The effect of thermocycling on the degree of conversion and mechanical properties of a microhybrid dental resin composite

  • Ghavami-Lahiji, Mehrsima (Department of Dental Biomaterials, School of Dentistry, Tehran University of Medical Sciences) ;
  • Firouzmanesh, Melika (Department of Dental Biomaterials, School of Dentistry, Tehran University of Medical Sciences) ;
  • Bagheri, Hossein (Dental Materials Research Center, School of Dentistry, Mashhad University of Medical Sciences) ;
  • Jafarzadeh Kashi, Tahereh S. (Department of Dental Biomaterials, School of Dentistry, Tehran University of Medical Sciences) ;
  • Razazpour, Fateme (Department of Dental Biomaterials, School of Dentistry, Tehran University of Medical Sciences) ;
  • Behroozibakhsh, Marjan (Department of Dental Biomaterials, School of Dentistry, Tehran University of Medical Sciences)
  • 투고 : 2017.12.11
  • 심사 : 2018.03.19
  • 발행 : 2018.05.31

초록

Objective: The purpose of this study was to investigate the degree of conversion (DC) and mechanical properties of a microhybrid Filtek Z250 (3M ESPE) resin composite after aging. Method: The specimens were fabricated using circular molds to investigate Vickers microhardness (Vickers hardness number [VHN]) and DC, and were prepared according to ISO 4049 for flexural strength testing. The initial DC (%) of discs was recorded using attenuated total reflectance-Fourier transforming infrared spectroscopy. The initial VHN of the specimens was measured using a microhardness tester under a load of 300 g for 15 seconds and the flexural strength test was carried out with a universal testing machine (crosshead speed, 0.5 mm/min). The specimens were then subjected to thermocycling in $5^{\circ}C$ and $55^{\circ}C$ water baths. Properties were assessed after 1,000-10,000 cycles of thermocycling. The surfaces were evaluated using scanning electron microscopy (SEM). Data were analyzed using 1-way analysis of variance followed by the Tukey honest significant difference post hoc test. Results: Statistical analysis showed that DC tended to increase up to 4,000 cycles, with no significant changes. VHN and flexural strength values significantly decreased upon thermal cycling when compared to baseline (p < 0.05). However, there was no significant difference between initial and post-thermocycling VHN results at 1,000 cycles. SEM images after aging showed deteriorative changes in the resin composite surfaces. Conclusions: The Z250 microhybrid resin composite showed reduced surface microhardness and flexural strength and increased DC after thermocycling.

