Preparation and Characterization of Poly(vinyl alcohol) Hydrogel Contain Metronidazole by Irradiation

감마선을 이용한 Metronidazole이 함유된 Poly(vinyl alcohol) 하이드로겔 제조 및 특성

  • Baik, Jae (Advanced Radiation Technology Institute, Korea Atomic Energy Reserach Institute) ;
  • Park, Jong-Seok (Advanced Radiation Technology Institute, Korea Atomic Energy Reserach Institute) ;
  • Jong, Jin-Oh (Advanced Radiation Technology Institute, Korea Atomic Energy Reserach Institute) ;
  • Jeong, Sung In (Advanced Radiation Technology Institute, Korea Atomic Energy Reserach Institute) ;
  • Gwon, Hui-Jeong (Advanced Radiation Technology Institute, Korea Atomic Energy Reserach Institute) ;
  • Ahn, Sung-Jun (Advanced Radiation Technology Institute, Korea Atomic Energy Reserach Institute) ;
  • Lim, Youn-Mook (Advanced Radiation Technology Institute, Korea Atomic Energy Reserach Institute)
  • 백재 (한국원자력연구원 첨단방사선연구소 공업환경연구부) ;
  • 박종석 (한국원자력연구원 첨단방사선연구소 공업환경연구부) ;
  • 정진오 (한국원자력연구원 첨단방사선연구소 공업환경연구부) ;
  • 정성인 (한국원자력연구원 첨단방사선연구소 공업환경연구부) ;
  • 권희정 (한국원자력연구원 첨단방사선연구소 공업환경연구부) ;
  • 안성준 (한국원자력연구원 첨단방사선연구소 공업환경연구부) ;
  • 임윤묵 (한국원자력연구원 첨단방사선연구소 공업환경연구부)
  • Received : 2016.02.11
  • Accepted : 2016.03.15
  • Published : 2016.03.31

Abstract

Periodontitis is disease of damaged gum tissue that is not removed the plaque onto teeth. In case that the symptoms of disease get pain worse, it will have to extract tooth because of tumefy or bleeding at gums so treatment of drug was required to periodontitis. In this study, the hydrogel was prepared by including superior viscous, excellent elastic, and biocompatibility of Poly(vinyl alcohol, PVA) and antimicrobial drug of Metronidazole (MD). The 15 wt% PVA was dissolved in deionized water and then prepared PVA solution was irradiated using gamma-ray at 25 kGy ($10kGy\;hr^{-1}$). In addition, PVA hydrogel was immersed in each 0.1, 0.25 and 0.5 wt% MD solution using stirrer for 24 hr. The result of the gelation, 0.5 wt% MD loaded PVA hydrogel(76%) was lower than PVA hydrogel (88.2%). The swelling ration of 0.5 wt% MD loaded PVA hydrogel (294.8%) was higher than PVA hydrogel (105.2%). The compressive strength and thermal properties of MD loaded PVA hydrogel was gradually lower. The drug release test of 0.5 wt% MD loaded PVA hydrogel (61%) was higher than 0.1 wt% MD loaded PVA hydrogel (12%). Therefore, MD loaded PVA hygrogel may be a promising tool for periodontitis medicine by gamma-ray.