Effect of cover depth and rebar diameter on shrinkage behavior of ultra-high-performance fiber-reinforced concrete slabs

  • Yoo, Doo-Yeol (Department of Architectural Engineering, Hanyang University) ;
  • Kwon, Ki-Yeon (Structural Systems & Site Evaluation Department, Korea Institute of Nuclear Safety) ;
  • Yang, Jun-Mo (Steel Structure Research Group, POSCO) ;
  • Yoon, Young-Soo (School of Civil, Environmental and Architectural Engineering, Korea University)
  • Received : 2015.01.09
  • Accepted : 2016.11.15
  • Published : 2017.03.25

Abstract

This study investigates the effects of reinforcing bar diameter and cover depth on the shrinkage behavior of restrained ultra-high-performance fiber-reinforced concrete (UHPFRC) slabs. For this, twelve large-sized UHPFRC slabs with three different rebar diameters ($d_b=9.5$, 15.9, and 22.2 mm) and four different cover depths (h=5, 10, 20, and 30 mm) were fabricated. In addition, a large-sized UHPFRC slab without steel rebar was fabricated for evaluating degree of restraint. Test results revealed that the uses of steel rebar with a large diameter, leading to a larger reinforcement ratio, and a low cover depth are unfavorable regarding the restrained shrinkage performance of UHPFRC slabs, since a larger rebar diameter and a lower cover depth result in a higher degree of restraint. The shrinkage strain near the exposed surface was high because of water evaporation. However, below a depth of 18 mm, the shrinkage strain was seldom influenced by the cover depth; this was because of the very dense microstructure of UHPFRC. Finally, owing to their superior tensile strength, all UHPFRC slabs with steel rebars tested in this study showed no shrinkage cracks until 30 days.

Keywords

Acknowledgement

Supported by : National Research Foundation of Korea (NRF)