키워드

참고문헌

  1. Anusavice KJ, Phillips RW, Shen C, Rawls HR. Phillips' science of dental materials. 12th ed. St. Louis, Mo: Elsevier/Saunders; 2013.
  2. Souza RO, Ozcan M, Michida SM, de Melo RM, Pavanelli CA, Bottino MA, Soares LE, Martin AA. Conversion degree of indirect resin composites and effect of thermocycling on their physical properties. J Prosthodont 2010;19:218-225. https://doi.org/10.1111/j.1532-849X.2009.00551.x
  3. Martos J, Osinaga PW, Oliveira E, Castro LA. Hydrolytic degradation of composite resins: effects on the microhardness. Mater Res 2003;6:599-604. https://doi.org/10.1590/S1516-14392003000400029
  4. Toledano M, Osorio R, Osorio E, Fuentes V, Prati C, Garcia-Godoy F. Sorption and solubility of resin-based restorative dental materials. J Dent 2003;31:43-50. https://doi.org/10.1016/S0300-5712(02)00083-0
  5. Ozcan M, Corazza PH, Marocho SM, Barbosa SH, Bottino MA. Repair bond strength of microhybrid, nanohybrid and nanofilled resin composites: effect of substrate resin type, surface conditioning and ageing. Clin Oral Investig 2013;17:1751-1758. https://doi.org/10.1007/s00784-012-0863-5
  6. Chung SM, Yap AU, Chandra SP, Lim CT. Flexural strength of dental composite restoratives: comparison of biaxial and three-point bending test. J Biomed Mater Res B Appl Biomater 2004;71:278-283.
  7. Obici AC, Sinhoreti MA, Frollini E, Sobrinho LC, Consani S. Degree of conversion of Z250 composite determined by fourier transform infrared spectroscopy: comparison of techniques, storage periods and photo-activation methods. Mater Res 2004;7:605-610. https://doi.org/10.1590/S1516-14392004000400014
  8. Tonetto MR, Pinto SC, Rastelli Ade N, Borges AH, Saad JR, Pedro FL, de Andrade MF, Bandeca MC. Degree of conversion of polymer-matrix composite assessed by FTIR analysis. J Contemp Dent Pract 2013;14:76-79.
  9. Jafarzadeh TS, Erfan M, Behroozibakhsh M, Fatemi M, Masaeli R, Rezaei Y, Bagheri H, Erfan Y. Evaluation of polymerization efficacy in composite resins via FT-IR spectroscopy and vickers microhardness test. J Dent Res Dent Clin Dent Prospects 2015;9:226-232. https://doi.org/10.15171/joddd.2015.041
  10. Goncalves L, Filho JD, Guimaraes JG, Poskus LT, Silva EM. Solubility, salivary sorption and degree of conversion of dimethacrylate-based polymeric matrixes. J Biomed Mater Res B Appl Biomater 2008;85:320-325.
  11. Tosun G, Ozturk N, Sener Y, Gunduz B. Effect of light curing units and storage time on the degree of conversion of fissure sealants. Rev Clin Pesqui Odontol 2009;5:111-119.
  12. Pallikari F, Iosifidou S. A study of aging in dental composites using IR and Raman spectroscopy. e-Polymers 2004;4:793-802.
  13. Moraes LG, Rocha RS, Menegazzo LM, de Araujo EB, Yukimito K, Moraes JC. Infrared spectroscopy: a tool for determination of the degree of conversion in dental composites. J Appl Oral Sci 2008;16:145-149. https://doi.org/10.1590/S1678-77572008000200012
  14. McCabe JF, Walls AW. Applied dental materials. Hoboken, NJ: John Wiley & Sons; 2013.
  15. de Oliveira JC, Aiello G, Mendes B, Urban VM, Campanha NH, Jorge JH. Effect of storage in water and thermocycling on hardness and roughness of resin materials for temporary restorations. Mater Res 2010;13:355-359. https://doi.org/10.1590/S1516-14392010000300013
  16. International Organization for Standardization. ISO/TS 11405 Dentistry -- Testing of adhesion to tooth structure. 3rd ed. Geneva: International Organization for Standardization; 2015.
  17. Gale MS, Darvell BW. Thermal cycling procedures for laboratory testing of dental restorations. J Dent 1999;27:89-99. https://doi.org/10.1016/S0300-5712(98)00037-2
  18. Tabatabaei MH, Sadrai S, Bassir SH, Veisy N, Dehghan S. Effect of food stimulated liquids and thermocycling on the monomer elution from a nanofilled composite. Open Dent J 2013;7:62-67. https://doi.org/10.2174/1874210601307010062
  19. Sideridou ID, Achilias DS. Elution study of unreacted Bis-GMA, TEGDMA, UDMA, and Bis-EMA from light-cured dental resins and resin composites using HPLC. J Biomed Mater Res B Appl Biomater 2005;74:617-626.
  20. Durner J, Obermaier J, Draenert M, Ilie N. Correlation of the degree of conversion with the amount of elutable substances in nano-hybrid dental composites. Dent Mater 2012;28:1146-1153. https://doi.org/10.1016/j.dental.2012.08.006
  21. Andrzejewska E. Photopolymerization kinetics of multifunctional monomers. Prog Polym Sci 2001;26:605-665. https://doi.org/10.1016/S0079-6700(01)00004-1
  22. Leprince J, Lamblin G, Truffier-Boutry D, Demoustier-Champagne S, Devaux J, Mestdagh M, Leloup G. Kinetic study of free radicals trapped in dental resins stored in different environments. Acta Biomater 2009;5:2518-2524. https://doi.org/10.1016/j.actbio.2009.04.034
  23. Leprince JG, Lamblin G, Devaux J, Dewaele M, Mestdagh M, Palin WM, Gallez B, Leloup G. Irradiation modes' impact on radical entrapment in photoactive resins. J Dent Res 2010;89:1494-1498. https://doi.org/10.1177/0022034510384624
  24. Leprince JG, Palin WM, Hadis MA, Devaux J, Leloup G. Progress in dimethacrylate-based dental composite technology and curing efficiency. Dent Mater 2013;29:139-156. https://doi.org/10.1016/j.dental.2012.11.005
  25. Truffier-Boutry D, Demoustier-Champagne S, Devaux J, Biebuyck JJ, Mestdagh M, Larbanois P, Leloup G. A physico-chemical explanation of the post-polymerization shrinkage in dental resins. Dent Mater 2006;22:405-412. https://doi.org/10.1016/j.dental.2005.04.030
  26. International Organization for Standardization. ISO 4049 Dentistry -- Polymer-based restorative materials. 4th ed. Geneva: International Organization for Standardization; 2015.
  27. Attar N, Tam LE, McComb D. Flow, strength, stiffness and radiopacity of flowable resin composites. J Can Dent Assoc 2003;69:516-521.
  28. Janda R, Roulet JF, Latta M. The effects of thermocycling on the flexural strength and flexural modulus of modern resin-based filling materials. Dent Mater 2006;22:1103-1108. https://doi.org/10.1016/j.dental.2005.09.005
  29. de Moraes RR, Marimon JL, Schneider LF, Brandt WC, Correr Sobrinho L, Bueno M. Hydrolytic stability of dental composites: one-year aging effect on surface roughness and surface/subsurface hardness. Rev Odontol UNESP 2007;36:383-387.
  30. Pereira SM, Castilho AA, Salazar-Marocho SM, Oliveira KM, Vaquez VZ, Bottino MA. Thermocycling effect on microhardness of laboratory composite resins. Braz J Oral Sci 2007;6:1372-1375.
  31. Ferracane JL, Condon JR. Rate of elution of leachable components from composite. Dent Mater 1990;6:282-287. https://doi.org/10.1016/S0109-5641(05)80012-0
  32. Ferracane JL, Berge HX, Condon JR. In vitro aging of dental composites in water--effect of degree of conversion, filler volume, and filler/matrix coupling. J Biomed Mater Res 1998;42:465-472. https://doi.org/10.1002/(SICI)1097-4636(19981205)42:3<465::AID-JBM17>3.0.CO;2-F

