laser scanning using VITA VM 9). Spraying technique was performed to coat the core. Profilometer, SEM, XRD, EDS, universal testing machine, and stereomicroscope were used to record surface roughness Ra, surface morphology, phase transformation, elemental compositions, shear bond strength SBS values, and failure types, respectively. Specimens were investigated in unaged (not immersed in artificial saliva) and aged (stored in artificial saliva for a month) conditions to evaluate SBS values. RESULTS. Grinding and GLN as first and second surface treatments provided satisfactory Ra values in both conditions ($1.05{\pm}0.24{\mu}m$, $1.30{\pm}0.21{\mu}m$) compared to sandblasting and other groups (P<.05). The group GLN showed the highest SBS values in both conditions ($30.97{\pm}3.12MPa$, $29.09{\pm}4.17MPa$), while group SLV recorded the lowest ($23.96{\pm}3.60MPa$, $22.95{\pm}3.68Mpa$) (P<.05). Sandblasting showed phase transformation from t-m. Mixed failure type was the commonest among all groups. CONCLUSION. GLN showed to be a reliable method which provided satisfactory bond strength between the veneer ceramic and zirconia. This method might preserve the integrity of fixed dental crowns.

Keywords

References

  1. Her SB, Kim KH, Park SE, Park EJ. The effect of zirconia surface architecturing technique on the zirconia/veneer interfacial bond strength. J Adv Prosthodont. 2018;10:259-64. https://doi.org/10.4047/jap.2018.10.4.259
  2. Gehrke P, Tabellion A, Fischer C. Microscopical and chemical surface characterization of CAD/CAM zircona abutments after different cleaning procedures. A qualitative analysis. J Adv Prosthodont 2015;7:151-9. https://doi.org/10.4047/jap.2015.7.2.151
  3. Eisenmenger-Sittner C, Nobauer C, Mozetic M, Kovac J, Zaplotnik R. Stabilization of tetragonal ZrO2 by oxygen plasma treatment of sputtered ZrCu and ZrAl thin films. Surf Coat Technol 2018;347:270-7. https://doi.org/10.1016/j.surfcoat.2018.04.061
  4. Ural C, Kulunk T, Kulunk S, Kurt M. The effect of laser treatment on bonding between zirconia ceramic surface and resin cement. Acta Odontol Scand 2010;68:354-9. https://doi.org/10.3109/00016357.2010.514720
  5. Mosharraf R, Rismanchian M, Savabi O, Ashtiani AH. Influence of surface modification techniques on shear bond strength between different zirconia cores and veneering ceramics. J Adv Prosthodont 2011;3:221-8. https://doi.org/10.4047/jap.2011.3.4.221
  6. Abd El-Ghany OS, Sherief AH. Zirconia based ceramics, some clinical and biological aspects: Review. Future Dent J 2016;2:55-64. https://doi.org/10.1016/j.fdj.2016.10.002
  7. Yamaguchi H, Ino S, Hamano N, Okada S, Teranaka T. Examination of bond strength and mechanical properties of Y-TZP zirconia ceramics with different surface modifications. Dent Mater J 2012;31:472-80. https://doi.org/10.4012/dmj.2011-237
  8. Tarib NA, Anuar N, Ahmad M. Shear bond strength of veneering ceramic to coping materials with different pre-surface treatments. J Adv Prosthodont 2016;8:339-44. https://doi.org/10.4047/jap.2016.8.5.339
  9. Cho JH, Kim SJ, Shim JS, Lee KW. Effect of zirconia surface treatment using nitric acid-hydrofluoric acid on the shear bond strengths of resin cements. J Adv Prosthodont 2017;9: 77-84. https://doi.org/10.4047/jap.2017.9.2.77
  10. Khayat W, Chebib N, Finkelman M, Khayat S, Ali A. Effect of grinding and polishing on roughness and strength of zirconia. J Prosthet Dent 2018;119:626-31. https://doi.org/10.1016/j.prosdent.2017.04.003
  11. Miyazaki T, Nakamura T, Matsumura H, Ban S, Kobayashi T. Current status of zirconia restoration. J Prosthodont Res 2013;57:236-61. https://doi.org/10.1016/j.jpor.2013.09.001
  12. de Lima E, Meira J, Ozcan M, Cesar P. Chipping of veneering ceramics in zirconium dioxide fixed dental prosthesis. Curr Oral Health Rep 2015;2:169-73. https://doi.org/10.1007/s40496-015-0066-7
  13. Marefati MT, Hadian AM, Hooshmand T, Yekta BE, Koohkan R. Wettability of zirconia by feldspathic veneer in dental restorations: Effect of firing atmosphere and surface roughness. Ceram Int 2018;44:4307-12. https://doi.org/10.1016/j.ceramint.2017.12.020
  14. Koenig V, Vanheusden AJ, Le Goff SO, Mainjot AK. Clinical risk factors related to failures with zirconia-based restorations: an up to 9-year retrospective study. J Dent 2013;41:1164-74. https://doi.org/10.1016/j.jdent.2013.10.009
  15. Agustin-Panadero R, Roman-Rodriguez JL, Ferreiroa A, Sola-Ruiz MF, Fons-Font A. Zirconia in fixed prosthesis. A literature review. J Clin Exp Dent 2014;6:e66-73.
  16. Soon G, Pingguan-Murphy B, Lai KW, Akbar SA. Review of zirconia-based bioceramic: Surface modification and cellular response. Ceram Int 2016;42:12543-55. https://doi.org/10.1016/j.ceramint.2016.05.077
  17. Kasraei S, Atefat M, Beheshti M, Safavi N, Mojtahedi M, Rezaei-Soufi L. Effect of surface treatment with carbon dioxide (CO2) laser on bond strength between cement resin and zirconia. J Lasers Med Sci 2014;5:115-20.
