Fig. 1. Heattreatment curve of standard specimen & alloy A.
Fig. 2. Heattreatment curve of alloy B & C.
Fig. 3. Hardness of standard specimen after heattreat-ment .
Fig. 4. Hardness change of alloy A after heattreatment.
Fig. 5. Hardness change of standard specimen, alloy B & C after 2nd heattreatment.
Fig. 6. Hardness of standard specimen, alloy B & C after 2nd heattreatment.
Fig. 7. Electrical conductivity of standard specimen, alloy A, B & C after 2nd heattreatment.
Table 1. Compositions of A 6061
Table 2. Heattreatment condition
Table 3. Hardness of standard specimen & alloy A after heattreatment
Table 4. Hardness of standard specimen, alloy B & C after heattreatment (HV)
Table 5. Electrical conductivity of standard specimen, alloy A, B & C after 2nd heattreatment (dS/m)
References
- 이지혜, 이동근, 정현수: 한국소성가공학회지, 제16권, 제 5호 (2007), 2-3.
- 김한균, 첨단기술정보분석, "용체화 처리한 Al-Si-Mg계 합금의 2단 시효 거동", 2-4.
- 최중한, 김종기, 최현규, 한국재료학회지, 제 9권, 제 7호 (1999), 696.
- 박진한, 백귀찬, 김용욱, "알루미늄 합금(6063)의 최적 강도 증가를 위한 연구(급냉 및 시효경화 열처리에 관한 연구)".
- 우기도, 한국과학재단 (1999), 12-16.
- 최중한, 김종기, 최현규, 한국재료학회지, 제 9권, 제 7호 (1999), 698-699.