피인용 문헌

  1. Effect of Thermocycling on Biaxial Flexural Strength of CAD/CAM, Bulk Fill, and Conventional Resin Composite Materials vol.44, pp.5, 2019, https://doi.org/10.2341/18-146-l
  2. Effect of Stress-decreasing Resin Thickness as an Intermediate Layer on Fracture Resistance of Class II Composite Restoration: An In Vitro Study vol.11, pp.2, 2018, https://doi.org/10.5005/jp-journals-10015-1712
  3. Ageing of Dental Composites Based on Methacrylate Resins—A Critical Review of the Causes and Method of Assessment vol.12, pp.4, 2018, https://doi.org/10.3390/polym12040882
  4. Effect of Different Surface Treatments of Resin Relined Fiber Posts Cemented With Self-adhesive Resin Cement on Push-out and Microtensile Bond Strength Tests vol.45, pp.4, 2018, https://doi.org/10.2341/19-108-l
  5. Evaluation of Immediate and Delayed Microleakage of Class V Cavities Restored with Chitosan-incorporated Composite Resins: An In Vitro Study vol.14, pp.5, 2018, https://doi.org/10.5005/jp-journals-10005-2043
  6. Impact of polymerization and storage on the degree of conversion and mechanical properties of veneering resin composites vol.40, pp.2, 2021, https://doi.org/10.4012/dmj.2019-394
  7. Fracture Load of CAD/CAM Fabricated Cantilever Implant-Supported Zirconia Framework: An In Vitro Study vol.26, pp.8, 2021, https://doi.org/10.3390/molecules26082259
  8. Intrapulpal Concentration of Hydrogen Peroxide of Teeth Restored With Bulk Fill and Conventional Bioactive Composites vol.46, pp.3, 2021, https://doi.org/10.2341/20-091-l
  9. The effect of radiation exposure and storage time on the degree of conversion and flexural strength of different resin composites vol.45, pp.1, 2018, https://doi.org/10.1186/s42269-021-00605-y