  18. Shukla PP, Lawrence J. Evaluation of fracture toughness of ZrO2 and Si3N4 engineering ceramics following CO2 and fibre laser surface treatment. Opt Lasers Eng 2011;49:229-39. https://doi.org/10.1016/j.optlaseng.2010.09.010
  19. Mirhashemi A, Sharifi N, Moharrami M, Chiniforush N. Evaluation of different types of lasers in surface conditioning of porcelains: A review article. J Lasers Med Sci 2017;8:101-11. https://doi.org/10.15171/jlms.2017.19
  20. ISO 4288. Geometrical Product Specifications (GPS)-Surface Texture: Profile method-Rules and procedures for the assessment of surface texture. International Standards Organization (ISO); Geneva; Switzerland, 1996.
  21. Kirmali O, Akin H, Ozdemir AK. Shear bond strength of veneering ceramic to zirconia core after different surface treatments. Photomed Laser Surg 2013;31:261-8. https://doi.org/10.1089/pho.2013.3487
  22. Wang G, Zhang S, Bian C, Kong H. Effect of zirconia surface treatment on zirconia/veneer interfacial toughness evaluated by fracture mechanics method. J Dent 2014;42:808-15. https://doi.org/10.1016/j.jdent.2014.04.005
  23. Yoon HI, Yeo IS, Yi YJ, Kim SH, Lee JB, Han JS. Effect of surface treatment and liner material on the adhesion between veneering ceramic and zirconia. J Mech Behav Biomed Mater 2014;40:369-74. https://doi.org/10.1016/j.jmbbm.2014.09.017
  24. Stubinger S, Homann F, Etter C, Miskiewicz M, Wieland M, Sader R. Effect of Er:YAG, CO(2) and diode laser irradiation on surface properties of zirconia endosseous dental implants. Lasers Surg Med 2008;40:223-8. https://doi.org/10.1002/lsm.20614
  25. Ural C, KalyoncuoGlu E, Balkaya V. The effect of different power outputs of carbon dioxide laser on bonding between zirconia ceramic surface and resin cement. Acta Odontol Scand 2012;70:541-6. https://doi.org/10.3109/00016357.2011.600718
  26. El-Shrkawy Z, El-Hosary M, Saleh O, Mandour M. Effect of different surface treatments on bond strength, surface and microscopic structure of zirconia ceramic. Future Dent J 2016;2:41-53. https://doi.org/10.1016/j.fdj.2016.04.005
  27. Muhammed F, Pollington S, Xudong S, Abdullah A, Liu Y. Novel coatings on zirconia for improved bonding with veneer ceramics. Coatings 2018;8:363. https://doi.org/10.3390/coatings8100363
  28. Farhan FA, Sulaiman E, Kutty MG. Effect of new zirconia surface coatings on the surface properties and bonding strength of veneering zirconia substrate. Surf Coat Technol 2018;333:247-58. https://doi.org/10.1016/j.surfcoat.2017.10.030
  29. Qeblawi DM, Munoz CA, Brewer JD, Monaco EA Jr. The effect of zirconia surface treatment on flexural strength and shear bond strength to a resin cement. J Prosthet Dent 2010; 103:210-20. https://doi.org/10.1016/S0022-3913(10)60033-9
  30. Sasse M, Kern M. CAD/CAM single retainer zirconia-ceramic resin-bonded fixed dental prostheses: clinical outcome after 5 years. Int J Comput Dent 2013;16:109-18.
  31. Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. Strength and reliability of surface treated Y-TZP dental ceramics. J Biomed Mater Res 2000;53:304-13. https://doi.org/10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S
  32. Monaco C, Tucci A, Esposito L, Scotti R. Microstructural changes produced by abrading Y-TZP in presintered and sintered conditions. J Dent 2013;41:121-6. https://doi.org/10.1016/j.jdent.2012.06.009
  33. Ryan DPO, Fais LMG, Antonio SG, Hatanaka GR, Candido LM, Pinelli LAP. Y-TZP zirconia regeneration firing: Microstructural and crystallographic changes after grinding. Dent Mater J 2017;36:447-53. https://doi.org/10.4012/dmj.2016-124
  34. Tada K, Sato T, Yoshinari M. Influence of surface treatment on bond strength of veneering ceramics fused to zirconia. Dent Mater J 2012;31:287-96. https://doi.org/10.4012/dmj.2011-163
  35. Kim JW, Covel NS, Guess PC, Rekow ED, Zhang Y. Concerns of hydrothermal degradation in CAD/CAM zirconia. J Dent Res 2010;89:91-5. https://doi.org/10.1177/0022034509354193
  36. Fischer J, Grohmann P, Stawarczyk B. Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites. Dent Mater J 2008;27:448-54. https://doi.org/10.4012/dmj.27.448
  37. Steiner PJ, Kelly JR, Giuseppetti AA. Compatibility of ceramic-ceramic systems for fixed prosthodontics. Int J Prosthodont 1997;10:375-80.

Cited by

  1. Comparative Effectiveness of Multiple Laser Scanning and Conventional Techniques on Zirconia Shear Bond Strength vol.9, pp.7, 2019, https://doi.org/10.3390/coatings9070422
  2. Effect of Low-Concentration Hydrofluoric Acid Etching on Shear Bond Strength and Biaxial Flexural Strength after Thermocycling vol.13, pp.6, 2019, https://doi.org/10.3390/ma13061409
  3. Does the glaze application on Y-TZP surface improve the bond strength to pressed veneering ceramic? vol.35, pp.13, 2021, https://doi.org/10.1080/01694243.2020.1846898