References

  1. AFGC (2013), Ultra high performance fibre-reinforced concretes. Interim Recommendations, AFGC Publication, France.
  2. Aïtcin, P.C. (1999), "Demystifying autogenous shrinkage", Concrete Int. 21(11), 54-56.
  3. American Society for Testing and Materials (ASTM) (2007), ASTM C 1437 Standard test method for flow of hydraulic cement mortar, Annual book of ASTM standards, ASTM, West Conshohocken, PA.
  4. American Society for Testing and Materials (ASTM) (2008), ASTM C 403 Standard test method for time of setting of concrete mixture by penetration resistance, Annual book of ASTM standards, ASTM, West Conshohocken, PA.
  5. American Society for Testing and Materials (ASTM) (2008), ASTM C 157/C 157M Standard test method for length change of hardened hydraulic-cement mortar and concrete, Annual book of ASTM standards, ASTM, West Conshohocken, PA.
  6. Chang-Wen, M., Qian, T., Wei, S. and Jia-Ping, L. (2007), "Water consumption of the early-age paste and the determination of "time-zero" of self-desiccation shrinkage", Cement Concrete Res., 37(11), 1496-1501. https://doi.org/10.1016/j.cemconres.2007.08.005
  7. Chen, H.L.R. and Choi, J.H. (2011), "Analysis of shrinkage and thermal stresses in concrete slabs reinforced with GFRP rebars", J. Mater. Civil Eng., 23(5), 612-627. https://doi.org/10.1061/(ASCE)MT.1943-5533.0000216
  8. Graybeal, B.A. (2008), "Flexural behavior of an ultrahighperformance concrete I-girder", J. Bridge Eng., 13(6), 602-610. https://doi.org/10.1061/(ASCE)1084-0702(2008)13:6(602)
  9. Habel, K., Charron, J.P., Denarie, E. and Bruhwiler, E. (2006), "Autogenous deformations and viscoelasticity of UHPFRC in structures. Part 1: Experimental results", Mag. Concr. Res., 58(3), 135-145. https://doi.org/10.1680/macr.2006.58.3.135
  10. Hossain, A.B. and Weiss, W.J. (2004), "Assessing residual stress development and stress relaxation in restrained concrete ring specimens", Cement Concrete Compos., 26(5), 531-540. https://doi.org/10.1016/S0958-9465(03)00069-6
  11. Japan Concrete Institute (JCI) (1999), Committee report, In: Tazawa E, editor, Autogenous shrinkage of concrete, E&FN Spon.
  12. Japan Society of Civil Engineers (JSCE) (2004), Recommendations for design and construction of ultra-high strength fiber reinforced concrete structures (Draft), Japan Society of Civil Engineers, Tokyo, Japan.
  13. Jiang, C., Yang, Y., Wang, Y., Zhou, Y. and Ma, C. (2014), "Autogenous shrinkage of high performance concrete containing mineral admixtures under different curing temperatures", Constr. Build. Mater., 61, 260-269. https://doi.org/10.1016/j.conbuildmat.2014.03.023
  14. Kamen, A., Denarie, E. and Bruhwiler, E. (2007), "Thermal effects on physico-mechanical properties of ultra-high-performance fiber-reinforced concrete", ACI Mater. J., 104(4), 415-423.
  15. Kim, Y.J., Park, S.Y., Park, J.S. and Kim, B.S. (2013), "State-ofthe-art of UHPC applications in the World", Korean Soc. of Civil Eng., 61(2), 39-50. (in Korean)
  16. Kobler, M. and Sobek, W. (2008), "The introduction of high forces into tine-walled UHPC elements by the use of implants", Proceedings of the Second International Symposium on Ultra High Performance Concrete, Kassel, Germany, 683-690.
  17. Park, J.J., Yoo, D.Y., Kim, S.W. and Yoon, Y.S. (2013), "Drying shrinkage cracking characteristics of ultra-high-performance fibre reinforced concrete with expansive and shrinkage reducing agents", Mag. Concrete Res., 65(4), 248-256. https://doi.org/10.1680/macr.12.00069
  18. Park, J.J., Yoo, D.Y., Kim, S.W. and Yoon, Y.S. (2014), "Benefits of using expansive and shrinkage reducing agents in ultra-highperformance concrete for volume stability", Mag. Concrete Res., 66(14), 745-750. https://doi.org/10.1680/macr.13.00317
  19. Perry, V. and Weiss, G. (2009), "Innovative field cast UHPC joints for precast bridge decks-Design, prototype testing and projects", Proceedings of the International Workshop on Ultra High Performance Fibre Reinforced Concrete, Designing and Building with UHPFRC: State of the Art Development, Marseille, France, AFGC/fib.
  20. Rajabipour, F., Sant, G. and Weiss, J. (2008), "Interactions between shrinkage reducing admixtures (SRA) and cement paste's pore solution", Cement Concrete Res., 38(5), 606-615. https://doi.org/10.1016/j.cemconres.2007.12.005
  21. Richard, P. and Cheyrezy, M. (1995), "Composition of reactive powder concretes", Cement Concrete Res., 25(7), 1501-1511. https://doi.org/10.1016/0008-8846(95)00144-2
  22. Saleem, M.A., Mirmiran, A., Xia, J. and Mackie, K. (2011), "Ultra-high-performance concrete bridge deck reinforced with high-strength steel", ACI Struct. J., 108(5), 601-609.
  23. Sant, G., Lothenbach, B., Juilland, P., Le Saout, G., Weiss, J. and Scrivener, K. (2011), "The origin of early age expansions induced in cementitious materials containing shrinkage reducing admixtures", Cement Concrete Res., 41(3), 218-229. https://doi.org/10.1016/j.cemconres.2010.12.004
  24. Yoo, D.Y., Banthia, N. and Yoon, Y.S. (2015), "Effectiveness of shrinkage-reducing admixture in reducing autogenous shrinkage stress of ultra-high-performance fiber-reinforced concrete", Cement Concrete Compos., 64, 27-36. https://doi.org/10.1016/j.cemconcomp.2015.09.005
  25. Yoo, D.Y., Park, J.J., Kim, S.W. and Yoon, Y.S. (2013), "Early age setting, shrinkage and tensile characteristics of ultra high performance fiber reinforced concrete", Const. Build. Mater., 41, 427-438. https://doi.org/10.1016/j.conbuildmat.2012.12.015
  26. Yoo, D.Y., Park, J.J., Kim, S.W. and Yoon, Y.S. (2014b), Influence of reinforcing bar type on autogenous shrinkage stress and bond behavior of ultra high performance fiber reinforced concrete," Cement Concrete Compos., 48, 150-161. https://doi.org/10.1016/j.cemconcomp.2013.11.014
  27. Yoo, D.Y., Park, J.J., Kim, S.W. and Yoon, Y.S. (2014c), "Combined effect of expansive and shrinkage-reducing admixtures on the properties of ultra high performance fiberreinforced concrete", J. Compos. Mater., 48(16), 1981-1991. https://doi.org/10.1177/0021998313493809
  28. Yoo, D.Y., Shin, H.O., Yang, J.M. and Yoon, Y.S. (2014a), "Material and bond properties of ultra high performance fiber reinforced concrete with micro steel fibers", Compos. Part B-Eng., 58, 122-133. https://doi.org/10.1016/j.compositesb.2013.10.081
  29. Yoo, D.Y., Yoon, Y.S. and Banthia, N. (2017), "Ultra-highperformance fiber-reinforced concrete: Shrinkage strain development at early ages and potential for cracking", J. Test. Eval., doi: http://dx.doi.org/10.1520/JTE20160114. (in Press)

Cited by

  1. Mitigating shrinkage cracking in posttensioning grout using shrinkage-reducing admixture vol.81, 2017, https://doi.org/10.1016/j.cemconcomp.2017.05.005
  2. Radial postbuckling of nanoscaled shells embedded in elastic foundations based on Ru's surface stress elasticity theory vol.47, pp.6, 2017, https://doi.org/10.1080/15397734.2019.1611447