Abstract

The rod-shaped $Ni_{0.5}Zn_{0.5}Fe_2O_4$ particles were synthesized via a topotactic reaction, in which goethite (${\alpha}-FeOOH$) particles are the main constituents. The phases, microstructures and magnetic properties of these particles were studied using XRD, FE-SEM and VSM. The precursor solution consisted of $NiSO_4{\cdot}xH_2O$, $ZnSO_4{\cdot}xH_2O$, goethite and D.I. water werereacted at four different temperatures (50, 70, 90, $100^{\circ}C$) to generate four differently precipitated particles respectively. During the co-precipitation reaction, the pH of the solution was maintained at 8.0 using NaOH. The particles co-precipitated and calcined at a temperature of $700^{\circ}C$, exhibited a rod-shape similar to its original goethite, which means that the shape of Ni-Zn ferrite particles can be topotactically controlled by the goethite. The particles synthesized at 70 and $90^{\circ}C$ have a saturation magnetization of 29 and 35 emu/g respectively; representing better values than the ones synthesized at the 50 and $100^{\circ}C$, in which some second phases such as $Fe_2O_3$ were observed.

Keywords

References

  1. G. R. Amiri, M. H. Yousefi, M. R. Abolhassani, S. Manouchehri, M. H. Keshavarz, and S. Fatahian, J. Magn. Magn. Mater., 323, 730 (2011). [DOI: https://doi.org/10.1016/ j.jmmm.2010.10.034]
  2. Y. Liu, J. J. Li, F. F. Min, J. B. Zhu, and M. X. Zhang, J. Magn. Magn. Mater., 354, 295 (2014). [DOI: https://doi.org/10.1016/j.jmmm.2013.11.005]
  3. N. Gupta, A. Verma, S. C. Kashyap, and D. C. Dube, J. Magn. Magn. Mater., 308, 137 (2007). [DOI: https://doi.org/10.1016/j.jmmm.2006.05.015]
  4. K.V.P.M. Shafi, Y. Koltypin, A. Gedanken, R. Prozorov, J. Balogh, J. Lendvai, and I. Felner, J. Phys. Chem. B, 101, 6409 (1997). [DOI: https://doi.org/10.1021/jp970893q]
  5. S. Prasad and N. S. Gajbhiye, J. Alloys Compd., 265, 87 (1998). [DOI: https://doi.org/10.1016/S0925-8388(97)00431-3]
  6. J. M. Yang, W. J. Tsuo, and F. S. Yen, J. Solid State Chem., 145, 50 (1999). [DOI: https://doi.org/10.1006/jssc.1999.8215]
  7. Y. Shi, J. Ding, X. Liu, and J. Wang, J. Magn. Magn. Mater., 205, 249 (1999). [DOI: https://doi.org/10.1016/S0304-8853(99) 00504-1]
  8. T. F. Marinca, I. Chicinas, O. Isnard, V. Pop, and F. Popa, J. Alloys Compd., 509, 7931 (2011). [DOI: https://doi.org/10.1016/j.jallcom.2011.05.040]
  9. D. H. Chen and X. R. He, Mater. Res. Bull., 36, 1369 (2001). [DOI: https://doi.org/10.1016/S0025-5408(01)00620-1]
  10. H. Kavas, N. Kasapoglu, A. Baykal, and Y. Koseoglu, Chem. Pap., 63, 450 (2009). [DOI: https://doi.org/10.2478/ s11696-009-0034-6]
  11. D. P. Volanti, D. Keyson, L. S. Cavalcante, A. Z. Simoes, M. R. Joya, E. Longo, J. A. Varela, P. S. Pizani, and A. G. Souza, J. Alloy. Compd., 459, 537 (2008). [DOI: https:// doi.org/10.1016/j.jallcom.2007.05.023]
  12. H. Harzali, F. Saida, A. Marzouki, A. Megriche, F. Baillon, F. Espitalier, and A. Mgaidi, J. Magn. Magn. Mater., 419, 50 (2016). [DOI: https://doi.org/10.1016/j.jmmm.2016.05.084]
  13. A. M. El-Sayed, Mater. Chem. Phys., 82, 583 (2003). [DOI: https://doi.org/10.1016/S0254-0584(03)00319-5]
  14. C. Srinivas, B. V. Tirupanyam, S. S. Meena, S. M. Yusuf, C. Seshu Babu, K. S. Ramakrishna, D. M. Potukuchi, and D. L. Sastry, J. Magn. Magn. Mater., 407, 135 (2016). [DOI: https://doi.org/10.1016/j.jmmm.2016.01.060]
  15. A. T. Raghavender, N. Biliskov, and Z. Skoko, Mater. Lett., 65, 677 (2011). [DOI: https://doi.org/10.1016/j.matlet.2010.11.071]
  16. A. P. Kazin, M. N. Rumyantseva, V. E. Prusakov, I. P. Suzdalev, and A. M. Gaskov, J. Solid State Chem., 184, 2799 (2011). [DOI: https://doi.org/10.1016/j.jssc.2011.08.029]
  17. V. C. Gopalratnam, G. F. Bennett, and R. W. Peters, J. Environ. Eng., 118, 923 (1992). [DOI: https://doi.org/10.1061/ (ASCE)0733-9372(1992)118:6(923)]
  18. K. Velmurugan, V.S.K. Venkatachalapathy, and S. Sendhil nathan, Mater. Res., 13, 299 (2010). [DOI: https://doi.org/10.1590/S1516-14392010000300005]
  19. C. Srinivas, B. V. Tirupanyam, A. Satish, V. Seshubai, D. L. Sastry, and O. F. Caltun, J. Magn. Magn. Mater., 382, 15 (2015). [DOI: https://doi.org/10.1016/j.jmmm.2015.01.008]
  20. R. Masrour, H. El Moussaoui, E. Salmani, O. Mounkachi, H. Ez-Zahraouy, M. Hamedoun, E. K. Hlil, and A. Benyoussef, J. Supercond. Novel Magn., 27, 177 (2014). [DOI: https:// doi.org/10.1007/s10948-013-2234-0]
  21. A. Goldman, Modern Ferrite Technology, 2nd ed. (Springer, Pittsburgh, 2006) p. 58.
  22. T. Slatineanu, A. R. Iordan, M. N. Palamaru, O. F. Caltun, V. Gafton, and L. Leontie, Mater. Res. Bull., 46, 1455 (2011). [DOI: https://doi.org/10.1016/j.materresbull.2011.05.002]